Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “volatility”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 595 records · Page 33

Effects of water-based binders on electrochemical performance of manganese dioxide cathode in mild aqueous zinc batteries

In the majority of rechargeable batteries including lithium ion batteries (LIBs), polyvinylidene fluoride (PVdF) binders are the most commonly used binder for both anode and cathode. However, using PVdF binder requires the organic solvent of N-methyl-2-pyrrolidone (NMP) which is expensive, volatile, combustible, toxic, and has poor recyclability. Therefore, switching to aqueous electrode processing routes with non-toxic binders would provide a great leap forward towards the realization of ideally fully sustainable and environmentally friendly electrochemical energy storage devices. Various water-soluble binders (aqueous binders) were characterized and compared to the performance of conventional PVDF. Our study demonstrates that the electrochemical performance of Zn/MnO2 aqueous batteries is significantly improved by using sodium carboxymethyl cellulose (CMC) binder. Additionally, CMC binders offers desirable adhesion, good wettability, homogeneous material distribution, and strong chemical stability at certain pH levels (3.5~5) without any decomposition for long-cycle life.

25 ENERGY STORAGE↗

Unraveling Electronic Effects that Influence the Bimolecular Chemistry of Fluorinated Criegee Intermediates

Ozonolysis is important for the removal of unsaturated volatile organic compounds emitted into the Earth's atmosphere. The alkene + ozone reaction (alkene ozonolysis) forms a carbonyl oxide – a Criegee intermediate (CI). CIs are interesting from an atmospheric chemistry perspective. They are implicated in enhancing the oxidizing capacity of the troposphere and in secondary organic aerosol formation. CIs may participate in bimolecular reactions with trace atmospheric vapors like water and methanol. Here, the chemistry of the two isomers of CFHOO and of CF 3 CHOO with water, water dimer, and methanol is explored. The present study confirms that the syn-conformer is the minimum energy structure for both CIs and that the reactions of anti-CFHOO display slightly lower activation energies cf. syn-CFHOO, thus promoting faster reaction. For both syn- and anti-CFHOO, the energy barrier in the pathway to adding water, water dimer, or methanol is lower—and the overall reaction exoergicity greater—than for the corresponding reactions involving the nonfluorinated analogue, CH 2 OO. Here, the corresponding bimolecular reaction rates are thus predicted to be faster for CFHOO than CH 2 OO. Similar reactivity trends are found when comparing the same reactions of syn-CF 3 CHOO, cf. syn-CH 3 CHOO, but not when comparing the energetics of the reactions involving anti-CF 3 CHOO cf. anti-CH 3 CHOO.

Guidry, Lily M. [University of Louisiana at Lafaye↗

Active and Stable PtPd Diesel Oxidation Catalysts under Industry‐Defined Test Protocols

Nanoparticle-supported Pt and Pd catalysts are employed industrially to convert CO and hydrocarbon residue from incomplete diesel fuel combustion into more environmentally-benign products. However, these catalysts deactivate over time due to sintering, especially for Pt nanoparticles which readily generate volatile species under high operating temperatures. Here, we turned the detrimental vapor-mediated sintering of Pt into an advantage by using a physical mixture of Pt and Pd catalysts prepared using a raspberry-colloid-templating (RCT) method. The RCT method produced Pt/Al 2 O 3 and Pd/Al 2 O 3 catalysts with partially embedded NPs to inhibit surface-mediated sintering pathways. As validated using an industry-defined emission control test protocol, aging a physical mixture of Pt/Al 2 O 3 and Pd/Al 2 O 3 at high temperature produced an alloyed PtPd/Al 2 O 3 catalyst that outperformed the fresh catalyst mixture and both individual catalysts for hydrocarbon conversion, while exhibiting high catalytic stability and resistance to sintering and to SO 2 poisoning. X-ray photoelectron spectroscopy revealed that in the aged catalyst mixture, half of the Pd content existed in the more active metallic state, compared to the less active oxide forms in the fresh mixture and both individual catalysts, explaining the unusual activity enhancement. Our results represent a practical approach to producing active and stable PtPd/Al 2 O 3 diesel oxidation catalysts for emission control applications.

Lim, Kang Rui Garrick [Harvard University, Cambrid↗

Upcycling Polyethylene Waste into Hybrid Graphitic Porous Carbon Materials Used in High‐Performance Zinc‐Ion Hybrid Capacitors

Polyethylene (PE) waste is a challenge to upcycle into useful materials because this plastic tends to decompose into volatile compounds when heated at relatively low temperatures. In this work, mixtures of PE wastes into a hybrid graphitic porous carbon (HGPC) by a thermal oxidation pretreatment step, with assistance of an inert solid additive (KCl), to functionalize, crosslink, and stabilize the PE waste followed by carbonization and catalytic graphitization steps with a potassium carbonate catalyst, are upcycled. The PE waste‐derived HGPC (PW‐HGPC) has a hybrid structure composed of graphene‐like carbon nanosheets grown on the surface of carbon particles, high porosity with specific surface area, up to 1,763 m 2 g −1 , and good graphitic degree with average Raman I 2D / I G ratios of 0.53. When used as cathode material for zinc‐ion hybrid capacitors, this PW‐HGPC exhibits an excellent specific capacity, up to 126.7 mAh g −1 , at high mass loading of 10 mg cm −2 . Moreover, PW‐HGPC exhibits remarkable cycling stability with capacity retention of >94% after 10 000 cycles. Additionally, the KCl is recycled and reused over five times. This method provides a new solution for upcycling PE wastes into high value‐added carbon materials, not only for zinc‐ion hybrid capacitors but also for other electrochemical energy storage device applications.

hybrid graphitic porous carbon↗

Molecular beam scattering from flat jets of liquid dodecane and water

Abstract Molecular beam experiments in which gas molecules are scattered from liquids provide detailed, microscopic perspectives on the gas–liquid interface. Extending these methods to volatile liquids while maintaining the ability to measure product energy and angular distributions presents a significant challenge. The incorporation of flat liquid jets into molecular beam scattering experiments in our laboratory has allowed us to demonstrate their utility in uncovering dynamics in this complex chemical environment. Here, we summarize recent work on the evaporation and scattering of Ne, CD 4 , ND 3 , and D 2 O from a dodecane flat liquid jet and present first results on the evaporation and scattering of Ar from a cold salty water jet. In the evaporation experiments, Maxwell–Boltzmann flux distributions with a cos θ angular distribution are observed. Scattering experiments reveal both impulsive scattering (IS) and trapping followed by thermal desorption (TD). Super‐specular scattering is observed for all four species scattered from dodecane and is attributed to anisotropic momentum transfer to the liquid surface. In the IS channel, rotational excitation of the polyatomic scatterers is a significant energy sink, and these species accommodate more readily on the dodecane surface compared to Ne. Our preliminary results on cold salty water jets suggest that Ar atoms undergo some vapor‐phase collisions when evaporating from the liquid surface. Initial scattering experiments characterize the mechanisms of Ar interacting with an aqueous jet, allowing for comparison to dodecane systems. Key Points Molecular beam scattering from flat liquid jets is a powerful technique to elucidate mechanistic detail at the gas–liquid interface. Previous dodecane scattering experiments have uncovered angularly‐resolved thermal desorption fractions and energy transfer at the interface for several small molecule scatterers. Preliminary results on scattering from cold salty water reveal mechanisms of interaction between argon and an aqueous jet.

Yang, Walt↗

Electrochemical mechanisms of leakage‐current in photovoltaic modules

Abstract This paper analyzes the mechanisms and pathways for leakage current flow observed in Si photovoltaic modules subjected to high temperature and humidity and a large voltage bias with respect to ground. The current inside of the frame is in the form of electron motion, but in the glass and polymer, it is in at least a large part attributable to the movement of ions. When the mode of current flow changes from electronic to ionic conduction, electrochemical reactions will take place at the interface. This can include reactions that produce volatile chemical species like H 2 , CO x , and O 2 , along with ionic species such as OH − and H 3 O + . Here, we see evidence of the importance of different charge carriers with different diffusion rates and the influence of electrochemical processes involved. The application of negative voltage to the cell circuit affects the resistivity of glass producing surfaces with poor conductivity but with some increases in the electrochemical potential producing complicated interactions that are important when the voltage is changed. In the polymer, there is the development of a space charge region and a chemical gradient providing two oppositional forces to current flow, which when released create a complicated discharge process. Here, we give a basic understanding of the charge/discharge of PV cells highlighting how the specific mechanisms are important in understanding some of the degradation processes in PV modules. We find that there is evidence of multiple significant charge carrier species with different diffusion time scales. The glass/polymer interface forms a depleted region of higher resistance after prolonged exposure to current. Charge also builds up at the polymer to cell antireflective coating interface and mostly flows to the gridlines to experience electrochemical reactions. These complexities result in non‐linear behavior where the apparent resistivities of the different layers change during charge/discharging processes, making the modeling of the current flow extremely difficult.

14 SOLAR ENERGY↗

Initiator‐Driven Tailoring of Reactivity and Inhibition in Frontally Polymerized Dicyclopentadiene‐Co‐Dihydrofuran Thermosets

Incorporating 2,3‐dihydrofuran (DHF) into dicyclopentadiene (DCPD) enables frontally polymerizable, deconstructible thermosets via acid hydrolysis. At 5–20 mol% DHF and low initiator concentration (~100 ppm), DHF inhibits front propagation, lowers the glass transition temperature ( T g ) by up to 20°C, and quenches the front, especially at 20% DHF. This paper demonstrates that increasing the initiator concentration to 250–1000 ppm overcomes inhibition, enhances front speeds by ~50%, and suppresses quenching at the expense of pot‐life. Above 5 mol% DHF, an emergence of a second exotherm is observed, attributed to increased rate dependence on the inhibition of the initiator by DHF. Void formation from volatile DHF is suppressed by applying 110 kPa nitrogen, though at the cost of reduced front speed. Dynamic mechanical analysis shows that higher initiator concentration produced more highly cross‐linked polymers, with a ~20% increase in storage modulus at 25°C and a 20°C increase in T g .

deconstructible thermosets↗

Thermal Stability of a Eutectic Mixture of Bis(2,2-dinitropropyl) Acetal and Formal: Part C. Kinetic Compensation Effect

Here, the aging behavior of a eutectic mixture of bis(2,2-dinitropropyl) acetal and formal [called NP here] has been studied in various atmospheres [dry (air or nitrogen) versus wet] at temperatures 70 °C and below. The properties of aged samples were analyzed using Fourier transform infrared (FTIR) spectroscopy, Karl Fischer (KF) titration, liquid chromatography/mass spectrometry (LC/MS), and thermogravimetric analysis (TGA) over a period of three years. The results indicate that at aging temperatures up to 55 °C, the initial rates of water production from nitrous acid (HONO) formation and decomposition into the water, NO, and NO 2 follows a 1st order rate law and the rate constants follow an Arrhenius law as a function of temperature. The activation energies and pre-factors for water and volatiles production yield a single linear kinetic compensation plot, suggesting a common degradation pathway between NP and the various combinations of its constituents. Within a narrow temperature range, around 55 °C, a trace amount of water in NP stabilizes its properties by preventing HONO elimination. When the aging temperature is substantially higher than 55 °C, the nature of the degradation mechanism changes. It is suspected that the degradation products of NO x , water, and HNO 3 serve as catalysts to auto-catalyze (kinetics beyond the 1st order) and further degrade NP. The effect of headspace volume on this auto-catalytic process will be discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Comparative analysis of sublimation and thermal decomposition of TATB

This experimental study investigated the effects of confinement, starting mass, and heating rate on TATB thermal decomposition and sublimation using a combined Thermo-Gravimetric Analyzer and Differential Scanning Calorimetry (TGA/DSC) instrument. The confinement of volatile products was varied using different pinhole sizes with TGA/DSC pans. The measurements showed the open pan experiments without lids/pinholes resulted in complete sublimation of TATB between 320 °C and 360 °C. The heat of sublimation was determined to be 176 kJ/mol (42 kcal /mol), consistent with literature data obtained from other experimental techniques. The use of pinholes suppressed the sublimation of TATB such that the decrease in pinhole size resulted in 1) an increase in the enthalpy of reaction and an increase in the amount of carbonaceous material remaining at the end of decomposition, and 2) convergence of the two peak temperatures corresponding to maximum heat flow and maximum weight loss. Also, a transition from a two-exotherm thermal decomposition behavior towards a single-exotherm occurred as the pinhole size was decreased for a given starting mass or as the starting mass was increased for a given pinhole size. These results indicate the kinetics of TATB sublimation, TATB thermal decomposition, and gas diffusion out of a TGA/DSC pan can all compete and result in significantly different enthalpies, amounts of remaining materials, and peak temperatures depending on the pinhole size and starting mass used in the measurements. Furthermore, the results also indicate precise control of process variables (pinhole size, starting mass, and heating rate) in TGA/DSC measurements is required for thermal safety assessment of explosives.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Sample Mass, Confinement, and Preheating Time on the Thermal Response of LLM‐105: Experiments and Kinetic Analysis

Various small-scale experiments were performed to provide data for developing a model to predict the thermal response of LLM-105 over a wide range of conditions. The thermal decomposition of LLM-105 was studied as a function of sample mass, confinement of volatile products, and preheating time in both isothermal and ramped heating experiments. The thermal decomposition of LLM-105 is a two-step process, as shown by the two exothermic peaks in the heat flow profiles, which were fitted to two nth-order autocatalytic reaction models with a similar activation energy of ∼289 kJ/mol. The magnitude and shape of these peaks varied with sample mass and confinement. Increasing sample mass enhanced the second exotherm with respect to the first one, while increasing the level of confinement promoted a transition from a sublimation-dominated regime towards thermal decomposition. The effect of LLM-105 particle size on the rate of weight loss was evident for open-pan experiments, where bigger particles sublimed at lower temperatures than smaller particles. Thermal response and solid residue composition of LLM-105 samples were analyzed following preheating for different durations. Longer preheating times caused a shift of the second exotherm to lower temperatures and a decrease in the reaction enthalpy, confirming that LLM-105 decay is a consecutive reaction mechanism, probably autocatalytic. In conclusion, the kinetic model derived from ramped experiments was validated against the measured LLM-105 fraction remaining and the enthalpy remaining of the solid residue as a function of preheating times and showed good agreement.

Chemistry - Chemical explosives↗

Xenon Trapping in Metal-Supported Silica Nanocages

Xenon (Xe) is a valuable and scarce noble gas used in various applications, including lighting, electronics, and anesthetics, among many others. It is also a volatile byproduct of the nuclear fission of uranium. In this work, a novel material architecture consisting of silicate nanocages in contact with a metal surface and an approach for trapping single Xe atoms in these cages is presented. The trapping is done at low Xe pressures and temperatures between 400 and 600 K, and the process is monitored in situ using synchrotron-based ambient pressure X-ray photoelectron spectroscopy. Release of the Xe from the cages occurs only when heating to temperatures above 750 K. A model that explains the experimental trapping kinetics is proposed and tested using Monte Carlo methods. Density functional theory calculations show activation energies for Xe exiting the cages consistent with experiments. This work can have significant implications in various fields, including Xe production, nuclear power, nuclear waste remediation, and nonproliferation of nuclear weapons. The results are also expected to apply to argon, krypton, and radon, opening an even more comprehensive range of applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Automated Programmable Logic Controller Memory Forensics Using RGB Image Analysis and Deep Learning

The introduction of Industry 4.0 and Internet-based technologies has enhanced industrial control system operations but have inadvertently increased their vulnerabilities to cyber attacks. When an industrial control system is compromised, security analysts need to identify the root cause quickly to start the recovery process and develop mitigation strategies. Memory forensics is critical in the incident analysis process to ascertain what occurred. Approaches for analyzing the persistent memory in industrial control devices are limited and almost nonexistent for volatile memory. This chapter proposes an automated methodology for programmable logic controller memory dump analysis using computer vision and deep learning techniques. The methodology converts the sequences of bytes in a programmable logic controller memory dump to red-green-blue pixels and employs a deep learning model that learns the underlying patterns and features of pre-labeled forensic artifacts in images and segments them into distinct regions. The trained model is employed to automatically segment new memory images and identify forensic artifacts. Evaluation of the methodology on a Schneider Electric Modicon M221 programmable logic controller under code injection and code modification attacks demonstrates its ability to detect attack artifacts in memory dumps.

Asmar Awad, Rima [ORNL] (ORCID:0000000233407742)↗

Mafic explosive volcanism at Llaima Volcano: 3D x-ray microtomography reconstruction of pyroclasts to constrain shallow conduit processes

Abstract Mafic volcanic activity is dominated by effusive to mildly explosive eruptions. Plinian and ignimbrite-forming mafic eruptions, while rare, are also possible; however, the conditions that promote such explosivity are still being explored. Eruption style is determined by the ability of gas to escape as magma ascends, which tends to be easier in low-viscosity, mafic magmas. If magma permeability is sufficiently high to reduce bubble overpressure during ascent, volatiles may escape from the magma, inhibiting violent explosive activity. In contrast, if the permeability is sufficiently low to retain the gas phase within the magma during ascent, bubble overpressure may drive magma fragmentation. Rapid ascent may induce disequilibrium crystallization, increasing viscosity and affecting the bubble network with consequences for permeability, and hence, explosivity. To explore the conditions that promote strongly explosive mafic volcanism, we combine microlite textural analyses with synchrotron x-ray computed microtomography of 10 pyroclasts from the 12.6 ka mafic Curacautín Ignimbrite (Llaima Volcano, Chile). We quantify microlite crystal size distributions (CSD), microlite number densities, porosity, bubble interconnectivity, bubble number density, and geometrical properties of the porous media to investigate the role of magma degassing processes at mafic explosive eruptions. We use an analytical technique to estimate permeability and tortuosity by combing the Kozeny-Carman relationship, tortuosity factor, and pyroclast vesicle textures. The groundmass of our samples is composed of up to 44% plagioclase microlites, > 85% of which are < 10 µm in length. In addition, we identify two populations of vesicles in our samples: (1) a convoluted interconnected vesicle network produced by extensive coalescence of smaller vesicles (> 99% of pore volume), and (2) a population of very small and completely isolated vesicles (< 1% of porosity). Computed permeability ranges from 3.0 × 10 −13 to 6.3 × 10 −12 m 2 , which are lower than the similarly explosive mafic eruptions of Tarawera (1886; New Zealand) and Etna (112 BC; Italy). The combination of our CSDs, microlite number densities, and 3D vesicle textures evidence rapid ascent that induced high disequilibrium conditions, promoting rapid syn-eruptive crystallization of microlites within the shallow conduit. We interpret that microlite crystallization increased viscosity while simultaneously forcing bubbles to deform as they grew together, resulting in the permeable by highly tortuous network of vesicles. Using the bubble number densities for the isolated vesicles (0.1-3 −3 × 10 4 bubbles per mm 3 ), we obtain a minimum average decompression rate of 1.4 MPa/s. Despite the textural evidence that the Curacautín magma reached the percolation threshold, we propose that rapid ascent suppressed outgassing and increased bubble overpressures, leading to explosive fragmentation. Further, using the porosity and permeability of our samples, we estimated that a bubble overpressure > 5 MPa could have been sufficient to fragment the Curacautín magma. Other mafic explosive eruptions report similar disequilibrium conditions induced by rapid ascent rate, implying that syn-eruptive disequilibrium conditions may control the explosivity of mafic eruptions more generally.

Valdivia, Pedro↗

Benzene homologues contaminants in a former herbicide factory site: distribution, attenuation, risk, and remediation implication

Benzene homologues often used as organic raw materials or as detergents in chemical industry are prone to accidental release into the environment which can cause serious long-term soil pollutions. In a large former herbicide factory site, we investigated 43 locations for benzene homologues contaminations in soil, soil gas, and groundwater; and studied the hydrogeological conditions. An inverse distance weighted interpolation method was employed to determine the pollutants three-dimensional spatial distribution in the soils. Results showed that benzene homologues residues were mainly originated from the herbicide production workshop; and that the pollution had horizontally expanded at the deeper soil layer. Contaminants had already migrated 15m downward from ground surface. Contaminant phase distribution study showed that NAPL was the primary phase (>99%) for the pollutants accumulated in the unsaturated zone; while it had not migrated to groundwater. The primary mechanism for contaminant transport and attenuation included dissolution of “occluded” NAPL into pore water and pollutant volatilization into soil pore space. Risk assessment revealed that the pollutants brought unacceptable high carcinogenic and non-carcinogenic risks to public health. In order to convert this former chemical processing factory site into a residential area, a remediation to the polluted production workshop sites is urgently required.

Yang, Shuo↗

Development of coal-derived carbon-based structural unit as a potential new building material

Coal combustion for energy has not only wasted the hydrogen-rich volatile matters but also results in CO 2 emission causing serious environmental issues. An integrated coal pyrolysis and solvent extraction process under elevated temperatures in an inert atmosphere is implemented to convert as-mined coal from Wyoming Powder River Basin to functional carbon elements such as pyrolysis char (PC). This paper presents the development and fabrication of new carbon-based structural unit (CSU) using pulverized PC and two coal-derived pitches (mesophase pitch and tar pitch) to attain high compressive strength greater than 30 MPa, low thermal conductivity less than 0.30 W/m.K, and low density less than 1.25 g/cm 3 . CSUs have the potential to overcome the current challenges with cement and concrete through pressurized fabrication followed by carbonization. This study aims to develop CSU with nearly 100% coal-derived carbon material for structural application in buildings. The effects of pressing pressures, carbonization temperatures, and binder contents on the density and mechanical and thermal properties of CSU samples are investigated. The study concludes that mesophase pitch produces a better performance of CSU samples, a combination of 100 MPa pressing pressure and carbonization temperature of 900 ⁰C yields the highest compressive strength, and a 25% MP content is recommended for low-cost CSU fabrication. Furthermoer, CSU has a much lower density, lower thermal conductivity, higher compressive strength, and higher strength-to-density ratio than normal concrete.

36 MATERIALS SCIENCE↗

Gamma-ray spectrometry analysis methods for radioisotope dissolution and mixing for nuclear forensics applications

We report the production of surrogate nuclear explosive debris involves the dissolution of irradiated fissile material, elemental isolation, and recombination based on required fission product ratios. Gamma-ray spectrometry is used following each step to assess the radioactive fission product inventory. A high-purity germanium detector is used to measure each sample, and the detector efficiencies are determined prior to sample measurements. Through radiochemical techniques, elements are isolated and recombined into samples with specific fission product ratios. As a result, a matrix-based approach can account for imperfect chemical separations to calculate the proper mixture volumes to obtain intended volatile-to-refractory fission product ratios, or R-values.

07 ISOTOPE AND RADIATION SOURCES↗

Time dependent chlorination of CeO 2 , La 2 O 3 and Nd 2 O 3 by ZrCl 4 dissolved in eutectic LiCl–KCl

Partial chlorination of CeO 2 , La 2 O 3 , and Nd 2 O 3 was achieved using ZrCl 4 dissolved in molten LiCl-KCl at 450°C over a period of 4-5 hr. ZrCl 4 was pre-volatilized into an argon stream to maintain a constant vapor pressure for equilibration with the salt. This approach was effective at maintaining the ZrCl 4 concentration at the solubility limit of 1.3 mol% in the molten salt throughout the duration of two of the chlorination experiments and within about 60% of the solubility limit in the third experiment. Based on the analysis of salt samples, fractional conversion after four hours of reaction for CeO 2 , and five hours for La 2 O 3 , and Nd 2 O 3 were calculated to be 0.97, 0.28, and 0.65 respectively. Assuming a shrinking core diffusion-limited model, the diffusivity of ZrCl 4 through the hypothesized ZrO 2 layer was calculated for the chlorination of CeO 2 , La 2 O 3 , and Nd 2 O 3 were 1.76 x 10 -10 cm 2 /sec, 7.85 x 10 -12 cm 2 /sec, and 7.42 x 10 -12 cm 2 /sec, respectively. Given the extremely low values calculated for diffusivity, it was concluded that the process is chemical reaction rate limited and that a complete reaction of each rare earth oxide could be achieved. Furthermore, a chemically controlled shrinking core model was shown to also fit the experimental data closely.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Use of a Pressurized Water Treatment to Prevent Cracking of Internal Gelation Sol-Gel Microspheres

Pressurized water treatments were investigated as a means to prevent cracking of internal gelation sol-gel microspheres upon drying and heating. A batch of gelled cerium oxide microspheres was prepared, split into two samples that were processed with and without a pressurized water treatment, and dried in air at room temperature. Thermal gravimetric analysis was used to compare the mass loss profiles between the two samples and to understand volatile emissions from cerium oxide microspheres during heat treatments up to 600 °C. Microspheres that were processed without a pressurized water treatment lost approximately 4.6 times more mass upon heating than microspheres that were subjected to a pressurized water treatment. Comparison of the cracking behavior of microspheres prepared with and without a pressurized water treatment indicated that microspheres subjected to a pressurized water treatment were virtually crack-free after heat treatments. Conversely, microspheres processed without a pressurized water treatment, which is typical of traditional washing processes, exhibited extensive cracking. Analysis of residues dried from pressurized water treatment effluents indicated that hexamethylenetetramine and urea, which are excess reactants from the internal gelation process, were removed from gelled microspheres during the pressurized water treatment step. Traditional processing methods for preparing internal gelation microspheres use specific feed solution and gelation parameters to reduce subsequent cracking upon drying and heating. Results from this study indicate that more aggressive gel-forming conditions may be used to produce crack-free microspheres, if a pressurized water treatment step is included after washing and before air-drying.

cerium oxide, internal gelation, microsphere, TRIS↗