Defect Dynamics at a Single Pt Nanoparticle during Catalytic Oxidation

Defects can affect all aspects of a material by altering its electronic properties and controlling its chemical reactivity. At defect sites, preferential adsorption of reactants and/or formation of chemical species at active sites are observed in heterogeneous catalysis. Understanding the structural response at defect sites during catalytic reactions provides a unique opportunity to exploit defect control of nanoparticle-based catalysts. However, it remains difficult to characterize the strain and defect evolution for a single nanocrystal catalyst in situ. Here, we report Bragg coherent X-ray diffraction imaging of defect dynamics in an individual Pt nanoparticle during catalytic methane oxidation. We observed that the initially tensile strained regions of the crystal became seed points for the development of further strain and subsequent disappearance of diffraction density during oxidation reactions. Our team's detailed understanding of the catalytically induced deformation at the defect sites and observed reversibility during the relevant steps of the catalytic oxidation process provide important insights of defect control and engineering of heterogeneous catalysts.

36 MATERIALS SCIENCE↗

Understanding and reducing deleterious defects in the metastable alloy GaAsBi

Technological applications of novel metastable materials are frequently inhibited by abundant defects residing in these materials. Using first-principles methods, we investigate the defect thermodynamics and phase segregation in the technologically important metastable alloy GaAsBi. Our calculations predict defect energy levels in good agreement with those from numerous previous experiments and clarify the defect structures giving rise to these levels. We find that vacancies in some charge states become metastable or unstable with respect to antisite formation, and this instability is a general characteristic of zincblende semiconductors with small ionicity. The dominant point defects that degrade the electronic and optical performances are predicted to be As Ga , Bi Ga , As Ga +Bi As , Bi Ga +Bi As , V Ga and V Ga +Bi As , of which the first four and last two defects are minority-electron and minority-hole traps, respectively. V Ga is also observed to have a critical role in controlling metastable Bi supersaturation by mediating Bi diffusion and clustering. To reduce the influences of these deleterious defects, we suggest shifting the growth away from an As-rich condition and/or using hydrogen passivation to reduce the minority-carrier traps. In conclusion, we expect this work to aid in the applications of GaAsBi for novel electronic and optoelectronic devices and to illuminate the control of deleterious defects in other metastable materials.

36 MATERIALS SCIENCE↗

A substitutional quantum defect in WS2 discovered by high-throughput computational screening and fabricated by site-selective STM manipulation

Abstract Point defects in two-dimensional materials are of key interest for quantum information science. However, the parameter space of possible defects is immense, making the identification of high-performance quantum defects very challenging. Here, we perform high-throughput (HT) first-principles computational screening to search for promising quantum defects within WS 2 , which present localized levels in the band gap that can lead to bright optical transitions in the visible or telecom regime. Our computed database spans more than 700 charged defects formed through substitution on the tungsten or sulfur site. We found that sulfur substitutions enable the most promising quantum defects. We computationally identify the neutral cobalt substitution to sulfur ( $${\rm{Co}}_{{{{{{{{\rm{S}}}}}}}}}^{0}$$ Co S 0 ) and fabricate it with scanning tunneling microscopy (STM). The $${\rm{Co}}_{{{{{{{{\rm{S}}}}}}}}}^{0}$$ Co S 0 electronic structure measured by STM agrees with first principles and showcases an attractive quantum defect. Our work shows how HT computational screening and nanoscale synthesis routes can be combined to design promising quantum defects.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Predicting defect behavior in B2 intermetallics by merging ab initio modeling and machine learning

We present a combination of machine learning and high throughput calculations to predict the points defects behavior in binary intermetallic (A-B) compounds, using as an example systems with the cubic B2 crystal structure (with equiatomic AB stoichiometry). To the best of our knowledge, this work is the first application of machine learning-models for point defect properties. High throughput first principles density functional calculations have been employed to compute intrinsic point defect energies in 100 B2 intermetallic compounds. The systems are classified into two groups: (i) those for which the intrinsic defects are antisites for both A and B rich compositions, and (ii) those for which vacancies are the dominant defect for either or both composition ranges. The data was analyzed by machine learning-techniques using decision tree, and full and reduced multiple additive regression tree (MART) models. Among these three schemes, a reduced MART (r-MART) model using six descriptors (formation energy, minimum and difference of electron densities at the Wigner-Seitz cell boundary, atomic radius difference, maximal atomic number and maximal electronegativity) presents the highest fit (98 %) and predictive (75 %) accuracy. This model is used to predict the defect behavior of other B2 compounds, and it is found that 45 % of the compounds considered feature vacancies as dominant defects for either A or B rich compositions (or both). The ability to predict dominant defect types is important for the modeling of thermodynamic and kinetic properties of intermetallic compounds, and the present results illustrate how this information can be derived using modern tools combining high throughput calculations and data analytics.

97 MATHEMATICS AND COMPUTING↗

Small-Angle Twist Grain Boundaries as Sinks for Point Defects

It is known that grain boundaries (GBs) provide sinks for defects induced into a solid by irradiation. At the same time radiation can change the atomic structure and chemistry of GBs, which in turn impacts the ability of GBs to continue absorbing defects. Although a number of studies have been reported for tilt GBs acting as defect sinks, the questions of how twist GBs evolve to absorb non-equilibrium concentrations of defects and whether GBs saturate as defect sinks for typical irradiation conditions have remained largely unanswered. Here, we used a combination of molecular dynamics and grand canonical Monte Carlo simulations to determine how twist GBs accommodate point defects. We used SiC and {001} and {111} twist GBs as model systems. We found that diffusion of defects along GBs in this material is slow and for most experimentally relevant conditions point defects will accumulate at twist GBs, driving structural and chemical evolution of these interfaces. During irradiation, screw dislocations within GB planes absorb interstitials by developing mixed dislocation segments that climb. Formation of mixed dislocations occurs either by nucleation of interstitial loops or by faulting/unfaulting of stacking faults. Furthermore both types of twist GBs can accommodate a high density of interstitials without losing the crystalline structure, irrespectively of the interstitial flux.

36 MATERIALS SCIENCE↗

The relationship between grain boundary structure, defect mobility, and grain boundary sink efficiency

Nanocrystalline materials have received great attention due to their potential for improved functionality and have been proposed for extreme environments where the interfaces are expected to promote radiation tolerance. However, the precise role of the interfaces in modifying defect behavior is unclear. Using long-time simulations methods, we determine the mobility of defects and defect clusters at grain boundaries in Cu. We find that mobilities vary significantly with boundary structure and cluster size, with larger clusters exhibiting reduced mobility, and that interface sink efficiency depends on the kinetics of defects within the interface via the in-boundary annihilation rate of defects. Thus, sink efficiency is a strong function of defect mobility, which depends on boundary structure, a property that evolves with time. Further, defect mobility at boundaries can be slower than in the bulk, which has general implications for the properties of polycrystalline materials. Finally, we correlate defect energetics with the volumes of atomic sites at the boundary.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of extended strain fields on point defect phonon scattering in thermoelectric materials

The design of thermoelectric materials often involves the integration of point defects (alloying) as a route to reduce the lattice thermal conductivity. Classically, the point defect scattering strength follows from simple considerations such as mass contrast and the presence of induced strain fields (e.g. radius contrast, coordination changes). While the mass contrast can be easily calculated, the associated strain fields induced by defect chemistry are not readily predicted and are poorly understood. In this work, we use classical and first principles calculations to provide insight into the strain field component of phonon scattering from isoelectronic point defects. Our results also integrate experimental measurements on bulk samples of SnSe and associated alloys with S, Te, Ge, Sr and Ba. These efforts highlight that the strength and extent of the resulting strain field depends strongly on defect chemistry. Strain fields can have a profound impact on the local structure. For example, in alloys containing Ba, the strain fields have significant spatial extent (1 nm in diameter) and produce large shifts in the atomic equilibrium positions (up to 0.5 A). Such chemical complexity suggests that computational assessment of point defects for thermal conductivity depression should be hindered. However, in this work, we present and verify several computational descriptors that correlate well with the experimentally measured strain fields. Furthermore, these descriptors are conceptually transparent and computationally inexpensive, allowing computation to provide a pivotal role in the screening of effective alloys. The further development of point defect engineering could complement or replace nanostructuring when optimizing the thermal conductivity, offering the benefits of thermodynamic stability, and providing more clearly defined defect chemistry.

30 DIRECT ENERGY CONVERSION↗

Defect-Limited Carrier Lifetime in Epitaxially Strained Germanium-On-Silicon Heterostructures

Epitaxially strained germanium-on-silicon (Ge-on-Si) heterostructures are central to next-generation photonic and electronic devices, yet their performance remains strongly constrained by defect-limited carrier lifetimes. In this work, we investigate the impact of defects on the carrier lifetime in relaxed Ge-on-Si and strained Ge-on-Si heterostructures. High-resolution X-ray diffraction quantifies the strain-state in Ge and reveals signatures of strain relaxation due to lattice mismatch. Cross-sectional and plan-view transmission electron microscopy analyses enable direct visualization of interfacial defects and quantification of threading dislocation densities (TDDs) within the Ge layer. However, the presence of a dense misfit dislocation network obscures the threading dislocation signatures, preventing reliable TDD determination by plan-view transmission electron microscopy in strained-Ge (..epsilon..-Ge). To assess the defect density in this case, etch-pit density measurements were performed, providing an alternative means of quantifying the TDDs in the ..epsilon..-Ge layer. Carrier lifetime measurements by microwave-reflection photoconductive decay reveal a clear relationship with TDDs ranging from 5 x 103 cm-2 to 2 x 1010 cm-2, confirming Shockley-Read-Hall recombination as the limiting mechanism at lower defect densities, with TDD-dominated recombination at higher defect densities. The Ge-on-Si relaxed heterostructure exhibited lifetimes much lower (~12 ns) than the lattice-matched Ge on gallium arsenide (GaAs) (~158 ns) heterostructure. Introducing controlled tensile strain reduces defect formation, suppresses strain-relaxation pathways, and leads to measurable improvements in minority carrier lifetime from 12 ns to 171 ns. These results establish a direct relation between defect suppression and carrier recombination dynamics in both relaxed Ge-on-Si grown directly on Si and strained Ge-on-Si heterostructures incorporating compound-semiconductor buffer layers, offering a materials-driven pathway for engineering Ge with improved carrier lifetime for photonic applications.

36 MATERIALS SCIENCE↗

Modeling and experimental characterization of stepped and v-shaped (311) defects in silicon

We propose an atomistic model to describe extended (311) defects in silicon. It is based on the combination of interstitial and bond defect chains. The model is able to accurately reproduce not only planar (311) defects but also defect structures that show steps, bends, or both. We use molecular dynamics techniques to show that these interstitial and bond defect chains spontaneously transform into extended (311) defects. Simulations are validated by comparing with precise experimental measurements on actual (311) defects. The excellent agreement between the simulated and experimentally derived structures, regarding individual atomic positions and shape of the distinct structural (311) defect units, provides strong evidence for the robustness of the proposed model.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Nonlinear effects in defect production by atomic and molecular ion implantation

This report deals with studies concerning vacancy related defects created in silicon due to implantation of 200 keV per atom aluminium and its molecular ions up to a plurality of 4. The depth profiles of vacancy defects in samples in their as implanted condition are carried out by Doppler broadening spectroscopy using low energy positron beams. In contrast to studies in the literature reporting a progressive increase in damage with plurality, implantation of aluminium atomic and molecular ions up to Al{sub 3}, resulted in production of similar concentration of vacancy defects. However, a drastic increase in vacancy defects is observed due to Al{sub 4} implantation. The observed behavioural trend with respect to plurality has even translated to the number of vacancies locked in vacancy clusters, as determined through gold labelling experiments. The impact of aluminium atomic and molecular ions simulated using MD showed a monotonic increase in production of vacancy defects for cluster sizes up to 4. The trend in damage production with plurality has been explained on the basis of a defect evolution scheme in which for medium defect concentrations, there is a saturation of the as-implanted damage and an increase for higher defect concentrations.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Investigation of defect structure of impurity-doped lithium niobate by combining thermodynamic constraints with lattice constant variations

The defect structures of impurity-doped congruent lithium niobates (c-LN) were determined for impurities with various valences, including divalent, trivalent, and tetravalent impurities, in a concentration range where antisite niobium (Nb{sub Li}) exists. On the basis of the “Li site vacancy model,” six kinds of defect structures in impurity-doped c-LN are possible. Using thermodynamic constraints, these can be narrowed down to two kinds. The first structure is that in which impurities, vacancies and Nb exist as defects in the Li site and no defects exist in the Nb site (structure A), described as ([Li{sub Li}] {sub 1-5x-jy}[Nb{sub Li}]{sub x}[M{sub Li}]{sub y}[V{sub Li}]{sub 4x+(j-1)y})[Nb{sub Nb}][O{sub O}] {sub 3} (V: vacancy, M: impurity, j: valence of impurity, x, y: compositional variable (≠0), Li/Nb = congruent ratio). ([Li{sub Li}{sup ×}] {sub 1-5x-2y}[Nb{sub Li}{sup ••••}]{sub x}[M{sub Li}{sup •}]{sub y}[V{sub Li}{sup ′}]{sub 4x+y})[Nb{sub Nb}{sup ×}][O{sub O}{sup ×}] {sub 3} is an example by the Kröger-Vink notation for divalent M. In the second structure, vacancies and Nb exist as defects in the Li site and impurities exist as defects in the Nb site (structure B), described as ([Li{sub Li}] {sub 1-5x-(j-5)y}[Nb{sub Li}]{sub x}[V{sub Li}]{sub 4x+(j-5)y})([Nb{sub Nb}] {sub 1-y}[M{sub Nb}]{sub y})[O{sub O}] {sub 3}. ([Li{sub Li}{sup ×}] {sub 1-5x+y}[Nb{sub Li}{sup ••••}]{sub x}[V{sub Li}{sup ′}]{sub 4x-y})([Nb{sub Nb}{sup ×}] {sub 1-y}[M{sub Nb}{sup ′}]{sub y})[O{sub O}{sup ×}] {sub 3} is an example for tetravalent M. Since the relationship between impurity concentration and lattice constants for structures A and B differs, the defect structures can be differentiated by analyzing lattice constant variations as a function of impurity concentration. The results show that the defect structure of divalent and trivalent impurity-doped c-LN is structure A and that of tetravalent impurity-doped c-LN is structure B. The Nb{sub Li} concentration increased with increasing tetravalent impurity concentration. In contrast, the Nb{sub Li} concentration decreased with increasing divalent and trivalent impurities, leading to suppression of optical damage. The valence of an impurity determines whether the impurity is located in the Li site or Nb site in c-LN, consequently determining whether Nb{sub Li} decreases or increases when the population of the impurity changes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Defects responsible for abnormal n-type conductivity in Ag-excess doped PbTe thermoelectrics

Density functional calculations have been performed to investigate the role of Ag defects in PbTe thermoelectric materials. Ag-defects can be either donor, acceptor, or isovalent neutral defect. When Ag is heavily doped in PbTe, the neutral (Ag-Ag) dimer defect at Pb-site is formed and the environment changes to the Pb-rich/Te-poor condition. Under Pb-rich condition, the ionized Ag-interstitial defect (Ag{sub I}{sup +}) becomes the major donor. The formation energy of Ag{sub I}{sup +} is smaller than other native and Ag-related defects. Also it is found that Ag{sub I}{sup +} is an effective dopant. There is no additional impurity state near the band gap and the conduction band minimum. The charge state of Ag{sub I}{sup +} defect is maintained even when the Fermi level is located above the conduction band minimum. The diffusion constant of Ag{sub I}{sup +} is calculated based on the temperature dependent Fermi level, formation energy, and migration energy. When T > 550 K, the diffusion length of Ag within a few minutes is comparable to the grain size of the polycrystalline PbTe, implying that Ag is dissolved into PbTe and this donor defect is distributed over the whole lattice in Ag-excess doped polycrystalline PbTe. The predicted solubility of Ag{sub I}{sup +} well explains the increased electron carrier concentration and electrical conductivity reported in Ag-excess doped polycrystalline PbTe at T = 450–750 K [Pei et al., Adv. Energy Mater. 1, 291 (2011)]. In addition, we suggest that this abnormal doping behavior is also found for Au-doped PbTe.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of the formation- and passivation rate of boron-oxygen defects for mitigating carrier-induced degradation in silicon within a hydrogen-based model

A three-state model is used to explore the influence of defect formation- and passivation rates of carrier-induced degradation related to boron-oxygen complexes in boron-doped p-type silicon solar cells within a hydrogen-based model. The model highlights that the inability to effectively mitigate carrier-induced degradation at elevated temperatures in previous studies is due to the limited availability of defects for hydrogen passivation, rather than being limited by the defect passivation rate. An acceleration of the defect formation rate is also observed to increase both the effectiveness and speed of carrier-induced degradation mitigation, whereas increases in the passivation rate do not lead to a substantial acceleration of the hydrogen passivation process. For high-throughput mitigation of such carrier-induced degradation on finished solar cell devices, two key factors were found to be required, high-injection conditions (such as by using high intensity illumination) to enable an acceleration of defect formation whilst simultaneously enabling a rapid passivation of the formed defects, and a high temperature to accelerate both defect formation and defect passivation whilst still ensuring an effective mitigation of carrier-induced degradation.

36 MATERIALS SCIENCE↗

Mechanism of Na accumulation at extended defects in Si from first-principles

Sodium (Na) impurities in silicon solar cells are considered to play an important role in potential-induced degradation (PID), a significant cause of solar cell degradation and failure. Shorting due to Na accumulation at extended defects has been suggested as a culprit for PID. However, it is not clear how the extended defects are decorated by Na impurities. Using first-principles density functional theory calculations, we find that Na impurities segregate from the bulk into extended defects such as intrinsic stacking faults and Sigma 3 (111) grain boundaries. The energy barrier required for Na to escape from the extended defects is substantial and similar to the sum of the barrier energy in bulk Si (1.1-1.2 eV) and the segregation energy to the stacking fault (~0.7 eV). Surprisingly, the migration barrier for Na diffusion within the extended defects is even higher than the energy barrier for escaping. Furthermore, the results suggest that the extended defects likely accumulate Na as the impurities segregate to the defects from the bulk, rather than because of migration through the extended defects. Published by AIP Publishing.

36 MATERIALS SCIENCE↗

Properties of V-defect injectors in long wavelength GaN LEDs studied by near-field electro- and photoluminescence

The efficiency of multiple quantum well (QW) light emitting diodes (LEDs) to a large degree depends on uniformity of hole distribution between the QWs. Typically, transport between the QWs takes place via carrier capture into and thermionic emission out of the QWs. In InGaN/GaN QWs, the thermionic hole transport is hindered by the high quantum confinement and polarization barriers. To overcome this drawback, hole injection through semipolar QWs located at sidewalls of V-defects had been proposed. However, in the case of the V-defect injection, strong lateral emission variations take place. In this work, we explore the nature of these variations and the impact of the V-defects on the emission spectra and carrier dynamics. The study was performed by mapping electroluminescence (EL) and photoluminescence (PL) with a scanning near-field optical microscope in LEDs that contain a deeper well that can only be populated by holes through the V-defects. Applying different excitation schemes (electrical injection and optical excitation in the far- and near-field), we have shown that the EL intensity variations are caused by the lateral nonuniformity of the hole injection. We have also found that, in biased structures, the PL intensity and decay time in the V-defect regions are only moderately lower that in the V-defect-free regions thus showing no evidence of an efficient Shockley-–Read–Hall recombination. In the V-defect regions, the emission spectra experience a red shift and increased broadening, which suggests an increase of the In content and well width in the polar QWs close to the V-defects.

Electroluminescence↗

Identification of dislocation-related and point-defects in III-As layers for silicon photonics applications

Abstract The aim of this paper is to identify, analyze and compare the defects present in III-As, as a function of dislocation density, and as a function of the presence/absence of quantum dots (QDs). Such materials are of fundamental importance for the development of lasers and photodiodes for silicon photonics. The study is based on an extensive deep-level transient spectroscopy investigation, carried out on GaAs pin diodes grown on Si and on GaAs (that differ in the dislocation density), with and without embedded QDs. The original results described in this paper demonstrate that: (a) we were able to identify four different defects within the device grown on Si (three electron and one hole traps) and one defect (hole trap) in the device on GaAs, common to both samples; (b) all the majority carrier traps identified are located near midgap, i.e. are efficient non-radiative recombination centers; (c) such defects are absent (or non-detectable) in the sample grown on GaAs substrate, having a very low dislocation density; (d) the presence of QDs does not result in additional defects within the semiconductor material; (e) the analysis of the capture kinetics revealed that two of the identified traps are related to point defects, whereas the other two traps can be associated with point defects located near a dislocation; (f) a comparison with previous reports indicate that the detected traps are related to native III-As defects, or to oxygen-related complexes.

Physics↗

Stringy models of modified gravity: space-time defects and structure formation

Starting from microscopic models of space-time foam, based on brane universes propagating in bulk space-times populated by D0-brane defects (''D-particles''), we arrive at effective actions used by a low-energy observer on the brane world to describe his/her observations of the Universe. These actions include, apart from the metric tensor field, also scalar (dilaton) and vector fields, the latter describing the interactions of low-energy matter on the brane world with the recoiling point-like space-time defect (D-particle). The vector field is proportional to the recoil velocity of the D-particle and as such it satisfies a certain constraint. The vector breaks locally Lorentz invariance, which however is assumed to be conserved on average in a space-time foam situation, involving the interaction of matter with populations of D-particle defects. In this paper we clarify the role of fluctuations of the vector field on structure formation and galactic growth. In particular we demonstrate that, already at the end of the radiation era, the (constrained) vector field associated with the recoil of the defects provides the seeds for a growing mode in the evolution of the Universe. Such a growing mode survives during the matter dominated era, provided the variance of the D-particle recoil velocities on the brane is larger than a critical value. We note that in this model, as a result of specific properties of D-brane dynamics in the bulk, there is no issue of overclosing the brane Universe for large defect densities. Thus, in these models, the presence of defects may be associated with large-structure formation. Although our string inspired models do have (conventional, from a particle physics point of view) dark matter components, nevertheless it is interesting that the role of ''extra'' dark matter is also provided by the population of massive defects. This is consistent with the weakly interacting character of the D-particle defects, which predominantly interact only gravitationally.

79 ASTRONOMY AND ASTROPHYSICS↗

Duality defect in a deformed transverse-field Ising model

Physical quantities with long lifetimes have both theoretical significance in the study of quantum many-body systems and practical implications for quantum technologies. In this manuscript, we investigate the roles played by topological defects in the construction of quasiconserved quantities, using as a prototypical example the Kramers-Wannier duality defect in a deformed one-dimensional quantum transverse-field Ising model. We construct the duality defect Hamiltonian in three different ways: half-chain Kramers-Wannier transformation, utilization of techniques in the Ising fusion category, and defect-modified weak integrability breaking deformation. The third method is also applicable for the study of generic integrable defects under weak integrability breaking deformations. We also work out the deformation of defect-modified higher charges in the model and study their slower decay behavior. Furthermore, we consider the corresponding duality defect twisted deformed Floquet transverse-field Ising model and investigate the stability of the isolated zero mode associated with the duality defect in the integrable Floquet Ising model, under such weak integrability breaking deformation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗