Texture evolution in Fe-3% Si steel treated under unconventional annealing conditions

The present work investigates texture evolution stages in grain-oriented steel heat-treated using unconventional conditions. The Fe-3%Si steel taken after final cold rolling reduction from an industrial line was subjected to a laboratory isothermal annealing at different temperatures. The annealing temperatures were varied in a range of 850-1150 deg. C. During the annealing each specimen was heated at 10 deg. C/s and kept at the stated temperature for 5 min. Development of microstructure and texture in the annealed specimens were followed by the DC measurements of magnetic properties. The grain oriented steel, taken from the same industrial line after final box annealing was also analyzed and compared with the laboratory annealed specimens. It was shown that there is an optimal temperature region that, with combination of a fast heating rate, led to the best conditions of a drastically reduced development time of the {l_brace}110{r_brace} < 001 > crystallographic texture in the cold rolled grain-oriented steel. Materials heat treated below the optimum temperature region account for a primary recrystallization, while applying heat above this region leads to a secondary recrystallization without abnormal grain growth. Moreover, in the optimum temperature range, there was a particular temperature leading to the most optimal microstructure and texture. The magnetic properties, measured after the optimal heat treatment, were close to that measured on specimens taken after the final box annealing. The electron back scattered diffraction measurement technique revealed that sharpness of the {l_brace}110{r_brace} < 001 > crystallographic texture, developed at the optimum temperature is comparable to the steel taken after the industrial final box annealing. This fact is evidence that there is a temperature where the abnormal grain growth proceeds optimally.

36 MATERIALS SCIENCE↗

Effect of V and Ta on the precipitation behavior of 12%Cr reduced activation ferrite/martensite steel

12%Cr reduced activation ferrite/martensite steels are promising candidate materials for good corrosion and irradiation resistance used for supercritical water-cooled reactor cladding and in-core components. V and Ta are considered to have improved the creep strength of high Cr steels by precipitating as MX phase. In this paper, a series of trial products microalloyed with V and V–Ta are produced, and the microstructure is characterized after quenching at 1050 °C and tempering at 780 °C by using TEM method to investigate the effect of these elements on the precipitation behavior of 12%Cr reduced activation ferrite/martensite steel. The results from both the experimental observations and thermodynamic and kinetic calculations reveal that V and V–Ta can promote the stable MX precipitation instead of M{sub 2}X, thus increasing the volume fraction of M{sub 23}C{sub 6}. Two-phase separation behavior of the (Ta, V)(C, N) carbonitride into a Ta(V)C(N) phase and a V(Ta)N(C) phase in 12Cr3WVTa steel is observed and further discussed. - Highlights: • Microalloyed with V and V-Ta can promote the precipitation of MX instead of M{sub 2}X. • The presence of delta-ferrite in microstructure affects the morphology of MX. • Two-phase separation of MX carbonitride was observed in 12Cr3WVTa steel.

36 MATERIALS SCIENCE↗

Effect of dew point on the formation of surface oxides of twinning-induced plasticity steel

The surface oxides of twinning-induced plasticity (TWIP) steel annealed at 800 °C for 43 s were investigated using transmission electron microscopy. During the annealing process, the oxygen potential was controlled by adjusting the dew point in a 15%H{sub 2}–N{sub 2} gas atmosphere. It was found that the type of surface oxides formed and the thickness of the oxide layer were determined by the dew point. In a gas mixture with a dew point of − 20 °C, a MnO layer with a thickness of ∼ 100 nm was formed uniformly on the steel surface. Under the MnO layer, a MnAl{sub 2}O{sub 4} layer with a thickness of ∼ 15 nm was formed with small Mn{sub 2}SiO{sub 4} particles that measured ∼ 70 nm in diameter. Approximately 500 nm below the MnAl{sub 2}O{sub 4} layer, Al{sub 2}O{sub 3} was formed at the grain boundaries. On the other hand, in a gas mixture with a dew point of − 40 °C, a MnAl{sub 2}O{sub 4} layer with a thickness of ∼ 5 nm was formed on most parts of the surface. On some parts of the surface, Mn{sub 2}SiO{sub 4} particles were formed irregularly up to a thickness of ∼ 50 nm. Approximately 200 nm below the MnAl{sub 2}O{sub 4} layer, Al{sub 2}O{sub 3} was found at the grain boundaries. Thermodynamic calculations were performed to explain the experimental results. The calculations showed that when a{sub O2} > ∼ 1.26 × 10{sup −28}, MnO, MnAl{sub 2}O{sub 4}, and Mn{sub 2}SiO{sub 4} can be formed together, and the major oxide is MnO. When a{sub O2} is in the range of 1.26 × 10{sup −28}–2.51 × 10{sup −31}, MnO is not stable but MnAl{sub 2}O{sub 4} is the major oxide. When a{sub O2} < ∼ 2.51 × 10{sup −31}, only Al{sub 2}O{sub 3} is stable. Consequently, the effective activity of oxygen is considered the dominant factor in determining the type and shape of surface oxides of TWIP steel. - Highlights: • The surface oxides of TWIP steel annealed at 800 °C were investigated using TEM. • The surface oxides were determined by the dew point during the annealing process. • The activity of oxygen is the major factor determining the oxides of TWIP steel.

36 MATERIALS SCIENCE↗

Grain refinement of a nickel and manganese free austenitic stainless steel produced by pressurized solution nitriding

Prolonged exposure at high temperatures during solution nitriding induces grain coarsening which deteriorates the mechanical properties of high nitrogen austenitic stainless steels. In this study, grain refinement of nickel and manganese free Fe–22.75Cr–2.42Mo–1.17N high nitrogen austenitic stainless steel plates was investigated via a two-stage heat treatment procedure. Initially, the coarse-grained austenitic stainless steel samples were subjected to an isothermal heating at 700 °C to be decomposed into the ferrite + Cr{sub 2}N eutectoid structure and then re-austenitized at 1200 °C followed by water quenching. Microstructure and hardness of samples were characterized using X-ray diffraction, optical and scanning electron microscopy, and micro-hardness testing. The results showed that the as-solution-nitrided steel decomposes non-uniformly to the colonies of ferrite and Cr{sub 2}N nitrides with strip like morphology after isothermal heat treatment at 700 °C. Additionally, the complete dissolution of the Cr{sub 2}N precipitates located in the sample edges during re-austenitizing requires longer times than 1 h. In order to avoid this problem an intermediate nitrogen homogenizing heat treatment cycle at 1200 °C for 10 h was applied before grain refinement process. As a result, the initial austenite was uniformly decomposed during the first stage, and a fine grained austenitic structure with average grain size of about 20 μm was successfully obtained by re-austenitizing for 10 min. - Highlights: • Successful grain refinement of Fe–22.75Cr–2.42Mo–1.17N steel by heat treatment • Using the γ → α + Cr{sub 2}N reaction for grain refinement of a Ni and Mn free HNASS • Obtaining a single phase austenitic structure with average grain size of ∼ 20 μm • Incomplete dissolution of Cr{sub 2}N during re-austenitizing at 1200 °C for long times • Reducing re-austenitizing time by homogenizing treatment before grain refinement.

36 MATERIALS SCIENCE↗

Austenite stabilization and high strength-elongation product of a low silicon aluminum-free hot-rolled directly quenched and dynamically partitioned steel

Microstructures composed of lath martensite and retained austenite with volume fraction between 8.0 vol.% and 12.0 vol.% were obtained in a low-C low-Si Al-free steel through hot-rolling direct quenching and dynamical partitioning (HDQ&DP) processes. The austenite stabilization mechanism in the low-C low-Si Al-free steel under the special dynamical partitioning processes is investigated by analyzing the carbon partition behavior from martensite to austenite and the carbide precipitation-coarsening behavior in martensite laths combining with the possible hot rolling deformation inheritance. Results show that the satisfying retained austenite amount in currently studied low-Si Al-free HDQ&DP steel is caused by the high-efficiency carbon enrichment in the 30–80 nm thick regions of austenite near the interfaces in the hot-rolled ultra-fast cooled structure and the avoidance of serious carbides coarsening during the continuous cooling procedures. The excellent strength-elongation product reaching up to 26,000 MPa% shows that the involved HDQ&DP process is a promising method to develop a new generation of advanced high strength steel. - Highlights: • HDQ&DP processes were applied to a low-C low-Si Al-free steel. • Effective partitioning time during the continuous cooling processes is 1–220 s. • Retained austenite with volume fraction between 8.0 vol. % and 12.0 vol. % has been obtained. • The special austenite stabilization mechanism has been expounded.

36 MATERIALS SCIENCE↗

Evolution of carbides in cold-work tool steels

This study aimed to present the complete history of carbide evolution in a cold-work tool steel along its full processing route for fabrication and application. A sequence of processes from cast to final hardening heat treatment was conducted on an 8% Cr-steel to reproduce a typical commercial processing route in a small scale. The carbides found at each process step were then identified by electron diffraction with energy dispersive spectroscopy in a scanning or transmission electron microscope. After solidification, MC, M{sub 7}C{sub 3} and M{sub 2}C carbides were identified and the last one dissolved during hot compression at 1180 °C. In a subsequent annealing at 870 °C followed by slow cooling, M{sub 6}C and M{sub 23}C{sub 6} were added, while they were dissolved in the following austenitization at 1030 °C. After the final tempering at 520 °C, fine M{sub 23}C{sub 6} precipitated again, thus the final microstructure was the tempered martensite with MC, M{sub 7}C{sub 3} and M{sub 23}C{sub 6} carbide. The transient M{sub 2}C and M{sub 6}C originated from the segregation of Mo and finally disappeared due to attenuated segregation and the consequent thermodynamic instability. - Highlights: • The full processing route of a cold-work tool steel was simulated in a small scale. • The carbides in the tool steel were identified by chemical–crystallographic analyses. • MC, M{sub 7}C{sub 3}, M{sub 2}C, M{sub 6}C and M{sub 23}C{sub 6} carbides were found during the processing of the steel. • M{sub 2}C and M{sub 6}C finally disappeared due to thermodynamic instability.

36 MATERIALS SCIENCE↗

Identification of the mechanism that confers superhydrophobicity on 316L stainless steel

This study develops a rapid method to confer superhydrophobicity on 316L stainless steel surfaces with an amphiphilic reagent such as dodecanoic acid. The highest contact angle (approaching 173°) was obtained after forming hierarchical structures with a non-aqueous electrolyte by an electrolytic process. Our goal was to induce superhydrophobicity directly on 316L stainless steel substrates and to establish which molecules cause the effect. The superhydrophobic behaviour is analysed by contact angle measurements, scanning electron microscopy (SEM), IR spectroscopy and atomic force microscopy (AFM). The growth mechanism is analysed using FE-SEM, TOF-SIMS and XPS in order to determine the molecules involved in the reaction and the growth. The TOF-SIMS analysis revealed that the Ni{sup 2+} ions react with lauric acid to create an ester on the stainless steel surface. - Highlights: • This study develops a rapid and facile approach to impart superhydrophobicity properties to 316L stainless steel surfaces with an amphiphilic reagent such as dodecanoic acid. Surface character changes from superhydrophilicity to superhydrophobicity. • This process changes the surface character from superhydrophilicity to superhydrophobicity. • The process based on electrolysis of a nickel salt in lauric acid provides superhydrophobic behaviour in 316L stainless steel. • The growth mechanism is proposed as a mode island (Volmert- Weber mode). • TOF-SIMS and XPS provided the identification of the molecules involved in the surface modification reaction on AISI 316L inducing superhydrophobicity.

36 MATERIALS SCIENCE↗

Identification of sigma and chi phases in duplex stainless steels

The aim of this work is to find out the most suitable method for detecting and analyzing accurately the formation conditions of secondary phases, particularly Sigma-phase (σ-phase) and Chi-phase (χ-phase) in duplex stainless steels (UNS S32205 and UNS S32750). The microstructure was characterized after a solution annealing at 1080 °C followed by an isothermal heating at 830 °C for different time ranges, ranging from 1 min to 9 h, in order to enlighten the controversial point concerning the mechanism of χ-phase nucleation in relation with the σ-phase. Etched samples were observed using optical microscopy (MO), and scanning electron microscopy (FESEM) with a backscattered electron detector (BSE) was used on unetched samples. Compositional microanalysis (EDS) was carried out for identifying the different phases present in the steels. Sigma phase was easily observed using different etching procedures, whereas χ-phase was only clearly detected with FESEM–BSE on unetched samples. The compositional analyses showed that the molybdenum content in χ-phase almost doubles the content of this element in σ-phase, and as a result the kinetics of nucleation and growth were also found to be remarkably faster when the alloy content in the steel is higher. In addition, chromium nitrides and carbides were also observed to precipitate as a result of the heat treatments and, in the case of the chromium nitrides, they act as a favorable site for the nucleation of σ-phase and χ-phase. - Highlights: • Microscopy was used on heat treated duplex steels for microstructure identification. • FESEM–BSE observation on unetched samples provided the best contrast between phases. • Analyses of carbides, nitrides, chi and sigma phases were possible by EDS and WDS. • Chromium nitrides act as favorable site for the nucleation of chi and sigma phases. • Secondary phases nucleation kinetics are faster in superduplex than in duplex steels.

36 MATERIALS SCIENCE↗

The effect of thermomechanical treatment and tempering on the subsurface microstructure and bendability of direct-quenched low-carbon strip steel

Highlights: • Surface properties mainly determine the bendability of high strength steel. • Tempering improves bendability by softening the microstructure. • Surface texture is affected by thermomechanical treatment but not by tempering. • Strong shear texture component and upper bainite are detrimental to bendability. - Abstract: Recent results in the literature have shown that subsurface properties play a key role during the bending of steel plates. Now, for the first time, surface microstructure, surface texture, subsurface hardness and dislocation density have been studied to reveal the effect of tempering and thermomechanical treatment on the bendability of a direct-quenched strip steel. In the experiments, different thermomechanical treatments as well as non-isothermal tempering treatments were performed with slow heating to 570 °C and slow cooling to simulate the tempering of large steel coils in a batch annealing furnace. The results show that in addition to the improved production efficiency obtained through direct quenching and a single tempering process, tempering improves bendability by reducing subsurface dislocation density and hardness without a significant loss of strip yield strength. The subsurface microstructure and texture of the strip are the result of thermo-mechanical processing and transformation behaviour. Upper bainite containing elongated Martensite-Austenite (MA) islands in addition to an intense shear texture component {112}<111>{sub α} leads to shear band formation, and therefore poorer bendability when the bend axis is perpendicular to the rolling direction. This texture is not affected by tempering. Therefore, tempering does not improve the bendability of steels with an unfavourable texture. When the subsurface layers comprise a softer ferritic microstructure, good bendability is obtained in the untempered direct-quenched condition with a modest improvement caused by tempering.

36 MATERIALS SCIENCE↗

Ensuring combination of strength, ductility and toughness in medium-manganese steel through optimization of nano-scale metastable austenite

Highlights: • Medium-Mn steel was innovatively designed for medium to heavy steel plates. • Three intercritical annealing processes were adopted to ensure TRIP effect. • Austenite-martensite submicro-laminate structure was obtained after annealing. • The reversed austenite with different stability led to improved ductility. • TRIP effect induced by metastable austenite contributed excellent impact properties. - Abstract: Medium-Mn steel was innovatively designed in terms of alloying elements for medium to heavy steel plates to obtain combination of high strength, good ductility, and excellent low temperature toughness. Martensite was the dominant microstructure in the directly quenched steel plate because of high hardenability obtained by the addition of 5.6 wt% Mn. Three intercritical annealing processes were adopted to ensure transformation-induced-plasticity (TRIP) effect through optimization of the volume fraction, morphology, and C and Mn-enriched reversed austenite. On annealing, the dislocation density of martensite plate was decreased because of recovery and recrystallization, and metastable austenite film nucleated at the interface. Both thermal and mechanical stability of austenite decreased with increase in annealing temperature. The high yield strength of 840 MPa, good elongation after fracture of 24.3%, and excellent toughness at − 60 °C of 130.3 J was obtained at intermediate annealing temperature of 650 °C, and the volume fraction of reversed austenite at room temperature and − 80 °C was 22% and 17%, respectively. The reversed austenite exhibited different stability with increased tensile strain, leading to improved ductility and delayed necking. Moreover, the crack initiation energy and crack propagation energy were increased via dynamic stress partitioning and relaxation together with the transformation of metastable austenite. Thus, significant degree of TRIP effect induced by moderate stability of austenite played an important role in governing mechanical properties.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

A study of microstructural evolution of Fe-18Cr-8Ni, Fe-17Cr-12Ni, and Fe-20Cr-25Ni stainless steels after mechanical alloying and annealing

In this study, high-energy mechanical alloying technique was used to produce nanocrystalline stainless steels of three different compositions from elemental powders. The microstructural evolution (grain growth and phase transformation) as a function of alloy compositions and annealing temperatures were investigated by room and high temperature x-ray diffraction experiments, transmission electron microscopy and focused ion beam microscopy. The results revealed that stainless steels with low nickel content (i.e., Fe-18Cr-8Ni) underwent a deformation-induced martensitic transformation during room temperature mechanical alloying. Deformation-induced martensitic transformation with increasing nickel content (i.e., Fe-17Cr-12Ni and Fe-20Cr-25Ni) would not be possible by room temperature milling but was created by high strain rate cryogenic processing, the degree to which was compositional dependent. Post process annealing induced the reverse transformation from martensite-to-austenite the ratio of which was found to be a factor of alloy composition and annealing temperature. The real time in-situ x-ray studies showed that the martensite-to-austenite reverse transformation was completed at around 600 °C and 800 °C for Fe-18Cr-8Ni and Fe-20Cr-25Ni steels, respectively. Microscopy studies revealed a significant enhancement in the resistance to grain growth for Fe-17Cr-12Ni steel over other compositions at elevated temperatures as high as 1200 °C. As such, cryogenic processing following by reverse martensitic transformation of high Ni containing alloys provides a pathway for developing higher heat resistant stainless steel alloys.

36 MATERIALS SCIENCE↗

Martensite crystallography and chemistry in dual phase and fully martensitic steels

Highlights: • Lath martensite islands and bands were indexed in variations of dual-phase steels. • Detail insight was obtained by combined EBSD, APT, TEM, nano-indentation analysis. • The islands predominantly consist of one main packet with all six variants. • The bands are composed of connected domains, each largely made of one main packet. • Tempering at ~450 °C causes carbon partition to lath boundaries and dislocation cores. - Abstract: Lath martensite is important in industry because it is the key strengthening component in many advanced high strength steels. The study of crystallography and chemistry of lath martensite is extensive in the literature, however, mostly based on fully martensitic steels. In this work, lath martensite in dual phase steels is investigated with a focus on the substructure identification of the martensite islands and microstructural bands using electron backscattered diffraction, and on the influence of the accompanied tempering process during industrial coating process on the distribution of alloying elements using atom probe tomography. Unlike findings for the fully martensitic steels, no martensite islands with all 24 Kurdjumov-Sachs variants have been observed. Almost all martensite islands contain only one main packet with all six variants and minor variants from the remaining three packets of the same prior austenite grain. Similarly, the martensite bands are typically composed of connected domains originating from prior austenite grains, each containing one main packets (mostly with all variants) and few separate variants. The effect of tempering at ~450 °C (due to the industrial zinc coating process) has also been investigated. The results show a strong carbon partitioning to lath boundaries and Cottrell atmospheres at dislocation core regions due to the thermal process of coating. In contrast, auto-tempering contributes to the carbon redistribution only in a limited manner. The substitutional elements are all homogenously distributed. The phase transformation process has two effects on the material: mechanically, the earlier-formed laths are larger and softer and therefore more ductile (as revealed by nanoindentation); chemically, due to the higher dislocation density inside the later-formed laths, which are generally smaller, carbon Cottrell atmospheres are predominantly observed.

36 MATERIALS SCIENCE↗

Effect of Nb micro-alloying on microstructure and properties of thermo-mechanically processed high carbon pearlitic steel

Highlights: • Effect of Nb micro-alloying on high carbon steels has been established. • Fine and degenerated pearlite with fine PAGS is achieved due to Nb micro-alloying. • AFM study indicates true interlamellar spacing which conforms well to TEM study. • Hardness and yield strength have been obviously improved with the addition of Nb. - Abstract: Two C-Mn-Si steels with and without Nb micro-alloying are selected in the present study. Both these high carbon steels have been thermo-mechanically processed using Gleeble 3800 simulator. Optical microscope (OM), scanning electron microscope (SEM), transmission electron microscope (TEM), atomic force microscope (AFM) were utilised for microstructural characterisation. The austenitising temperature was varied from 1150 °C to 1200 °C followed by hot compression and subjected to free cooling to evaluate the influence of austenite grain size on transformed microstructure and mechanical properties. It is evident that higher austenite grain size is obtained for both types of steels subjected to higher austenitising temperature. The refinement of pearlite interlamellar spacing (<0.20 μm) with degenerated morphology as well as finer prior austenite grain size (<40 μm) is found to be more prominent for Nb micro-alloyed sample. The average hardness values of both the steels are higher for the specimens, treated at a higher austenitising temperature which is attributed to finer interlamellar spacing. Finally, the correlation between the evolving microstructure and resulting mechanical properties (hardness and yield strength) has been made.

36 MATERIALS SCIENCE↗

TEM study the corrosion behavior of the low alloy steels developed for flue gas desulfurization system

Highlights: • Corrosion mechanism of low alloy steels for flue gas desulfurization was studied. • An amorphous corrosion layer enriched with Fe, O, S formed on the blank specimen. • Added Cu concentrated, crystallized and grown to particles in corrosion layer. • Corrosion resistance of the steels depended on the form of Cu in corrosion layer. • Sb addition slows the crystallization and growth of Cu particles in corrosion layer. - Abstract: This study investigated the corrosion behavior and underline mechanisms of low alloy steels with a minor addition of 0.4 wt% Cu, 0.2 wt% Ni, 0.1 wt% Sb and 0.05 wt% Co developed for a flue gas desulfurization (FGD) system. Corrosion tests were carried out in an aggressive solution of 16.9 vol% H{sub 2}SO{sub 4} + 0.35 vol% HCl + Bal. H{sub 2}O at 60 °C for up to 48 h. The experimental results revealed enrichment of the additional elements (Cu, Sb and Ni) in the corrosion layer, whose concentration increased with test time. As the concentrations of Cu increased, the crystallization and growth of the Cu particles (from several nm to 320 nm)) within the corrosion layer was accelerated. At the initial stage of the test, a continuous amorphous layer rich with the additional elements formed and covered the surface of the steel, which then gradually developed defects, pores and cracks, as the crystallization and growth of Cu particles with the elapse of time. The results indicated that the corrosion resistance of the low alloy steel depends on the existence form of Cu in the corrosion layer, i.e., as solute atoms or as nanoparticles strengthened the corrosion layer and increased corrosion resistance. As the coarsening of Cu particles weakened the corrosion layer and deteriorated the corrosion resistance.

36 MATERIALS SCIENCE↗

Hydrogen induced cracking susceptibility of API 5L X70 pipeline steel in relation to microstructure and crystallographic texture developed after different thermomechanical treatments

Highlights: • crack propagated mainly along deformed-banded microstructure. • Lower failure strength manifested at pipeline steel surface compared to the mid-thickness. • Greater fraction of martensite/austenite constituents featured in specimen WG relative to specimen WH. • Early onset of cracking in specimen WH showed no preference to specific crystallographic orientation. • Multi-component inclusion particle was revealed along crack propagation path. - Abstract: Thermomechanical treatments offer an innovative means of controlling microstructure development and improving resistance to hydrogen induced cracking (HIC) in pipeline steel. This study was conducted on two X70 pipeline steels (labelled WG and WH) of the same chemical composition, but processed with different thermomechanical parameters. Specimen WG was hot rolled at a higher temperature range of 880–820 {sup °}C, while specimen WH was hot rolled between 830 and 760 {sup °}C before cooling at a rate of 25 {sup °}C/s. Early onset of HIC was observed in specimen WH after electrochemical hydrogen charging for 12 h in a solution of 0.2 M H{sub 2}SO{sub 4} and 3 g/l NH{sub 4}SCN, without any applied stress. Also, test pieces from the surface and mid-thickness layers of each pipeline steel were subjected to slow strain rate tensile (SSRT) test with in-situ hydrogen charging. Characterization techniques such as Optical Microscopy, Scanning Electron Microscopy, Electron Backscattered Diffraction and X-ray Diffraction were used to investigate the structure pipeline steel specimens. The role of inclusions on HIC was studied by Energy Dispersive X-ray Spectroscopy. Although the microstructure of both specimens were predominantly ferritic, more martensite/retained austenite (M/A) constituents featured in WG. Further crystallographic texture analysis indicates that grain orientation at the surfaces of both test specimens were similar with deviations towards <111> on the inverse pole figure (IPF); whereas, pole intensity at the mid-thickness deviated towards the <001> direction. Considering the increased fraction of banded-deformed grains with high stored energy, the lower HIC resistance of specimen WH in comparison to specimen WG was justified.

36 MATERIALS SCIENCE↗

Competitive grain boundary segregation of phosphorus and carbon governs delamination crack in a ferritic steel

Highlights: • Trace amounts of P in the steel cause delamination in case of Lt-high Temp. holding. • Anisotropic microstructure did not affect the delamination in this study. • Crack-linked GBs in Lt-high Temp. steel had higher P and lower C segregation. • Crack-interrupt GBs in St-high Temp. steel had lower P and higher C segregation. • Competitive segregation controlled by high Temp. holding time affects delamination. - Abstract: The present study aims at unveiling the influence of trace amounts of phosphorus on the macro-scale delamination in a ferritic steel. Two different steels with trace amounts of phosphorus were examined to reveal the cause: One was made by long-time high temperature holding to maximize the phosphorus segregation, and the other one was made by short-time high temperature holding to minimize the phosphorus segregation. The atom probe results at the grain boundaries ahead of the delamination-related cracks provide a strong evidence that phosphorus-enrichment and carbon-depletion for the long-time high temperature holding induces a larger degree of delamination as compared to the short-time high temperature holding. Reasons for the different segregation tendency were discussed by correlating the isothermal holding time at high temperature and the competitive segregation between phosphorus and carbon.

36 MATERIALS SCIENCE↗

Liquid metal embrittlement in laser lap joining of TWIP and medium-manganese TRIP steel: The role of stress and grain boundaries

Highlights: • This work shows liquid metal embrittlement in externally loaded laser lap welding. • Results confirmed a direct relation between external load and LME susceptibility. • TWIP steel showed a higher LME susceptibility compared to medium-Mn TRIP steel. • Results indicated stress-assisted diffusion of Zn into austenite grain boundaries. • High angle grain and Σ3 twinning boundaries play major role in Zn penetration. - Abstract: High-Manganese austenite-containing steels with superior combination of strength and ductility have shown potential for enhancement of passenger safety and body-in-white (BIW) weight reduction. Even though Zn-coated austenitic steels have improved corrosion resistance, they are highly susceptible to liquid metal embrittlement (LME) during welding. The present work is aimed to address LME susceptibility during restrained laser lap joining of high-Mn twinning induced plasticity (TWIP) and medium-Mn transformation induced plasticity (MMn-TRIP) steels. Electron probe micro-analysis (EPMA) results showed that stress-assisted diffusion of Zn into the austenite grain boundaries and further liquid Zn formation by a peritectic reaction lead to grain boundary decohesion. Electron backscatter diffraction (EBSD) results demonstrated that high angle and special grain boundaries are prone to Zn-penetration within the heat-affected-zone (HAZ). Additionally, LME sensitivity was observed to be highly dependent on the magnitude of applied stress.

36 MATERIALS SCIENCE↗

Additive manufacturing as a processing route for steel-aluminum bimetallic structures

Here we present results on the fabrication of steel-aluminum bi-metallic structures using directed energy deposition additive manufacturing. The challenges associated with the fabrication of a sharp transition from steel to aluminum are uncovered using ex-situ characterization techniques and thermo-mechanical modeling of the deposition process. It was found that the fabrication of a sharp steel-aluminum transition is challenging with extensive cracking observed at the interface. The cracking was attributed to the combined effect of residual stress development due to thermal expansion coefficient mismatch and the presence of ordered intermetallics with low ductility at the interface. Using a coupled thermodynamic and thermo-mechanical modeling approach, potential pathways to enable the fabrication of steel-aluminum bi-metallic structures using additive manufacturing are proposed. The results presented here can lay the foundation for future work on the fabrication of bi-metallic steel-aluminum structures using directed energy deposition.

36 MATERIALS SCIENCE↗