At least 595 records · Page 33

High-temperature oxidation of a rapidly solidified amorphous Ta-Ir alloy

The oxidation products formed at 500 and 700 C on an amorphous Ta-44.5 at. pct Ir alloy in an Ar-0.1 percent O2 gas mixture were characterized using SEM, XRD, EPMA, TEM, STEM, AES, and XPS. Initially, a thin (3-4 nm) layer of Ta2O5 formed at the surface of the alloy. Continued growth of the Ta2O5, which occurred very rapidly, involved diffusion of oxygen anions from the Ta2O5/gas interface to the alloy/Ta2O5 interface, where tantalum was selectively oxidized. Because the oxide grew more quickly than iridium could diffuse back into the alloy, the iridium coalesced into platelets of crystalline iridium-rich alloy that were oriented approximately parallel to the oxide/alloy interface, and which became embedded in a matrix of Ta2O5. The unoxidized core remained in the glassy state. The oxidation process and/or the dissolution of oxygen into the unoxidized alloy caused the alloy to become embrittled.

Cotell, Catherine M.↗

Slip casting and extruding shapes of rhemium with metal oxide additives. Part 2: Development of grain stabilized rhenium parts for resistojets

The adaptation of the powdered particle process used for pure metal oxides to the coprocessing of rhenium oxides suitable to produce pure miniature resistojet hardware has been successful. Both slip casting and extrusion processes were used. The metal oxide ZrO2 was stabilized into the cubic phase with Y2O3, for use as a potentially grain stabilizing additive to rhenium. Straight meter long tubing in two sizes are reported. Tubing suitable for resistojet ohmic heater use of fully fired dimensions of nominally 3.8 mm o.d. x 2.2 mm i.d.. and 1.26 mm o.d. x .45 mm i.d. with 0, 0.5, 1.0 and 5.0% zirconia additives were produced for further study. Photomicrographs of these are discussed. The addition of the metal oxide zirconia to rhenium resulted in more dense and less porous parts. The additions of phase stabilized zirconia most likely act as a sintering aid. Tubes of varying diameter were slip cast which were representative of miniature pressure cases.

Barr, Francis A.↗

Oxidation behavior of FeAl+Hf,Zr,B

The oxidation behavior of Fe-40Al-1Hf, Fe-40Al-1Hf-0.4B, and Fe-40Al-0.1Zr-0.4B (at. percent) alloys was characterized after 900, 1000, and 100 C exposures. Isothermal tests revealed parabolic kinetics after a period of transitional theta-alumina scale growth. The parabolic growth rates for the subsequent alpha-alumina scales were about five times higher than those for NiAl+0.1Zr alloys. The isothermally grown scales showed a propensity toward massive scale spallation due to both extensive rumpling from growth stresses and to an inner layer of HfO2. Cyclic oxidation for 200 1-hr cycles produced little degradation at 900 or 1000 C, but caused significant spallation at 1100 C in the form of small segments of the outer scale. The major difference in the cyclic oxidation of the three FeAl alloys was increased initial spallation for FeAl+Zr,B. Although these FeAl alloys showed many similarities to NiAl alloys, they were generally less oxidation resistant. It is believed that this resulted from nonoptimal levels of dopants and larger thermal expansion mismatch stresses.

Smialek, James L.↗

Pretreatment of CO oxidation catalysts

CO oxidation catalysts with high activity in the range of 25 C to 100 C are important for long-life, closed-cycle operation of pulsed carbon dioxide 2 lasers. A reductive pretreatment with either CO or H sub 2 was shown to significantly enhance the activity of a commerically-available platinum on tin (IV) oxide (Pt/SnO2) catalyst relative to an oxidative or inert pretreatment or no pretreatment. Pretreatment at temperatures of 175 C and above caused an initial dip in observed CO or O sub 2 loss or CO sub 2 formation in a test gas mixture of 1 percent CO and 0.5 percent O sub 2 in a He gas matrix before a steady-state yield was obtained. This dip was found to be caused by dehydration of the surface of the catalyst and was readily eliminated by humidifying the catalyst or the test gas mixture. It was also found that too much moisture resulted in a lower overall yield of CO sub 2. Under similar conditions, it is hypothesized that the effect of the humidification is to increase the concentration of OH groups on the surface of the catalyst. The effect of having high concentration of CO sub 2 in the test gas mixture upon the loss of CO and O sub 2 as well as the effect of periods of relaxation of the catalyst under non-test gas conditions was studied. The purpose of these studies was to gain an insight into the mechanism of CO oxidation on this type of catalyst.

Vannorman, John D.↗

Microbial reduction of manganese oxides - Interactions with iron and sulfur

Alteromonas putrefaciens (strain MR-1) is capable of rapid Mn(IV) reduction under conditions of neutral pH and temperatures characteristic of the Oneida Lake, New York, sediments from which it was isolated. MR-1 also reduces Fe(3+) to Fe(2+), and disproportionates thiosulfate to sulfide and sulfite; independently, the Fe(2+) and sulfide act as rapid reductants of Mn. The addition of Fe(3+) or thiosulfate to cultures of MR-1 in the presence of oxidized Mn increases the rate and the extent of Mn reduction relative to that observed in the absence of Fe(3+) or thiosulfate. Furthermore, when Fe(3+) and Mn oxides are present conjointly, Fe(2+) does not appear until the reduction of the oxidized Mn is complete. These results demonstrate that the observed rates of Fe(2+) and sulfide production may underestimate the total rates of Fe and sulfate reduction in those environments containing oxidized Mn. These results also demonstrate the potential impact that a single microbe can exert on sediment geochemistry, and provide the basis for preliminary models of the complexity of microbial and geochemical interactions that occur.

Myers, Charles R.↗

Fundamental kinetics and mechanistic pathways for oxidation reactions in supercritical water

Oxidation of the products of human metabolism in supercritical water has been shown to be an efficient way to accomplish the on-board water/waste recycling in future long-term space flights. Studies of the oxidation kinetics of methane to carbon dioxide in supercritical water are presented in this paper in order to enhance the fundamental understanding of the oxidation of human waste compounds in supercritical water. It is concluded that, although the elementary reaction models remain the best hope for simulating oxidation in supercritical water, several modifications to existing mechanisms need to be made to account for the role of water in the reaction mechanism.

Webley, Paul A.↗

Submicron nickel-oxide-gold tunnel diode detectors for rectennas

The characteristics of a metal-oxide-metal (MOM) tunnel diode made of nickel, nickel-oxide, and gold, designed and fabricated by standard integrated circuit technology for use in FIR rectennas, are presented. The MOM tunnel diode was formed by overlapping a 0.8-micron-wide layer of 1000-A of nickel, which was oxidized to form a thin layer of nickel oxide, with a 1500 A-thick layer of gold. The dc current-voltage characteristics of the MOM diode showed that the current dependence on voltage was linear about zero bias up to a bias of about 70 mV. The maximum detection of a low-level signal (10-mV ac) was determined to be at a dc voltage of 70 mV across the MOM diode. The rectified output signal due to a chopped 10.6-micron CO2 laser incident upon the rectenna device was found to increase with dc bias, with a maximum value of 1000 nV for a junction bias of 100 mV at room temperature.

Hoofring, A. B.↗

Surface-catalyzed air oxidation reactions of hydrazines: Tubular reactor studies

The surface-catalyzed air oxidation reactions of hydrazine, monomethylhydrazine, unsymmetrical dimethylhydrazine, symmetrical dimethylhydrazine, trimethylhydrazine and tetramethylhydrazine were investigated in a metal-powder packed turbular flow reactor at 55 plus or minus 3 C. Hydrazine was completely reacted on all surfaces studied. The major products of monomethylhydrazine (MMH) oxidation were methanol, methane and methyldiazene. The di-, tri- and tetra-methyl hydrazines were essentially unreactive under these conditions. The relative catalytic reactivities toward MMH are: Fe greater than Al2O3 greater than Ti greater than Zn greater than 316 SS greater than Cr greater than Ni greater than Al greater than 304L SS. A kinetic scheme and mechanism involving adsorption, oxidative dehydrogenation and reductive elimination reactions on a metal oxide surface are proposed.

Kilduff, Jan E.↗

Process for making a noble metal on tin oxide catalyst

A quantity of reagent grade tin metal or compound, chloride-free, and high-surface-area silica spheres are placed in deionized water, followed by deaerating the mixture by boiling and adding an oxidizing agent, such as nitric acid. The nitric acid oxidizes the tin to metastannic acid which coats the spheres because the acid is absorbed on the substrate. The metastannic acid becomes tin oxide upon drying and calcining. The tin-oxide coated silica spheres are then placed in water and boiled. A chloride-free precious metal compound in aqueous solution is then added to the mixture containing the spheres, and the precious metal compound is reduced to a precious metal by use of a suitable reducing agent such as formic acid. Very beneficial results were obtained using the precious metal compound tetraammine platinum(II) hydroxide.

Upchurch, Billy T.↗

Effects of grain size and grain boundary on critical current density of high T(sub c) superconducting oxides

By means of adding impurity elements in high T sub c oxides, the effects were studied of grain size and grain boundary on the critical current density of the following systems: YBa2Cu3O(7-y) and Bi-Pr-Sr-Ca-Cu-O. In order to only change the microstructure instead of the superconductivity of the grains in the samples, the impurity elements were added into the systems in terms of the methods like this: (1) substituting Y with the lanthanide except Pr, Ce, and Tb in YBa2Cu3O(7-y) system to finning down grains in the samples, therefore, the effect can be investigated of the grain size on the critical current density of 1:2:3 compounds; (2) mixing the high T sub c oxides with the metal elements, such as Ag, according to the composition of (high T sub c oxide)1-xAgx to metallize the grain boundaries in the samples, studying the effect of the electric conductivity of the grain boundaries on the critical current density; (3) adding SiO2, PbO2, and SnO2 into the high T sub c oxide to form impurity phases in the grain boundaries, trying to find out the effects of the impurity phases or metalloid grain boundaries on the critical current density of the high T sub c superconductors. The experimental results indicate that in the case of of the presence of the metalloid grain boundaries finning down grains fails to enhance the j sub c, but restrains it strongly, the granular high T sub c superconductors with the small size grains coupled weakly is always the low j sub c system.

Zhao, Y.↗

Oxidation behavior of FeAl+Hf,Zr,B

The oxidation behavior of Fe-40Al-1Hf, Fe-40Al-1Hf-0.4B, and Fe-40Al-0.1Zr-0.4B (at. percent) alloys was characterized after 900, 1000, and 100 C exposures. Isothermal tests revealed parabolic kinetics after a period of transitional theta-alumina scale growth. The parabolic growth rates for the subsequent alpha-alumina scales were about five times higher than those for NiAl+0.1Zr alloys. The isothermally grown scales showed a propensity toward massive scale spallation due to both extensive rumpling from growth stresses and to an inner layer of Hf02. Cyclic oxidation for 200 1-hr cycles produced little degradation at 900 or 1000 C, but caused significant spallation at 1100 C in the form of small segments of the outer scale. The major difference in the cyclic oxidation of the three FeAl alloys was increased initial spallation for FeAl+Zr,B. Although these FeAl alloys showed many similarities to NiAl alloys, they were generally less oxidation resistant. It is believed that this resulted from nonoptimal levels of dopants and larger thermal expansion mismatch stresses.

Smialek, James L.↗

Oxidation kinetics of model compounds of metabolic waste in supercritical water

In this NASA-funded study, the oxidation kinetics of methanol and ammonia in supercritical water have been experimentally determined in an isothermal plug flow reactor. Theoretical studies have also been carried out to characterize key reaction pathways. Methanol oxidation rates were found to be proportional to the first power of methanol concentration and independent of oxygen concentration and were highly activated with an activation energy of approximately 98 kcal/mole over the temperature range 480 to 540 C at 246 bar. The oxidation of ammonia was found to be catalytic with an activation energy of 38 kcal/mole over temperatures ranging from 640 to 700 C. An elementary reaction model for methanol oxidation was applied after correction for the effect of high pressure on the rate constants. The conversion of methanol predicted by the model was in good agreement with experimental data.

Webley, Paul A.↗

Investigation of anodic and chemical oxides grown on p-type InP with applications to surface passivation for n(+)-p solar cell fabrication

Most of the previously reported InP anodic oxides were grown on a n-type InP with applications to fabrication of MISFET structures and were described as a mixture of In2O3 and P2O5 stoichiometric compounds or nonstoichiometric phases which have properties similar to crystalline compounds In(OH)3, InPO4, and In(PO3)3. Details of the compositional change of the anodic oxides grown under different anodization conditions were previously reported. The use of P-rich oxides grown either by anodic or chemical oxidation are investigated for surface passivation of p-type InP and as a protective cap during junction formation by closed-ampoule sulfur diffusion. The investigation is based on but not limited to correlations between PL intensity and X-ray photoelectron spectroscopy (XPS) chemical composition data.

Faur, Maria↗

Advanced Launch System advanced development oxidizer turbopump program: Technical implementation plan

The Advanced Launch Systems (ALS) Advanced Development Oxidizer Turbopump Program has designed, fabricated and demonstrated a low cost, highly reliable oxidizer turbopump for the Space Transportation Engine that minimizes the recurring cost for the ALS engines. Pratt and Whitney's (P and W's) plan for integrating the analyses, testing, fabrication, and other program efforts is addressed. This plan offers a comprehensive description of the total effort required to design, fabricate, and test the ALS oxidizer turbopump. The proposed ALS oxidizer turbopump reduces turbopump costs over current designs by taking advantage of design simplicity and state-of-the-art materials and producibility features without compromising system reliability. This is accomplished by selecting turbopump operating conditions that are within known successful operating regions and by using proven manufacturing techniques.

Ferlita, F.↗

A comparison of fiber effects on polymer matrix composite oxidation

A number of thermo-oxidative stability studies addressing the effects of fiber reinforcement on composite thermal stability and influence of geometry on the results of aging studies were performed at NASA-Lewis. The information presented herein, a compilation of some results from these studies, shows the influence of the reinforcement fibers on the oxidative degradation of various PMR-15 composites. Reinforcement of graphite and ceramics were studied and three composite oxidation mechanisms were observed. One was a dominant attack of the reinforcement fiber, the second was the aggressive oxidation of the matrix material, and the third was interfacial degradation.

Bowles, Kenneth J.↗

Nitric oxide in star-forming regions - Further evidence for interstellar N-O bonds

Nitric oxide has been newly detected toward several star-forming clouds, including Orion-KL, Sgr B2(N), W33A, W51M, and DR21(OH) via its J = 3/2-1/2 transitions near 150 GHz, using the FCRAO 14 m telescope. Both lambda-doubling components of NO were observed toward all sources. Column densities derived for nitric oxide in these clouds are 10 to the 15th-10 to the 16th/sq cm, corresponding to fractional abundances of 0.5-1.0 x 10 to the -8th, relative to H2. Toward Orion-KL, the NO line profile suggests that the species arises primarily from hot, dense gas. Nitric oxide may arise from warm material toward the other clouds as well. Nitric oxide in star-forming regions could be synthesized by high-temperature reactions, although the observed abundances do not disagree with values predicted from low-temperature, ion-molecule chemistry by more than one order of magnitude.

Ziurys, L. M.↗

Effect of sinter fracture and ohmic resistance on capacity retention in the nickel oxide electrode

The lifetime of batteries which utilize the nickel oxide electrode is often limited because this electrode loses a significant portion of its capacity as it is cycled. It is asserted that this capacity loss may often be attributed to cracking or separation of the conductive nickel sinter in the electrode, which forces electronic current to pass through the poorly conducting hydrated oxide and thus imposes a significant ohmic resistance. The model indicates that the oxide develops a nearly insulating layer which prevents complete discharge in the cycled electrode at usable rates. The capacity retention can be improved by reducing the cyclic stresses or strengthening the current collecting structure, redistributing it to provide a shorter current path through the solid phase, or by increasing the conductivity of the oxide to delay the formation of an insulating layer.

Lanzi, Oscar↗

Crack healing in silicon nitride due to oxidation

The crack healing behavior of a commercial, MgO-containing, hot pressed Si3N4 was studied as a function of temperature in oxidizing and inert annealing environments. Crack healing occurred at a temperature 800 C or higher due to oxidation regardless of crack size, which ranged from 100 microns (indentation crack) to 1.7 mm (SEPB precrack). The resulting strength and apparent fracture toughness increased at crack healing temperature by 100 percent and 300 percent, respectively. The oxide layer present in the crack plane was found to be highly fatigue resistant, indicating that the oxide is not solely silicate glass, but a mixture of glass, enstatite, and/or cristobalite that was insensitive to fatigue in a room temperature water environment.

Choi, Sung R.↗