Water-Fed, Photovoltaic-Driven Anion-Exchange Membrane Water Electrolysis for Solar Hydrogen Production

Direct coupled photovoltaic (PV)-electrolysis is a promising approach for low-cost hydrogen production, avoiding the need for separate electricity generation. Without solar concentration, the operating current densities of a PV-electrolyzer are small, and low capital costs are needed to reach hydrogen production cost targets (<$2/kg). Anion-exchange membrane (AEM) electrolyzers could be well-suited for this application due to their ability to use platinum group metal (PGM)-free catalysts and operate without supporting electrolytes, but a water-fed PV-AEM system has not yet been demonstrated. In this work, the performance of two AEM electrolyzer designs under pure-water, low-temperature, and diurnal-cycling conditions was evaluated. A simple PV-electrolyzer system design with direct electric coupling to a commercial 84 cm2 Si mini module and passive heating and water flow to the electrolyzer was used for on-sun testing in October 2025. The best-performing PV-AEM system achieved an average solar-to-hydrogen (STH) efficiency of 6.6% and a production rate of 15 mg/kWh/m2 of solar irradiance over 11 days. Minimal electrolyzer corrosion was observed, with no loss in efficiency over the diurnal cycles. While highlighting areas for improved electrolyzer and system design, this work is a proof of concept for distributed hydrogen production using inexpensive and abundant materials.

08 HYDROGEN↗

Applying laboratory methods for durability assessment of vitrified material to archaeological samples

Abstract Laboratory testing used to assess the long-term chemical durability of nuclear waste forms may not be applicable to disposal because the accelerated conditions may not represent disposal conditions. To address this, we examine the corrosion of vitrified archeological materials excavated from the near surface of a ~1500-year old Iron Age Swedish hillfort, Broborg, as an analog for the disposal of vitrified nuclear waste. We compare characterized site samples with corrosion characteristics generated by standard laboratory durability test methods including the product consistency test (PCT), the vapor hydration test (VHT), and the EPA Method 1313 test. Results show that the surficial layer of the Broborg samples resulting from VHT displays some similarities to the morphology of the surficial layer formed over longer timescales in the environment. This work provides improved understanding of long-term glass corrosion behavior in terms of the thickness, morphology, and chemistry of the surficial features that are formed.

36 MATERIALS SCIENCE↗

An Integrated Approach for Hydrogen Production and Storage in Complex Hydrides of Transitional Elements and Carbonbased Nanostructural materials (Final Report)

The goal of our project is to improve solar-to-hydrogen generation efficiency of the PhotoElectroChemical (PEC) conversion process by developing photoanodes with high absorption efficiency in the visible region of the solar radiation spectrum and to increase photo-corrosion resistance of the electrode for generating hydrogen from water. To meet this goal, we synthesized nanostructured heterogeneous semiconducting photoanodes with a higher light absorption efficiency compared to that of TiO 2 and used a corrosion protective layer of TiO 2 . While the advantages of photoelectrochemical (PEC) production of hydrogen have not yet been realized, the recent developments show emergence of new nanostructural designs of photoanodes and choices of materials with significant gains in photoconversion efficiency.

14 SOLAR ENERGY↗

Regenerative Gas Dryer for In-Situ Propellant Production

Rocket propellant can be produced anywhere that water is found by splitting it into hydrogen and oxygen, potentially saving several tons of mass per mission and enabling the long term presence of humans in space beyond LEO. When water is split into hydrogen and oxygen, the gaseous products can be very humid (several thousand ppm). Propellant-grade gases need to be extremely dry before being converted into cryogenic liquids (less than 26 ppm water for grade B Oxygen). The primary objective of this project is to design, build and test a regenerative gas drying system that can take humid gas from a water electrolysis system and provide dry gas (less than 26ppm water) to the inlet of a liquefaction system for long durations. State of the art work in this area attempted to use vacuum as a means to regenerate desiccant, but it was observed that water would migrate to the dry zone without a sweep gas present to direct the desorbed vapor. Further work attempted to use CO2 as a sweep gas, but this resulted in a corrosive carbonic acid. In order for in-situ propellant production to work, we need a way to continuously dry humid gas that addresses these issues.

Paz, Aaron↗

Experimental Demonstration of Advanced Palladium Membrane Separators for Central High Purity Hydrogen Production

The overall objectives for this project were to: (1) confirm the high stability and resistance of a PdCu trimetallic alloy to carbon and carbide formation and, in addition, resistance to sulfur, halides, and ammonia; (2) develop a sulfur, halide, and ammonia resistant alloy membrane with a projected hydrogen permeance of 25 m{sup 3}m{sup -2}atm{sup -0.5}h{sup -1} at 400 C and capable of operating at pressures of 12.1 MPa ({approx}120 atm, 1750 psia); and (3) construct and experimentally validate the performance of 0.1 kg/day H{sup 2} PdCu trimetallic alloy membrane separators at feed pressures of 2 MPa (290 psia) in the presence of H{sub 2}S, NH{sub 3}, and HCl. This project successfully increased the technology readiness level of palladium-based metallic membranes for hydrogen separation from coal-biomass gasifier exhaust or similar hydrogen-containing gas streams. The reversible tolerance of palladium-copper (PdCu) alloys was demonstrated for H{sub 2}S concentrations varying from 20 ppmv up to 487 ppmv and NH{sub 3} concentrations up to 9 ppmv. In addition, atomistic modeling validated the resistance of PdCu alloys to carbon formation, irreversible sulfur corrosion, and chlorine attack. The experimental program highlighted two key issues which must be addressed as part of future experimental programs: (1) tube defects and (2) non-membrane materials of construction. Four out of five FCC PdCu separators developed leaks during the course of the experimental program because {approx}10% of the alloy tubes contained a single defect that resulted in a thin, weak point in the tube walls. These defects limited operation of the existing tubes to less than 220 psig. For commercial applications of a PdCu alloy hydrogen separator under high sulfur concentrations, it was determined that stainless steel 316 is not suitable for housing or supporting the device. Testing with sulfur concentrations of 487 {+-} 4 ppmv resulted in severe corrosion of the stainless steel components of the separators. The project identified an experimental methodology for quantifying the impact of gas contaminants on PdCu alloy membrane performance as well as an atomistic modeling approach to screen metal alloys for their resistance to irreversible sulfur corrosion. Initial mathematical descriptions of the effect of species such as CO and H{sub 2}S were developed, but require further experimental work to refine. At the end of the project, an improvement to the experimental approach for acquiring the necessary data for the permeability model was demonstrated in preliminary tests on an enhanced PdCu separator. All of the key DOE 2010 technical targets were met or exceeded except for the hydrogen flux. The highest flux observed for the project, 125 ft{sup 3}ft{sup -2}h{sup -1}, was obtained on a single tube separator with the aforementioned enhanced PdCu separator with a hydrogen feed pressure of 185 psig at 500 C.

08 HYDROGEN↗

Corrosion Assessment of Candidate Materials for the SHINE Subcritical Assembly Vessel and Components—FY14 Report

Laboratory corrosion testing of candidate alloys—including Zr-4 and Zr-2.5Nb representing the target solution vessel, and 316L, 2304, 304L, and 17-4 PH stainless steels representing process piping and balance-of-plant components—was performed in support of the proposed SHINE process to produce 99 Mo from low-enriched uranium. The test solutions used depleted uranyl sulfate in various concentrations and incorporated a range of temperatures, excess sulfuric acid concentrations, nitric acid additions (to simulate radiolysis product generation), and iodine additions. Testing involved static immersion of coupons in solution and in the vapor above the solution, and was extended to include planned-interval tests to examine details associated with stainless steel corrosion in environments containing iodine species. A large number of galvanic tests featuring couples between a stainless steel and a zirconium-based alloy were performed, and limited vibratory horn testing was incorporated to explore potential erosion/corrosion features of compatibility. In all cases, corrosion of the zirconium alloys was observed to be minimal, with corrosion rates based on weight loss calculated to be less than 0.1 mil/year with no change in surface roughness. The resulting passive film appeared to be ZrO 2 with variations in thickness that influence apparent coloration (toward light brown for thicker films). Galvanic coupling with various stainless steels in selected exposures had no discernable effect on appearance, surface roughness, or corrosion rate. Erosion/corrosion behavior was the same for zirconium alloys in uranyl sulfate solutions and in sodium sulfate solutions adjusted to a similar pH, suggesting there was no negative effect of uranium resulting from fluid dynamic conditions aggressive to the passive film. Corrosion of the candidate stainless steels was similarly modest across the entire range of exposures. However, some sensitivity to corrosion of the stainless steels was observed in solutions with 50 wppm iodine (the actual SHINE process expects 0.1–1 wppm) with the highest corrosion rates (up to ~6 mil/year) observed on specimens exposed in the vapor phase. Lower concentrations of iodine species (5 or 28 wppm) proved much less corrosive, and the planned-interval data indicated that metal corrodibility decreased with time for all immersed exposures and, with one minor exception, all vapor exposures. Little change in susceptibility to corrosion was observed as a result of nitric acid additions to the test environment (simulating radiolysis products). The trend toward reduced corrosion (immersion and vapor phase) with decreasing iodine concentration suggests that, at the expected conditions in the SHINE process, it is unlikely that iodine species will generate a general corrosion concern for the candidate stainless steels.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Corrosion Studies Of Raw And Treated Biomass-Derived Pyrolysis Oils

Rapid pyrolysis of biomass generates a liquid with properties that are particularly attractive for production of hydrocarbons that could be substituted for liquid fuels derived from petroleum. However, the high oxygen content of the biomass derived liquids presents a number of problems because of the high water content and the considerable concentration of carboxylic acids. Measurements of total acid number (TAN) of pyrolysis oil (bio-oil) samples show that values in the 90-100 range are fairly common. This level of acidity has been shown to cause corrosion problems that have to be addressed in the selection of structural materials that are used in the production, subsequent processing, storage and transport of the pyrolysis oils. Chemical analyses have been performed and laboratory corrosion studies have been conducted in order to assess the aggressiveness of the raw pyrolysis oil from several sources as well as the corrosion caused by a bio-oil that has been treated to reduce the acid and oxygen content. Components of biomass pyrolyzers have also been fabricated from various candidate alloys, and these components have been exposed for extended periods during operation of the pyrolyzers. This paper will report on results of these analyses and corrosion studies.

02 PETROLEUM↗

Microstructure evolution during low-strain thermo-mechanical processing and its repercussion on intergranular corrosion in alloy 600H

Highlights: • GBE microstructure in alloy 600H is realized through the sole activation of SIBM. • Higher TRD size and lower fractal dimension are characteristics of GBE microstructure. • Partially/fully recrystallized specimen shows higher DOS than as-received condition. • GBE specimen shows remarkable resistance against percolation and grain dropping. • Extent of percolation is governed by residual strain and random HAGBs connectivity. - Abstract: The current investigation deals with the evolution of microstructures as a consequence of varying processing parameters viz. extent of deformation, annealing temperature and time during grain boundary engineering (GBE) type thermo-mechanical processing in alloy 600H. Furthermore, the influence of the various product microstructures (viz. partially recrystallized, fully recrystallized and GBE) on intergranular corrosion is evaluated and compared with the as-received condition. Detailed characterization of the as-processed specimens have revealed that lower extent of deformation (7.5%) followed by a longer annealing treatment (i.e. 60 min) at a higher temperature (1373 K) could lead to a GBE microstructure with a higher proportion of Σ3{sup n} boundaries (~72%) due to the predominant activation of multiple twinning. In contrast, the specimens associated with moderately higher extent of deformation (10% and 15%) have revealed the occurrence of static recrystallization. The GBE specimen has demonstrated an excellent resistance against percolation essentially due to its discontinuous random high angle boundaries (HAGBs) network. In contrast, the nucleation of the finer grains in the recrystallized specimens caused the regeneration of random HAGBs network (as substantiated by the fractal analysis) that leads to higher percolation and severe grain dropping. In spite of the similar grain boundary character distribution, the severity of corrosion is relatively lesser in the as-received condition than the completely recrystallized specimen owing to its coarse-grained microstructure that commendably retarded the diffusion of chromium from the grain interior to the boundary.

36 MATERIALS SCIENCE↗

MIS Shelf-Life Final Report for Plutonium Oxide Item 1000089 (SSR136 and SSR136A) from Rocky Flats Peroxide Precipitation and Calcination Process

A plutonium dioxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied to determine the gas generation and corrosion behavior in a storage environment. Sample 1000089 represents product-quality plutonium oxides produced in the Rocky Flats peroxide precipitation process currently stored in 3013 containers. This study followed over time the gas pressure and composition of a sample with nominally 0.5 wt% water in a sealed container with an internal volume scaled to 1/500th of the volume of a 3013 container. Gas compositions had been measured periodically over almost 13 years. The maximum observed gas pressure was 204 kPa and was related to a temperature excursion. The maximum observed gas pressure from gas generation was 126 kPa. The increase over the initial pressure of 86.7 kPa was due to the generation of hydrogen, oxygen, and nitrogen. Carbon dioxide, methane and carbon monoxide were minor components of the headspace gas. The material exhibited unusual behavior in that the atmosphere reached flammable levels of hydrogen and oxygen within the first 30 days and remained flammable for the duration of the experiment. It has been determined that the sample inside the reactor was a mixture of the AR material, material calcined at 800 °C, and material calcined at 950 °C. The experiment was terminated in 2012 and unloaded in 2016. A new reactor, SSR136A, was loaded with the original sample freshly calcined at 950 °C. The total pressure inside SSR136A remained close to the initial value of 93 kPa. The total pressure is composed of He (steady levels after the reloading) and hydrogen which is 10% of the reactor’s total pressure. Nitrogen and oxygen compose trace amounts of the reactor headspace. The internal components of SSR136 were inspected in 2021, five years after it was removed from the array. The inside surfaces of the inner bucket exposed to the original sample for 4,576 days had an etched appearance, and pit-like features were observed in the microscopic analysis. No corrosion was observed on the SSR136A inner bucket that held the freshly calcined sample that was exposed for 1,303 days.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advanced cryogenic propellant tank development status

The design and development of cryogenic propellant tanks with reduced weight and production costs is described with reference to applications for the National Launch System. The development program focused on the use of an aluminum-lithium alloy to demonstrate the production capability, manufacturability, and strength inherent in the novel material. Other key parameters for the alloy include fracture toughness, stress-corrosion resistance, and conformance to NASA specifications for cryogenic propellant tanks. The commercially produced aluminum-lithium alloy product forms are shown to operate acceptably in the temperature range for cryogenic propellant tanks. The alloy under consideration and the tank design are important advances in the development of ultralightweight launch-vehicle structures.

Scholz, E. F.↗

Investigation of Fission Product Interaction with the SiC Containment Layer of High Turnup TRISO Fuel Particles

Tri-structural Isotropic (TRISO) encapsulated fuel particles are used in high-temperature gas-cooled nuclear reactors. Fuel performance is limited by the propensity of metallic fission products to be released under high temperature testing to simulate hypothesized accident scenarios. The current particle design consists of a 350 μm or 425 μm UO{sub 2} or UCO fuel kernel surrounded by a 100μm porous carbon buffer layer, a 40μm inner pyrolytic carbon (IPyC) layer, a 35μm high-density silicon carbide (SiC) layer, and a 40μm outer pyrolytic carbon (OPyC) layer. Of interest is the fission product interaction with the SiC layer, which provides the most structural support and is the main barrier to the diffusion of fission products. Previous laboratory examination studies have indicated the release of Ag through seemingly intact particles and the localized corrosion of the SiC due to Pd. Although a number of studies have been conducted, the specifics of both the Ag and Pd reaction mechanisms, in addition to U and Pu, through SiC are currently not well understood. This work aims to understand the pathways and kinetics of these interactions under normal operation as well as accident conditions. In order to improve our understanding of this, we have the unique opportunity to examine irradiated TRISO particles to study post-irradiation effects on these materials. Experimental data is necessary to constrain the current models used to predict the behavior of fission products in the SiC layer of TRISO fuels. This work aims to understand the interaction of fission products with the SiC containment layer in TRISO particles. We have systematically examined three SiC shells from irradiated TRISO particles using XAFS, TEM, and EDS. Results indicate the formation of palladium silicides, and uranium and plutonium carbides. Additionally, silver is seen to be metallic. Preliminary microscopy results indicate fission products throughout the SiC layer of the TRISO particles, and microstructural changes have been observed between the as-irradiated and safety tested particles. These results have provided key information on the fission product transport behavior through irradiated SiC at varying temperatures. Knowledge of these reaction pathways will allow for better simulation of the long-term behavior of TRISO fuels. They may also suggest ways to modify the SiC layer to improve fuel performance and mitigate fission product release, which is critical for safety strategies required to commercialize these nuclear fuel technologies. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hot corrosion of TD nickel and TD nickel chromium in a high velocity gas stream.

Results of cyclical tests of TD nickel (2% thoria-dispersed nickel) and TD nickel chromium (2% thoria-dispersed nickel-20% chromium alloy) 1.5 mm (60 mil) sheet specimens for susceptibility to hot corrosion in a Mach 0.5 gas stream of Jet A-1 fuel combustion products containing 2 ppm sea salt. Tests as long as 500 one-hour cycles between room temperature and specimen hot zone temperatures of 899 C (1650 F), 982 C (1800 F), and 1149 C (2100 F) were performed. Evidence of hot corrosion was found for both materials in the 899 C (1650 F) and 982 C (1800 F) tests, but not at 1149 C (2100 F). It was concluded that because of high metal thickness losses neither alloy in sheet form is suitable for long-time engine application in a hot corrosion environment at temperatures of 982 C (1800 F) or above.

Sanders, W. A.↗

Superhydrophobic to superhydrophilic wettability transition of functionalized SiO 2 nanoparticles

The superhydrophobic and superhydrophilic surfaces and their transitions are of great interest for the production of self-cleaning, anti-biofouling, or corrosion-resistant materials. This research reports the wettability transition from superhydrophobic to superhydrophilic SiO 2 nanoparticles functionalized with 1H, 1H, 2H, 2H-perfluorooctyltriethoxysilane (POTS) and induced by temperature. The functionalization of these nanoparticles was confirmed by Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy (XPS), and transmission electron microscopy. The functionalization of SiO 2 nanoparticles with POTS resulted in superhydrophobic surfaces with water contact angles up to 157°. A sudden transition to superhydrophilic behavior with water contact angles (WCA) below 5° was observed when the sample was heat-treated at 500 °C, despite the presence of fluorine on the surface of these nanoparticles, as confirmed by XPS and transmission electron microscopy. XPS suggested that the transition was caused by the change in orientation of the fluoroalkyl molecules and its partial decomposition due to the loss of the –CF 3 group, resulting in shorter chains with a tail-end group with C–O bonds, which promoted the superhydrophilicity.

36 MATERIALS SCIENCE↗

Degradation of yttria-stabilized zirconia thermal barrier coatings by vanadium pentoxide, phosphorous pentoxide, and sodium sulfate

The presence of vanadium, phosphorus, and sodium impurities in petcoke and coal/petcoke blends used in integrated gasification combined cycle (IGCC) plants warrants a clear understanding of high-temperature material degradation for the development of fuel-flexible gas turbines. In this study, degradation reactions of free-standing air plasma-sprayed (APS) yttria-stabilized zirconia (YSZ) in contact with V{sub 2}O{sub 5}, P{sub 2}O{sub 5}, and Na{sub 2}SO{sub 4} were investigated at temperatures up to 1200{sup o}C. Phase transformations and microstructural development were examined using X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. Molten V{sub 2}O{sub 5} reacted with solid YSZ to form ZrV{sub 2}O{sub 7} at temperatures below 747{sup o}C. However, at temperatures above 747{sup o}C, molten V{sub 2}O{sub 5} reacted with YSZ to form yttrium vanadate (YVO{sub 4}). The formation of YVO{sub 4} led to the depletion of the Y2O{sub 3} stabilizer and deleterious transformation to the monoclinic ZrO{sub 2} phase. In addition, studies on YSZ degradation by Na{sub 2}SO{sub 4} and a Na{sub 2}SO{sub 4}+V{sub 2}O{sub 5} mixture (50-50 mol%) showed that Na{sub 2}SO{sub 4} itself had no effect on the degradation of YSZ. However, in the presence of V{sub 2}O{sub 5} at high temperatures, Na{sub 2}SO{sub 4} forms vanadate compounds having a lower melting point such as sodium metavanadate (610{sup o}C), which was found to degrade YSZ by the formation of YVO{sub 4} at a relatively lower temperature of 700{sup o}C. P{sub 2}O{sub 5} was found to react with APS YSZ by the formation of ZrP{sub 2}O{sub 7} at all the temperatures studied. At temperatures as low as 200{sup o}C and as high as 1200{sup o}C, molten P{sub 2}O{sub 5} was observed to react with solid YSZ to yield ZrP{sub 2}O{sub 7}, which led to the depletion of ZrO{sub 2} in YSZ that promoted the formation of the fluorite-cubic ZrO{sub 2} phase.

20 FOSSIL-FUELED POWER PLANTS↗

Molten Silicate Reactivity with Environmental Barrier Coating Materials for Gas Turbine Engine Applications

Rare earth (RE) disilicates are utilized in environmental barrier coatings (EBCs) to protect SiC-based ceramic matrix composites (CMCs) from destructive reactions with water vapor and other combustion species. These coating materials, however, degrade when exposed to molten silicate deposits primarily composed of calcium-magnesium aluminosilicates (CMAS). Coating materials are exposed to CMAS by engine ingestion of dust particulates from terrestrial sources during operation. Due to continual increases in engine operating temperature, it is important to understand the high temperature thermochemical mechanisms that drive corrosion of these materials. This work focuses on characterizing reaction products between disilicates and CMAS and optimizing coating chemistries to mitigate damage.

Stokes, Jamesa L.↗

Review of CTF's Fuel Rod Modeling Using FRAPCON-4.0's Centerline Temperature Predictions

Coolant Boiling in Rod Arrays-Two Fluid (COBRA-TF), or CTF1, is a nuclear thermal hydraulic subchannel code used throughout academia and industry. CTF's fuel rod modeling is originally developed for VIPRE code. Its methodology is based on GAPCON and FRAP fuel performance codes, and material properties are included from MATPRO handbook. This work focuses on review of CTF's fuel rod modeling to address shortcomings in CTF's temperature predictions. CTF is compared to FRAPCON which is U.S. NRC's steady-state fuel performance code for light-water reactor fuel rods. FRAPCON calculates the changes in fuel rod variables and temperatures including the effects of cladding hoop strain, cladding oxidation, hydriding, fuel irradiation swelling, densification, fission gas release and rod internal gas pressure. It uses fuel, clad and gap material properties from MATPRO. Additionally, it has its own models for fission gas release, cladding corrosion and cladding hydrogen pickup. It allows finite difference or finite element approaches for its mechanical model. In this study, FRAPCON-4.0 is used as a reference fuel performance code. In comparison, Halden Reactor Data for IFA432 Rod 1 and Rod 3. CTF simulations are performed in two ways; informing CTF with gap conductance value from FRAPCON, and using CTF's dynamic gap conductance model. First case is chosen to show temperature is predicted correctly with CTF's models for thermal and cladding conductivities once gap conductance is provided. Latter is to review CTF's dynamic gap conductance model. These Halden test cases are selected to be representative of cases with and without any physical contact between fuel-pellet and clad while reviewing functionality of CTF's dynamic gap conductance model. Improving the CTF's dynamic gap conductance model will allow prediction of fuel and cladding thermo-mechanical behavior under irradiation, and better temperature feedbacks from CTF in transient calculations.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of Oxyfuel Combustion on Superheater Corrosion

Combustion of coal in an oxygen environment (as opposed to air) will facilitate the sequestering of carbon dioxide by minimizing the amount of nitrogen in the exit gas stream. The presence of higher levels of certain gases associated with oxyfuel combustion (eg, CO2, SO2, and H2O) may impact the corrosion of waterwalls, superheaters, headers, reheaters, and other boiler components. Research is being conducted on bare and ash-embedded boiler tube materials in simulated oxyfuel- combustion and air-combustion environments at a superheater temperature of 675°C. Alloys were exposed at temperature to two different gaseous environments. Preliminary results show: (1) an increase in corrosion rate of bare K02707, K11547, K21590, K91560, K92460, S30409, S34700, and N06617 exposed to the oxyfuel combustion environment when compared to the air combustion environment; (2) an increase in corrosion rate of alloys K21590, K92460, S34700, and N06617, when embedded in ash in comparison to bare exposure; and (3) no effect of gaseous environment on alloy corrosion rate when embedded in ash.

36 MATERIALS SCIENCE↗