Synthesis and structural study of Ti-rich Mg-Ti hydrides

Mg x Ti 1-x (x = 0.15, 0.25, 0.35) alloys were synthesized by means of ball milling. Under a hydrogen pressure of 8 MPa at 423 K these Mg–Ti alloys formed a hydride phase with a face centered cubic (FCC) structure. The hydride for x = 0.25 consisted of single Mg 0.25 Ti 0.75 H 1.62 FCC phase but TiH 2 and MgH 2 phases were also formed in the hydrides for x = 0.15 and 0.35, respectively. X-ray diffraction patterns and the atomic pair distribution function indicated that numbers of stacking faults were introduced. There was no sign of segregation between Mg and Ti in Mg 0.25 Ti 0.75 H 1.62 . Electronic structure of Mg 0.25 Ti 0.75 H 1.62 was different from those of MgH 2 and TiH 2 , which was demonstrated by 1 H nuclear magnetic resonance. This strongly suggested that stable Mg–Ti hydride phase was formed in the metal composition of Mg 0.25 Ti 0.75 without disproportion into MgH 2 and TiH 2 .

Asano, Kohta↗

Structural and magnetic properties of hard magnetic system Ce(Co 1 -Fe ) 4.4 Cu 0.6 (0 ≤ x ≤ 0.19)

The Ce(Co 1 -Fe ) 4.4 Cu 0.6 (0 ≤ x ≤ 0.19) is a composite, hard magnetic system that is based on the CaCu 5 -type structure (1:5). It shows both, unique magnetic and microstructural features that are essential for permanent magnets, e.g., exceptional squareness of the 2nd. quadrant of the magnetization loops and microstructural features typically needed for pinning. Samples solidified in alumina crucibles are coarse-grained and often clearly faceted and readily align in a magnetic field. X-ray, SEM, and TEM analyses show a 1:5-type single-phase material when quenched from high temperature, which, after heat treatment, transforms into a laminar coherent nanostructure through the formation of a dense array of extended intercalated regions. Furthermore, these extended intercalated regions are comprised of segments of the Ce 2 Ni 7 –type structure (2:7) which segregate into various closely related precipitates forming a nanostructure similar to the SmCo 5 - Sm 2 Co 17 composites seen in Sm-Co permanent magnets. Based on TEM and Lorentz microscopy of well-aligned single grain particles, the magnetic domains’ reversal mechanism is regulated by anisotropy fluctuations occurring along the easy direction of magnetization and strong exchange interactions between the matrix and defects (e.g.: stacking faults). Lorentz microscopy suggests the domain wall is not physically pinned by the defect, but rather is offset/deflected when it interacts with the defect. The Lorentz and magnetization data suggest that defects cause a bending of the moment away from the c axis inside the grains.

36 MATERIALS SCIENCE↗

Heterogenous activation of dynamic recrystallization and twinning during friction stir processing of a Cu-4Nb alloy

An interplay between high degree of shear deformation and deformation-induced heating occurs during friction stir processing (FSP) of metals. In medium-to-low stacking fault energy Cu alloys, this can lead to a complex spatially heterogenous activation of dynamic recrystallization (DRX) and twinning mechanisms. Within the Cu-Nb system, the presence of Nb is further expected to influence the DRX mechanism of the Cu matrix. However, the microstructural changes induced by the co-deformation of Nb during FSP are still not well understood. So, this study uses a combination of multimodal microstructural characterization, solution thermodynamics-based predictions, and computational crystal plasticity simulation to reveal the various microstructural evolution mechanisms that can occur during FSP of a Cu-4at.%Nb binary model alloy. The formation of softer DRX zones, and harder shear localization regions are revealed using electron backscatter diffraction, transmission electron microscopy, atom probe tomography, and crystal plasticity modeling.

36 MATERIALS SCIENCE↗

Effect of substrate orientation on CdS homoepitaxy by molecular dynamics

CdS homoepitaxy growth was performed by molecular dynamics using different substrate orientations and structures in order to analyze the CdS crystallinity. As anticipated from thermodynamics of homoepitaxy, highly crystalline films with only point defects were obtained on substrates with rectangular surface geometries, including View the MathML source[112¯] zinc blende (ZB), [101¯0] wurtzite (WZ), [112¯0] WZ, [110][110] ZB, [010][010] ZB, and View the MathML source[1101110] ZB. In contrast, films grown on substrates with hexagonal surface geometries, corresponding to the [0001][0001] WZ and [111][111] ZB growth directions, showed structures with a large number of defects including; anti-sites, vacancies, stacking faults, twinning, and polytypism. WZ and ZB transitions and grain boundaries are identified using a lattice identification algorithm and represented graphically in a structural map. A dislocation analysis was performed to detect, identify, and quantify linear defects within the atomistic data. Systematic simulations using different temperatures, deposition rates, and substrate polarities were perform to analyze the trends of dislocation densities on [0001][0001] WZ direction and showed persistent polytypism. As a result, the polytypism observed in the films grown on the substrates with hexagonal surface geometry is attributed to the similar formation energies of the WZ and ZB phases.

36 MATERIALS SCIENCE↗

Phase degradation in B x Ga 1–x N films grown at low temperature by metalorganic vapor phase epitaxy

Using metalorganic vapor phase epitaxy, a comprehensive study of B x Ga 1-x N growth on GaN and AlN templates is described. BGaN growth at high-temperature and high-pressure results in rough surfaces and poor boron incorporation efficiency, while growth at low-temperature and low-pressure (750–900 °C and 20 Torr) using nitrogen carrier gas results in improved surface morphology and boron incorporation up to ~7.4% as determined by nuclear reaction analysis. However, further structural analysis by transmission electron microscopy and x-ray pole figures points to severe degradation of the high boron composition films, into a twinned cubic structure with a high density of stacking faults and little or no room temperature photoluminescence emission. Films with <1% triethylboron (TEB) flow show more intense, narrower x-ray diffraction peaks, near-band-edge photoluminescence emission at ~362 nm, and primarily wurtzite-phase structure in the x-ray pole figures. For films with >1% TEB flow, the crystal structure becomes dominated by the cubic phase. As a result, only when the TEB flow is zero (pure GaN), does the cubic phase entirely disappear from the x-ray pole figure, suggesting that under these growth conditions even very low boron compositions lead to mixed crystalline phases.

36 MATERIALS SCIENCE↗

Correlation of Early-Stage Growth Process Conditions with Dislocation Evolution in MOCVD-Based GaP/Si Heteroepitaxy

To identify the complex relationships between early-stage growth processes and the resultant defect microstructure in GaP/Si heteroepitaxy, a holistic study of several key metal-organic chemical vapor deposition (MOCVD) parameters was conducted, focusing on Si surface preparation and GaP atomic layer epitaxy (ALE) based nucleation processes. Here, crystalline defects related to the lattice mismatch and/or interfacial heterovalency, namely misfit dislocations (MD), threading dislocations (TD), and stacking fault pyramids (SFP), were quantitatively characterized via electron channeling contrast imaging (ECCI) and correlated against the different process variations. Choice of Si surface preparation method between the two examined (dilute SiH4 annealing versus Si2H6 based homoepitaxy) had little impact on resultant GaP film morphology and defect content, whereas differing GaP ALE nucleation conditions produced much more substantial changes. In particular, the initial precursor species (tert-butylphosphine versus triethygallium) and ALE cycle purge times both yielded significant influence over threading dislocation densities (TDD) in thin (100 nm), post-critical thickness GaP/Si films, with TDD spanning two orders of magnitude, from 6.7×10 7 cm -2 to 7.1×10 5 cm -2 , depending on the specific process conditions employed. SFP densities were also found to follow a similar trend, ranging from 2.0×10 7 cm -2 to 1.8×10 5 cm -2 , but with no apparent causal relationship between SFP density and TDD. To help explain the dramatic differences observed, detailed, large-area MD network characterization was used to provide statistically-relevant quantitative analyses of the critical dislocation dynamics (introduction rates and glide velocities) associated with the different process variants. These extracted values are then correlated against the ALE process variants to provide insight into the potential mechanistic roles of the different growth processes.

36 MATERIALS SCIENCE↗

Distribution of fission products palladium, silver, cerium and cesium in the un-corroded areas of the locally corroded SiC layer of a neutron irradiated TRISO fuel particle

Here, detailed electron microscopy studies were performed to investigate the distribution and composition of fission products in the SiC layer of a tristructural isotropic coated particle exhibiting localized corrosion. Previous studies on this particle indicated that pure carbon areas in the SiC layer, resulting from localized corrosion of SiC by Pd, provide pathways for Ag, Cd and Cs migration. This study reveals the presence of Ag- and/or Cd-containing precipitates in un-corroded SiC areas. Ag/Cd may exist by themselves or coexist with Pd. Ag/Cd mainly transport along SiC grain boundaries. An Ag-Pd-Cd precipitate was identified at a stacking fault inside a SiC grain, suggesting that intragranular transport of Ag/Cd is possible. Ce is present with Pd or Pd-U in some precipitates >50 nm. U and Ce frequently coexist with each other, whereas Ag/Cd usually does not coexist with U or Ce. No Cs was detected in any precipitates in the areas examined.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Field-assisted sintering and phase transition of ZnS-CaLa 2 S 4 composite ceramics

In the present study, zinc sulfide (ZnS) and calcium lanthanum sulfide (CaLa 2 S 4 , CLS) composite ceramics were consolidated via field-assisted sintering of 0.5ZnS-0.5CLS (volume ratio) composite powders at 800–1050 °C. Through sintering curve analyses and microstructural observations, it was determined that between 800 and 1000 °C, grain boundary diffusion was the main mechanism controlling grain growth for both the ZnS and CLS phases within the composite ceramics. The consolidated composite ceramics were determined to be composed of sphalerite ZnS, wurtzite ZnS and thorium phosphate CLS. The sphalerite-wurtzite phase transition of ZnS was further demonstrated to be accompanied by the formation of stacking faults and twins in the ceramics. Furthermore, it was also found that the addition of the CLS phase improved the indentation hardness of the ceramics relative to pure ZnS by homogeneous dispersion of ZnS and CLS small grains.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Exceptional radiation resistance of hardened amorphous SiC under high-temperature hydrogen ion implantation

This study provides a compelling comparison of the structural and mechanical responses of single-crystal silicon carbide (sc-SiC), nanocrystalline silicon carbide (nc-SiC), and amorphous silicon carbide (am-SiC) to hydrogen ion implantation at 650 °C across three distinct fluences: low, medium, and high (LF, MF, HF). While both sc-SiC and nc-SiC exhibit blistering, microcracking, and exfoliation, am-SiC remains free of blisters, demonstrating superior resilience. Notably, nc-SiC, with its high density of stacking faults (SFs), requires a higher fluence to initiate blistering compared to sc-SiC. At high fluences, hydrogen accumulation at grain boundaries (GBs) in nc-SiC elevates internal gas pressure, intensifying exfoliation. In sc-SiC, blistering leads to increased hardness, whereas in nc-SiC, the degradation of the SF structure results in a reduction in hardness. In contrast, am-SiC undergoes structural relaxation during irradiation, resulting in a significant increase in hardness while maintaining its structural integrity, with only the formation of nano-sized spherical bubbles observed. Furthermore, these findings highlight the exceptional suitability of am-SiC for nuclear applications, where resistance to radiation-induced microcracking is critical.

36 MATERIALS SCIENCE↗

Activation of dislocations in Mg with solute Y

Mg-Y cast alloy shows excellent ductility (elongation to failure > 15%) compared with pure Mg and commercial Mg cast alloys. By monitoring the microstructure evolution during an in situ tensile test of a Mg-2.5 wt%Y alloy, we identify the activation of prismatic slip, which is rare in Mg. Synchrotron X-ray micro-beam Laue diffraction (μ-Laue) and transmission electron microscopy revealed the morphology of prismatic slip bands and individual dislocations. Density functional theory and molecular dynamics calculations indicate that solute Y can significantly reduce the stacking fault energy (SFE) along direction on prismatic plane in Mg lattice and thus facilitate the nucleation of dislocations during deformation. The presence of free dislocations in the Mg lattice can also lead to nucleation of {10–12} twins even under unfavorable geometric conditions.

36 MATERIALS SCIENCE↗

An analysis of key characteristics of the Frank-Read source process in FCC metals

A well-known intragranular dislocation source, the Frank-Read (FR) source plays an important role in size-dependent dislocation multiplication in crystalline materials. Despite a number of studies in this topic, a systematic investigation of multiple aspects of the FR source in different materials is lacking. Here, in this paper, we employ large scale quasistatic concurrent atomistic-continuum (CAC) simulations to model an edge dislocation bowing out from an FR source in Cu, Ni, and Al. First, a number of quantities that are important for the FR source process are quantified in the coarse-grained domain. Then, two key characteristics of the FR source, including the critical shear stress and critical dislocation configuration, are investigated. In all crystalline materials, the critical stresses and the aspect ratio of the dislocation half-loop height to the FR source length scale well with respect to the FR source length. In Al, the critical stress calculated by CAC simulations for a given FR source length agrees reasonably well with a continuum model that explicitly includes the dislocation core energy. Nevertheless, the predictions of the isotropic elastic theory do not accurately capture the FR source responses in Cu and Ni, which have a relatively large stacking fault width and elastic anisotropy. Our results highlight the significance of directly simulating the FR source activities using fully 3D models and shed light on developing more accurate continuum models.

36 MATERIALS SCIENCE↗

Phase field dislocation dynamics (PFDD) modeling of non-Schmid behavior in BCC metals informed by atomistic simulations

Body-Centered Cubic (BCC) metals exhibit anomalous mechanical properties such as twinning/anti-twinning and tension/compression asymmetry, which are attributed to asymmetric behavior of screw dislocations. Unlike Face-Centered Cubic (FCC) metals, the Critical Resolved Shear Stress (CRSS) of BCC metals deviates from the Schmid law. Here, we use a mesoscale modeling approach called Phase Field Dislocation Dynamics (PFDD) to understand the critical factors that control this non-Schmid behavior and reproduce atomistic predictions of the CRSS (Peierls stress). All inputs to the PFDD model are obtained from Molecular Statics (MS) simulations. Multiple pathways for modeling the non-Schmid behavior are investigated by incorporating the representative dislocation properties into different energy terms in the PFDD model. One way to understand non-Schmid behavior is to incorporate stress components projected on inclined planes into the external energy term within PFDD. Alternatively, we propose that non-Schmid behavior can also be accounted for by considering the variation of the {110} unstable stacking fault energy and the dislocation core width as a function of the applied tensorial stress field. The CRSS predicted using PFDD modeling is in excellent agreement with MS predictions.

36 MATERIALS SCIENCE↗

Dislocation nano-hydrides in nickel: Nucleation, evolution and effects on dislocation behaviors

Nano-hydrides have been predicted to precipitate at the core of edge dislocations in the Ni-H system, a mechanism that may promote hydrogen embrittlement. However, nano-hydride nucleation, growth, and effects on dislocation behavior have seldom been explored. This work combines molecular dynamics grand canonical Monte Carlo (MD-GCMC) simulations and continuum modeling to uncover a wide range of phenomena linked to dislocation nano-hydrides. Simulations reveal that nano-hydrides can be stabilized at dislocation cores with all character angles, including screw segments, due to the hydrostatic stresses around the cores of the Shockley partials. Nano-hydride nucleation takes place in these regions, and growth is dictated by the character angle θ of the perfect dislocation. The equilibrium stacking fault width d eq varies dynamically to increase the local hydrostatic stress field and facilitate the formation of the nano-hydride, forming a constriction-like feature and leading to three distinct behaviors: d eq decreases for θ > 30°, d eq remains unchanged for θ = 30°, and d eq increases for θ < 30°. Remote hydrostatic and Escaig stresses are also shown to influence the nucleation stage, implying stress concentrations such as those ahead of crack tips may facilitate nano-hydride precipitation. Moreover, we identify a new hydrogen-induced 60° dislocation reaction that emits a Shockley partial on a conjugate plane, with potential implications for twin nucleation. Testable predictions from this study are then used to reinterpret previous results from the literature. In conclusion, these findings provide a comprehensive framework to assess nano-hydride formation and evolution at dislocations in nickel and other face-centered cubic metals, with important implications to hydrogen embrittlement.

Dislocations↗

Investigation of defect clusters in ion-irradiated Ni and NiCo using diffuse X-ray scattering and electron microscopy

The nature of defect clusters in Ni and Ni$_{50}$Co$_{50}$ (NiCo) irradiated at room temperature with 2–16 MeV Ni ions is studied using asymptotic diffuse X-ray scattering and transmission electron microscopy (TEM). Analysis of the scattering data provides separate size distributions for vacancy and interstitial type defect clusters, showing that both types of defect clusters have a smaller size and higher density in NiCo than in Ni. Diffuse scattering results show good quantitative agreement with TEM results for cluster sizes greater than 4 nm diameter, but find that the majority of vacancy clusters are under 2 nm in NiCo, which, if not detected, would lead to the conclusion that defect density was actually lower in the alloy. Interstitial dislocation loops and stacking fault tetrahedra are identified by TEM. Lastly comparison of diffuse scattering lineshapes to those calculated for dislocation loops and SFTs indicates that most of the vacancy clusters are SFTs.

36 MATERIALS SCIENCE↗

Modeling of dislocation channel width evolution in irradiated metals

Defect-free dislocation channel formation has been reported to promote plastic instability during tensile testing via localized plastic flow, leading to a distinct loss of ductility and strain hardening in many low-temperature irradiated materials. In order to study the underlying mechanisms governing dislocation channel width and formation, the channel formation process is modeled via a simple stochastic dislocation-jog process dependent upon grain size, defect cluster density, and defect size. Dislocations traverse a field of defect clusters and jog stochastically upon defect interaction, forming channels of low defect-density. And based upon prior molecular dynamics (MD) simulations and in-situ experimental transmission electron microscopy (TEM) observations, each dislocation encounter with a dislocation loop or stacking fault tetrahedron (SFT) is assumed to cause complete absorption of the defect cluster, prompting the dislocation to jog up or down by a distance equal to half the defect cluster diameter. Channels are predicted to form rapidly and are comparable to reported TEM measurements for many materials. Predicted channel widths are found to be most strongly dependent on mean defect size and correlated well with a power law dependence on defect diameter and density, and distance from the dislocation source. Due to the dependence of modeled channel width on defect diameter and density, maximum channel width is predicted to slowly increase as accumulated dose increases. The relatively weak predicted dependence of channel formation width with distance, in accordance with a diffusion analogy, implies that after only a few microns from the source, most channels observed via TEM analyses may not appear to vary with distance because of limitations in the field-of-view to a few microns. Furthermore, examinations of the effect of the so-called “source-broadening” mechanism of channel formation showed that its effect is simply to add a minimum thickness to the channel without affecting channel dependence on the given parameters.

36 MATERIALS SCIENCE↗

Characterization and mechanical properties of cladded stainless steel 316L with nuclear applications fabricated using electron beam melting

The ability to fabricate or join components of 316 L austenitic stainless steel using additive manufacturing (AM) processes such as laser and electron beam melting (EBM®) offers several advantages including enhanced part complexity, narrow or absent heat affected zones, increased part precision, avoidance of filler materials (such as traditional welds), and the ability to create metallurgically sound bonds. These attributes can contribute to improved mechanical properties of the fabricated components and component repair in nuclear, aerospace, and chemical industries. In the present work, we report that austenitic 316 L stainless steel additively manufactured by EBM exhibits a 76% increase in the yield strength and a corresponding increase of 29% in the ultimate tensile strength in contrast to the wrought substrate and commercial forged 316 L stainless steel. The EBM clad 316 L stainless steel elongation was 36%. The wrought substrate equiaxed grain size was ~30 μm in contrast to elongated, columnar grains ~0.1 mm wide and >1 mm in length for the EBM cladding. Transmission Electron Microscopy (TEM) analysis revealed that these columnar grains, which exhibited very straight, and presumably special grain boundaries having a very high (100) texture, contained a variety of sub-grain microstructures consisting of low-angle sub-grain boundaries containing dislocation tangles and stacking-fault arrays, and homogeneously distributed Cr 23 C 6 carbide precipitates, with no preferential carbide precipitation on either the straight, special columnar grain boundaries, or the very low-angle sub-grain boundaries. This observation and the formation of hierarchical microstructures which produce high strength and possibly corrosion resistance as a consequence of the absence of grain boundary carbide precipitation, illustrate the prospects for AM as a novel concept for achieving grain boundary engineering to promote high-strength and corrosion resistant alloys for high-temperature, corrosive environments, including elevated temperature nuclear reactor applications.

36 MATERIALS SCIENCE↗