At least 577 records · Page 32

Processing of Dilute Mg–Zn–Mn–Ca Alloy/Nb Multilayers by Accumulative Roll Bonding

Recent advancements in the severe plastic deformation process called accumulative roll bonding (ARB) can help to address the long-standing need for manufacturing lightweight, high-strength Mg sheet materials. However, the fabrication of Mg alloy-based laminates via ARB remains a challenge due to the intrinsically poor formability of Mg. Herein, it is shown that Mg-based composite laminates with refined layers can be fabricated via several room-temperature ARB cycles with appropriate intermediate annealing and alloy selection. The final laminates made here consist of equal volume fractions of a dilute Mg–Zn–Mn–Ca alloy phase and a pure Nb phase with fine 150 μm layer thicknesses. Deformation texture evolution in both phases within the composite is analyzed via neutron diffraction measurements taken at different stages in the process. The analysis suggests that the annealing step recrystallizes the Mg-alloy phase. It is also shown that for both phases, the stabilized deformation textures within the composite correspond to the classic stable textures of the individual constituents. Polycrystal texture modeling implies that {10–12} <-1011> extension twinning developed in the Mg alloy during rolling.

36 MATERIALS SCIENCE↗

Self–Healing and Stretchable Molecular Ferroelectrics with High Expandability

The interplay between crystal ordering and stretchability is frequently encountered in contemporary materials science, particularly in the case of ferroelectrics. The inherent dilemma arises when these materials need to withstand repetitive mechanical deformations or stretching without sacrificing their crystal integrity, all while retaining their remarkable ferroelectric properties and even exhibiting self-healing capabilities. This complexity further presents a significant challenge in the design and engineering of mechanically rigid molecular ferroelectric crystals, particularly for applications where both precise crystalline structure and mechanical adaptability are crucial. In this study, the humidity-controlled expansion and contraction, dissolution, and recrystallization of a self-assembled molecular ferroelectric-in-hydrogel framework are reported. Self-healing ferroelectric-in-hydrogel networks exhibit a recyclable humidity-tailored ionic conductivity from 2.86 × 10 –6 to 1.36 × 10 –5 S cm –1 , facilitating the stretchable piezoelectric sensing. Additionally, the dynamic bond reforming interactions are observed, leading to the tailoring of Young's modulus from 452 to 170 MPa, maintaining ferroelectricity under a strain of 20% with a piezoelectric coefficient of 15.7 pC N –1 . Upon lattice contraction, the molecular contacts undergo reforming, leading to the restoration of stretchable ferroelectrics/piezoelectrics and paving the way for stretchable bioelectronics for full-body motion monitoring. The capabilities highlighted here open avenues for stretchable and self-healing ferroelectric-in-hydrogel bioelectronic technologies.

36 MATERIALS SCIENCE↗

Effect of pH on the Activity of Ice-Binding Protein from Marinomonas primoryensis

The ability of an ice-binding protein (IBP) from Marinomonas primoryensis (MpIBP) to influence ice crystal growth and structure in nonphysiological pH environments was investigated in this work. The ability for MpIBP to retain ice interactivity under stressed environmental conditions was determined via (1) a modified splat assay to determine ice recrystallization inhibition (IRI) of polycrystalline ice and (2) nanoliter osmometry to evaluate the ability of MpIBP to dynamically shape the morphology of a single ice crystal. Circular dichroism (CD) was used to relate the IRI and DIS activity of MpIBP to secondary structure. The results illustrate that MpIBP secondary structure was stable between pH 6 and pH 10. It was found that MpIBP did not interact with ice at pH=4 or pH=13. At 6=pH=12 MpIBP exhibited a reduction in grain size of ice crystals as compared to control solutions and demonstrated dynamic ice shaping at 6=pH=10. The results substantiate that MpIBP retains some secondary structure and function in non-neutral pH environments; thereby, enabling its potential utility in nonphysiological materials science and engineering applications.

antifreeze proteins↗

Structural Evolution of a Ni Alloy Surface During High-Temperature Oxidation

We show that considerable structural transformations occur at a Ni alloy surface during the transient stages of high-temperature oxidation. This was demonstrated by exposing the alloy to high-temperature CO 2 for short times at both atmospheric and supercritical pressures. A protective Cr-rich oxide layer formed after only 5 min at 700 °C and persisted for longer exposures up to 500 h. Voids formed and grew over time by the condensation of metal vacancies generated during oxidation, while the alloy surface recrystallized after sufficient oxidation had occurred. The oxygen potential established at the oxide/alloy interface led to oxidation along the newly formed grain boundaries as well as adjacent to and inside of the voids. Al, the most stable oxide-former and present at low concentration in the alloy, was preferentially oxidized in these regions. Furthermore, the results provide an improved understanding of the internal oxidation of Al and its role in enhancing scale adhesion for this class of Ni alloys.

20 FOSSIL-FUELED POWER PLANTS↗

Oxidation Behavior of Welded Fe-Based and Ni-Based Alloys in Supercritical CO 2

Next-generation supercritical CO 2 (sCO 2 ) power cycles will require different classes of alloy throughout the operational temperatures to optimize tradeoff of creep strength, oxidation performance and cost. This will necessitate joining methods such as welding, which might pose compatibility concerns at the joined interfaces. In this study, similar and dissimilar metal welds were generated from a variety of candidate alloys for sCO 2 systems including ferritic/martensitic steels, austenitic steels, and Ni-based superalloys. Samples were extracted from different regions of the welds and exposed to sCO 2 at 550 °C and 20 MPa for 2500 h, then characterized to understand their behavior in this environment. Unsurprisingly, the local oxidation behavior was largely dictated by the Cr content in the underlying metal. High-Cr austenitic steels and Ni alloys formed slow-growing Cr-rich oxide scales with minimal carburization of the underlying metal, while low-Cr ferritic/martensitic steels formed fast-growing Fe-rich oxide scales with significant carburization. Most welds did not show any unusual oxidation behavior at the interfaces, considering the local Cr content. The one exception was the 347H similar metal weld, where a larger grain size and complex grain structure in the fusion zone led to a significantly higher rate of Fe-rich oxide nodule formation compared to the base metal. This suggests that microstructural changes at joined interfaces can play an important role on the oxidation-limited lifetimes in future sCO 2 systems. The composition changes across the interfaces enabled study of the effect of Fe on the growth rate of Cr-rich oxides and of the origins of the sub-surface recrystallization zone that forms beneath them.

36 MATERIALS SCIENCE↗

Influence of Thermomechanical Treatment on Structural-Phase Transformations and Mechanical Properties of the Cu–Al–Ni Shape-Memory Alloys

Using the methods of optical and electron microscopy and electron and X-ray diffraction analyses, the influence of thermomechanical treatment on the mechanical properties, average grain size, and structural and phase transformations is investigated in the Cu–Al–Ni triple alloys exhibiting a shape memory effect. In the alloys under study with a fixed content of 3wt% Ni the concentration of aluminum was varied from 9 to 14 wt%. It is shown that in the alloys subjected to thermal treatment, including forging and homogenizing annealing using controlled recrystallization in the austenitic state followed by quenching, the grain-boundary disintegration and segregation disappear. It is found out that the microstructure of the alloys in the hot-forged and hardened states with the content of aluminum 9–10 wt%. consists of the grains of the average dimensions within 60–80 μm, with the content of aluminum 10–12 wt% – 100–350 μm, while in the alloys with the content of aluminum up to 14 12 wt% the average grain size reaches 1 mm. According to the data of mechanical testing at room temperature, with a decrease in the content of aluminum the ultimate tensile strength (σ{sub UTS}), the yield strength (σ{sub М}) and the relative elongation (δ) increase. An improvement of the mechanical properties of the alloys is attributed to the grain structure refinement of the β{sub 2}-austenite and package substructure of the β'{sub 1}-and γ'{sub 1}-martensites as the content of aluminum in the alloys decreases. For instance, in the fine-grained alloys containing 9.2 and 9.5 wt% Al the value of relative elongation remains at a high level (>10%), while for the other alloys with 10–14 wt% Al it does not exceed 5%. As the content of aluminum in the alloys decreases, the character of the specimen fracture under uniaxial tension changes (from brittle to ductile).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Texture Evolution and Phase Transformation in Titanium Investigated by In-Situ Neutron Diffraction

We report in-situ neutron diffraction studies of texture evolution and the (hcp) (bcc) phase transformation in commercially pure cold-drawn titanium upon continuous heating and cooling, complemented by differential scanning calorimetry (DSC) measurements. We show that the recrystallization of the phase at elevated temperature enhanced the preexisting fiber texture, which eventually facilitated the nucleation and growth of the phase favored by the Burgers orientation relationship, i.e., {0001} //{110} . More strikingly, upon completion of the transformation, the {110} texture (or preferred orientation) in was eliminated immediately by the rapid grain growth of intergranular allotriomorphs. This resulted in the loss of the original -texture when Ti was transformed back to from to upon subsequent cooling, distinct from the known texture memory effect for rolling textures in titanium. Our present work provides useful experimental results for understanding the mechanisms of texture evolution and phase transformation in titanium and its alloys and, by and large, low-symmetry alloys such as zirconium.

36 MATERIALS SCIENCE↗

Hot Ductility and Compression Deformation Behavior of TRIP980 at Elevated Temperatures

The hot ductility tests of a kind of 980 MPa class Fe-0.31C (wt pct) TRIP steel (TRIP980) with the addition of Ti/V/Nb were conducted on a Gleeble-3500 thermomechanical simulator in the temperatures ranging from 873 K to 1573 K (600 °C to 1300 °C) at a constant strain rate of 0.001 s{sup −1}. It is found that the hot ductility trough ranges from 873 K to 1123 K (600 °C to 850 °C). The recommended straightening temperatures are from 1173 K to 1523 K (900 °C to 1250 °C). The isothermal hot compression deformation behavior was also studied by means of Gleeble-3500 in the temperatures ranging from 1173 K to 1373 K (900 °C to 1100 °C) at strain rates ranging from 0.01 s{sup −1} to 10 s{sup −1}. The results show that the peak stress decreases with the increasing temperature and the decreasing strain rate. The deformation activation energy of the test steel is 436.7 kJ/mol. The hot deformation equation of the steel has been established, and the processing maps have been developed on the basis of experimental data and the principle of dynamic materials model (DMM). By analyzing the processing maps of strains of 0.5, 0.7, and 0.9, it is found that dynamic recrystallization occurs in the peak power dissipation efficiency domain, which is the optimal area of hot working. Finally, the factors influencing hot ductility and thermal activation energy of the test steel were investigated by means of microscopic analysis. It indicates that the additional microalloying elements play important roles both in the loss of hot ductility and in the enormous increase of deformation activation energy for the TRIP980 steel.

36 MATERIALS SCIENCE↗

Interfacial Microstructural Evolution and Metallurgical Bonding Mechanisms for IN718 Superalloy Joint Produced by Hot Compressive Bonding

The novel metallurgical joining process for bonding IN718 superalloy was investigated by hot compressive bonding (HCB) process under the deformation temperature range of 1000 °C to 1150 °C and true strains ranging from 0 to 0.5 at a strain rate of 0.001 s{sup −1}. The effect of HCB process parameters on the tensile strength was analyzed. Both the as-deformed and the interfacial microstructures were characterized using the optical microscope, electron backscattered diffraction and transmission electron microscope (TEM) analysis. The results of tensile property revealed that the degree of metallurgical bonding is promoted by increasing deformation temperature and strain. The evolution of the interfacial microstructure showed that the migration of interfacial grain boundary (IGB), which is characterized by discontinuous dynamic recrystallization, is the dominant metallurgical bonding mechanism in the early stages of bonding. TEM analysis indicated that the dislocation density is distributed heterogeneously over both sides of IGB, which is the significant reason for the migration of IGB, during the initial stage of HCB process.

36 MATERIALS SCIENCE↗

Characteristics of the Hot Workability of an AZ91D Magnesium Alloy Using 3D Processing Maps

Hot compression tests were carried out on an a homogenized as-cast AZ91D magnesium alloy at temperatures ranging from 220 °C to 380 °C and strain rates ranging from 0.001 to 10 s{sup −1} by means of a Gleeble-3500 thermo mechanical simulator. True stress-–true strain curves were given. A constitutive modeling of the homogenized alloy was proposed to describe the flow characteristic. The deformation activation energy was estimated to be 142.27 kJ mol{sup −1}. Continuous three-dimensional (3D) processing maps were developed based on the true stress–true strain data as a function of strain, temperature, and strain rate. A detailed interpretation of the established 3D processing maps was conducted. The results showed that the variation of the 3D processing maps was significantly strain dependent. Dynamic recrystallization domains with high-power dissipation efficiencies and instability domains with negative instability coefficient were identified from the 3D power dissipation maps and the 3D instability maps, respectively. It was also revealed that the instability domains distinctly became enlarged with the increasing strain. Optimized temperature and strain rate ranges at various strains were determined. Furthermore, hot workability characteristics were clarified through examining the microstructures obtained under conditions falling within stability and instability domains with various strains. The results proved that the developed 3D processing maps can provide an accurate prediction of the hot deformation behavior for the homogenized AZ91D alloy.

36 MATERIALS SCIENCE↗

Characteristics of Bi-metallic Interfaces Formed During Direct Energy Deposition Additive Manufacturing Processing

Various additive manufacturing processes are being evaluated to reduce the time and cost for fabrication of low volume, complex, and multifunctional assemblies. This study evaluated two direct energy deposition processes for the fabrication of large bi-metallic structures. The materials evaluated were Inconel 625 and copper alloy C18150, which are used in various high heat flux applications. Inconel was deposited onto the C18150 substrate using blown powder and wire-fed processes. Complete bonding was obtained in both processes and the resulting interfaces were evaluated using microscopy and indentation testing. Differences were observed in the interface region suggesting the kinetic energy of the blown powder process resulted in more residual stress at the interface, promoting recrystallization and enhanced diffusion. This created a broader interface in the blown powder specimens compared to a narrower mechanically mixed interface with the wire-fed process.

36 MATERIALS SCIENCE↗

Microstructure and Properties of Inconel 718 Fabricated by Directed Energy Deposition with In-Situ Ultrasonic Impact Peening

Many inherent issues, such as the detrimental residual stress, columnar grains with anisotropy, and weak mechanical properties, have severely impeded the adoption of metal additive manufacturing (AM) techniques including powder bed fusion and directed energy deposition (DED) processes. In this study, a hybrid AM process that consists of layer-wise laser metal deposition (i.e., a DED process) and in-situ ultrasonic impact peening (UIP) was applied to obtain Inconel 718 superalloy workpieces. Also, for further property enhancement, a post-heat treatment was applied to the deposited material obtained by the hybrid AM process. Scanning electron microscopy and transmission electron microscope were used to investigate the microstructure morphology and reveal the underlying strengthening mechanism. Electron backscatter diffraction was employed to quantitatively study the microstructure resulted from the hybrid AM process and the post-heat treatment. The profile of residual stress along the depth direction was obtained through X-ray diffraction. The results demonstrate that this hybrid AM process is capable of producing high-quality metal parts with significantly refined microstructure, and beneficial compressive residual stress along the depth into surface. Severe plastic strains are introduced by UIP, and the resulted mechanical twinning and dynamic recrystallization play an important role in refining microstructure. The material microstructure is further refined down to 100 µm, and the texture anisotropy is significantly diminished after solution treatment at 980 °C for 1 hour. Under the as-built condition, in-situ ultrasonic peening alters the residual stress component from a tensile state to an overall compressive state with a maximum value of − 190 MPa within the range of measurement depth.

36 MATERIALS SCIENCE↗

Effect of Aging Treatment on the Precipitation Behavior and Mechanical Properties of Mg-9Gd-3Y-1.5Zn-0.5Zr Alloy

Aging heat treatments of an extruded Mg-9Gd-3Y-1.5Zn-0.5Zr (wt.%) alloy at 200, 225, and 250 °C for various times were studied. The results show that dynamic recrystallization (DRX) occurred during the extrusion process and the alloy exhibited a significant aging hardening response at temperatures ranging from 200 to 225 °C. The precipitation sequence of the alloy at 225 °C was supersaturated solid solution (SSSS) → β″ (D0{sub 19}, Mg{sub 3}RE) → β′ (bco, Mg{sub 15}RE{sub 3}), where the β′ phase was the primary precipitated phase. A large amount of discontinuous lamellar-shaped 14H-structure long period stacking ordered (LPSO) phase was also observed in the α-Mg matrix before and after aging treatments. Owing to the combined strengthening effect of fine DRXed grains, β′ nanoparticles, and widespread LPSO phases, the ultimate tensile strength and tensile yield strength of the peak-aged extruded alloy reached 409 and 303 MPa, respectively. The elongation in this circumstance was ~7.1%, which was slightly lower than that of the alloy before aging treatment.

36 MATERIALS SCIENCE↗

Effect of Microstructural Evolution on Sagging Behavior of Cold-Rolled Aluminum Foil During the Brazing Thermal Cycle

Effect of microstructural evolution on sagging behavior of aluminum foil was investigated during the brazing thermal cycle. During the brazing thermal cycle, the sagging behavior consists of three stages: slight sagging stage, accelerative sagging stage and slow sagging stage. The sagging of cold-rolled aluminum foil mainly occurs in the accelerative sagging stage, which is governed by recovery under external stress in the sagging test. The coarse recrystallized grain is responsible for the slow sagging stage by reducing grain boundary sliding. Increasing cold-rolled reduction and addition of final annealing heat treatment can improve sagging resistance by shortening recovery process during the brazing thermal cycle. Dissolution of dispersoids has few effects on sagging deformation.

36 MATERIALS SCIENCE↗

Effects of Roughing on Finish Rolling Simulations in Microalloyed Strip Steels

The effects of a roughing pass in hot rolling simulations were assessed in VN and Nb-Ti steels. Continuous cooling phase transformation temperatures, flow curves, softening mechanisms (dynamic transformation DT and dynamic recrystallization DRX), and deformed microstructure morphologies were analyzed. The application of one or more roughing passes eliminates the effects of prior microstructural history and ensures that all stock material experiences equivalent hot working conditions and state of the microalloying elements. It has been shown that roughing in hot simulation has the following positive influences: (1) provide more reliable flow stress data; (2) give greater consistencies and accuracy in analysis of softening mechanisms giving three distinct regimes (DT regime at temperatures below 800 °C, DT/DRX inter-mode regime between 800 and 950 °C and DRX regime for temperatures above 950 °C for VN steel); (3) promotion of softening mechanisms as evidence by low critical strains (ε{sub c DT} was within the range 0.08-0.12, while for finishing-only pass, the ε{sub c DT} was in the range of 0.11-0.14 at ε-dot =0.1 s{sup −1}); (4) for roughing and finishing schedules, DT was verified to occur at temperatures 117 and 133 °C above Ae{sub 3} for VN steel and Nb-Ti steel, respectively, compared to the F-only schedules which showed that DT can only occur at temperatures below the Ae{sub 3}; (5) RF schedules promoted uniform microstructural morphologies compared to inhomogeneous microstructures realized in F-only schedules.

36 MATERIALS SCIENCE↗

Effect of 0.1 wt.% Co on the Hot Deformation and Toughness of Fine-Grained Low-Carbon Steel at Sub-zero Temperatures

The effect of 0.1 wt.% Co on the hot deformation behavior of fine-grained low-carbon microalloyed steel was investigated at temperatures of 850-1200 °C and a strain rate of 5 s{sup −1}. Furthermore, the toughness of the steel with and without Co at sub-zero temperatures was evaluated. The results suggest that the addition of 0.1 wt.% Co increases the flow stress and delays the occurrence of dynamic recrystallization (DRX) at the same deformation temperature and strain. The DRX fraction of steel specimens without and with 0.1 wt.% Co was about 67.4 and 43.9% at 850 °C, respectively. Then, it increased to 100% at 1100 °C. Compared with steel without Co, cementite particles in the tempered sorbite of steel with 0.1 wt.% Co decreased in size but increased in quantity, yield strength increased from 756 to 787 MPa, and Charpy V-notch energy at − 20 and − 50 °C improved from 69 and 41 to 102 and 65 J, respectively. The fracture morphology and crack propagation characteristics were consistent with the variation in impact energy.

36 MATERIALS SCIENCE↗

The Effect of Grain Size on the Strain Hardening Behavior for Extruded ZK61 Magnesium Alloy

The effects of grain size on the tensile and compressive strain hardening behaviors for extruded ZK61 alloys have been investigated by uniaxial tensile and compressive tests along the extrusion directions. Cylindrical tension and compression specimens of extruded ZK61 alloys with various sized grain were fabricated by annealing treatments. Tensile and compressive tests at ambient temperature were conducted at a strain rate of 0.5 × 10{sup −3} s{sup −1}. The results indicate that both tensile strain hardening and compressive strain hardening of ZK61 alloys with different grain sizes have an athermal regime of dislocation accumulation in early deformation. The threshold stress value caused dynamic recovery is predominantly related to grain size in tensile strain hardening, but the threshold stress values for different grain sizes are almost identical in compressive strain hardening. There are obvious transition points on the tensile strain hardening curves which indicate the occurrence of dynamic recrystallization (DRX). The tensile strain hardening rate of the coarse-grained alloy obviously decreases faster than that of fine-grained alloys before DRX and the tensile strain hardening curves of different grain sizes basically tend to parallel after DRX. The compressive strain hardening rate of the fine-grained alloy obviously increases faster than that of coarse-grained alloy for twin-induced strain hardening, but compressive strain hardening curves also tend to parallel after twinning is exhausted.

36 MATERIALS SCIENCE↗

Microstructure Characteristic and Mechanical Properties of High-Strength Mg-Nd-Zn-Zr Alloy Seamless Tube Produced by Integrated Extrusion

Large size seamless tubes of Mg-3.0Nd-0.4Zn-0.4Zr alloy (NZ30K, in weight percent) were prepared by integrating backward extrusion with forward extrusion. Microstructure, mechanical properties, aging behavior and texture of the tubes were investigated. The microstructure of as-extruded tube is characterized by the blend of considerably elongated grains and fine equiaxed grains. The maximum values of yield strength and ultimate tensile strength, i.e., 191 and 245 MPa, were obtained in the as-extruded tubes, and these values were increased to 212 and 267 MPa in the peak-aged tubes (T5), implying an increasing ratio of 9 and 11%, respectively. The peak value of the Vickers’ micro-hardness of the NZ30K tubes extruded at 673, 723 and 753 K are 66, 64 and 60 (kilogram-force per square millimeter), respectively. The texture of NZ30K tube is weak, the primary mechanism behind which is suggested to be the particle-induced nucleation responsible for the promotion of recrystallization.

36 MATERIALS SCIENCE↗