Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Solidification microstructures”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 595 records · Page 33

Interactions Between Solidification and Compositional Convection in Alloys

This project combined theoretical and experimental ground-based studies of the interactions between convection and solidification of binary melts. Particular attention was focused on the alteration of the composition and microstructure of castings caused by convective flows through the interstices of mushy layers. Two different mechanisms causing convection were investigated. (i) Compositional, buoyancy driven convection is known to cause chimneys and freckles in directionally cast alloys on Earth. The analytical studies provide quantitative criteria for the formation of chimneys that can be used to assess the expediency of producing alloys in Space. (ii) Flow of the melt is also driven by the contraction (expansion) that typically occurs during change of phase. Such convection will occur even in the absence of gravity, and may indeed be the primary cause of macrosegregation during the production of alloys in Space. The studies will employed asymptotic methods in order to determine conditions for the stability of various states of solidifying systems. Further, simple macroscopic models of complete systems were developed and solved. These analytical studies were augmented by laboratory experiments using aqueous solutions, in which the convective flows could be easily observed and the effects of convection could be readily measured. These y experiments guided the development of the theoretical models and provided data against which the predictions of the models can be tested.

Davis, S. H.↗

Plasma Sprayed Hydroxyapatite Coatings: Influence of Spraying Power on Microstructure

The plasma sprayed hydroxyapatite (HA) coatings are used on metallic implants to enhance the bonding between the implant and bone in human body. The coating process was implemented at different spraying power for each spraying condition. The coatings formed from a rapid solidification of molten and partly molten particles that impact on the surface of substrate at high velocity and high temperature. The study was concentrated on different spraying power that is between 23 to 31 kW. The effect of different power on the coatings microstructure was investigated using scanning electron microscope (SEM) and phase composition was evaluated using X-ray diffraction (XRD) analysis. The coatings surface morphology showed distribution of molten, partially melted particles and some micro-cracks. The produced coatings were found to be porous as observed from the cross-sectional morphology. The coatings XRD results indicated the presence of crystalline phase of HA and each of the patterns was similar to the initial powder. Regardless of different spraying power, all the coatings were having similar XRD patterns.

36 MATERIALS SCIENCE↗

Characterization of Dendritic Spatially Extended 3D Patterns in Directional Solidification: Microgravity Experiments in DECLIC-DSI onboard ISS and 3D Phase-field Simulations

To clarify and characterize the fundamental physical mechanisms active in the dynamical formation of three-dimensional (3D) arrays of dendrites under diffusive growth conditions, in situ monitoring of series of experiments on transparent model alloy succinonitrile – 0.46 wt% camphor was carried out under low gravity in the DECLIC Directional Solidification Insert onboard the International Space Station. These experiments offer the very unique opportunity to observe in situ and characterize the dynamics of the microstructure formation and evolution in extended 3D patterns under microgravity environment. The analyses of the dendritic patterns for a broad range of growth velocities displaying different levels of sidebranching will be presented. Especially, the time evolution of primary spacing, in case of solidifications at constant pulling rate as well as for experiments with pulling rate jump, will be compared to 3D phase-field simulations, and the results will be discussed in terms of stable spacing range.

Kaihua Ji↗

Characterization of Dendritic Spatially Extended 3D Patterns in Directional Solidification: Microgravity Experiments in DECLIC-DSI Onboard ISS and 3D Phase-field Simulations

To clarify and characterize the fundamental physical mechanisms active in the dynamical formation of three-dimensional (3D) arrays of dendrites under diffusive growth conditions, in situ monitoring of series of experiments on transparent model alloy succinonitrile – 0.46 wt% camphor was carried out under low gravity in the DECLIC Directional Solidification Insert onboard the International Space Station. These experiments offer the very unique opportunity to observe in situ and characterize the dynamics of the microstructure formation and evolution in extended 3D patterns under microgravity environment. The analyses of the dendritic patterns for a broad range of growth velocities displaying different levels of sidebranching will be presented. Especially, the time evolution of primary spacing, in case of solidifications at constant pulling rate as well as for experiments with pulling rate jump, will be compared to 3D phase-field simulations, and the results will be discussed in terms of stable spacing range.

Kaihua Ji↗

Solidification Behavior of Calcium Ferrite Under Ultrasonic Vibration

Ultrasonic vibration was applied to the solidification process of calcium ferrite (CF) to modify the grain size and improve the homogeneity of the solidified microstructure. The effects of ultrasound on microstructure, density, compressive strength, and reducibility were studied. The acoustic pressure decreased and then increased along the axis symmetry due to the attenuation of acoustic pressure and reflection of ultrasonic waves in the melt under a fixed power. When the ultrasonic power was increased, the general acoustic pressure increased, which was beneficial to the avoidance of macropores and to improvement of the microstructure. Coarse acicular CF grains were significantly refined; the grain size decreased from 1967 to 442 μm when the ultrasonic power was increased from 0 to 300 W. The density of the samples increased from 4370 to 4680 kg/m{sup 3} due to cavitation and acoustic streaming effects. Ultrasonic vibration greatly improved the ultimate compressive strength of CF; the values were 41.8 ± 2.1 to 67.3 ± 3.4 MPa for ultrasonic powers of 100 to 300 W, respectively. Without ultrasonic treatment, it was only 37.4 ± 1.9 MPa. Ultrasonic vibration also influenced the reduction time of CF due to the composition segregation in the slag during solidification.

36 MATERIALS SCIENCE↗

Influence of convection on microstructure

The primary motivation for this research was to determine the cause for space processing altering the microstructure of some eutectics, especially the MnBi-Bi eutectic. Four primary hypotheses were to be tested under this current grant: (1) A fibrous microstructure is much more sensitive to convection than a lamellar microstructure, which was assumed in our prior theoretical treatment. (2) An interface with one phase projecting out into the melt is much more sensitive to convection than a planar interface, which was assumed in our prior theoretical treatment. (3) The Soret effect is much more important in the absence of convection and has a sufficiently large influence on microstructure that its action can explain the flight results. (4) The microstructure is much more sensitive to convection when the composition of the bulk melt is off eutectic. These hypotheses were tested. It was concluded that none of these can explain the Grumman flight results. Experiments also were performed on the influence of current pulses on MnBi-Bi microstructure. A thorough review was made of all experimental results on the influence of convection on the fiber spacing in rod eutectics, including results from solidification in space or at high gravity, and use of mechanical stirring or a magnetic field. Contradictory results were noted. The predictions of models for convective influences were compared with the experimental results. Vigorous mechanical stirring appears to coarsen the microstructure by altering the concentration field in front of the freezing interface. Gentle convection is believed to alter the microstructure of a fibrous eutectic only when it causes a fluctuating freezing rate with a system for which the kinetics of fiber branching differs from that for fiber termination. These fluctuations may cause the microstructure to coarsen or to become finer, depending on the relative kinetics of these processes. The microstructure of lamellar eutectics is less sensitive to freezing rate fluctuations and to gentle convection.

Wilcox, William R.↗

Metallic Powder Core Tubular Wire (PCTW) Development for Additive Manufacturing

NASA Langley Research Center (LaRC) in Hampton, VA, and the Center for Welding, Joining, and Coating Research (CWJCR) in the Department of Metallurgical and Materials Engineering at the Colorado School of Mines (CSM) in Golden, CO, have collaborated for nearly fifteen years to develop metallic powder core tubular wire (PCTW) feedstock for additive manufacturing (AM) using electron beam deposition. The motivation for this development was to offset dealloying observed during deposition of titanium and aluminum alloy solid wire feedstock in the LaRC electron beam freeform fabrication (EBF3) system and to explore novel alloy compositions by tailoring the powder fill. EBF3 is a fusion-based AM process that is performed under vacuum and is consequently prone to vaporization loss of low vapor pressure alloying elements. Research spanning four graduate student research projects succeeded in developing the basic methodology to fabricate PCTW, the mass balance equations used to define the powder fill, microstructure control through particulate inoculation, and the feasibility of producing metal matrix composite materials. Metallic PCTW is comprised of a thin foil sheath wrapped around a powder blend. Fabrication of PCTW at CSM was accomplished using a tubular wire mill system to first bend a flat strip into a u-shaped cross section, deposit a powder fill, create a lap joint to seal the wire, and draw to final diameter. Powder management systems were developed to ensure uniform mixing of powder constituents and identify feed rates for optimum fill ratios. Processing parameters were successfully developed for titanium and aluminum alloy sheaths to account for material work hardening during drawing. Mass balance equations were developed to account for compositional contributions of the sheath and powder fill. PCTW composition can be adjusted through selection of the sheath or powder materials. PCTWs were successfully developed to offset Al loss in deposits of Ti-6-4 and Mg loss in Al 6061, resulting in deposits that were within the composition limits for each material. Ti-6-4 deposits were fabricated using PCTW comprised of commercially pure (CP) titanium sheath and a fill of pre-alloyed Ti-6-4 powder with additions of elemental Al and V powders. Additions of both elements were required to account for the CP Ti from the sheath, and Al was further enhanced to offset documented losses in EBF3 deposits. For Al 6061 deposits, composition was modulated through the choice of sheath material. The PCTW was made using an Al 5052 sheath to supplement Mg content and a fill composition of pre-alloyed 6061 powder with additions of Si and Cu.The slower solidification rate of the EBF3 process compared with laser powder bed fusion processes can lead to coarse-grained microstructures and mechanical property anisotropy. EBF3deposits of Ti-6-4 exhibited large epitaxially grown β grains, which result in degraded mechanical properties in the deposition direction. Microstructure refinement was achieved through a combination of electron beam modulation and the use of a PCTW designed for Ti-6-4 deposits and modified by the addition of powder made from Fe and B. Resulting deposits exhibited reductions in β grain size, α phase colony intercept length and lath width, and an increased volume fraction of β phase. The mechanism of microstructure refinement was related to precipitation of boride particles. Hardness testing confirmed that mechanical property anisotropy was reduced and an overall increase in hardness was achieved.Metal matrix composite (MMC) materials offer strength and stiffness benefits over unreinforced materials. Two methods were investigated using PCTW technology for producing Al 6061 basedMMC materials; the direct addition of SiC reinforcing particles and the in-situ generation of reinforcements through reaction synthesis of precursor powders. Al 6061 based MMCs reinforced with SiC exhibited particle clustering and formation of aluminum carbides during deposition. The application of a Ni coating to the SiC particles prior to incorporation into the powder fill eliminated aluminum carbide formation and aided particle distribution during deposition. Modulation of beam focus and power further reduced aluminum carbide formation and aided particle distribution. In reaction synthesis, precursor additions undergo an exothermic reaction during deposition to form new ceramic products, generally of finer scale than the initial precursor components. The product phases provide reinforcement in the MMC and act as nucleation sites during solidification, resulting in grain refinement, improved mechanical properties, and reduced susceptibility to solidification cracking. Higher tensile strength and stiffness were demonstrated in Al 6061 based MMCs with 2 vol% reinforcement. These combined research efforts demonstrate the potential of PCTW technology for customizing of alloy composition and achieving microstructure control. A manufacturing process for titanium- and aluminum-based PCTWs was developed based on iterative design, theoretical calculations, and empirical data. PCTW technology successfully mitigated Al loss from Ti-6-4 and Mg loss in Al 6061, resulted in grain refinement in Ti-6-4, and demonstrated fabrication of Al based MMCs

Marcia S Domack↗

Solubility and microstructure in the pseudo-binary PbTe-Ag{sub 2}Te system

The solvus lines of the PbTe and Ag{sub 2}Te phases in the pseudo-binary PbTe-Ag{sub 2}Te system have been determined using diffusion couples and unidirectional solidification by the Bridgman method. The solubilities of both Ag{sub 2}Te in PbTe and PbTe in Ag{sub 2}Te decrease with decrease in temperature. For the former, this change is from 14.9 at% Ag (694 deg. C) to 0.5 at% Ag (375 deg. C), while for the latter it is from 12.4 at% Pb (650 deg. C) to 3.1 at% Pb (375 deg. C). The decrease in solubilities leads to the formation of precipitates of Ag{sub 2}Te in PbTe and PbTe in Ag{sub 2}Te. In particular, fast atomic diffusion in Ag{sub 2}Te results in the precipitation of PbTe even in quenched samples. From the temperature dependence of these solubilities, heats of solution have been determined. In the diffusion couple, the phase boundary moves toward PbTe. In the region between the phase boundary and the initial interface, PbTe transforms to {beta}-Ag{sub 2}Te (cubic) retaining the cube-on-cube orientation relationship. - Graphical abstract: The precipitation in the diffusion couple in fast cooling suggests high chemical diffusivity. The large heat of solution for the Ag{sub 2} Te dissolution in PbTe leads to fine microstructure. Highlights: > The solvus lines were determined by diffusion couples and unidirectional solidification. > The solubilities in both phases decrease with decrease in temperature. > Chemical diffusivity in Ag2Te phase is high. > Heat of solution is one of the key parameters to control the number density of precipitates. > The Ag2Te phase transformed from PbTe in diffusion couples holds the cube-on-cube relationship.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Materials for Advanced Ultrasupercritical Steam Turbines Task 4: Cast Superalloy Development

The Steam Turbine critical stationary structural components are high integrity Large Shell and Valve Casing heavy section Castings, containing high temperature steam under high pressures. Hence to support the development of advanced materials technology for use in an AUSC steam turbine capable of operating with steam conditions of 760°C (1400°F) and 35 Mpa (5000 psia), Casting alloy selection and evaluation of mechanical, metallurgical properties and castability with robust manufacturing methods are mandated. Alloy down select from Phase 1 based on producability criteria and creep rupture properties tested by NETL-Albany and ORNL directed the consortium to investigate cast properties of Haynes 282 and Haynes 263. The goals of Task 4 in Phase 2 are to understand a broader range of mechanical properties, the impact of manufacturing variables on those properties. Scale up the size of heats to production levels to facilitate the understanding of the impact of heat and component weight, on metallurgical and mechanical behavior. GE Power & Water Materials and Processes Engineering for the Phase 2, Task 4.0 Castings work, systematically designed and executed casting material property evaluation, multiple test programs. Starting from 15 lbs. cylinder castings to world’s first 17,000 lbs. poured weight, heavy section large steam turbine partial valve Haynes 282 super alloy casting. This has demonstrated scalability of the material for steam Turbine applications. Activities under Task 4.0, Investigated and characterized various mechanical properties of Cast Haynes 282 and Cast Nimonic 263. The development stages involved were: 1) Small Cast Evaluation: 4 inch diam. Haynes 282 and Nimonic 263 Cylinders. This provided effects of liquidus super heat range and first baseline mechanical data on cast versions of conventional vacuum re-melted and forged Ni based super alloys. 2) Step block castings of 300 lbs. and 600 lbs. Haynes 282 from 2 foundry heats were evaluated which demonstrated the importance of proper heat treat cycles for Homogenization, and Solutionizing parameters selection and implementation. 3) Step blocks casting of Nimonic 263: Carried out casting solidification simulation analysis, NDT inspection methods evaluation, detailed test matrix for Chemical, Tensile, LCF, stress rupture, CVN impact, hardness and J1C Fracture toughness section sensitivity data and were reported. 4) Centrifugal Casting of Haynes 282, weighing 1400 lbs. with hybrid mold (half Graphite and half Chromite sand) mold assembly was cast using compressor casing production tooling. This test provided Mold cooling rates influence on centrifugally cast microstructure and mechanical properties. Graphite mold section out performs sand mold across all temperatures for 0.2% YS; %Elongation, %RA, UTS at 1400°F. Both Stress-LMP and conditional Fracture toughness plots data were in the scatter band of the wrought alloy. 5) Fundamental Studies on Cooling rates and SDAS test program. Evaluated the influence of 6 mold materials Silica, Chromite, Alumina, Silica with Indirect Chills, Zircon and Graphite on casting solidification cooling rates. Actual Casting cooling rates through Liquidus to Solidus phase transition were measured with 3 different locations based thermocouples placed in each mold. Compared with solidification simulation cooling rates and measurement of SDAS, microstructure features were reported. The test results provided engineered casting potential methods, applicable for heavy section Haynes 282 castings for optimal properties, with foundry process methods and tools. 6) Large casting of Haynes 282 Drawings and Engineering FEM models and supplemental requirements with applicable specifications were provided to suppliers for the steam turbine proto type feature valve casing casting. Molding, melting and casting pouring completed per approved Manufacturing Process Plan during 2014 Q4. The partial valve casing was successfully cast after casting methods were validated with solidification simulation analysis and the casting met NDT inspection and acceptance criteria. Heat treated and sectioned to extract trepan samples at different locations comparing with cast on coupons test data. Material properties requisite for design, such as tensile, creep/rupture, LCF, Fracture Toughness, Charpy V-notch chemical analysis testing were carried out. The test results will be presented in the final report. The typical Haynes 282 large size Steam Turbine production casting from Order to Delivery foundry schedule with the activity break up is shown in Figures 107 and 108. • From Purchase Order placement to Casting pouring ~ 26 weeks. 1. Sales and commercial review 3 2. Engineering Drawings/models review 4 3. Pattern and core box manufacturing 6 4. Casting process engineering review 4 5. FEM and solidification simulation analysis 4 6. Gating & Feeder Attachments, Ceramic tiling 2 7. Molding and coremaking production scheduling 6 8. Melting planning and schedule 3 9. Pouring, cooling and shake out 2 • From Pouring to casting Delivery ~ 29 weeks 10. Shot blast and riser cutting, gates removal 3 11. Homogenizing , solutionizing HT furnace prep 4 12. Grinding, Fettling 2 13. Aging HT Cycle, cooling 2 14. VT and LPT NDT inspections 2 15. Radiographic inspection 4 16. Mechanical testing, Chemical analysis test certs 4 17. Casting weld repair upgrades and Aging PWHT 4 18. NDT after weld repairs and casting upgrades 3 19. Casting Final Inspection and test certifications 3 20. Package and delivery 2 Hence the Total Lead time from P.O to Casting delivery is approximately 55 weeks. The Task 4.2 and Task 4.3 activities and reporting completed.

Thangirala, Mani↗

Surface film effects on drop tube undercooling studies

The effects of various gaseous atmospheric constituents on drop-tube solidified samples of elemental metals were examined from a microstructural standpoint. All specimens were prepared from the purest available elements, so effects of impurities should not account for the observed effects. The drop-tube gas has a definite effect on the sample microstructure. Most dramatically, the sample cooling rate is effected. Some samples receive sufficient cooling to solidify in free fall while others do not, splating at the end of the drop tube in the sample catcher. Gases are selectively absorbed into the sample. Upon solidification gas can become less soluble and as a result forms voids within the sample. The general oxidation/reduction characteristics of the gas also affect sample microstructures. In general, under the more favorable experimental conditions including reducing atmospheric conditions and superheatings, examination of sample microstructures indicates that nucleation has been suppressed. This is indicated by underlying uniform dendrite spacings throughout the sample and with a single dendrite orientation through most of the sample. The samples were annealed yielding a few large grains and single or bi-crystal samples were commonly formed. This was especially true of samples that were inadvertently greatly superheated. This is in contrast with results from a previous study in which surface oxides were stable and contained numerous sites of nucleation. The number of nucleation events depends upon the surface state of the specimen as determined by the atmosphere and is consistent with theoretical expectations based upon the thermodynamic stability of surface oxide films. Oxide-free specimens are characterized by shiny surfaces, with no observable features under the scanning electron microscope at 5000X.

Ethridge, E. C.↗

M551 metals melting experiment

The Metals Melting Skylab Experiment consisted of selectively melting, in sequence, three rotating discs made of aluminum alloy, stainless steel, and tantalum alloy. For comparison, three other discs of the same three materials were similarly melted or welded on the ground. The power source of the melting was an electron beam unit. Results are presented which support the concept that the major difference between ground base and Skylab samples (i.e., large elongated grains in ground base samples versus nearly equiaxed and equal sized grains in Skylab samples) can be explained on the basis of constitutional supercooling, and not on the basis of surface phenomena. Microstructural observations on the weld samples and present explanations for some of these observations are examined. In particular, ripples and their implications to weld solidification were studied. Evidence of pronounced copper segregation in the Skylab A1 weld samples, and the tantalum samples studied, indicates a weld microhardness (and hence strength) that is uniformly higher than the ground base results, which is in agreement with previous predictions. Photographs are shown of the microstructure of the various alloys.

Li, C. H.↗

Senary refractory high-entropy alloy Cr x MoNbTaVW

This paper demonstrates that a senary refractory high-entropy alloy Cr x MoNbTaVW can be tailored over a certain range of Cr content with the BCC structure for different microstructures and physical properties, assisted by CALPHAD simulations. Microstructure characterizations are performed using X-ray diffraction and scanning electron microscopy. Chemical microsegregation during solidification predicted using the Scheil model generally agrees with the experimental results. The lattice constant, density, and Vickers’ micro-hardness of the highentropy alloy samples in the as-cast state are measured and discussed. For Cr x MoNbTaVW, x=2.0 case appears exceeding the upper limit of maintaining a single BCC phase HEA, determined by the XRD patterns. The elemental dependence of the mixing thermodynamic properties (entropy, enthalpy and Gibbs energy) in BCC phase in the senary system is analyzed. The calculated entropy of mixing and enthalpy of mixing for CrMoNbTaVW are 14.7 J/K/mol and -662.5 J/mol respectively.

36 MATERIALS SCIENCE↗

Assessment of phase constitution on the Al-rich region of rapidly solidified Al-Co-Fe-Cr alloys

The formation of quasicrystalline approximants in rapidly solidified Al-Co-Fe-Cr alloys was investigated. Alloys of atomic composition Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8}, Al{sub 77}Co{sub 11}Fe{sub 6}Cr{sub 6} and Al{sub 76}Co{sub 19}Fe{sub 4}Cr{sub 1} were produced using melt spinning and arc melting methods and their microstructural characterization was carried out by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. Up to the present there is no consensus in the literature regarding the formation of quasicrystalline phase or quasicrystalline approximants in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy. This work presents, for the first time, a detailed structural characterization of selected alloys in the Al-Co-Fe-Cr system close to the atomic composition Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8}. The results indicated the samples to be composed, mostly, by two intermetallic phases, which are quaternary extensions of Al{sub 5}Co{sub 2} and Al{sub 13}Co{sub 4} and are quasicrystalline approximants. Although the Al{sub 5}Co{sub 2} phase has already been reported in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy, the presence of the monoclinic Al{sub 13}Co{sub 4} is now identified for the first time in the as cast state. In the binary Al-Co system a quasicrystalline phase is known to form in a rapidly solidified alloy with composition close to the monoclinic and orthorhombic Al{sub 13}Co{sub 4} phases. This binary quasicrystalline phase presents an average valence electron per atom (e/a) between 1.7 and 1.9; thus, in addition to the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy, the compositions Al{sub 77}Co{sub 11}Fe{sub 6}Cr{sub 6} and Al{sub 76}Co{sub 19}Fe{sub 4}Cr{sub 1} were chosen to be within the region of formation of the quaternary extension of the Al{sub 13}Co{sub 4} phase and also within the (e/a) of 1.7 to 1.9. However, no quasicrystalline phase is present in any of the studied alloys. The Al-Co-Fe-Cr system, around the compositions studied, is composed of quaternary extensions of Al-Co intermetallic phases, which present solubility of Fe and Cr at Co atomic sites. - Highlights: •The Al rich region of the AlCoFeCr system is studied concerning phase formation on rapidly solidified alloys. •The alloys were composed mostly by quaternary extensions of Al-Co intermetallic phases. •Al{sub 5}Co{sub 2} and Al{sub 13}Co{sub 4} were the major phases observed in the alloys and are approximants of a quasicrystalline phase. •No quasicrystalline phase was observed in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} composition.

36 MATERIALS SCIENCE↗

Characterization of texture and grain boundary character distributions of selective laser melted Inconel 625 alloy

Highlights: • <110> texture along layer build direction was generated in as-SLMed Inconel 625. • The stress relief process dominates texture and GBCD evolution. • SLMed IN 625 alloy can be GBEed via suitable post annealing. - Abstract: Select laser melting (SLM) is one of the practical metal additive manufacturing processes to fabricate complex structures. The inhomogeneous microstructure and high residual stress are typically resulted from a non-uniform melting and rapid solidification during a SLM process, which has the significant impact on part dimensional instability, corrosion resistance, and mechanical properties. The bulk of current research is limited to the general characterization of grain size, texture, and mechanical properties. However, grain boundary character distribution (GBCD) and its relationship with texture are yet to be understood. This study has shown that the preferred <110> along building direction and <100> along laser scanning direction were produced. The high density of low angle grain boundary (LAGB) can be an indicator of residual stress levels in the as-SLMed samples. The newly-developed ∑3, ∑9 and ∑27 grain boundaries were heavily populated, and the cluster of grains interfaced by ∑3{sup n} (n = 0, 1, 2…) was introduced at the expense of LAGB only at high recrystallization annealing (1150°C or over). The research results suggest that GBCD optimization be possible in the SLMed Inconel 625 alloy via suitable post annealing, which allows improving intergranular corrosion resistance and enhancing mechanical properties.

36 MATERIALS SCIENCE↗

Ternary eutectic growth of nanostructured thermoelectric Ag-Pb-Te materials

Nanostructured Ag-Pb-Te thermoelectric materials were fabricated by unidirectionally solidifying the ternary Ag-Pb-Te eutectic and near-eutectic alloys using the Bridgeman method. Specially, the Bridgman-grown eutectic alloy exhibited a partially aligned lamellar microstructure, which consisted of Ag{sub 5}Te{sub 3} and Te phases, with additional 200-600 nm size particles of PbTe. The self-assembled interfaces altered the thermal and electronic transport properties in the bulk Ag-Pb-Te eutectic alloy. Presumably due to phonon scattering from the nanoscale microstructure, a low thermal conductivity ({kappa} = 0.3 W/mK) was achieved of the eutectic alloy, leading to a zT peak of 0.41 at 400 K.

36 MATERIALS SCIENCE↗

Additive Manufactured Composite Phase-Change Material for Thermal Energy Storage Applications

Phase-change materials play a critical role in industrial energy storage applications to drive efficiency improvements, thermal energy management, and carbon emissions reductions. Recently, it has been shown that rapid solidification of alloys with metastable immiscibility in the liquid phase has the potential to form unique microstructures in which a low-melting phase is uniformly distributed in a high-melting matrix. This feature can be exploited using additive manufacturing to produce components with complex geometries containing such unique phase-change microstructures. Phase-field simulations utilizing high-performance computing were used to provide a detailed description of the evolution of the active phase during service in terms of their morphology and composition in different polycrystalline matrix grain morphologies that are typically produced during additive manufacturing. Phase field simulations were performed using, MEUMAPPS-SL (Microstructure Evolution Using Massively Parallel Phase-field Simulations – Solid Liquid) code that was developed in-house by the Oak Ridge National Laboratory. The simulations utilized the capabilities of the Kestrel supercomputer at the National Renewable Energy Laboratory. The simulation results were compared with experimental results generated at Siemens Energy, Inc. The results indicate that the kinetics of liquid spreading along grain boundaries is largely determined by the mobility of the triple line along the intersection of the grain boundary liquid and the grain boundary plane.

25 ENERGY STORAGE↗

Bulk undercooling

Bulk undercooling methods and procedures will first be reviewed. Measurement of various parameters which are necessary to understand the solidification mechanism during and after recalescence will be discussed. During recalescence of levitated, glass-encased large droplets (5 to 8 mm diam) high speed temperature sensing devices coupled with a rapid response oscilloscope are now being used at MIT to measure local thermal behavior in hypoeutectic and eutectic binary Ni-Sn alloys. Dendrite tip velocities were measured by various investigators using thermal sensors or high speed cinematography. The confirmation of the validity of solidification models of bulk-undercooled melts is made difficult by the fineness of the final microstructure, the ultra-rapid evolution of the solidifying system which makes measurements very awkward, and the continuous modification of the microstructure which formed during recalescence because of precipitation, remelting and rapid coarsening.

Kattamis, T. Z.↗

Splat Quenching as a High Throughput Rapid Solidification Testing Method for Developing Additive Manufacturing Alloys

Splat quenching as a high throughput rapid solidification screening tool is evaluated. Samples were made using known alloys (SS316, IN625, Ti-5553) to evaluate and establish the microstructures for a variety of alloy systems as well as the predicted cooling rates. The samples are inductively heated and levitated prior to being struck between two platens that produce a high contact pressure and a thin sample resulting in cooling rates on the order of 10 6 to 10 7 K/s. Process parameters were evaluated with analytical models in addition to numerical simulations to provide an effect of process variables such as substrate material, melt superheat, and platen velocity on the resulting solidification. The splat thickness was found to be controlled by platen velocity, melt superheat, as well as the feedstock volume. The sample thickness is the key controlling factor for varying the average cooling rate experienced by the splat quenched sample. The splat quenching techniques can reach regions of rapid solidification space that meet and exceed laser and electron beam techniques across the sample. In conclusion, the results of the study provide a useful foundation in understanding the splat quenching technique and its potential as a low effort tool to explore rapid solidification effects on alloys.

Alloy Design↗