Process development for Ni-Cr-ThO2 and Ni-Cr-Al-ThO2 sheet

A process was developed for the production of thin gauge Ni-Cr-ThO2 sheet. The process was based on the elevated temperature deposition of chromium onto a wrought Ni-2%ThO2 sheet and subsequent high temperature diffusion heat treatments to minimize chromium concentration gradients within the sheet. The mechanical properties of the alloy were found to be critically dependent on those of the Ni-2%ThO2 sheet. A similar process for the production of a Ni-Cr-Al-ThO2 alloy having improved oxidation resistance was investigated but the non-reproducible deposition of aluminum from duplex Cr/Al packs precluded successful scale-up. The mechanical properties of the Ni-Cr-Al-ThO2 alloys were generally equivalent to the best Ni-Cr-ThO2 alloy produced in the programme.

Cook, R. C.↗

Structural studies on carbon materials for advanced space technology. Part 1: Structure and oxidation behavior of some carbon/carbon composite materials

The microstructure and some microstructural effects of oxidation have been investigated for laminar carbon fiber cloth/cloth binder matrix composite materials. It was found that cloth wave is important in determining the macrostructure of the composites X-ray diffraction analysis showed that the composites were more graphitic than the constituent fiber phases, indicating a graphitic binder matrix phase. Various tests which were conducted to investigate specific properties of the material are described. It was learned that under the moderate temperature and oxidant flow conditions studied, C-700, 730 materials exhibit superior oxidation resistance primarily because of the inhibiting influence of the graphitized binder matrix.

Fischbach, D. B.↗

Non-equilibrium stagnation region aerodynamic heating of hypersonic glide vehicles

A simple method of predicting aerodynamic heating and corresponding radiation equilibrium surface temperature-time histories for critical locations on space shuttle orbiter-type vehicles is presented. The method is based on a generalization of correlation equations developed earlier by Rosner for predicting the energy transfer and radiation equilibrium temperatures of surfaces with arbitrary catalytic activity and total hemispheric emittance. Recently obtained experimental data for O and N atom recombination probabilities on candidate material surfaces above 1000 K are used to assess nonequilibrium effects for a range of nose radii and a specific space shuttle re-entry trajectory. It is concluded that low catalytic activity will be especially important in locations of large effective nose radii by both increasing oxidation-resistant coating lifetime and reducing energy transfer into the vehicle.

Rosner, D. E.↗

Aluminized alloy boosts turbine blade life

Description of an aluminized alloy coating technique that involves first the application of a ductile, oxidation-resistant overlay, such as NiCrAl, which is then partially aluminized. The duplex protective system has performance advantages over conventional aluminide coatings in that it provides higher-temperature hot corrosion resistance over a longer service life.

Gedwill, M. A.↗

Quinoxaline polymers and copolymers derived from 1, 4-BIS(1'-napthalenyloxayl) benzene

A route for the synthesis of a new monomer, 1,4-bis(1'-naphthalenyl)-oxayl benzene, was devised, and six polymers and copolymers were prepared from this monomer, 1,4-bis(phenyloaxaly)benzene, 3,3'-diaminobenzidine and 3,3',4,4'-tetraaminobenzophenone. Thermogravimetric analysis showed that decomposition of these quinoxaline polymers and copolymers sets in at about 500 C but does not become significant in an inert atmosphere below 600 C. Oxidation becomes significant at about 550 C and the phenylquinoxaline homopolymer is somewhat more oxidation resistant than is the 1-naphthalenylquinoxaline homopolymer. Stress-relaxation measurements showed that, with two exceptions, the homopolymers and copolymers exhibited two second-order transition temperatures, one at about 204.4 C (400 F) and the other at about 315.6 C (600 F). No gross differences in the high temperature plasticity was observed between the naphthalenyl- and the phenyl-quinoaxaline homopolymers. Work was begun on a method for cross-linking polyquinoxalines. A new monomer, p-(methyloxaly)benzil, was synthesized, and model reaction studies showed that cross-linking of 2-methylquinoxaline polymers by a Michael condensation with dimaleimides will probably occur.

Port, W. S.↗

Study of the effects of fuel vortex film cooling on high temperature coating durability

A report on the effects of fuel vortex film cooling on high temperature coating durability is presented. The program evaluated candidate high temperature oxidation resistant reaction control system engine thrust chamber material. As a result of the evaluation, the current and future programs may be optimized from the materials standpoint. Engine firing data for the evaluation of one material system is generated. The subjects considered are: (1) screening of materials, (2) thrust chamber fabrication, (3) engine testing, and (4) analysis of the data.

Source record↗

Quaternary and quinary modifications of eutectic superalloys strengthened by delta Ni3Cb lamellae and gamma prime Ni3Al precipitates

By means of a compositional and heat treatment optimization program based on the quaternary gamma/gamma prime-delta, a tantalum modified gamma/gamma prime-delta alloy with improved shear and creep strength combined with better cyclic oxidation resistance was identified. Quinary additions, quaternary adjustments, and heat treatment were investigated. The tantalum modified gamma/gamma prime-delta alloy possessed a slightly higher liquidus temperature and exhibited rupture strength exceeding NASA VIA by approximately three and one-half Larson-Miller parameters (C = 20) above 1000 C. Although improvements in longitudinal mechanical properties were achieved, the shear and transverse strength property goals of the program were not met and present a continuing challenge to the alloy metallurgist.

Lemkey, F. D.↗

Plasma-sprayed, self-lubricating coatings for use from cryogenic temperatures to 870 deg C (1600 deg F)

A plasma-sprayed coating is described with good lubricating properties over a wide temperature range. The coating, designated NASA LUBE PS101, contains silver, nichrome, calcium fluoride, and an oxidation protective glass. Oscillating tests were conducted of self-aligning, plain cylindrical bearings, in which the bore was lined with 0.025 cm (0.010 in.) thick coatings of PS101; these were conducted at a radial load of 3.5 x 10 to the 7th power N/sq m (5000 psi) in nitrogen gas at -107 C (-160 F), in vacuum at room temperature, and in air from room temperature to 870 C (1600 F). Friction coefficients were less than 0.25 in all cases and wear rates were low. The coating is not brittle, and it has adequate oxidation resistance in air to at least 870 C.

Sliney, H. E.↗

New high-temperature noble-metal thermocouple pairing

A new thermocouple pairing was formed by combining thermocouple elements from two existing commercially available thermocouples to form a new combination (Ir-40 Rh/Pt-40 Rh) thermocouple. The output of this new pairing is nearly linear with temperature, and approximately equal to the output of one of the originating pairs (Ir-40 Rh/Ir), and more than double that of the other pair (Pt-40 Rh/Pt-20 Rh). This new pairing was evolved during a search for a noble-metal thermocouple combination which could operate above the temperature limit of a Pt-13 Rh/Pt thermocouple and have a higher oxidation resistance than an Ir-40 Rh/Ir thermocouple.

Glawe, G. E.↗

Comparison of isothermal and cyclic oxidation behavior of twenty-five commercial sheet alloys at 1150 C

Twenty-five commercial nickel-, iron-, and cobalt-base sheet alloys incorporating chromium or chromium and aluminum additions for oxidation resistance were tested at 1150 C in air for 100 hr in both isothermal and 1-hr cyclic furnace exposures. The alloys were evaluated by sample specific weight change, by type of scale formed, by amount and type of spall, and by sample thickness change and microstructure.-

Barrett, C. A.↗

Optimization of an oxide dispersion strengthened Ni-Cr-Al alloy for gas turbine engine vanes

The investigation was carried out to determine the optimum alloy within the Ni-16Cr-Al-Y2O3 system for use as a vane material in advanced aircraft gas turbine engines. Six alloys containing nominally 4%, 5% and 6% Al with Y2O3 levels of 0.8% and 1.2% were prepared by mechanical attrition. Six small-scale, rectangular extrusions were produced from each powder lot for property evaluation. The approximate temperatures for incipient melting were found to be 1658 K (2525 F), 1644 K (2500 F) and 1630 K (2475 F) for the 4%, 5% and 6% aluminum levels, respectively. With the exception of longitudinal crystallographic texture, the eight extrusions selected for extensive evaluation either exceeded or were close to mechanical property goals. Major differences between the alloys became apparent during dynamic oxidation testing, and in particular during the 1366 K (2000 F)/500 hour Mach 1 tests carried out by NASA-Lewis. An aluminum level of 4.75% was subsequently judged to be optimum based on considerations of dynamic oxidation resistance, susceptibility to thermal fatigue cracking and melting point.

Klarstrom, D. L.↗

Quaternary and quinary modifications of the eutectic superalloy gamma/gamma prime-delta

Quaternary modifications and quinary additions from the elements Co, Ti, Mo, W, Re, B, Si, and Ta to the baseline quaternary alloy gamma/gamma prime-delta Ni-19.7 at.% Nb-6.0 at.% Cr-2.5 at.% Al are examined for various concentrations. From modification studies five alloys were chosen for detailed mechanical property characterization: Ni-19.7 Nb-6.0 Cr-2.5 Al-1.0 W; Ni-19.7 Nb-6.0 Cr-2.5 Al-1.0 Mo; Ni-18.6 Nb-6.0 Cr-2.5 Al-0.87 Ti; Ni-20.2 Nb-6.0 Cr-2.5 Al-2.0 Co; and Ni-17.9 Nb-6.0 Cr-2.5 Al-3.0 Ta. It is shown that extensive alloying of the baseline quaternary alloy is possible for elements exhibiting a wide solubility range in both phases, and that limited substitution of W, Mo, Re, Si, and B is possible for elements with restricted solid solubility especially in the delta phase. Improvement of creep rupture strength and cyclic oxidation resistance at 1100 C is discussed.

Lemkey, F. D.↗

Directionally solidified eutectic alloy gamma-beta

A pseudobinary eutectic alloy composition was determined by a previously developed bleed-out technique. The directionally solidified eutectic alloy with a composition of Ni-37.4Fe-10.0Cr-9.6Al (in wt%) had tensile strengths decreasing from 1,090 MPa at room temperature to 54 MPa at 1,100 C. The low density, excellent microstructural stability, and oxidation resistance of the alloy during thermal cycling suggest that it might have applicability as a gas turbine vane alloy while its relatively low high temperature strength precludes its use as a blade alloy. A zirconium addition increased the 750 C strength, and a tungsten addition was ineffective. The gamma=beta eutectic alloys appeared to obey a normal freezing relation.

Tewari, S. N.↗

A Directionally Solidified Iron-chromium-aluminum-tantalum Carbide Eutectic Alloy

A eutectic alloy, Fe-13.6CR-3.7Al+9TaC, was directionally solidified in a high gradient furnace, producing a microstructure of alined TaC fibers in an oxidation resistant alpha-iron matrix. Tensile and stress rupture properties, thermal cycling resistance, and microstructures were evaluated. The alloy displays at 1000 C an ultimate tensile strength of 58 MPa and a 100-hour rupture life at a stress of 21 MPa. Thermal cycling to 1100 C induces faceting in the TaC fibers.

Harf, F. H.↗

Polymeric membrane systems of potential use for battery separators

Two membrane systems were investigated that may have potential use as alkaline battery separators. One system comprises two miscible polymers: a support polymer (e.g., polyvinyl formal) and an ion conductor such as polyacrylic acid. The other system involves a film composed of two immiscible polymers: a conducting polymer (e.g., calcium polyacrylate) suspended in an inert polymer support matrix, polyphenylene oxide. Resistivities in 45-percent potassium hydroxide and qualitative mechanical properties are presented for films comprising various proportions of conducting and support polymers. In terms of these parameters, the results are encouraging for optimum ratios of conducting to support polymers.

Philipp, W. H.↗

Directionally solidified eutectic gamma plus beta nickel-base superalloys

A directionally solidified multivariant eutectic gamma + beta nickel-base superalloy casting having improved high temperature strength and oxidation resistance properties is provided. This comprises a two phase eutectic structure containing, on a weight percent basis, 5.0-15.0 tungsten, 8.5-14.5 aluminum, 0.0-35.0 cobalt and the balance being nickel. Embedded within the gamma phase nickel-base matrix are aligned eutectic beta phase (primarily (NiCo)Al reinforcing lamellae.

Jackson, M. R.↗

Effect of double vacuum melting and retained austenite on rolling-element fatigue life of AMS 5749 bearing steel

AMS 5749 steel combines the tempering, hot hardness, and hardness retention characteristics of AISI M-50 steel with the corrosion and oxidation resistance of AISI 440C stainless steel. The five-ball fatigue tester was used to evaluate the rolling-element fatigue life of AMS 5749. Double vacuum melting (vacuum induction melting plus vacuum arc remelting, VIM-VAR) produced AMS 5749 material with a rolling-element fatigue life at least 14 times that of vacuum induction melting alone. The VIM-VAR AMS 5749 steel balls gave lives from 6 to 12 times greater than VIM-VAR AISI M-50 steel balls. The highest level of retained austenite, 14.6 percent, was significantly detrimental to rolling-element fatigue life relative to the intermediate level of 11.1 percent.

Parker, R. J.↗