At least 613 records · Page 34

Measuring the Weibull modulus of microscope slides

The objectives are that students will understand why a three-point bending test is used for ceramic specimens, learn how Weibull statistics are used to measure the strength of brittle materials, and appreciate the amount of variation in the strength of brittle materials with low Weibull modulus. They will understand how the modulus of rupture is used to represent the strength of specimens in a three-point bend test. In addition, students will learn that a logarithmic transformation can be used to convert an exponent into the slope of a straight line. The experimental procedures are explained.

Sorensen, Carl D.↗

Improving the low temperature ductility of NiAl

The intermetallic NiAl exhibits excellent potential as a structural material for application in air-breathing and single-stage-to-orbit engines. Unfortunately NiAl is brittle at ambient temperature, which is partly attributed to the lack of five independent slip systems as required by von Mises criterion for uniform, volume conserving deformation since the operative group of zone axes (100) slip offers only three independent slip systems. Isostructural FeAl, however, deforms by group of zone axes (111) slip at room temperature which provides five independent slip systems. Thus, it was decided to macroalloy NiAl with Fe to promote group of zone axes (111) slip thereby possibly improving the ductility. For Ni - 30 at. (percent) Al - 20 at. (percent) Fe having essentially bcc microstructure indicated up to 6 percent tensile elongation combined with high yield strength (about 800 MPa). The results compare favorably with those of stoichiometric Ni - 50 at. (percent) Al which, however, deforms by group of zone axes (100) slip at room temperature. The multi-phase alloy approach has proven even more successful for Ni - 20 at. (percent) Al - 30 at. (percent) Fe. The high temperature ductility of the multi-phase alloy was attributed to deformation transfer across interphase boundaries and the crack stopping action of the constituent gamma/gamma' phase. While the constituent phase became increasingly brittle, the beta' phase became more ductile at elevated temperatures. Thus the multi-phase alloy did not exhibit any elevated temperature embrittlement. Similarly, while the beta' phase became weak at high temperatures, the gamma/gamma' phase exhibited better strength retention leading to the improved elevated temperature strength of the multi-phase alloy. Thus, the multi-phase alloy benefits from both its constituent phases, with each phase alleviating the disadvantages associated with the other phase over any temperature range. The multi-phase alloy approach is suggested as a possible approach to designing intermetallic-based alloys.

Guha, Sumit↗

Vacuum ultraviolet radiation/atomic oxygen synergism in fluorinated ethylene propylene Teflon erosion

A micrographic investigation is reported of samples of the fluorinated ethylene propylene (FEP) Teflon thermal-blanketing materials recovered from the Long-Duration Exposure Facility (LDEF) satellite. The samples are taken from the trailing edge and row 8 which correspond to exposures to vacuum UV (VUV) and VUV + atomic O, respectively. Data are taken from SEM and IR-spectra observations, and the LDEF leading-edge FEP shows a high degree of erosion, roughening, and sharp peaks angled in the direction of the flow of atomic O. The trailing edge sample influenced primarily by VUV shows a hard brittle layer and some cracked mosaic patterns. Comparisons to a reference sample suggest that the brittle layer is related to exposure to VUV and is removed by atomic-O impingement. Polymers that are stable to VUV radiation appear to be more stable in terms of atomic oxygen.

Stiegman, A. E.↗

Impact damage tolerance of thin wall composite struts

An experimental investigation was made to study the impact damage tolerance of thin wall composite struts made of both brittle epoxy and toughened epoxy based composite materials. Damage parameters such as barely visible surface damage and internal damage represented by the ultrasonic C-scan, and residual compressive strengths were evaluated against impact energy for two impactor sizes. From both a damage resistance (internal damage vs. impact energy) and a damage tolerance (residual compressive strength vs. internal damage) point of view, the toughened IM7/977-2 struts exhibited better performance than the brittle epoxy based T50/934 struts. This is attributed to the toughening mechanism in 977-2 which impedes delamination initiation from impact, and delamination growth and subsequent buckling under a compression loading. At barely visible damage thresholds, regardless of the impactor sizes, a maximum strength reduction of 45-55 percent was observed for the T50/934 struts, and approximately 10 percent for IM7/977-2 struts. This is of great interest for developing a damage tolerance design approach and risk assessment methodology in which the design allowable would be defined by the residual strength at the threshold of barely visible damage.

Chen, G.-S.↗

A Numerical Round Robin for the Reliability Prediction of Structural Ceramics

A round robin has been conducted on integrated fast fracture design programs for brittle materials. An informal working group (WELFEP-WEakest Link failure probability prediction by Finite Element Postprocessors) was formed to discuss and evaluate the implementation of the programs examined in the study. Results from the study have provided insight on the differences between the various programs examined. Conclusions from the study have shown that when brittle materials are used in design, analysis must understand how to apply the concepts presented herein to failure probability analysis.

Powers, Lynn M.↗

Scanning electron acoustic microscopy of residual stresses in ceramics - Theory and experiment

The paper presents a three-dimensional mathematical model of signal generation and contrast in brittle materials and uses the model to simulate the effect of residual stress fields on the scanning electron acoustic microscopy (SEAM)-generated electron acoustic signal. According to the model, a positive (tensile) strain produces an increase in the output signal, whereas a negative (compressive) strain produces a decrease in the ouput signal. Dark field contrast conditions occur at a chopping frequency at which V2 - V1 is greater than 0 (where V2 = V is the SEAM output in a region of residual stresses, and V1 is the output in a stress-free region of the sample). Under ideal conditions (maximum contrast) V1 approaches zero. It was found that tensile strains of the order 0.2-0.3 percent, possible in brittle materials, would produce a variation of the acoustic output signal of the order 10 nV (about 1 percent), well within the image contrast and signal processing capability of the SEAM electronics.

Cantrell, John H.↗

Behavior of Materials Under Conditions of Thermal Stress

A review is presented of available information on the behavior of brittle and ductile materials under conditions of thermal stress and thermal shock. For brittle materials, a simple formula relating physical properties to thermal-shock resistance is derived and used to determine the relative significance of two indices currently in use for rating materials. For ductile materials, thermal-shock resistance depends upon the complex interrelation among several metallurgical variables which seriously affect strength and ductility. These variables are briefly discussed and illustrated from literature sources. The importance of simulating operating conditions in tests for rating materials is especially to be emphasized because of the importance of testing conditions in metallurgy. A number of practical methods that have been used to minimize the deleterious effects of thermal stress and thermal shock are outlined.

Manson, S S↗

A thermodynamic theory of dynamic fragmentation

We present a theory of dynamic fragmentation of brittle materials based on thermodynamic arguments. We recover the expressions for average fragment size and number as originally derived by Grady. We extend the previous work by obtaining descriptions of fragment size distribution and compressibility change due to the fragmentation process. The size distribution is assumed to be proportional to the spectral power of the strain history and a sample distribution is presented for a fragmentation process corresponding to a constant rate strain history. The description of compressibility change should be useful in computational studies of fragmentation. These results should provide insight into the process of fragmentation of brittle materials from hypervelocity impact.

Ching H Yew↗

Property enchancement of polyimide films by way of the incorporation of lanthanide metal ions

Lanthanide metal ions were incorporated into the polyimide derived from 2,2-bis(3,4-dicarboxyphenyl) hexafluoropropane dianhydride (6FDA) and 1,3-bis(aminophenoxy) benzene (APB) in an attempt to produce molecular level metal-polymer composites. The lanthanide series of metal ions (including aluminum, scandium, and yttrium) provide discrete and stable metal ions in the 3+ oxidation state. Throughout the series there is a uniform variation in ionic size ranging from 50 pm for aluminum to a maximum of 103.4 pm for cerium and gradually decreasing again to 84.8 pm for lutetium. The high charge-to-size ratio for these ions as well as the ability to obtain large coordination numbers makes them excellent candidates for interacting with the polymer substructure. The distinct lack of solubility of simple lanthanide salts such as the acetates and halides has made it difficult to obtain metal ions distributed in the polymer framework as discrete ions or metal complexes rather than microcomposites of metal clusters. (Lanthanum nitrates are quite soluble, but the presence of the strongly oxidizing nitrate ion leads to serious degradation of the polymer upon thermal curing. This work was successful at extending the range of soluble metals salts by using chelating agents derived from the beta-diketones dipivaloylmethane, dibenzoylmethane, trifluoroacetylacetone, and hexafluoroacetylacetone. Metal acetates which are insoluble in dimethylacetamide dissolve readily in the presence of the diketones. Addition of the polyimide yields a homogeneous resin which is then cast into a clear film. Upon curing clear films were obtained with the dibenzoylmethane and trifluoroacetylacetone ligands. The dipavaloylmethane precipitates the metal during the film casting process, and hexafluoroacetylacetone gives cured films which are deformed and brittle. These clear films are being evaluated for the effect of the metal ions on the coefficient of thermal expansion, resistance to atomic oxygen, and on selective gas permeability. Much more commonly than above, polyimide films are prepared by casting the film as the poly(amic acid) precursor which is then converted to the imidized form during the thermal cure cycle. Very limited success was achieved in the past in adding lanthanide metal ions to the amide precursors because of gellation and lack of solubility. With the use of the diketone ligands cited above, the solubility and gellation problems were overcome. However, the films after curing were clear but unacceptably brittle. Attempts to overcome this cure embrittlement problem are in progress.

Thompson, David W.↗

The unique radar scattering properties of silicic lava flows and domes

Silicic (silica-rich) lava flows, such as rhyolite, rhyodacite, and dacite, possess unique physical properties primarily because of the relatively high viscosity of the molten lava. Silicic flows tend to be thicker than basaltic flows, and the resulting large-scale morphology is typically a steep-sided dome or flow lobe, with aspect ratios (height/length) sometimes approaching unity. The upper surfaces of silicic domes and flows are normally emplaced as relatively cool, brittle slabs that fracture as they are extruded from the central vent areas, and are then rafted away toward the flow margin as a brittle carapace above a more ductile interior layer. This mode of emplacement results in a surface with unique roughness characteristics, which can be well-characterized by multiparameter synthetic aperture radar (SAR) observations. In this paper, we examine the scattering properties of several silicic domes in the Inyo volcanic chain in the Eastern Sierra of California, using AIRSAR and TOPSAR data. Field measurements of intermediate-scale (cm to tens of m) surface topography and block size are used to assess the mechanisms of the scattering process, and to quantify the unique roughness characteristics of the flow surfaces.

Plaut, Jeffrey J.↗

Scanning electron acoustic microscopy of residual stresses in ceramics: Theory and experiment

Several reviews have highlighted a number of applications of scanning electron acoustic microscopy (SEAM) to metals and semiconductors which show that SEAM can provide new information on surface and near-surface features of such materials, but there have been few studies attempting to determine the capabilities of SEAM for characterizing ceramic materials. We have recently observed image contrast in SEAM from residual stress fields induced in brittle materials by Vickers indentations that is strongly dependent on the electron beam chopping frequency. We have also recently developed a three-dimensional mathematical model of signal generation and contrast in SEAM, appropriate to the brittle materials studied, that we use as a starting point in this paper for modeling the effect of residual stress fields on the generated electron acoustic signal. The influence of the electron beam chopping frequency is also considered under restrictive assumptions.

Cantrell, John H.↗

An investigation of the loss of ductility in hydrogen charged beta-Ti alloys

The high strength, low density, and good corrosion resistance of Ti-based alloys make them candidate materials for a number of applications in the aerospace industry. A major limitation in the use of these alloys in the advanced hypersonic flight vehicle program is their susceptibility to hydrogen embrittlement. This study focuses on the hydrogen sensitivity of TIMETAL 21S beta-Ti alloy. The material received was in the form of grip-ends of failed tensile test samples which had been exposed to different charging conditions (combinations of hydrogen pressure and temperature). The samples received, the charging conditions, and their fracture mode are discussed. It can be seen that the fracture behavior changes from ductile to brittle with increasing hydrogen content, but the transition in behavior occurs for a small increase in hydrogen concentration. The aim of this program was to assess the microstructural differences between the ductile and brittle alloys to ascertain the embrittlement mechanism. A range of tools which included x-ray diffraction, scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used.

Robertson, Ian M.↗

Durability and life prediction modeling in polyimide composites

Sudden appearance of cracks on a macroscopically smooth surface of brittle materials due to cooling or drying shrinkage is a phenomenon related to many engineering problems. Although conventional strength theories can be used to predict the necessary condition for crack appearance, they are unable to predict crack spacing and depth. On the other hand, fracture mechanics theory can only study the behavior of existing cracks. The theory of crack initiation can be summarized into three conditions, which is a combination of a strength criterion and laws of energy conservation, the average crack spacing and depth can thus be determined. The problem of crack initiation from the surface of an elastic half plane is solved and compares quite well with available experimental evidence. The theory of crack initiation is also applied to concrete pavements. The influence of cracking is modeled by the additional compliance according to Okamura's method. The theoretical prediction by this structural mechanics type of model correlates very well with the field observation. The model may serve as a theoretical foundation for future pavement joint design. The initiation of interactive cracks of quasi-brittle material is studied based on a theory of cohesive crack model. These cracks may grow simultaneously, or some of them may close during certain stages. The concept of crack unloading of cohesive crack model is proposed. The critical behavior (crack bifurcation, maximum loads) of the cohesive crack model are characterized by rate equations. The post-critical behavior of crack initiation is also studied.

Binienda, Wieslaw K.↗

Instrumented Materials Testing

This presentation starts with an introduction to the need for materials testing. Classic failures (such as brittle ship hull fractures) are discussed before fundamental discoveries in fracture analysis (Griffith, Westergaard, and Irwin). Next standard tests are identified, followed by a look at brittle versus ductile failure. Griffith's result (the composite paradigm) that smaller composite specimens are stronger because they have smaller flaws, is covered. This leads into composite tests. And finally, stress waves are shown as an example that will initiate damage.

Mackin, Thomas J.↗

CARES/Life Software for Designing More Reliable Ceramic Parts

Products made from advanced ceramics show great promise for revolutionizing aerospace and terrestrial propulsion, and power generation. However, ceramic components are difficult to design because brittle materials in general have widely varying strength values. The CAPES/Life software eases this task by providing a tool to optimize the design and manufacture of brittle material components using probabilistic reliability analysis techniques. Probabilistic component design involves predicting the probability of failure for a thermomechanically loaded component from specimen rupture data. Typically, these experiments are performed using many simple geometry flexural or tensile test specimens. A static, dynamic, or cyclic load is applied to each specimen until fracture. Statistical strength and SCG (fatigue) parameters are then determined from these data. Using these parameters and the results obtained from a finite element analysis, the time-dependent reliability for a complex component geometry and loading is then predicted. Appropriate design changes are made until an acceptable probability of failure has been reached.

Nemeth, Noel N.↗

Effect of Processing Route on Strain Controlled Low Cycle Fatigue Behavior of Polycrystalline NiAl

The present investigation examines the effects of manufacturing process on the total axial strain controlled low cycle fatigue behavior of polycrystalline NiAl at 1000 K, a temperature above the monotonic Brittle-to-Ductile Transition Temperature (BDTT). The nickel aluminide samples were produced by three different processing routes: hot isostatic pressing of pre- alloyed powders, extrusion of prealloyed powders, and extrusion of vacuum induction melted ingots. The LCF behavior of the cast plus extruded material was also determined at room temperature (below the BD77) for comparison to the high temperature data. The cyclic stress response, cyclic stress-strain behavior, and strain-life relationships were influenced by the alloy preparation technique and the testing temperature. Detailed characterization of the LCF tested samples was conducted by optical and electron microscopy to determine the variations in fracture and deformation modes and to determine any microstructural changes that occurred during LCF testing. The dependence of LCF properties on processing route was rationalized on the basis of starting microstructure, brittle-to-ductile transition temperature, deformation induced changes in the basic microstructure, deformation substructure, and synergistic interaction between the damage modes.

Rao, K. Bhanu Sankara↗

Oxidation Behavior of Binary Niobium Alloys

This investigation concludes a study to determine the effects of up to 25 atomic percent of 55 alloying additions on the oxidation characteristics of niobium. The alloys were evaluated by oxidizing in an air atmosphere for 4 hours at 1000 C and 2 hours at 1200 C. Titanium and chromium improved oxidation resistance at both evaluation conditions. Vanadium and aluminum improved oxidation resistance at 1000 C, even though the V scale tended to liquefy and the Al specimens became brittle and the scale powdery. Copper, cobalt, iron, and iridium improved oxidation resistance at 1200 C. Other investigations report tungsten and molybdenum are protective up to about 1000 C, and tantalum at 1100 C. The most important factor influencing the rate of oxidation was the ion size of the alloy additions. Ions slightly smaller than the Nb(5+) ion are soluble in the oxide lattice and tend to lower the compressive stresses in the bulk scale that lead to cracking. The solubility of the alloying addition also depends on the valence to some extent. All of the elements mentioned that improve the oxidation resistance of Nb fit this size criterion with the possible exception of Al, whose extremely small size in large concentrations would probably lead to the formation of a powdery scale. Maintenance of a crack-free bulk scale for as long as possible may contribute to the formation of a dark subscale that ultimately is rate- controlling in the oxidation process. The platinum-group metals, especially Ir, appear to protect by entrapment of the finely dispersed alloying element by the incoming Nb2O5 metal-oxide interface. This inert metallic Ir when alloyed in a sufficient amount with Yb appears to give a ductile phase dispersed in the brittle oxide. This scale would then flow more easily to relieve the large compressive stresses to delay cracking. Complex oxide formation (which both Ti and Zr tend to initiate) and valence effects, which probably change the vacancy concentration in the scale, are masked by the overriding tendency for a porous scale.

Barrett, Charles A.↗

Diagnostic Clast-Texture Criteria for Recognition of Impact Deposits

It is difficult to find definitive evidence for impact in the geological record because there are many endogenous geological processes that can produce diamictites similar to those generated by impact ejecta. The classic impact criteria of shock fabrics in certain minerals, and iridium layers, for example, may be either difficult to find, or long-since erased from the impact site (shock fabrics also anneal with time). It is important to be able to recognize impact-generated materials in order to understand earth's crustal development and biological evolution. In future exploration of Mars and other solar-system bodies, recognition of impact materials will be important for elucidating planetary evolution, planetary volatile inventories, and exobiological issues. The cobble depicted is typical of many that have been found in diamictite deposits in Belize generated by the Chicxulub K-T impact event. The pebbles are roughly-hewn in general shape with smoothed corners and edges. Surfaces are almost uniformly frosted (on both protuberances and hollows), but some asperities are glazed. Optical microscopy and thin-section petrographic microscopy reveal the frosting to be only a few microns thick, with a well-defined granular structure; grains are the same size as those composing the bulk of the limestone, but their clearer appearance may represent annealing. One or two adjacent pebble faces are often decorated with striated gouges and closely-spaced hemispherical depressions representing indentation hollows produced by well-rounded impacting clasts of up to 0.5 cm in diameter. Some of the impactors are still embedded in the cobble surface. Non-destructive x-ray diffraction techniques showed the impactors to be of the same mineralogy as the target cobble. We believe this unusual glazing and frosting to be related to the impact event, but this must be reconciled with its survival for over 60 my. since it is composed of one of the most alterable substances, CaCO3. We focus, however, on the non-fractured rounded pebbles that appear to have impacted the larger cobble as a swarm of clasts, probably encountered during ballistic flight. It cannot be defined whether the cobble swept through the pebble cloud, or the pebbles rained upon a slowermoving cobble. Two interesting questions arise: (1) Where did large numbers of such well rounded pebbles come from in the ejecta curtain?, and (2) How did they embed themselves in a nominally brittle rock without suffering damage? Are the well-rounded pebbles crystalline (devitrified) melt spherules? Further investigations are in progress. If the cobble was cold and brittle, impact of well-rounded pebbles would have produced Hertzian fracture patterns (a) in the virtually elastically isotropic cobble target. For penetration depths of about 0.5 of the impactor diameter, the pebbles would require a relative impact velocity sufficient to cause pebble fragmentation and crushing, and the development of a complex Hertzian-Boussinesq fracture field (b) involving deep fracturing and lateral surface spalling (impact velocities > 50 m/s). The existing relationship could only evolve by the impact of cold, hard pebbles into a soft, plastic cobble surface (c). For limestone to have been plastic, it must have been at elevated temperature, but to prevent calcification of the material, the ambient pressure must also have been elevated. This would be possible either in the impact's gas plume, or within the confines of a thin aerodynamically-produced shock bow generated by supersonic ballistic motion of the cobble. In the latter case, it is implied that the cobble swept through the pebbles rather than vice-versa. Although there are high T-P conditions associated with volcanism, such textures have not been reported on volcaniclastic materials, nor from other high T-P environments; e.g., metamorphic (as far as the authors are aware). We propose that this very easily recognizable embedding and indentation surface texture can be used as a diagnostic criterion for the recognition of impact ejecta. The term "peening texture" is suggested, because it is absolutely analogous to the plastic-deformation induced, metal-surface textures generated by ball-bearing bombardment used in engineering metallurgy to work-harden metal surfaces. Additional information is contained in the original (Figures).

Marshall, J. R.↗