At least 595 records · Page 33

Particle transport-driven flow dynamics and heat transfer modulation in solar photovoltaic modules: Implications on soiling

Wind-swept debris and excessive heating reduce solar photovoltaic efficiency and accelerate panel degradation. For many solar plants in open environments, particle deposition is well-understood to exacerbate efficiency losses by blocking useable light and insulating panel surfaces. However, little is known about particle behavior in multi-panel systems, where complex wakes dominate and alter trajectories. This study examines debris-laden flow within a scaled array of two model solar panels, observing convective cooling and focusing on turbulent inter-panel flow dynamics. Convection is compared between the first and second panels (P 1 and P 2 ) and for a single inflow velocity at four particle concentrations (Φ v ), including a neutrally buoyant particle (i.e. tracer) case and three water droplet cases. Tracers and Φ v > 0 concentrations show increased convective heat transfer for P 2 compared to P 1 , while inertial particle presence and increased concentration reduces this improvement from +170% to +90%. Particle image velocimetry surrounding P 2 reveals dampened inter-panel wake features for particle-laden flow compared to the tracer case, where diminished mean flow and mean kinetic energy breakdown are observed for the particles due to their inertia. Together, the reduction in comparative convection and dampened wake effects accompanying inertial particle concentration motivates further studies on coupled array physics in debris-filled flow.

14 SOLAR ENERGY↗

Next-Generation Reverse Logistics Networks of Photovoltaic Recycling: Perspectives and Challenges

With the growing adoption of solar energy as a key component of the global energy transition and its new industrial policy (the Inflation Reduction Act and others), the United States is witnessing a significant increase in solar investments. This surge in installations and domestic and reshored manufacturing of solar photovoltaic (PV) panels brings with it a pressing issue: the proper management of end-of-life (EoL) PV panels. As these panels are decommissioned, either due to reaching the end of their lifespans or due to breakage across the various stages of the forward supply chain, it becomes crucial to establish efficient reverse supply chain logistics systems to address the challenges associated with their disposal, while also unlocking the value of the inherent materials that are of critical value for other forward supply chains. This perspective article examines the challenges regarding EoL PV panels and relevant reverse supply chain and logistics networks, and proposes future research directions based on the gaps observed among academic research, industry, and policy-making challenges. We identify the main bottlenecks and hurdles including, among others, the lack of supportive regulations and absence of structured, optimized recycling infrastructure. To this end, it is proposed that the key to achieving a sustainable reverse supply chain network for solar PV panels lies in relentless end-to-end supply chain cost optimization efforts supported by enabling policies. Moreover, it is proposed that designing systematic decision-making modeling frameworks is vital for examining different possibilities and scenarios for state, region or nation-wide optimization of solar PV reverse supply chain networks. Indicative to this effect, we discuss the development of a Resource-Task-Network (RTN)-based model and demonstrate its application and benefits through a case study. We wrap up with conclusions and future research directions.

circular economy↗

Rapid characterization and failure analysis of 6276 rooftop-harvested photovoltaic connectors

Photovoltaic (PV) connectors, which link modules in series and connect PV strings in parallel, have increasingly been recognized as a primary contributor to PV system failures and a source of numerous fire incidents. However, publicly available data on the rates and types of connector failures are scarce, primarily due to the proprietary nature of the information and the need for comprehensive analysis. This study represents the first large-scale investigation of harvested PV connectors, drawing from a dataset of 6276 connectors from residential rooftop solar systems across the United States. The outcome of this work is twofold: 1) we have established a rapid characterization method for large populations of harvested connectors, incorporating visual inspection, resistance measurements, and X-ray imaging; and 2) the analysis made possible by our rapid-processing method has revealed, for a population of connector models provided by a single rooftop installer, failure statistics and insights for various connector makes and models, installation practices, operating currents, and internal component displacements. This research identifies common failure modes that could be considered in future connector designs standards, and operations and maintenance practices, to ultimately improve the reliability of this vital component of PV infrastructure.

MC4↗

Durability of ionomer encapsulants in photovoltaic modules

Ethylene vinyl acetate (EVA) has for decades been the preferred material for photovoltaic (PV) module encapsulation. However, while it is relatively inexpensive and initially adheres well to module components, EVA discolors with age and - as interfacial adhesion degrades - becomes susceptible to delamination, ultimately resulting in reduced module efficiency and shortened service lifetimes. As potential replacements for EVA, ionomer thermoplastic materials cure faster, are more resistant to discoloration and potential induced degradation, and do not evolve corrosive acetic acid, making them compatible with new device materials such as perovskites. Since there is limited information on ionomer durability for PV module applications, a series of field and accelerated laboratory aging studies were conducted to assess ionomer interface stability in the presence of terrestrial environmental stressors. It is shown that adhesion to the glass and cell interfaces of PV modules is inferior to EVA, both before and after aging, rendering ionomers particularly susceptible to delamination after short timeframes. Potential solutions to improve ionomer adhesion are discussed.

14 SOLAR ENERGY↗

Characterizing photovoltaic backsheet adhesion degradation using the wedge and single cantilever beam tests, Part II: Accelerated tests

Photovoltaic (PV) backsheets provide critical moisture, mechanical, and electrical insulation to the backside of PV modules, but their continued functionality depends upon their ability to remain well adhered over years of harsh environmental exposure. A study of adhesive strength was conducted on several PV backsheet types exposed to indoor accelerated weathering. Two adhesion tests – the wedge test and single cantilever beam test – were used to measure adhesion energy in four backsheets: two with fluoropolymer-based outer (airside) layers – polyvinyl fluoride (PVF), polyvinylidene fluoride (PVDF) – and two with non-fluoropolymer-based outer layers–polyamide (PA) and polyethylene terephthalate (PET). The effects of changes in temperature, ultraviolet (UV) irradiance, relative humidity, and a periodic water spray were studied. The PET-, PVF- and PVDF-based backsheets all showed instances of debonding in an adhesive layer, which is commonly reported. Furthermore, for the PA-, PET-, and PVDF-based backsheets, adhesion energy dropped fairly rapidly with exposure, reaching very low levels by 4000 h. The PVF-based backsheet was relatively robust to weathering. Pull-off of an outer chalking layer in the PA- and PET-based backsheets suggested a sensitivity to UV. Adhesion in these two backsheets was also highly sensitive to changes in moisture level. Changes in UV irradiance and temperature did not show a statistically significant effect on adhesion loss for the exposure levels used. The present work is part of a two-part adhesion study on both field-weathered and indoor-exposed backsheets, and forms a basis for understanding adhesion degradation across a variety of backsheet types and degradation factors.

14 SOLAR ENERGY↗

Characterizing photovoltaic backsheet adhesion degradation using the wedge and single cantilever beam tests, Part I: Field Modules

Photovoltaic backsheets are exposed to harsh outdoor weathering conditions throughout their service lives that can compromise their protective function, through adhesive debonding between their constituent layers and between the backsheet and the module. We report a large-scale study on adhesive degradation was conducted on 37 field-exposed modules, that spanned 19 different module manufacturers, that were deployed among six Köppen–Geiger climatic zones, and that were fielded between 0 and 28 years. Six outer layer polymer classes were identified among the backsheets: polyamide (PA), polyethylene terephthalate (PET), polyvinyl fluoride (PVF), polyvinylidene fluoride (PVDF), fluoroethylene vinyl ether copolymer (FEVE), and tetrafluoroethylene hexafluoropropylene vinylidene fluoride copolymer (THV). Two adhesion tests were used to measure the adhesive strength: the wedge test and the width-tapered single-cantilever beam (SCB) test. Adhesion energies were compared across exposure time and Köppen–Geiger climatic zone. Many of the PET-, PVF-, and PVDF-based backsheets experienced degradation of the adhesive layer between the backsheet outer and core layers. A consistent trend of decreasing adhesion energy with exposure time was observed in five out of the six backsheet types. Trends among adhesion energy and climatic zone, while expected, were not observed, possibly due to broad ranges in temperature, humidity, and precipitation defining Köppen–Geiger climatic zones. The cantilever beam measurements produced an upper cutoff of approximately 100 J/m 2 , above which no modules exhibited field delamination. The results are part of a two-part study quantifying adhesion in both field-weathered and indoor-exposed PV backsheets.

14 SOLAR ENERGY↗

Outdoor performance of a tandem InGaP/Si photovoltaic luminescent solar concentrator

Here, we report the design, fabrication and outdoor characterization of a tandem luminescent solar concentrator/Si multi-junction photovoltaic module. Our tandem LSC/Si device consists of an InGaP LSC functioning as a top cell and a passivated contact Si bottom cell. The LSC comprises of an InGaP microcell array coupled to a polymer waveguide, loaded with CdSe/CdS core-shell quantum dot luminophores. The light trapping efficiency of the LSC waveguide is enhanced by encapsulation with photoluminescence trapping mirrors consisting of dielectric multilayer thin films. We demonstrate the performance of the LSC/Si device through a series of outdoor tests under various irradiance conditions conducted at the National Renewable Energy Laboratory. We report the first outdoor testing data of an LSC/Si tandem module, displaying maintained performance across varied diffusivity conditions for the LSC component. Finally, we model the tandem module performance using a ray optic simulation-based multiphysics model and forecast a pathway for high efficiency tandem LSC/Si module performance.

14 SOLAR ENERGY↗

Understanding interfacial chemistry of positive bias high-voltage degradation in photovoltaic modules

Photovoltaic module degradation from a high system voltage is a prevalent degradation mode in the field, where the enabling degradation mechanisms are inherently dependent on the voltage bias polarity of the installed system. In this study, the effects of positive bias on module performance are confirmed and the underlying chemical degradation processes are more thoroughly investigated to reveal different degradation pathways from those previously reported in negative bias studies. When cells are under +1000 V stress, crystalline silicon mini-modules with poly(ethylene-co-vinyl acetate) (EVA) encapsulant demonstrated a significant photocurrent loss due to EVA discoloration and delamination from increased chemical reactivity at the front-side EVA/cell metallization interface. Brown discoloration of the EVA encapsulant near the cell gridlines is linked to an electrochemical reaction at the Ag gridlines under hot and humid conditions (85 °C, 85% relative humidity). Chemical compositional analysis using X-ray photoelectron spectroscopy (XPS) confirmed that the discoloration is attributed to the formation of silver sulfide (Ag 2 S) and/or silver oxide (Ag 2 O) species at the EVA/Ag gridline interface. The subsequent migration of Ag ions from the cell gridlines into the bulk of the EVA was evident from XPS depth profiling and optical microscopy. However, the Ag signal was not detected at the EVA/glass interface, inferring limited ionic transport through the nominally 0.45 mm thick encapsulant. For the samples studied herein, the sulfur is believed by the process of elimination to come from the ambient air, diffusing into the module through the permeable polymer backsheet.

14 SOLAR ENERGY↗

Fragmentation of photovoltaic backsheets after accelerated weathering exposure

The backsheet of a photovoltaic (PV) module functions primarily to provide safe operation through electrical insulation and protect the interior from environmental exposure. For most applications, backsheets consist of opaque, but highly reflective, films that protect inner layers from degradation from ultraviolet (UV) light. Backsheets can fail if they delaminate or form cracks under strain. In a PV module, the maximum strains that can be applied are only on the order of a few percent. The greatest strains are likely to be highly localized around topographical features. Therefore, to assess the likelihood of a crack being initiated in a backsheet, we apply small amplitude strains to backsheet films under microscopic examination using a laser scanning confocal microscope. Furthermore, this allows us to monitor both the depth and density of cracks as well as the onset strain. Here we perform these measurements after exposure to UV light.

14 SOLAR ENERGY↗

Characterization of front contact degradation in monocrystalline and multicrystalline silicon photovoltaic modules following damp heat exposure

Reliability and durability tests play a key role in the photovoltaic (PV) industry by minimizing potential failure risks for both existing and new cell and module technologies. In this work, a detailed study of contact degradation in monocrystalline and multicrystalline PV modules is performed. The modules are subjected to a sequence of damp heat (DH) exposures followed by electrical characterization after each step. Electroluminescence (EL) imaging shows different darkening patterns for monocrystalline modules compared to multicrystalline modules; the former shows darkening near the busbars and the latter shows it across virtually the entire cell surface. The primary loss mechanism is confirmed to be resistive after comparing the current-voltage (I–V) characteristics at each DH exposure step. Representative samples have been cored out from both the degraded modules and controls for materials characterization to gain further insights into the degradation mechanism. Top-down and cross-sectional scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and top-down high-resolution X-ray photoelectron spectroscopy (XPS) analysis performed on the cored samples confirm the degradation is due to metallization corrosion. Our study suggests that the difference in the darkening pattern can most likely be attributed to the different silver paste composition used for contacting each cell technology, particularly the composition of the glass frit.

36 MATERIALS SCIENCE↗

Technoeconomic Analysis of High-Value, Crystalline Silicon Photovoltaic Module Recycling Processes

Recycling is an important circular economy strategy, and for photovoltaics (PV), the one that has received the greatest research attention. Recycling of PV modules is required in Europe; everywhere else it competes in the market of end-of-life options, where cost is a primary decision factor. The vast majority of PV modules sold globally are crystalline-silicon (c-Si); most of the rest of the market are cadmium telluride thin film modules whose primary manufacturer runs its own commercial-scale recycling program. While many different c-Si recycling approaches and technologies have been proposed, they generally lack accompanying cost estimates or enough process information to model costs. Herein we develop detailed estimates of seven categories of capital and operating costs along with estimates of revenue from recovered materials for each step in two proposed recycling processes for c-Si PV modules. Using these results, we develop a hypothetical third recycling process merging process steps from the original two, estimate surcharges required to achieve minimum sustainable prices for each recycling process, as well as consider how economies of scale could reduce costs. Increasing the purity of and identifying higher-value markets for recovered materials are approaches to reducing costs and increasing recycling rates in voluntary markets.

crystalline silicon↗

Dependence of adhesion on degradation mechanisms of ethylene co-vinyl acetate encapsulants over the lifetime of photovoltaic modules

The long-term reliability of encapsulation has a critical impact on the overall cost and effectiveness of photovoltaic modules. An often overlooked but important element of this reliability concerns adhesive degradation of the encapsulant, which results in delamination. This work critically examines the degradation mechanisms – deacetylation, β-scission, and hydrolytic depolymerization – primarily responsible for adhesion loss in ethylene co-vinyl acetate (EVA) encapsulants to provide evidence and clarity regarding the contribution of these mechanisms to the adhesive degradation over the lifetime of a module. EVA samples obtained from mini-modules exposed in two sets of controlled, accelerated conditions – with and without ultraviolet (UV) radiation – are characterized to find specific evidence for the proposed degradation mechanisms. The mini-modules were exposed up to 10,000 h, which represents up to 15–20 years in the field. Results affirm that initially, deacetylation dominates the degradation before scission takes over, followed by hydrolytic depolymerization. Additional analysis highlights the climacteric interdependency between deacetylation and hydrolytic depolymerization as it relates to eventual delamination, where deacetylation products catalyze interfacial hydrolysis reactions. Furthermore, effects occurring at a given interface are isolated, explicitly providing evidence for how these mechanisms are nonuniform throughout the thickness of the EVA. Results demonstrate that the EVA that interfaces with the glass as opposed to the cell experiences increased levels of degradation, explaining why this initially stronger interface becomes the preferential interface for delamination after longer periods of exposure. Additionally, elevated temperatures alone are shown to induce limited migration of sodium ions across the glass/EVA interface.

36 MATERIALS SCIENCE↗

In-situ determination of moisture- and temperature-driven deflection of an encapsulated Si photovoltaic cell

Module reliability and service lifetime are critical factors in improving photovoltaic system performance and reducing the levelized cost of electricity (LCOE). Soldering and lamination of the cell impart residual stresses that persist over time and superimpose additional loads during operation. This paper demonstrates the use of X-ray Topography (XRT) to image in-situ the dynamic response of a glass/backsheet mini-module upon drying at elevated temperature after saturation at humidity levels compatible with accelerated testing. The local water content in the encapsulant is also determined in-situ over time via Water Reflectometric Detection (WaRD), with diffusion of water in the front (glass side) and rear (backsheet side) resolved. As water diffuses out from the back of the glass/backsheet module, the cell curves towards the backsheet concomitantly. Here we find that the cell edges deflect 40μm out-of-plane with respect to its center while the encapsulant dries, compared to ~100 μm deflection when heating from 25°C to 85°C. The local cell deflections (changes in cell orientation) are correlated with the dynamic loss of water in the backside encapsulant. We conclude that the observed cell deflections are the result of hygroscopic stress induced by the encapsulant upon moisture outdiffusion. Therefore, the cell experiences a continually changing stress state and curvature dependent on local humidity and temperature. Depending on cell architecture and interconnection, this “breathing” mode of the cell may induce wear out and fatigue of the interconnects, affect the electrical connection of cracked pieces or cause failure near the interconnected edges of two cells.

14 SOLAR ENERGY↗

Mitigating urban climate-energy feedback with citywide building-integrated photovoltaics implementation

Urban heat islands (UHIs) intensify cooling demands, whose waste heat further exacerbates UHI, creating a self-reinforcing feedback loop. Building-integrated photovoltaics (BIPV) can break this cycle by generating electricity and altering urban climate-energy interactions, yet its net impact remains unresolved. Using a cross-scale modeling framework for 118,521 buildings in Hong Kong, we demonstrate that BIPV glazing reduces cooling demand through improved insulation and lower solar heat gain, while inducing diurnal thermal asymmetry of daytime warming (up to +1.9°C) and nighttime cooling (up to −2.5°C). This microclimate regulation indirectly contributes to a 0.6% reduction in citywide building energy use. Cumulative savings from electricity generation and reduced energy use reach 4.7% (2,060.2 GWh) and 10.1% (4,401.3 GWh) under low- and high-coverage deployment, respectively, with building-level savings of −20.1% ± 11.7% (mean ± SD) at high coverage. We establish BIPV as a configurable climate-energy regulator that enables net-zero, heat-resilient planning and quantifies deployment trade-offs in cooling-dominated cities worldwide.

Building-integrated photovoltaics (BIPV)↗

Organic Photovoltaic Efficiency Predictor: Data-Driven Models for Non-Fullerene Acceptor Organic Solar Cells

In the design of organic solar cells, there has been a need for materials with high power conversion efficiencies. Scharber’s model is commonly used to predict efficiency; however, it exhibits poor performance with new non-fullerene acceptor (NFA) devices, since it was designed for fullerene-based devices. In this work, an empirical model is proposed that can be a more accurate alternative for NFA organic solar cells. Additionally, many screening studies use computationally expensive methods. A model based on using semiempirical simplified time-dependent density functional theory (sTD-DFT) as an alternative method can accelerate the calculations and yield a similar accuracy. The models presented in this paper, termed organic photovoltaic efficiency predictor (OPEP) models, have shown significantly lower errors than previous models, with OPEP/B3LYP yielding errors of 1.53% and OPEP/sTD- DFT of 1.55%. As a result, the proposed computational models can be used for the fast and accurate screening of new high-efficiency NFAs/donor pairs.

14 SOLAR ENERGY↗

Light Management in Bifacial Photovoltaics with Spectrally Selective Mirrors

Spectrally-selective mirrors that simultaneously provide above-bandgap anti-reflection and sub-bandgap light rejection are tested for their ability to provide passive cooling to partially sub-bandgap transparent bifacial photovoltaics. The optical and thermal benefits of both idealized and real, low-complexity spectrally-selective mirrors on single-axis tracking, bifacial PERC arrays under realistic conditions are tested via rigorous finite element simulations. Four- and six-layer mirror designs increased carrier generation beyond what traditional antireflection coatings can provide without the associated cell heating. Here, idealized mirrors were found to provide up to 2.4 °C of cooling when included on both air/glass interfaces of the bifacial module.

14 SOLAR ENERGY↗

A Multi-modal Approach to Understanding Degradation of Organic Photovoltaic Materials

State-of-the-art organic photovoltaic (OPV) materials are composed of complex, chemically diverse polymeric and molecular structures that form highly intricate solid-state interactions, collectively yielding exceptional tunability in performance and aesthetics. These properties are especially attractive for semitransparent power-generating windows or shades in living environments, greenhouses, or other architectural integrations. However, before such a future is realized, a broader and deeper understanding of property stability must be acquired. Stability during operating and environmental conditions is critical, namely, material color steadfastness, optoelectronic performance retention, morphological rigidity, and chemical robustness. To date, no single investigation encompasses all four distinct, yet interconnected, metrics. Here, we present a multimodal strategy that captures a dynamic and interconnected evolution of each property during the course of an accelerated photobleaching experiment. We demonstrate this approach across relevant length scales (from molecular to visual macroscale) using X-ray photoelectron spectroscopy, grazing-incidence X-ray scattering, microwave conductivity, and time-dependent photobleaching spectroscopies for two high-performance semitransparent OPV blends—PDPP4T:PC 60 BM and PDPP4T:IEICO-4F, with comparisons to the stabilities of the individual components. We present direct evidence that specific molecular acceptor (fullerene vs nonfullerene) designs and the resulting donor–acceptor interactions lead to distinctly different mechanistic routes that ultimately arrive at what is termed “OPV degradation.” We directly observe a chemical oxidation of the cyano endcaps of the IEICO-4F that coincides with a morphological change and large loss in photoconductivity while the fullerene acceptor-containing blend demonstrates a significantly greater fraction of oxygen uptake but retains 55% of the photoconductivity. Finally, this experimental roadmap provides meaningful guidance for future high-throughput, multimodal studies, benchmarking the sensitivity of the different analytical techniques for assessing stability in printable active layers, independent of complete device architectures.

14 SOLAR ENERGY↗

Characterizing and Improving the Thermal Stability of Organic Photovoltaics Based on Halogen-Rich Non-Fullerene Acceptors

In this work, the thermal stability of inverted, halogen-rich non-fullerene acceptor (NFA)-based organic photovoltaics (OPVs) with MoO x as the hole transporting layer is studied at temperatures up to 80°C. Over time, the power conversion efficiency shows a “check-mark” shaped thermal aging pattern, featuring an early decrease, followed by a long-term recovery. A high Cl concentration at the BHJ/MoO x interface in the thermally aged device is found using energy dispersive X-ray spectroscopy. X-Ray photoelectron spectroscopy shows that the MoO x is chlorinated after thermal aging. With bulk quantum efficiency analysis, we propose an explanation to the check-mark shaped pattern. Inserting a thin C 70 layer between the BHJ and MoO x suppresses the thermal degradation mechanisms, resulting in 3 orders of magnitude increase in device lifetime at 80°C.