Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “IRON COMPOUND”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 577 records · Page 32

Self-modulated nanostructures in super-large-period Bi{sub 11}(Fe{sub 5}CoTi{sub 3}){sub 10/9}O{sub 33} epitaxial thin films

Super-large-period Aurivillius thin films with a pseudo-period of ten were grown on (0 0 1) SrTiO{sub 3} substrates using the pulsed laser deposition method. The as-grown films are found to be coherently strained to the substrate and atomically smooth. X-ray diffraction indicates an average periodicity of ten, while analysis with the high resolution scanning transmission electron microscopy reveals a self-modulated nanostructure in which the periodicity changes as the film thickness increases. Finally, we discuss the magnetic and possible ferroelectric properties of the self-modulated large period Aurivillius films at the room temperature.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Controlled motion of domain walls in submicron amorphous wires

Results on the control of the domain wall displacement in cylindrical Fe{sub 77.5}Si{sub 7.5}B{sub 15} amorphous glass-coated submicron wires prepared by rapid quenching from the melt are reported. The control methods have relied on conical notches with various depths, up to a few tens of nm, made in the glass coating and in the metallic nucleus using a focused ion beam (FIB) system, and on the use of small nucleation coils at one of the sample ends in order to apply magnetic field pulses aimed to enhance the nucleation of reverse domains. The notch-based method is used for the first time in the case of cylindrical ultrathin wires. The results show that the most efficient technique of controlling the domain wall motion in this type of samples is the simultaneous use of notches and nucleation coils. Their effect depends on wire diameter, notch depth, its position on the wire length, and characteristics of the applied pulse.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Annealing induced structural changes in amorphous Co{sub 23}Fe{sub 60}B{sub 17} film on Mo buffer layer

Structural changes occurring in a thin amorphous Co{sub 23}Fe{sub 60}B{sub 17} film sandwiched between two Mo layers, as a function of thermal annealing has been studied. Thermal stability of the Co{sub 23}Fe{sub 60}B{sub 17} film is found to be significantly lower than the bulk ribbons. SIMS measurements show that during crystallization, boron which is expelled out of the crystallites, has a tendency to move towards the surface. No significant diffusion of boron in Mo buffer layer is observed. This result is in contrast with some earlier studies where it was proposed that the role of buffer layer of refractory metal is to absorb boron which is expelled out of the bcc FeCo phase during crystallization.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of boron on the structural and magnetic properties of Co{sub 2}FeSi{sub 1-x}B{sub x} Heusler alloys

The partial substitution of Si with B on the structural and magnetic properties of Co{sub 2}FeSi{sub 1-x}Bx (x = 0-0.5) alloys was systematically investigated. X-ray and microstructural investigations show the presence of second phase at the grain boundaries which increases with increasing boron content. From thermal analysis studies, it was observed that L2{sub 1}-B2 ordering temperature remain constant whereas the melting point decreases with increase in boron addition and merges with ordering temperature at x = 0.5. The increase in T{sub C} for the alloys x ≥ 0.25 was attributed to the increase in second phase due to boron.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of 2mol% Na/Bi excess on multiferroic properties of (Na{sub 0.5}Bi{sub 0.5}) {sub 0.99}La{sub 0.01}Ti{sub 0.988} Fe{sub 0.012}O{sub 3} lead free system

Lead free (Na{sub 0.5}Bi{sub 0.5}) {sub 0.99}La{sub 0.01}Ti{sub 0.988} Fe{sub 0.012}O{sub 3} (NBLTF) system has been synthesized by sol gel method without and with 2 mol% excess of Na and Bi. X-ray diffraction patterns of NBLTF samples confirm perovskite structure having rhombohedral R3c phase symmetry. Metal oxide band observed at ~ 629 cm{sup −1} wavnumber in FTIR spectra also confirm formation of perovskite phase in samples. Microstructural analysis exhibits dense crystal growth having better grains connectivity for NBLTF sample with 2 mol% excess Na/Bi which is supported by room temperature DC resistivity measurements. Dense crystal growth and low leakage current with 2 mol% excess Na/Bi is reported to improve multiferroic properties of NBLTF sample and provides new insight to explore single phase lead free multiferroic system.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic properties of DyFe{sub 3}(BO{sub 3}){sub 4}

The magnetic properties of an easy-axis trigonal DyFe{sub 3}(BO{sub 3}){sub 4} antiferromagnetic crystal have been theoretically studied. On this basis, recent experimental data [1] on the field and temperature dependences of magnetization and the temperature dependence of the initial magnetic susceptibility for three crystallographic directions in this antiferromagnet have been interpreted. The characteristics of the trigonal crystal field for the rare earth ion and the parameters of the Fe-Fe and Fe-Dy exchange interactions are determined. Limitations imposed by features of the magnetic characteristics (anisotropic magnetization in the three crystallographic directions, Schottky-type anomalies in the magnetic susceptibility, etc.) on the possible splitting of the ground-state multiplet in the crystal field and the splitting of the lowest doublet due to the f-d interaction for Dy{sup 3+} ions are established.

36 MATERIALS SCIENCE↗

Manufacturing of Sputtering Composite Targets Containing Phases of Co{sub 2}FeSi or Co{sub 2}MnSi Heusler Alloy

The paper presents a method for manufacturing mechanically strong sputtering composite targets containing the phase of the Co{sub 2}FeSi or Co{sub 2}MnSi Heusler alloy of the stoichiometric composition, which can be used for fabrication of spin electronic devices by high-frequency magnetron deposition and pulsed laser deposition of thin films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis of TiO{sub 2} Nanoparticles from Ilmenite Through the Mechanism of Vapor-Phase Reaction Process by Thermal Plasma Technology

Synthesis of nanoparticles of TiO{sub 2} was carried out by non-transferred arc thermal plasma reactor using ilmenite as the precursor material. The powder ilmenite was vaporized at high temperature in plasma flame and converted to a gaseous state of ions in the metastable phase. On cooling, chamber condensation process takes place on recombination of ions for the formation of nanoparticles. The top-to-bottom approach induces the disintegration of complex ilmenite phases into simpler compounds of iron oxide and titanium dioxide phases. The vapor-phase reaction mechanism was carried out in thermal plasma zone for the synthesis of nanoparticles from ilmenite compound in a plasma reactor. The easy separation of iron particles from TiO{sub 2} was taken place in the plasma chamber with deposition of light TiO{sub 2} particles at the top of the cooling chamber and iron particles at the bottom. The dissociation and combination process of mechanism and synthesis are studied briefly in this article. The product TiO{sub 2} nanoparticle shows the purity with a major phase of rutile content. TiO{sub 2} nanoparticles produced in vapor-phase reaction process shows more photo-induced capacity.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Investigation of Fe/Mo Ordering and Magnetic Properties of Ca{sub 2}Fe{sub x}Mo{sub 2−x}O{sub 6} (x = 0.9, 1.0, 1.1 and 1.2) Double Perovskites Prepared by Sonochemical Method

Characterization, Fe/Mo ordering and magnetic properties of Ca{sub 2}Fe{sub x}Mo{sub 2−x}O{sub 6} (x = 0.9, 1.0, 1.1 and 1.2) (CFMO) double perovskite have been studied. Sonochemical methodology is adopted to synthesize Ca{sub 2}Fe{sub x}Mo{sub 2−x}O{sub 6} double perovskite at low temperature (950 {sup ∘} C) under Ar/H{sub 2} atmosphere. Single-phase monoclinic structure by space group P2{sub 1}/n, lattice parameters (a, b and c) and unit cell volume (V ) have been confirmed from X-ray diffraction (XRD) patterns. Average grain sizes of 145 nm with a variation of porosity were observed from scanning electron microscopy (SEM) pictures. Elemental analysis using energy-dispersive X-ray spectroscopy (EDS) confirmed the presence of elements Ca, Fe, Mo and O with no trace of foreign elements, and the compound is found to be pure. Fourier transform infrared spectroscopy (FTIR) data confirmed perovskite formation by identifying three characteristic absorption bands in the wave number range 400–1000 cm{sup − 1} for Mo-O and Fe-O vibrations. Magnetic properties like M{sub s}, M{sub r} and H{sub c} were studied for CFMO series using vibrating sample magnetometer (VSM). Saturation magnetization is found to vary with Fe composition (x).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of Deposition Temperature on the Structural and Physical Properties of Ba(Fe{sub 1.8}Co{sub 0.2}){sub 2}As{sub 2} Thin Film

Ba(Fe{sub 1.8}Co{sub 0.2}){sub 2}As{sub 2} thin films have been grown directly on (001) SrTiO{sub 3} (STO) substrates by pulsed laser deposition at the temperatures from 640 to 700 {sup ∘}C. Effects of deposition temperature (T{sub s}) on the structure, magnetic, and superconducting properties of the films are investigated systematically. It is found that Ba(Fe{sub 1.8}Co{sub 0.2}){sub 2}As{sub 2} film grown at lower deposition temperature is polycrystalline, and the optimized temperature of 685 {sup ∘}C can yield high-quality epitaxial Ba(Fe{sub 1.8}Co{sub 0.2}){sub 2}As{sub 2} film. The (002) diffraction peak of Fe metal at 2𝜃 =∼ 65{sup ∘} is observed along with the (00l) diffraction peaks of Ba(Fe{sub 1.8}Co{sub 0.2}){sub 2}As{sub 2} films deposited at all temperatures, which is attributed to the decomposition of BaFe{sub 1.8}Co{sub 0.2}As{sub 2} target when a high-energy pulsed laser hit on the target in a high vacuum. X-ray photoelectron spectra of Fe 2p show that the relative percentage of zerovalent ion (Fe{sup 0}) is almost equal to that of divalent ion (Fe{sup 2+}) for the film deposited at 670 {sup ∘}C, which is different from that most Fe{sup 2+} ions exist in the BaFe{sub 1.8}Co{sub 0.2}As{sub 2} target. The saturation magnetization (M{sub s}) increases from 7.88 to 240.5 emu/cm{sup 3} monotonously with the increase of Ba(Fe{sub 1.8}Co{sub 0.2}){sub 2}As{sub 2} film deposition temperature. The maximum zero-resistance temperature (T{sub c}{sup 0}) of ∼16 K was obtained, which can be attributed to the high quality of the Ba(Fe{sub 1.8}Co{sub 0.2}){sub 2}As{sub 2} film. The coexistence of superconductivity (SC) and ferromagnetism (FM) in the BaFe{sub 1.8}Co{sub 0.2}As{sub 2} films was discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Processing of High-Entropy AlCoCr{sub 0.75}Cu{sub 0.5}FeNi Alloy by Spray Forming

Compositionally complex AlCoCrCuFeNi alloy system is one of the extensively studied high-entropy alloys (HEA). Most of these studies have been carried out on as-cast materials that witness slow cooling rate during solidification. In the present investigation, HEA based on AlCoCrCuFeNi system was processed employing spray forming so as to realize its inherent rapid solidification effect and unique microstructural evolution mechanism. The spray formed as well as the as-cast alloys were compared in terms of their microstructural features, phase constitution and hardness. These microstructural features were also compared with that of the overspray powders (< 250 µm) obtained as a by-product of spray forming. Both the as-cast and spray formed alloys showed a mixture of mainly two phases, i.e., face-centered and body-centered cubic (BCC) phases, in contrast to a single BCC phase in overspray powders. However, the spray formed alloy revealed unidentified phases, as against the as-cast material, which disappeared after heat treatment at 1473 K for 3 h. The grain size of the as-cast alloy was around 600-1000 μm compared to a highly refined grain size of 25-30 μm in the as-spray formed alloy. It was found that the hardness of the regions dominated by the constituent phases as well as the bulk of the spray formed material was higher than that of the as-cast alloy. The results validate the efficacy of the process in achieving drastic refinement in grain size, in a single step of large-scale spray forming. The characteristic microstructural features and the phase constitutions have been discussed in light of the prevailing mechanisms of structural evolution and possible solidification phenomena during spray atomization and deposition. This study gives a new direction in processing of these alloys and understanding their solidification behavior under the conditions of layer-by-layer deposition of semi-solid/liquid droplets.

36 MATERIALS SCIENCE↗

Possibility to Use Hydrothermally Synthesized CuFeS{sub 2} Nanocomposite as an Acceptor in Hybrid Solar Cell

Here we have approached the plausible use of CuFeS{sub 2} nanocomposite as an acceptor in organic–inorganic hybrid solar cell. To produce CuFeS{sub 2} nanocomposite, hydrothermal strategy was employed. The room-temperature XRD pattern approves the synthesized material as CuFeS{sub 2} with no phase impurity (JCPDS Card no: 37-0471). The elemental composition of the material was analyzed from the TEM-EDX data. The obtained selected area electron diffraction (SAED) planes harmonized with the XRD pattern of the synthesized product. Optical band gap (4.14 eV) of the composite from UV–Vis analysis depicts that the synthesized material is belonging to wide band gap semiconductor family. The HOMO (− 6.97 eV) and LUMO (− 2.93 eV) positions from electrochemical study reveal that there is a possibility of electron transfer from MEH-PPV to CuFeS{sub 2}. The optical absorption and photoluminescence spectra of MEH-PPV:CuFeS{sub 2} (donor:acceptor) composite were recorded sequentially by varying weight ratios. The monotonic blue shifting of the absorption peak position indicated the interaction between donor and acceptor materials. The possibility of electron transfer from donor (MEH-PPV) to acceptor (CuFeS{sub 2}) was approved with photoluminescence analysis. Subsequently, we have fabricated a hybrid solar cell by incorporating CuFeS{sub 2} nanocomposite with MEH-PPV in open atmosphere and obtained 0.3% power conversion efficiency.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Dynamic Analysis of Recalescence Process and Interface Growth of Eutectic Fe{sub 82}B{sub 17}Si{sub 1} Alloy

By employing the glass fluxing technique in combination with cyclical superheating, the microstructural evolution of the undercooled Fe{sub 82}B{sub 17}Si{sub 1} alloy in the obtained undercooling range was studied. With increase in undercooling, a transition of cooling curves was detected from one recalescence to two recalescences, followed by one recalescence. The two types of cooling curves were fitted by the break equation and the Johnson–Mehl–Avrami–Kolmogorov model. Based on the cooling curves at different undercoolings, the recalescence rate was calculated by the multi-logistic growth model and the Boettinger–Coriel–Trivedi model. Both the recalescence features and the interface growth kinetics of the eutectic Fe{sub 82}B{sub 17}Si{sub 1} alloy were explored. The fitting results that were obtained using TEM (SAED), SEM and XRD were consistent with the changing rule of microstructures. Finally, the relationship between the microstructure and hardness was also investigated.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Three-Layer TIG-Welded 2219 Aluminum Alloys with Dissimilar Heat Treatments

2219-C10S and 2219-CYS aluminum alloys are 2219 aluminum alloys with different heat treatment processes, and they have been widely used in the aerospace industry. In the present study, 2219-C10S and 2219-CYS aluminum alloys were butt-welded by three-layer tungsten inert gas arc welding (with the welding center of the third layer shifted toward the CYS side), and the microstructure characteristics and mechanical properties of the welded joint were investigated. The lamellar θ′ phases, the bulk or rod θ phases, and the coarse rod-shaped or pancake-shaped Al-Cu-Fe-Mn phases coexisted in the two aluminum alloys. The Cu content of the α-Al matrix and the distribution of eutectic structures of different welding layers in the weld zone (WZ) were varied, implying that the segregation degrees of the Cu element were different due to the different welding thermal cycles in different welding layers. The microhardness values of the CYS side were much higher than those of the C10S side in each region on both sides of the joint. The tensile test deformation was concentrated mainly in the regions of WZ and the over aged zone (OAZ), where the microhardness values were relatively low. The main deformation concentrated region was transferred from the CYS side to the C10S side with the increase in the tensile load during the tensile test. The fracture behavior of the tensile test showed that the macroscopic crack initiated near the front weld toe had gone through the crack blunt region, the shear fracture region of the partially melted zone (PMZ), and the shear fracture region of OAZ. Meanwhile, the fracture characteristics gradually evolved from brittle to ductile. The concentrated stress and the dense eutectic structure in the region near the front weld toe of the C10S side contributed to the fracture of the joint. The shift of the welding center of the third layer to the CYS side resulted in two effects: (i) the microhardness values from the middle layer to the top layer in the PMZ of the CYS side were the most significantly increased and (ii) the distance between the front weld toe and the fusion line of the CYS side was significantly larger.

36 MATERIALS SCIENCE↗

Effect of Ceramic Rolling and Annealing on Mechanical Properties of AlCoCrFeNi{sub 2.1} Eutectic High-Entropy Alloys

It was firstly proved that AlCoCrFeNi{sub 2.1} could optimize the strength-ductility combination by ceramic rolling at room temperature. The technique greatly enhanced the strength of the materials at the price of slight ductility, which is different from the previous studies. When the thickness reduction was 23.06%, the yield strength and compressive strength were 1611.42 and 2212.99 MPa, respectively, with the plastic strain of 28.36%. Such an excellent combination of strength and ductility was attributed to the distribution of the residual stress, the high hydrostatic stress and the shear bands in ceramic rolling process. The plastic strain of the material increased to 38.54%, and the strength reduced to 1900.73 MPa after annealing at 800 °C for 1 h. A lot of like-flower patterns of recrystallized ultrafine grain were observed after annealing at 800 °C due to the sluggish diffusion in HEAs and the effect of ceramic rolling. In addition, after annealing at 800 °C, the fracture mode changed to shearing fracture of microvoid aggregation from cleavage/quasi-cleavage fracture of as-rolled sample due to the deposition of the second phase in the tested sample.

36 MATERIALS SCIENCE↗

Low Solution Temperature Heat Treatment of AlSi{sub 9}Cu{sub 3}(Fe) High-Pressure Die-Casting Actual Automotive Components

Usually, high-pressure die-casting (HPDC) components cannot be heat-treated at high temperature without the occurrence of surface blisters, which are unacceptable for surface finish and may reduce the mechanical properties. In this context, the purpose of the present paper was to analyze the effectiveness of special low solution temperature T6 heat treatment in overcoming this limit for HPDC AlSi{sub 9}Cu{sub 3} alloy. Very low solution temperatures (< 450 °C, followed by 165 °C aging) to prevent the occurrence of blisters were combined with commonly used times (from 1 to 16 h) ensuring the feasibility of industrial application. Treatments were conducted on samples extracted from actual castings to evaluate the typical defects encountered in common production. Properties were analyzed by means of visual inspection, microstructural observations, image analysis, hardness, tensile tests and fractography. The results showed that it is possible to use solubilization temperatures below 450 °C for several hours in a T6 treatment to give strengthening without relevant blistering in AlSi{sub 9}Cu{sub 3} alloy. The optimum match of properties was provided by a solution treatment at 430 °C for 4 h followed by an aging at 165 °C for 8 h, which gave a yield increase of ~ 50 MPa, an increase in ductility and the best Quality Index value.

36 MATERIALS SCIENCE↗

Crystal chemistry of the divalent cation in alluaudite-type phosphates: A structural and infrared spectral study of the Na{sub 1.5}(Mn{sub 1-x}M{sub x}{sup 2+}){sub 1.5}Fe{sub 1.5}(PO{sub 4}){sub 3} solid solutions (x=0 to 1, M{sup 2+}=Cd{sup 2+}, Zn{sup 2+})

Compounds of the Na{sub 1.5}(Mn{sub 1-x}M{sub x}{sup 2+}){sub 1.5}Fe{sub 1.5}(PO{sub 4}){sub 3} (M{sup 2+}=Cd{sup 2+}, Zn{sup 2+}) alluaudite-type solid solutions were synthesized by solid-state reactions in air, between 800 and 900 deg. C, and were investigated by X-ray powder diffraction and infrared spectroscopy. The site occupancy factors of the Na{sub 1.5}(Mn{sub 1-x}Cd{sub x}{sup 2+}){sub 1.5}Fe{sub 1.5}(PO{sub 4}){sub 3} compounds, obtained from the Rietveld refinements of the X-ray powder patterns, indicate that the replacement of Mn{sup 2+} by Cd{sup 2+} takes place on the M(1) site for x=0.25 and 0.50, and then on the M(1) and M(2) sites for x=0.75 and 1.00. Small amounts of Cd{sup 2+} were also detected on the A(1) site, compensated by small amounts of Na{sup +} occurring on M(1). This partially disordered distribution is probably due to the similar effective ionic radii of Cd{sup 2+} and Na{sup +}. The cationic distributions in the Na{sub 1.5}(Mn{sub 1-x}Zn{sub x}{sup 2+}){sub 1.5}Fe{sub 1.5}(PO{sub 4}){sub 3} solid solution indicate that Zn{sup 2+} was first introduced in the M(2) site, before to replace Mn{sup 2+} in the M(1) site. The unit-cell parameters show a significant increase when Mn{sup 2+} is replaced by Cd{sup 2+}, and a significant decrease when it is replaced by Zn{sup 2+}. The variations of the {beta} angle were also correlated with the M(1)-M(2) distances. The infrared spectra show the displacement of an absorption band at ca. 400-425 cm{sup -1}, which is assigned to the vibrations of the M{sup 2+} cations localized on the M(1) site. This assignment is confirmed by the excellent correlations between the M(1)-O bond distances and the energy of the absorption band. - Graphical abstract: The crystal structure of Na{sub 1.5}Zn{sub 1.5}Fe{sup 3+}{sub 1.5}(PO{sub 4}){sub 3}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗