Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 595 records · Page 33

Constitutive Model for Hot Deformation of the Cu-Zr-Ce Alloy

Hot compressive deformation behavior of the Cu-Zr-Ce alloy has been investigated according to the hot deformation tests in the 550-900 °C temperature range and 0.001-10 s{sup −1} strain rate range. Based on the true stress–true strain curves, the flow stress behavior of the Cu-Zr-Ce alloy was investigated. Microstructure evolution was observed by optical microscopy. Based on the experimental results, a constitutive equation, which reflects the relationships between the stress, strain, strain rate and temperature, has been established. Material constants n, α, Q and ln A were calculated as functions of strain. The equation predicting the flow stress combined with these materials constants has been proposed. The predicted stress is consistent with experimental stress, indicating that developed constitutive equation can adequately predict the flow stress of the Cu-Zr-Ce alloy. Dynamic recrystallization critical strain was determined using the work hardening rate method. According to the dynamic material model, the processing maps for the Cu-Zr and Cu-Zr-Ce alloy were obtained at 0.4 and 0.5 strain. Based on the processing maps and microstructure observations, the optimal processing parameters for the two alloys were determined, and it was found that the addition of Ce can promote the hot workability of the Cu-Zr alloy.

36 MATERIALS SCIENCE↗

The Precipitation Behavior and Hot Deformation Characteristics of Electron Beam Smelted Inconel 740 Superalloy

The Inconel 740 superalloy was prepared by the electron beam smelting (EBS) technology, the precipitation behavior and strengthening mechanism were studied, and the hot deformation characteristics of EBS 740 superalloy were investigated. The results indicate that the EBS 740 superalloy is mainly strengthened by the mechanism of weakly coupled dislocation shearing, and the resulting critical shear stress is calculated to be 234.6 MPa. The deformation parameters show a great influence on the flow behavior of EBS 740 superalloy. The strain rate sensitivity exponent increases with the increasing of deformation temperature, and the strain hardening exponent shows a decreasing trend with the increasing of strain. The activation energy of EBS 740 above 800 °C is measured to be 408.43 kJ/mol, which is higher than the 740H superalloy. A hyperbolic-sine-type relationship can be observed between the peak stress and Zener–Hollomon parameter. Nevertheless, the influence of deformation parameters is found to be considerably different at temperatures below and above 800 °C. The size of dynamic recrystallization (DRX) grains decreases with the increasing of strain rate when the strain rate is lower than 1/s, and reverse law can be found at higher strain rate. As a result, a piecewise function is established between the DRX grain size and hot working parameters.

36 MATERIALS SCIENCE↗

The Evolution of Second-Phase Particles in 6111 Aluminum Alloy Processed by Hot and Cold Rolling

The evolution of coarse Al{sub 9.9}Fe{sub 2.65}Ni{sub 1.45} phase, spherical Al{sub 12}(Mn,Fe){sub 3}Si phase and rod-like Q phase in a 6111 aluminum alloy during hot and cold rolling deformation processes was systematically investigated in this work. The results showed that the coarse Al{sub 9.9}Fe{sub 2.65}Ni{sub 1.45} particles are mainly distributed at the grain boundaries, accompanied by the co-formation of Al{sub 12}(Fe,Mn){sub 3}Si phase and Mg{sub 2}Si phase, while the spherical Al{sub 12}(Mn,Fe){sub 3}Si particles are mainly distributed in the grain interiors. Hot rolling has little effects on the size and distribution of both phases, but cold deformation can severely decrease the size of the particles by breaking the particles into small pieces. In addition, the temperature of 450 °C is not high enough for the dissolution of Q phase in the Al matrix, but the Q particles can be broken into small pieces due to the stress concentration during both hot and cold rolling deformation. In addition, the influences of phase evolution, dislocations and recrystallization on the mechanical properties evolution were also discussed.

36 MATERIALS SCIENCE↗

Deformation Mechanisms and Formability Window for As-Cast Mg-6Al-2Ca-1Sn-0.3Sr Alloy (MRI 230D)

The hot deformation characteristics of MRI 230D alloy have been evaluated in the temperature range 260-500 °C and strain rate range 0.0003-10 s{sup −1}, on the basis of processing map. The processing map exhibited two domains in the ranges: (1) 300-370 °C and 0.0003-0.001 s{sup −1} and (2) 370-480 °C and 0.0003-0.1 s{sup −1}. Dynamic recrystallization occurs in the both domains with basal slip dominating in the first domain along with climb as recovery process and second-order pyramidal slip dominating in the second with the recovery by cross-slip. In Domains (1) and (2), the apparent activation energy values estimated using the kinetic rate equation are 143 and 206 kJ/mole, respectively, the first one being close to that for lattice self-diffusion confirming climb. It is recommended that the alloy is best processed at 450 °C and strain rates less than 0.1 s{sup −1}, where non-basal slip and cross-slip occur extensively to impart excellent workability. The alloy exhibits flow instability in the form of adiabatic shear band formation and flow localization at lower temperatures and higher strain rates. Forging of a cup-shaped component was performed under various conditions, and the results validated the predictions of the processing map on the workability domains as well as the instability regimes.

36 MATERIALS SCIENCE↗

Properties of Rolled AZ31 Magnesium Alloy Sheet Fabricated by Continuous Variable Cross-Section Direct Extrusion

Rolling is currently a widely used method for manufacturing and processing high-performance magnesium alloy sheets and has received widespread attention in recent years. Here, we combined continuous variable cross-section direct extrusion (CVCDE) and rolling processes. The microstructure and mechanical properties of the resulting sheets rolled at different temperatures from CVCDE extrudate were investigated by optical microscopy, scanning electron microscope, transmission electron microscopy and electron backscatter diffraction. The results showed that a fine-grained microstructure was present with an average grain size of 3.62 μm in sheets rolled from CVCDE extrudate at 623 K. Dynamic recrystallization and a large strain were induced by the multi-pass rolling, which resulted in grain refinement. In the 573-673 K range, the yield strength, tensile strength and elongation initially increased and then declined as the CVCDE temperature increased. The above results provide an important scientific basis of processing, manufacturing and the active control on microstructure and property for high-performance magnesium alloy sheet.

36 MATERIALS SCIENCE↗

Tensile Properties and Fracture Characteristics of Nanostructured Copper and Cu-SiC Nanocomposite Produced by Mechanical Milling and Spark Plasma Sintering Process

The presence of large grains within nanometric and ultrafine grain matrix is an effective method in order to enhance strength while keeping the high ductility of metals. For this purpose, in this research, spark plasma sintering (SPS) was used to consolidate milled Cu and Cu-SiC powders. In SPS process, local sparks with high temperature between particles take place and locally lead to intense grain growth, and therefore, this method has the ability to produce bimodal grain structures in copper and copper-based composites. Microstructural and mechanical studies showed ≈ 185 and ≈ 437 nm matrix grain sizes, high tensile yield strength values of ≈ 188.4 and ≈ 296.9 MPa, and fracture strain values of 15.1 and 6.7% for sintered Cu and Cu-4 vol.% SiC nanocomposite materials, respectively. The presence of nanoparticles promoted the occurrence of static recrystallization and decreased the fraction of coarse grains in microstructure. The high tensile properties of the produced materials are attributed to fine grain size, homogenous dispersion of nanoparticles and retarded grain boundary migration during sintering.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Characterization of the Hot Deformation Behavior of a Newly Developed Nickel-Based Superalloy

To clarify the microstructural evolution and hot workability of GH4282 during hot forming processes, the hot deformation behavior of this superalloy was investigated by isothermal compression tests in the temperature interval of 950-1210 °C and the strain rate range of 0.01-10 s{sup −1} with a true strain of 0.7. The results show that the flow stresses decrease with an increase in the deformation temperature and a decrease in the strain rate. The characteristic of dynamic recrystallization is revealed by the flow curves. The variation rule of the flow stress can be well described by the hyperbolic sine type equation, and the thermal deformation activation energy is determined to be 498.118 kJ/mol. The optimum hot working parameters are 1100-1180 °C and 0.01-0.1 s{sup −1}, under which the fine and uniform microstructure can be obtained.

36 MATERIALS SCIENCE↗

Effect of Hot Deformation on Texture and Microstructure in Fe-Mn Austenitic Steel During Compression Loading

Hot compression tests of a new high-Mn austenitic steel were carried out at deformation temperatures of 700, 800, 900, and 1000 °C under strain rate of 0.01 s{sup −1}. The hot deformation behavior was investigated by the analyses of flow curves, texture, and deformed microstructures. Microstructures of the deformed specimens and macrotexture were examined using electron backscatter diffraction and x-ray diffraction methods, respectively. The results showed that the flow stress depended strongly on the deformation temperature and decreased by increasing deformation temperature. The microstructural evidence indicated that the dynamic recrystallization (DRX) process of experimental steel was initiated at 800 °C with necklace structure. The volume fraction of DRX grains was considerably increased by increasing deformation temperature to 1000 °C. Texture of the DRX grains tended to become a weak texture and was associated with the formation of Goss and R-Cube components. Meanwhile, martensitic transformation was detected in the hot-deformed austenite. The martensitic transformation was the most difficult in the DRX grains because of the effect of small grain size. The tendency of transformation was decreased after compression at 1000 °C.

36 MATERIALS SCIENCE↗

X-ray Diffraction Investigation of Annealing Behavior of Peened Surface Deformation Layer on Precipitation Hardening Stainless Steel

In order to investigate the recrystallization behavior of peened surface deformation layer of precipitation hardening stainless steel, a classic x-ray diffraction line profile analysis, Voigt method, was carried out on peened 17-4PH with different isothermal annealing temperatures. The activation energy of domain boundary migration (Q{sub a}) and the activation energy of microstrain relaxation (Q{sub b}) were calculated by regression analysis in different annealing temperature conditions. The results show that the value of Q{sub a} decreases with annealing temperature increasing, which is due to the influence of precipitation (ε-Cu) size on the movements of grain and subgrain boundaries. The maximum growth rate of ε-Cu particles occurs during 400 to 500 °C interval. Compared with growth behavior of domain size, microstrain relaxation behavior is less sensitive to precipitation particle size. The effects of annealing temperature and time on dislocation density are both significant when annealing temperature is lower than 500 °C. However, the effect of annealing temperature on dislocation density becomes insignificant when annealing temperature is higher than 500 °C. 300 °C annealing temperature only leads to the microstrain relaxation but nearly cannot lead to the domain size growth even if prolonging annealing time. Microstructure enhancement effect still exists in plastic deformation layer when 300 °C annealing temperature lasts for 60 min but nearly disappears when 600 °C annealing temperature lasts for 20 min.

36 MATERIALS SCIENCE↗

Effect of Ceramic Rolling and Annealing on Mechanical Properties of AlCoCrFeNi{sub 2.1} Eutectic High-Entropy Alloys

It was firstly proved that AlCoCrFeNi{sub 2.1} could optimize the strength-ductility combination by ceramic rolling at room temperature. The technique greatly enhanced the strength of the materials at the price of slight ductility, which is different from the previous studies. When the thickness reduction was 23.06%, the yield strength and compressive strength were 1611.42 and 2212.99 MPa, respectively, with the plastic strain of 28.36%. Such an excellent combination of strength and ductility was attributed to the distribution of the residual stress, the high hydrostatic stress and the shear bands in ceramic rolling process. The plastic strain of the material increased to 38.54%, and the strength reduced to 1900.73 MPa after annealing at 800 °C for 1 h. A lot of like-flower patterns of recrystallized ultrafine grain were observed after annealing at 800 °C due to the sluggish diffusion in HEAs and the effect of ceramic rolling. In addition, after annealing at 800 °C, the fracture mode changed to shearing fracture of microvoid aggregation from cleavage/quasi-cleavage fracture of as-rolled sample due to the deposition of the second phase in the tested sample.

36 MATERIALS SCIENCE↗

Ultrafine Grain Refinement and Superplasticity of Ti-55 Alloy Obtained by Hydrogen Absorption and Desorption

Hydrogen absorption and desorption treatment consists of two processes for near α-phase Ti-55 titanium alloy: (1) hydrogenation with different contents and (2) hydrogen desorption by vacuum annealing at 700 °C and with pressure less than 10{sup −4}Pa for 2 h. Equiaxed ultrafine-grained structure with a grain size range between 0.5 and 1 μm has been obtained. Compared with as-received alloy, the grain size of fully dehydrogenated specimen is reduced by ten times. The grain refinement mainly results from α{sub H} ↔ β{sub H} transformation and accompanied recrystallization. The optimum superplastic temperature of Ti-55 alloy is reduced by about 150 °C, which arises from more grain boundary area and higher proportion of extremely deformable β phase in the ultrafine-grained alloy.

36 MATERIALS SCIENCE↗

Rapid Strengthening Without Loss of Ductility via Electropulsing Treatment in Ti-6Al-4V Alloy

The commercial (hot-rolled and annealed) Ti-6Al-4V alloy subjected to electropulsing was investigated in this study. The results show that the electropulsing-treated sample with optimized parameter exhibits greatly refined microstructure and notable strength improvement without loss of ductility. The main strengthening mechanism is recognized as phase transformation and rapid grain refinement induced by recrystallization under EPT.

36 MATERIALS SCIENCE↗

Cryorolling-Induced Texture, Mechanical Properties and Fracture Behavior of Al-Mg-Si Alloys During Cold Deformation

This study investigated the texture, mechanical properties, and fracture behavior during cold working of cryorolled (CR) Al-Mg-Si alloys. An x-ray texture goniometer was used to examine the crystallographic texture, and tensile tests were performed to understand the deformation behavior in more detail. SEM/EBSD/TEM was used to observe the microstructures and fracture morphology of the alloy during cryorolling. The microstructures indicated that a large number of ultrafine grains and dislocations formed after cryorolled. The recrystallization was prohibited due to low temperature during deformation. The ultrafine grains and dislocation strength improved the tensile strength from 279.38 MPa for the room-rolled alloy to 313.98 MPa for the cryorolled alloy; better plasticity (4.6%) was observed in the CR sheet. Ductile and intergranular fractures were observed in the CR sheet deformation from 20 to 90%.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Al-Mg-Sc-Zr Alloy Variable Polarity Plasma Arc Welding Joint

Al-Mg-Sc-Zr alloy plates were welded by variable polarity plasma arc welding (VPPAW) with Sc-containing filler wire. The microstructure and mechanical properties were investigated. Results show that the weld zone and heat-affected zone (HAZ) are narrow due to the high concentrated heat input of VPPAW. Primary Al{sub 3}(Sc,Zr) particles are nice nucleating sites for α-Al, which can significantly refine the grains of α-Al, helping the weld zone maintain an outstanding strength. The unmelted Al{sub 3}(Sc,Zr) precipitates of the base metal aggregated near the fusion boundary result in the formation of a fine equiaxed grains zone, which improves the bonding degree between the weld zone and the base metal. The Al{sub 3}(Sc,Zr) precipitates in the HAZ have excellent inhibition effect on recrystallization. According to the observed microhardness distribution and microstructure characteristics, the microstructure model of welded joint is obtained. The fractured position of welded joint locates in the weld zone. The tensile strength of the welded joint without reinforcing rib is 330 MPa. The welding coefficient reaches 74%.

36 MATERIALS SCIENCE↗

Deformation Behavior of AM30 Magnesium Alloy

In this study, deformation behavior of AM30 magnesium alloy is investigated in the hot working regime and empirical relations are developed. Compression tests were performed in the 0.001-10 s{sup −1} strain rate range and 423-623 K temperature range to obtain the mechanical properties. The compression curves were fitted using two approaches, viz. piecewise linear fitting and a Johnson–Cook type relation. Piecewise linear fit is found to be appropriate for describing the mechanical behavior in the dynamic recrystallization (DRX) regime as compared to the proposed Johnson–Cook type relation. The Johnson–Cook type model is not able to capture the essential feature of DRX, particularly at high strain rates.

36 MATERIALS SCIENCE↗

High-Temperature Deformation Behavior of Ti-6Al-2Sn-4Zr-2Mo Alloy with Lamellar Microstructure Under Plane-Strain Compression

High-temperature plane-strain compression of a Ti-6Al-2Sn-4Zr-2Mo (Ti-6242) alloy with a lamellar structure was applied by a thermal simulation machine Gleeble 3800 at a temperature of 1223-1370 K and a strain rate of 0.01-10 s{sup −1}. Constitutive relations between the flow stress and strain at different temperatures and strain rates were constructed based on the Arrhenius equation. Processing maps based on the dynamic material model at strains of 0.5, 1.0, and 1.25 were also constructed to analyze the mechanism and instability of high-temperature deformation. Dynamic recrystallization was found to occur at 1223-1313 K and 0.01-0.1 s{sup −1}, with a peak efficiency of power dissipation of 70%. Observations of the microstructure demonstrated that α platelets and dynamic globularization were responsible for dynamic softening in the α + β phase field. Flow instability behaviors occurred at 1263-1343 K/1.78-10 s{sup −1}, 1233-1283 K/0.1-3.16 s{sup −1}, and 1353-1373 K/0.56-1.78 s{sup −1}, and adiabatic shear bands and microcracks were observed in these domains. Thus, for the lamellar Ti-6242 alloy, the recommended hot rolling parameters were 1243-1333 K and 0.01-0.1 s{sup −1}. Electron backscattered diffraction results revealed that the dynamic restoration mechanism in the β phase field was dynamic recovery when the strain rate was as high as 10 s{sup −1}.

36 MATERIALS SCIENCE↗

Hot Deformation Behavior of the 20 vol.% TiC/Cu-Al{sub 2}O{sub 3} Composites

Hot deformation behavior of the 20 vol.% TiC/Cu-Al{sub 2}O{sub 3} composite was studied using the Gleeble-1500D thermo-mechanical simulator with various strain rates at different deformation temperatures. The softening mechanism due to dynamic recrystallization was a feature of the high-temperature true stress–strain curves. The peak stress increased at the lower deformation temperature and the higher strain rate. Microstructure evolution was explored. Thermal deformation activation energy was calculated as 218.9 kJ/mol, and the constitutive equation was established. The processing map was constructed to obtain optimal processing domain of 700-850 °C and 0.001-0.04 s{sup −1} for hot working.

36 MATERIALS SCIENCE↗

Experimental Study on the Hot Deformation Characterization of Low-Carbon Nb-V-Ti Microalloyed Steel

X80 steel, as typical low-carbon Nb-V-Ti microalloyed steel, is getting more and more attention in oil and gas transmission pipeline manufacturing. In this paper, the hot deformation behavior of X80 steel has been investigated. Hot compression tests of the steel were conducted under different temperatures and strain rates. Based on the experimental data, the flow stress constitutive equations were established. It is found that the hot deformation activation energy of this steel is higher than C-Mn and low-carbon steel. Then, the kinetics model and grain size model of dynamic recrystallization were developed according to the flow curves and the optical microstructures. In addition, the processing maps were developed to analyze the workability of X80 steel at elevated temperature. The analysis results show that the optimum processing window is at the temperature of 1300-1473 K and the strain rate of 0.01-10 s{sup −1}. The microstructure observation indicates that the optimum processing parameters are applicable to the tested steel.

36 MATERIALS SCIENCE↗