Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Shear Strength”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 595 records · Page 33

On the Steel–Aluminum Hybrid Casting by Sand Casting

Hybrid casting is a well-known technology to join steel inserts and aluminum. In order to achieve a high-performance material-based joining between steel and aluminum, a new PVD Al-Si-(Fe) coating, which consists of two sub-layers, has been successfully developed for high-pressure die casting. This coating system has been investigated further in this work for the sand casting process. By extending the sand casting process to the plaster casting process with preheating possibilities for the coated steel inserts, a material-based connection between steel and aluminum with a tensile shear strength of 7.7 MPa could be created. The ductility of this connection is decreased comparing with the connection manufactured by die casting. SEM and EDS analysis and diffusion experiments show that the difference of mechanical properties between plaster and die casting is caused by the extensive diffusion and the corresponding layer growth at plaster casting. The edge separation in plaster casting is a result of the edge stresses due to the different thermal expansion of steel and aluminum which can be suppressed at high-pressure die casting. To improve the joining properties at sand casting, it is necessary to control the layer diffusion by adding other alloy elements such as Mn into the Al-Si-(Fe) coating layer.

36 MATERIALS SCIENCE↗

Brazing of Martensitic Stainless Steel to Copper Using Electroplated Copper and Silver Coatings

Brazing of 3 mm thick sheets of low-carbon martensitic stainless steel and Cu-Cr-Zr-Ti alloy was attempted using electroplated coatings of Cu and Ag. Ni coating of 5 µm thick was provided on the MSS base metal to enhance the wettability. Brazing experiments were carried out at 985 °C for a holding of 15 min. Detailed microstructural studies, hardness, lap-shear, tensile, and pressure tests were carried out on the brazed joints. The reaction between the Cu and Ag coatings lead to the formation of in situ braze metal. The microstructure of the braze metal was found to consist of Cu-rich primary alpha (α{sub P}) and Ag-rich eutectic mixture (β + α{sub E}). In lap-shear tests, the brazed joints produced with an overlap of 9 and 6 mm were found to fail in copper base metal, while the joints produced with an overlap of 3 mm failed in the braze metal exhibiting a lap-shear strength of 147 MPa. In tensile tests, the butt brazed joints were found to fail in copper base metal as well with an average tensile strength of 213 MPa. The braze metal hardness was found to be higher than the hardness of the copper base metal. In pressure tests, the brazed panels were found to survive a pressure of 750 bar without undergoing any damage. These results show that electroplated coatings of Cu and Ag can be advantageously utilized for brazing of large, complex-shaped parts such as thrust chambers in space industry.

36 MATERIALS SCIENCE↗

Plasma treatment on both adhesive tape and adherends for significantly enhanced CFRTP-related adhesive joints

Unlike existing literature that primarily concentrates on either the plasma treatment of adherends alone or solely on adhesive surfaces, this work leverages plasma modification of both adhesive in tape form and adherend surfaces to largely enhance the interfacial bonding between a thermoset-based adhesive tape and carbon-fiber-reinforced thermoplastic polymer (CFRTP) for structural bonding applications. Here, by conducting single lap shear tests on adhesively-bonded AA6061-CFRPPA (carbon-fiber-reinforced polyphthalamide) dissimilar joints, it is shown that the plasma treatment of adherends alone can increase the lap shear strength (LSS) of the joints by approximately 200% compared to non-treated counterparts. An additional plasma treatment of adhesive tape surfaces leads to even higher LSS improvement, reaching up to 315%, due to the formation of a denser crosslinked network of covalent bonds and a reduced area fraction of interfacial voids at the CFRPPA/adhesive interface. The highest plasma-enhanced LSS of the metal-CFRTP dissimilar joints rivals that of metal-metal joints, which is typically stronger than the joints associated with fiber-reinforced polymers. This study is important for achieving strong CFRTP-related structural components bonded using adhesive tape, providing better compatibility with plasma treatment and other joining methods like riveting compared to adhesive paste or liquid.

36 MATERIALS SCIENCE↗

Relating storm-snow avalanche instabilities to data collected from the Differential Emissivity Imaging Disdrometer (DEID)

Storm-snow avalanches are challenging to forecast due to complex alpine terrain and during rapidly changing weather conditions. They can result in loss of lives and significant economic impact. We describe how a new device that continuously measures with high-frequency snowflake mass, size, density, and type, the Differential Emissivity Imaging Disdrometer (DEID), and show how the DEID can be used to aid avalanche forecasting when coupled with a storm-snow stability model. DEID measurements of snow accumulation, snow water equivalent (SWE), and snow density obtained during seventeen storms taken at the mid-Collins Snow-Study Plot at Alta Ski Area in Utah's Central Wasatch mountain range during winter 2020–2021 show excellent agreement with infrequent manual measurements. Additionally, two new variables, the Shape Density Index (SDI) and Complexity, are proposed and used to classify snowflake habit and estimate storm-snow shear strength. We illustrate how these DEID-derived data can be used to identify layers of concern in the storm snow such as density inversions, in real-time without digging snow pits. Furthermore, the DEID-data are used to run four variations of the SNOw Slope Stability model (SNOSS) for the storms investigated. The results are evaluated with data collected from tilt-board tests, infrasound measurements, and visual observations of avalanches. For a total fourteen storms analyzed, the DEID-driven SNOSS-modeled minimum stability index predicts the general stability of the storm-snow as indicated by observed avalanches, both natural and of unknown cause. Finally, the results provide a promising approach for nowcasting instabilities within storm-snow layers with a single instrument.

54 ENVIRONMENTAL SCIENCES↗

Sizing comingled CF/PA 6 fibers with cellulose nanofibrils for enhanced performance properties

Compatibility between the reinforcing phase and the polymer matrix is critical to achieving the desired mechanical and thermal performance of composite materials. Several mechanisms can enhance this interfacial interaction, including surface treatments (e.g., oxidation, plasma, or irradiation), in-situ nanoparticle deposition, and fiber sizing. Here, in this study, cellulose nanofibrils (CNF) were employed as a sustainable sizing agent to modify the interface in commingled carbon fiber (CF)/polyamide 6 (PA 6) yarns, in which CF and PA6 filaments are intimately blended to enable simultaneous consolidation. A 0.25 wt% CNF aqueous suspension was applied under bath sonication to ensure uniform dispersion and minimize agglomeration. CNF-sized and unsized yarns were used to fabricate unidirectional composite plates via filament winding on a flat mandrel, followed by compression molding. Scanning electron microscopy confirmed CNF presence on both CF and PA6 filaments. CNF-sized composites exhibited increments in interlaminar shear strength (ILSS) by 50%, flexural strength by 11%, and tensile strength by 2.5% compared to unsized composites. Thermal analysis showed minimal changes in degradation temperature and crystallinity. These findings demonstrate that CNF sizing enhances interfacial bonding and mechanical performance, offering a scalable and environmentally friendly strategy for thermoplastic composite manufacturing along with yarn/tow handleability.

Cellulose nanofibrils (CNF)↗

4D electrical resistivity tomography for assessing the influence of vegetation and subsurface moisture on railway cutting condition

Instability of slopes, embankments, and cuttings on the railway network is increasingly prevalent globally. Monitoring vulnerable infrastructure aids in geotechnical asset management, and improvements to transport safety and efficiency. Here, we examine the use of a novel, near-real-time Electrical Resistivity Tomography (ERT) monitoring system for assessing the stability of a railway cutting in Leicestershire, United Kingdom. In 2015, an ERT monitoring system was installed across a relict landslide (grassed) and an area of more stable ground on either side (wooded), to monitor changes in electrical resistivity through time and space, and to assess the influence of different types of vegetation on the stability of transportation infrastructure. Two years of 4-Dimensional ERT monitoring results are presented here, and petrophysical relationships developed in the laboratory are applied to calibrate the resistivity models in order to provide an insight into hydrogeological pathways within a railway cutting. The influence of vegetation type on subsurface moisture pathways and on slope stability is also assessed – here we find that seasonal subsurface changes in moisture content and soil suction are exacerbated by the presence of trees (wooded area). This results in shrink-swell behaviour of the clays comprising the railway cutting, resulting in fissuring and a reduction in shear strength, leading to instability. As such, it is proposed that on slopes comprised of expansive soils, grassed slopes are beneficial for stability. Insights into the use of 4-D ERT for monitoring railway infrastructure gained from this study may be applied to the monitoring of critical geotechnical assets elsewhere.

58 GEOSCIENCES↗

Experimental evidence for chemo-mechanical coupling during carbon mineralization in ultramafic rocks

It is known that storing carbon dioxide in the subsurface as carbonate minerals has the benefit of long-term stability and immobility. Ultramafic rock formations have been suggested as a potential reservoir for this type of storage due to the availability of cations to react with dissolved carbon dioxide and the fast reaction rates associated with minerals common in ultramafic formations; however, the rapid reactions have the potential to couple with the mechanical and hydraulic behavior of the rocks and little is known about the extent and mechanisms of this coupling. In this study, we argue that the dissolution of primary minerals and the precipitation of secondary minerals along pre-existing fractures in samples lead to reductions in both the apparent Young's modulus and shear strength of aggregates, accompanied by reduction in permeability. Hydrostatic and triaxial deformation experiments were run on dunite samples saturated with de-ionized water and carbon dioxide-rich solutions while stress, strain, permeability and pore fluid chemistry were monitored. Sample microstructures were examined after reaction and deformation using scanning electron microscopy (SEM). The results show that channelized dissolution and carbonate mineral precipitation in the samples saturated with carbon dioxide-rich solutions modify the structure of grain boundaries, leading to the observed reductions in stiffness, strength and permeability. A geochemical model was run to help interpret fluid chemical data, and we find that the apparent reaction rates in our experiments are faster than rates calculated from powder reactors, suggesting mechanically enhanced reaction rates. In conclusion, we find that chemo-mechanical coupling during carbon mineralization in dunites leads to substantial modification of mechanical and hydraulic behavior that needs to be accounted for in future modeling efforts of in situ carbon mineralization projects.

58 GEOSCIENCES↗

Reformulating a Gurson-based dynamic damage model and demonstrating improved predictive power and numerical robustness

The original Tepla (TEnsile PLAsticity) ductile damage model, based on the Gurson yield surface, has long been used to model damage evolution and material failure under dynamic loading. Unfortunately, Tepla suffered from mesh sensitivity, numerical instability, and limited predictive capability. Here, we theoretically reformulate Tepla to address these issues. We especially focus on the prediction of porosity, which is the key state variable used for modeling ductile damage, as compared to more easily measured surface velocities, which are at best an indirect measure of damage. Key model changes include separating the viscosity during volumetric void growth from underlying shear strength behavior and switching to an iterative bisection solver. The new Tepla is then calibrated on incipient spall experiments on half-hard copper and tantalum, which demonstrate its ability to simultaneously fit the model to recovered porosity distributions and measured surface velocities, a stringent test. Improved numerical behavior, such as greatly reduced mesh sensitivity, is also shown in those simulations. Finally, the new Tepla model is applied to several high-explosive loaded, sweeping wave experiments, showing the ability of the model to predict behavior on tests with significantly different loading conditions and histories than the calibration data.

36 MATERIALS SCIENCE↗

In situ observation of the deformation and fracture of an alumina-alumina ceramic-matrix composite at elevated temperature using x-ray computed tomography

The deformation and fracture of a 0/90° Nextel 720 mullite fibre / alumina matrix ceramic-matrix composite material has been observed by in situ synchrotron x-ray computed micro-tomography at ambient temperature and at 1100 °C. A three-point loading configuration was used and samples were loaded monotonically until final fracture. Here, the flexural strength was found to be unaffected by temperature. 3D visualisation of the microstructure showed fracture occurred by propagation of internal cracks at stresses close to the flexural strength. Shear fractures propagated across fibre bundles that were oriented perpendicular to the flexural stress at both room temperature and 1100 °C. At the higher temperature, an additional failure mode of delamination was observed, that may arise from relaxation of thermal residual stresses and creep.

36 MATERIALS SCIENCE↗

Irradiation resistance of silicon carbide joint at light water reactor–relevant temperature

We fabricated and irradiated monolithic silicon carbide (SiC) to SiC plate joints with neutrons at 270–310 °C to 8.7 dpa for SiC. The joining methods included solid state diffusion bonding using titanium and molybdenum interlayers, SiC nanopowder sintering, reaction sintering with a Ti-Si-C system, and hybrid processing of polymer pyrolysis and chemical vapor infiltration (CVI). All the irradiated joints exhibited apparent shear strength of more than 84 MPa on average. Significant irradiation-induced cracking was found in the bonding layers of the Ti and Mo diffusion bonds and Ti-Si-C reaction sintered bond. Furthermore, the SiC-based bonding layers of the SiC nanopowder sintered and hybrid polymer pyrolysis and CVI joints all showed stable microstructure following the irradiation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Grain structure, texture and mechanical property evolution of automotive aluminium sheet during high power ultrasonic welding

High power ultrasonic spot welding (HPUSW) is a joining technique which is performed within less than a second and provides a more energy-efficient alternative to friction stir spot welding (FSSW), which is considered a longer cycle manufacturing process for joining automotive alloys. To date, only a few reports exist on the deformation mechanisms that take place during high power ultrasonic spot welding. In this work, dynamic recrystallization and grain growth were examined using electron backscatter diffraction (EBSD). HPUSW causes extensive deformation within the weld zone where the temperature increases to 440 °C. An ultra-fine grain structure was observed in a thin band of flat weld interface within a short welding time of 0.10 s. With increasing welding time the interface was displaced and ‘folds’ or ‘crests’ appeared together with shear bands. The weld interface progressively changed from flat to sinusoidal and eventually to a convoluted wave-like pattern when the tool fully penetrated the workpiece, having a wavelength of ~ 1 mm after 0.40 s. Finally, the microstructure and texture varied significantly depending on the location within the weld. Although the texture near the weld interface was relatively weak, a shift was observed with increasing welding time from an initially Cube-dominated texture to one where the typical β-fibre Brass component prevailed. - Highlights: •Lap shear strength of ~2.9 kN was achieved in 0.30 sec welding time. •Temperature approached 440 °C along the weld centreline for the highest welding time. •The texture near the teeth was dominated by Brass, P and S components at optimum condition. •The weld interface showed typical β-fibre deformation texture at optimum condition.

36 MATERIALS SCIENCE↗

A novel interface strengthening layer: Nanoscale AuCu super-structure formed during Au80Sn20/Cu rapid solidification soldering process

Highlights: • The nanoscale AuCu super-structure formed in Au80Sn20/Cu soldering joint. • The phase-transformation diffusion mechanism of Au80Sn20/Cu soldering process was studied. • The orientation relationship of Au80Sn20/Cu intermetallic compounds was investigated. • The interfacial strengthening mechanism of nanoscale AuCu layer was discussed. - Abstract: Phase composition and orientation of intermetallic compounds layers determine the functional and mechanical properties of solder joints. In this paper, interfacial reaction and strengthening mechanism of Au80Sn20/Cu joint by rapid solidification reflow soldering were studied. The Au80Sn20/Cu solder joint by rapid solidification reflow soldering exhibit a superior shear property, and the shear strength reaches up to 90 MPa. It is found that a new nanoscale AuCu super-structure formed in the interfacial intermetallic compounds layer, which is coherent with the [001] Cu substrate. The orientation relationship of Cu matrix/interfacial intermetallic compounds is determined to be [001]{sub Cu}∥[001]{sub AuCu}∥[ 2-bar 4 2-bar 3]{sub (AuCu){sub 5Sn}} and (200){sub Cu}∥(200){sub AuCu}∥(10 1-bar 0){sub (AuCu){sub 5Sn}}. Nanoscale AuCu super-structure influences the interface slip direction and provides interface misfit dislocation, hinder the dislocation movement, lead to the interface strengthening effect. Our finding on nanoscale AuCu super-structure formed during Au80Sn20/Cu soldering process not only sheds light on future research direction but also provides practical guidance to the engineers in solder industry.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microstructure evolution and mechanical properties of Cu/Sn/Ag TLP-bonded joint during thermal aging

Highlights: • The thermal reliability of the Cu/Sn/Ag TLP-bonded joint was investigated through high-temperature storage. • A diffusion reaction occurred at the interface between Cu{sub 3}Sn and Ag{sub 3}Sn during thermal aging. • The mechanism of the Cu{sub 3}Sn/Ag{sub 3}Sn interfacial reaction was investigated from thermodynamics and kinetics. - Abstract: Low-temperature transient liquid phase (TLP) bonding is a promising joining technology for high-temperature electronic devices packaging. However, the effect of thermal aging on the joint microstructure and performance has been rarely studied so far. In this paper, the relationship between microstructural evolution and mechanical property was developed for the Cu/Sn/Ag TLP-bonded joint during 350 °C aging. Experimental results show that an interfacial reaction occurs between the intermetallic compounds (IMCs) of Cu{sub 3}Sn and Ag{sub 3}Sn, which induces that a great amount of Cu{sub 3}Sn particles or wedges embed into the Ag-Sn phase layer. The reaction process is controlled by a volume diffusion of Cu elements from the Cu substrate, and capable of promoting the transformation from Ag{sub 3}Sn into Ag(Sn) solid solution. Cu{sub 41}Sn{sub 11} phase can be formed at the expense of Cu{sub 3}Sn and Cu, of which transformation process is completely achieved after aging for 480 h, and the Cu(Sn) solid solution intimately contacts with the opposite Ag(Sn) solid solution in many areas after aging for 960 h. The joint mechanical property initially declines due to the formation of Cu{sub 41}Sn{sub 11} phase and Cu-Sn IMCs grain coarsening, and then increases because of the complete depletion of Cu{sub 3}Sn and substantial precipitation of Cu(Sn) solid solution. After aging for nearly 1000 h, the joint still maintains a high shear strength of >40 MPa, indicating an excellent thermal reliability.

36 MATERIALS SCIENCE↗

Improvement of interfacial adhesion of unidirectional textile grade carbon fiber (TCF) with unsized, epoxy and urethane sizing reinforced in thermoset urethane composites

This work considers a unique wide tow (450k filaments) form of low-cost carbon fiber intended for non-aerospace applications. TCF is currently produced in epoxy and urethane sizing, and there is a need to understand its resulting composite properties. In this work, the interfacial adhesion of sized TCF reinforced in thermoset urethane (TSU) composites are examined through the surface, thermal and mechanical characterization techniques. Atomic force microscopy (AFM) results showed an increase in surface roughness for urethane (276%) and epoxy sized (78%) versus unsized TCF. XPS results showed 531% increase in O in epoxy sized TCF and 250% N content in urethane sized TCF compared to unsized TCF. The surface energy of epoxy and urethane sized TCF is enhanced by 78% and 96%, respectively compared to unsized TCF. The storage modulus showed improvement for urethane (23%) and epoxy (21%) sized than unsized TCF-TSU composites. The flexural, interlaminar shear strength (ILSS), and impact properties of urethane sized TCF increase by 24%, 50%, and 273%, respectively, than unsized TCF. The results demonstrate that the surface and thermal properties correlate with the mechanical properties of TCF-TSU composites and sizing enhances the wettability of the composites.

36 MATERIALS SCIENCE↗

Large scale centrifuge test of a geomembrane-lined landfill subject to waste settlement and seismic loading

Highlights: • A large centrifuge model of a geomembrane-lined landfill was seismically loaded. • The scaled peak acceleration of the strongest input motion was 0.6 g. • Laboratory testing was conducted to obtain properties of the model materials. • Collected data included liner strains due to downdrag and seismic loading. • Results show that settlement and seismic loading can potentially damage geomembranes. • Results can be used to validate numerical models for geomembrane performance. •The laboratory and centrifuge testing data is publicly available. - Abstract: A large scale centrifuge test of a geomembrane-lined landfill subject to waste settlement and seismic loading was conducted to help validate a numerical model for performance based design of geomembrane liner systems. The test was conducted using the 240 g-ton centrifuge at the University of California at Davis under the U.S. National Science Foundation Network for Earthquake Engineering Simulation Research (NEESR) program. A 0.05 mm thin film membrane was used to model the liner. The waste was modeled using a peat-sand mixture. The side slope membrane was underlain by lubricated low density polyethylene to maximize the difference between the interface shear strength on the top and bottom of the geomembrane and the induced tension in it. Instrumentation included thin film strain gages to monitor geomembrane strains and accelerometers to monitor seismic excitation. The model was subjected to an input design motion intended to simulate strong ground motion from the 1994 Hyogo-ken Nanbu earthquake. Results indicate that downdrag waste settlement and seismic loading together, and possibly each phenomenon individually, can induce potentially damaging tensile strains in geomembrane liners. The data collected from this test is publically available and can be used to validate numerical models for the performance of geomembrane liner systems.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Textile-Grade Carbon Fiber-Reinforced Polycarbonate Composites: Effect of Epoxy Sizing

In this work, epoxy-sized textile-grade polyacrylonitrile (PAN) carbon fiber (TCF) with 450 K filaments (CFTF, ORNL) was reinforced in the polycarbonate (PC) matrix using a compression molding technique. The epoxy sizing effect on the surface, thermal, and mechanical properties of TCF–PC was investigated. X-ray photoelectron spectroscopy and Fourier transform infrared spectroscopy results of the TCF–PC composite show the absence of an oxirane group (epoxy-sized TCF), which suggests a covalent bond formation between the oxirane ring and carbonyl groups from TCF and PC. Dynamic mechanical analysis results confirm a strong immobilized interface (b > 1) present between TCF and PC. The tensile, flexure, compression, and interlaminar shear strength of TCF–PC composites were 323 ± 53, 371 ± 31, 397 ± 87, and 36 ± 3 MPa, correspondingly. The fracture analysis through scanning electron microscopy shows good wettability between TCF and the PC matrix which validates the results obtained from surface and thermal characterization.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Enhanced Mechanical and Adhesion Properties in Sustainable Triblock Copolymers via Non-covalent Interactions

ABA triblock copolymers are used as thermoplastic elastomers (TPEs) for a wide variety of applications. In this paper, we describe incorporation of sugar-based glassy components to create sustainable triblock copolymers as alternatives for commodity TPEs. Poly(glucose-6-acrylate-1,2,3,4-tetraacetate) [PGATA] and poly(acetylated acrylic isosorbide) [PAAI] end blocks were chain-extended from a poly( n -butyl acrylate) [PnBA] midblock. PAAI–PnBA–PAAI exhibited excellent adhesion properties: peel = 8.74 N cm –1 , loop tack = 2.96 N cm –2 , no shear failure up to 100 h, and shear adhesion failure temperature (SAFT) = 60 °C. Although similar peel adhesion and higher loop tack were observed for PGATA–PnBA–PGATA, the shear strength and SAFT were moderate (18 h and 42 °C, respectively). PAAI–PnBA–PAAI are tough elastomers and demonstrated high stress and elongation at break (σ = 6.5 MPa and ε = 620%, respectively) while the GATA-based analogue exhibited weaker tensile properties (σ = 0.8 MPa and ε = 476%). To address this, the anomeric hydroxyl groups of GATA units were selectively deprotected to promote self-complementary hydrogen bonding in the glassy domains, resulting in 80% enhancement in the ultimate tensile stress at break (σ = 1.5 MPa). This study aims to demonstrate effects of noncovalent interactions, such as chain entanglements and self-complementary hydrogen bonding, to enhance the adhesion and mechanical performance of sugar-derived TPEs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Oil-Soluble Silver–Organic Molecule for in Situ Deposition of Lubricious Metallic Silver at High Temperatures

A major challenge in lubrication technology is to enhance lubricant performance at extreme temperatures that exceed conventional engine oil thermal degradation limits. Soft noble metals such as silver have low reactivity and shear strength, which make them ideal solid lubricants for wear protection and friction reduction between contacting surfaces at high temperatures. However, achieving adequate dispersion in engine lubricants and metallic silver deposition over predetermined temperatures ranges presents a significant chemical challenge. Here we report the synthesis, characterization, and tribological implementation of the trimeric silver pyrazolate complex, [Ag(3,5-dimethyl-4-n-hexyl-pyrazolate)]3 (1). This complex is oil-soluble and undergoes clean thermolysis at ~310 °C to deposit lubricious, protective metallic silver particles on metal/metal oxide surfaces. Temperature-controlled tribometer tests show that greater than 1 wt % loading of 1 reduces wear by 60% in PAO4, a poly-α-olefin lubricant base fluid, and by 70% in a commercial fully formulated 15W40 motor oil (FF oil). This silver–organic complex also imparts sufficient friction reduction so that the tribological transition from oil as the primary lubricant through its thermal degradation, to 1 as the primary lubricant, is experimentally undetectable.

Desanker, Michael↗