Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FLY ASH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 577 records · Page 32

Copper-doped silica materials silanized with bis-(triethoxy silyl propyl)-tetra sulfide for mercury vapor capture

The use of Cu-S sites for Hg capture from the gas phase has been successfully applied to a silica-based platform using an S4 organic polysulfane and copper sulfate. The maximum fixed-bed equilibrium capacity achieved using these materials was 19 789 {mu}g Hg.g{sup -1} sorbent for a material with 2.5 wt % Cu and 6 wt % S. An optimal S level was determined to be around 3 wt % because enhancement of capacity was only 18% when increasing from this 3 to 6 wt %. The rate of adsorption in pure beds ranged from 0.6 to 1.6 {mu}g Hg.min{sup -1} depending on the inlet concentration. Differences in breakthrough times suggest that material deposition is not uniform. When compared to two other platforms, commercially available Darco HG-LH and previously tested Fe-Cu-S4 nanoaggregates, the Si-1 material performed the best in fixed-bed testing. During entrained-flow testing, a steady-state Hg removal of 82% was achieved using Si-1 at injection rates of both 6 x 10{sup -5} and 1.2 x 10{sup -4} g.L{sup -1}.h{sup -1}. The lack of increase in Hg removal when the injection rate is doubled suggests that pore accessibility is the rate-controlling step during dynamic Hg capture. A calculation of the approximate pore usage based on injection testing helped confirm this observation. During injection testing, the performance of Si-1 was only diminished 10% when exposed to 20 ppm SO{sub 3}. This is an encouraging result for flue-gas applications where SO{sub 3} levels range from 1 to 40 ppm. Testing demonstrated that Si-1 is stable when exposed to leaching conditions after concrete blending and cement impregnation. This is an important aspect to consider for injection because the sale of fly ash for concrete is a key cost-recovery tool for power plants. 27 refs., 8 figs., 5 tabs.

01 COAL, LIGNITE, AND PEAT↗

Effect of bed pressure drop on performance of a CFB boiler

The effect of bed pressure drop and bed inventory on the performances of a circulating fluidized bed (CFB) boiler was studied. By using the state specification design theory, the fluidization state of the gas-solids flow in the furnace of conventional CFB boilers was reconstructed to operate at a much lower bed pressure drop by reducing bed inventory and control bed quality. Through theoretical analysis, it was suggested that there would exist a theoretical optimal value of bed pressure drop, around which the boiler operation can achieve the maximal combustion efficiency and with significant reduction of the wear of the heating surface and fan energy consumption. The analysis was validated by field tests carried out in a 75 t/h CFB boiler. At full boiler load, when bed pressure drop was reduced from 7.3 to 3.2 kPa, the height of the dense zone in the lower furnace decreased, but the solid suspension density profile in the upper furnace and solid flow rate were barely influenced. Consequently, the average heat transfer coefficient in the furnace was kept nearly the same and the furnace temperature increment was less than 17{sup o}C. It was also found that the carbon content in the fly ash decreased first with decreasing bed pressure drop and then increased with further increasing bed pressure drop. The turning point with minimal carbon content was referred to as the point with optimal bed pressure drop. For this boiler, at the optimum point the bed pressure was around 5.7 kPa with the overall excess air ratio of 1.06. When the boiler was operated around this optimal point, not only the combustion efficiency was improved, but also fan energy consumption and wear of heating surface were reduced. 23 refs., 6 figs., 4 tabs.

01 COAL, LIGNITE, AND PEAT↗

In-situ determination of atmospheric aerosol composition as a function of hygroscopic growth

An in-situ measurement setup to determine the chemical composition of aerosols as a function of hygroscopicity is presented. This has been done by connecting a custom-built Hygroscopicity Tandem Differential Mobility Analyzer (HTDMA) and an Aerosol Time-of-Flight Mass Spectrometer (ATOFMS), commercially available from TSI (Model 3800). Single particle bipolar mass spectra from aerosols leaving the HTDMA could thus be obtained as a function of the hygroscopic growth factor. For these studies the HTDMA was set at a relative humidity of 82% and particles with a dry diameter of 260 nm were selected. The setup was first laboratory tested after which field experiments were performed. Two datasets were obtained during wintertime 2007 in Switzerland: the first in the urban Zurich environment and the other at the remote high alpine research station Jungfraujoch (JFJ). In Zurich several thousand mass spectra were obtained in less than two days of sampling due to a high aerosol loading. At the JFJ, due to low particle concentrations in free tropospheric airmasses, a longer sampling period was required. Both in Zurich and at the JFJ two different growth factor modes were observed. Results from these two locations show that most aerosol particles were a mixture of several compounds. A large contribution of organics and combustion species was found in the less hygroscopic growth mode for both locations. Non-combustion refractory material (e.g. metals, mineral dust, and fly ash) was also highly enhanced in the non-hygroscopic particles. Sulfate, normally considered highly soluble, was found to be a constituent in almost all particles independent of their hygroscopic growth factor.

54 ENVIRONMENTAL SCIENCES↗

Novel aqueous amine looping approach for the direct capture, conversion and storage of CO 2 to produce magnesium carbonate

Designing novel integrated chemical pathways for the capture, conversion, and storage of CO 2 is a crucial need for advancing sustainable energy conversion. The accelerated conversion of CO 2 to water-insoluble and stable magnesium carbonate is a thermodynamically downhill route for permanently storing CO 2 . However, a practical constraint of carbon mineralization is the slow kinetics at low CO 2 concentrations. In this study, we investigate a direct integrated mineralization approach, whereby CO 2 , amine solvents (such as monoethanolamine, MEA), water and alkaline Mg-bearing solids are reacted in a slurry reaction environment. About 70% conversion of magnesium oxide to magnesium carbonate was achieved at 50 °C after 3 hours. The looping of amine-bearing solvents between the CO 2 loaded and release states, facilitates the accelerated conversion of magnesium-bearing oxides to magnesium carbonate. Hydrated magnesium carbonate and magnesium hydroxide phases were noted when less than complete conversion of magnesium oxide was achieved. The morphological features were determined using in operando ultra-small and small angle X-ray scattering (USAXS/SAXS) and grazing incidence-small angle X-ray scattering (GI-SAXS) measurements. The proposed pathway is an adaptive, low temperature, single-step approach for the direct capture, conversion and storage of CO 2 . By demonstrating the effectiveness of aqueous alkaline amine looping approach for the accelerated carbon mineralization of MgO, we aim to expand this approach to include heterogeneous alkaline industrial residues such as coal fly ash and steel slag and naturally occurring minerals such as magnesium silicate and calcium silicate.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of Cement Changes and Aggregate System on Mechanical Properties of Concrete

In this paper, mechanical properties of concrete mixtures containing different cementitious combinations and two aggregate systems were investigated under plastic and drying conditions. Emphasis was laid on durability and shrinkage of concrete. Life Cycle Analysis was also conducted by using Green Concrete LCA Webtool. Results indicated that the presence of larger aggregate sizes tend to enhance durability of concrete. The presence of nanosilica also imparted superior mechanical properties to concrete. A cementitious combination containing Portland Limestone Cement and fly ash with larger aggregate sizes emerged as a better performing mixture in terms of mechanical properties and with minimum environmental impact.

36 MATERIALS SCIENCE↗

Studies on the production of ultra-clean coal by alkali-acid leaching of low-grade coals

The use of low-grade coal in thermal power stations is leading to environmental pollution due to the generation of large amounts of fly ash, bottom ash, and CO{sub 2} besides other pollutants. It is therefore important to clean the coal before using it in thermal power stations, steel plants, or cement industries etc. Physical beneficiation of coal results in only limited cleaning of coal. The increasing environmental pollution problems from the use of coal have led to the development of clean coal technologies. In fact, the clean use of coal requires the cleaning of coal to ultra low ash contents, keeping environmental norms and problems in view and the ever-growing need to increase the efficiency of coal-based power generation. Therefore this requires the adaptation of chemical cleaning techniques for cleaning the coal to obtain ultra clean coal having ultra low ash contents. Presently the reaction conditions for chemical demineralization of low-grade coal using 20% aq NaOH treatment followed by 10% H{sub 2}SO{sub 4} leaching under reflux conditions have been optimized. In order to reduce the concentration of alkali and acid used in this process of chemical demineralization of low-grade coals, stepwise, i.e., three step process of chemical demineralization of coal using 1% or 5% aq NaOH treatment followed by 1% or 5% H{sub 2}SO{sub 4} leaching has been developed, which has shown good results in demineralization of low-grade coals. In order to conserve energy, the alkali-acid leaching of coal was also carried out at room temperature, which gave good results.

01 COAL, LIGNITE, AND PEAT↗

Electrochemistry of Praseodymium in Aqueous Solution Using a Liquid Gallium Cathode

We report the electrochemistry of liquid Ga electrodes in aqueous media was examined in the presence of praseodymium acetate (PrOAc) as an alternate path for low temperature reduction of rare earth elements (REE). This study investigated the aqueous electrochemistry of Ga with and without REEs (Pr). Cyclic voltammetry experiments showed that in the presence of PrOAc, an order of magnitude increase in cathodic current was observed for the Ga electrode, compared to that in the absence of Pr. Decrease in the reduction current with the increase of scan rate, with and without Pr, suggests catalytic reactions following electron transfer, which was attributed to the Ga 2 O disproportionation reaction. Chronoamperometric experiments performed in Pr containing solutions formed a precipitate. Over 50% of the Pr ions from the aqueous electrolyte were immobilized in the precipitate; a solid Ga-rich phase. Formation of this precipitate was only possible when Ga oxidation was induced. This condition was achieved by circulation of liquid Ga from the pool via external pump and returned dropwise to the liquid Ga pool. When the collected precipitate was leached in dilute HCl, Pr was released with H 2 evolved as a byproduct, and Ga returned to its initial liquid metallic state. These preliminary results show encouraging new routes that could be applied for the recovery of diluted REE leachates, such as those obtained from magnets, coal fly ash, and ores.

25 ENERGY STORAGE↗

Chemical, Calcium Phosphate Cements for Geothermal Wells - Corrosion Protection, Bond Strength and Matrix Self-Healing

The data set shows performance of economical calcium phosphate cement (Fondu) blended with fly ash, class F (FAF) in carbon steel corrosion protection tests (corrosion rate, corrosion current and potential), bond- and matrix strength, as well as matrix strength recovery after imposed damage at 300C. The corrosion protection and lap-shear bond strength data are given for different Fondu/FAF ratios, the matrix strength data recoveries are reported for 60/40 weight % Fondu/FAF ratios. Effect of sodium phosphate on bond strength, corrosion protection and self-healing is demonstrated.

15 GEOTHERMAL ENERGY↗

MAGNESIUM MONO POTASSIUM PHOSPHATE GROUT FOR P-REACTOR VESSEL IN-SITU DECOMISSIONING

The objective of this report is to document laboratory testing of magnesium mono potassium phosphate grouts for P-Reactor vessel in-situ decommissioning. Magnesium mono potassium phosphate cement-based grout was identified as candidate material for filling (physically stabilizing) the 105-P Reactor vessel (RV) because it is less alkaline than portland cement-based grout (pH of about 12.4). A less alkaline material ({<=} 10.5) was desired to address a potential materials compatibility issue caused by corrosion of aluminum metal in highly alkaline environments such as that encountered in portland cement grouts. Information concerning access points into the P-Reactor vessel and amount of aluminum metal in the vessel is provided elsewhere. Fresh and cured properties were measured for: (1) commercially blended magnesium mono potassium phosphate packaged grouts, (2) commercially available binders blended with inert fillers at SRNL, (3) grouts prepared from technical grade MgO and KH{sub 2}PO{sub 4} and inert fillers (quartz sands, Class F fly ash), and (4) Ceramicrete{reg_sign} magnesium mono potassium phosphate-based grouts prepared at Argonne National Laboratory. Boric acid was evaluated as a set retarder in the magnesium mono potassium phosphate mixes.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

DISTRIBUTION COEFICIENTS (KD) GENERATED FROM A CORE SAMPLE COLLECTED FROM THE SALTSTONE DISPOSAL FACILITY

Core samples originating from Vault 4, Cell E of the Saltstone Disposal Facility (SDF) were collected in September of 2008 (Hansen and Crawford 2009, Smith 2008) and sent to SRNL to measure chemical and physical properties of the material including visual uniformity, mineralogy, microstructure, density, porosity, distribution coefficients (K{sub d}), and chemical composition. Some data from these experiments have been reported (Cozzi and Duncan 2010). In this study, leaching experiments were conducted with a single core sample under conditions that are representative of saltstone performance. In separate experiments, reducing and oxidizing environments were targeted to obtain solubility and Kd values from the measurable species identified in the solid and aqueous leachate. This study was designed to provide insight into how readily species immobilized in saltstone will leach from the saltstone under oxidizing conditions simulating the edge of a saltstone monolith and under reducing conditions, targeting conditions within the saltstone monolith. Core samples were taken from saltstone poured in December of 2007 giving a cure time of nine months in the cell and a total of thirty months before leaching experiments began in June 2010. The saltstone from Vault 4, Cell E is comprised of blast furnace slag, class F fly ash, portland cement, and Deliquification, Dissolution, and Adjustment (DDA) Batch 2 salt solution. The salt solution was previously analyzed from a sample of Tank 50 salt solution and characterized in the 4QCY07 Waste Acceptance Criteria (WAC) report (Zeigler and Bibler 2009). Subsequent to Tank 50 analysis, additional solution was added to the tank solution from the Effluent Treatment Project as well as from inleakage from Tank 50 pump bearings (Cozzi and Duncan 2010). Core samples were taken from three locations and at three depths at each location using a two-inch diameter concrete coring bit (1-1, 1-2, 1-3; 2-1, 2-2, 2-3; 3-1, 3-2, 3-3) (Hansen and Crawford 2009). Leaching experiments were conducted with a section of core sample 3-2. All cores from location 3 were drilled without using water. Core sample 3-2 was drilled from approximately six inches to a depth of approximately 13 inches. Approximately six inches of the core was removed but it broke into two pieces during removal from the bit. At the time of drilling, core material appeared olive green in color (Smith 2008). The fact that the samples were cored as olive green and were received after storage with a gray outer layer is indicative that some oxidation had occurred prior to leaching studies.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Full Scale Field Trial of the Low Temperature Mercury Capture Process

CONSOL Energy Inc., with partial funding from the Department of Energy (DOE) National Energy Technology Laboratory, designed a full-scale installation for a field trial of the Low-Temperature Mercury Control (LTMC) process, which has the ability to reduce mercury emissions from coal-fired power plants by over 90 percent, by cooling flue gas temperatures to approximately 230°F and absorbing the mercury on the native carbon in the fly ash, as was recently demonstrated by CONSOL R&D on a slip-stream pilot plant at the Allegheny Energy Mitchell Station with partial support by DOE. LTMC has the potential to remove over 90 percent of the flue gas mercury at a cost at least an order of magnitude lower (on a $/lb mercury removed basis) than activated carbon injection. The technology is suitable for retrofitting to existing and new plants, and, although it is best suited to bituminous coal-fired plants, it may have some applicability to the full range of coal types. Installation plans were altered and moved from the original project host site, PPL Martins Creek plant, to a second host site at Allegheny Energy's R. Paul Smith plant, before installation actually occurred at the Jamestown (New York) Board of Public Utilities (BPU) Samuel A. Carlson (Carlson) Municipal Generating Station Unit 12, where the LTMC system was operated on a limited basis. At Carlson, over 60% mercury removal was demonstrated by cooling the flue gas to 220-230°F at the ESP inlet via humidification. The host unit ESP operation was unaffected by the humidification and performed satisfactorily at low temperature conditions.

20 FOSSIL-FUELED POWER PLANTS↗

Degradation Of Cementitious Materials Associated With Saltstone Disposal Units

The Saltstone facilities at the DOE Savannah River Site (SRS) stabilize and dispose of low-level radioactive salt solution originating from liquid waste storage tanks at the site. The Saltstone Production Facility (SPF) receives treated salt solution and mixes the aqueous waste with dry cement, blast furnace slag, and fly ash to form a grout slurry which is mechanically pumped into concrete disposal cells that compose the Saltstone Disposal Facility (SDF). The solidified grout is termed “saltstone”. Cementitious materials play a prominent role in the design and long-term performance of the SDF. The saltstone grout exhibits low permeability and diffusivity, and thus represents a physical barrier to waste release. The waste form is also reducing, which creates a chemical barrier to waste release for certain key radionuclides, notably Tc-99. Similarly, the concrete shell of an SDF disposal unit (SDU) represents an additional physical and chemical barrier to radionuclide release to the environment. Together the waste form and the SDU compose a robust containment structure at the time of facility closure. However, the physical and chemical state of cementitious materials will evolve over time through a variety of phenomena, leading to degraded barrier performance over Performance Assessment (PA) timescales of thousands to tens of thousands of years. Previous studies of cementitious material degradation in the context of low-level waste disposal have identified sulfate attack, carbonation influenced steel corrosion, and decalcification (primary constituent leaching) as the primary chemical degradation phenomena of most relevance to SRS exposure conditions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Tanks 18 And 19-F Structural Flowable Grout Fill Material Evaluation And Recommendations

Cementitious grout will be used to close Tanks 18-F and 19-F. The functions of the grout are to: 1) physically stabilize the final landfill by filling the empty volume in the tanks with a non-compressible material; 2) provide a barrier for inadvertent intrusion into the tank; 3) reduce contaminant mobility by a) limiting the hydraulic conductivity of the closed tank and b) reducing contact between the residual waste and infiltrating water; and 4) providing an alkaline, chemically reducing environment in the closed tank to control speciation and solubility of selected radionuclides. The objective of this work was to identify a single (all-in-one) grout to stabilize and isolate the residual radionuclides in the tank, provide structural stability of the closed tank and serve as an inadvertent intruder barrier. This work was requested by V. A. Chander, High Level Waste (HLW) Tank Engineering, in HLW-TTR-2011-008. The complete task scope is provided in the Task Technical and QA Plan, SRNL-RP-2011-00587 Revision 0. The specific objectives of this task were to: 1) Identify new admixtures and dosages for formulating a zero bleed flowable tank fill material selected by HLW Tank Closure Project personnel based on earlier tank fill studies performed in 2007. The chemical admixtures used for adjusting the flow properties needed to be updated because the original admixture products are no longer available. Also, the sources of cement and fly ash have changed, and Portland cements currently available contain up to 5 wt. % limestone (calcium carbonate). 2) Prepare and evaluate the placement, compressive strength, and thermal properties of the selected formulation with new admixture dosages. 3) Identify opportunities for improving the mix selected by HLW Closure Project personnel and prepare and evaluate two potentially improved zero bleed flowable fill design concepts; one based on the reactor fill grout and the other based on a shrinkage compensating flowable fill mix design. 4) Prepare samples for hydraulic property measurements for comparison to the values in the F- and H- Tank Farm Performance Assessments (PAs). 5) Identify a grout mix for the Tanks 18-F and 19-F Grout Procurement Specification. Results for two flowable zero bleed structural fill concepts containing 3/8 inch gravel (70070 Series and LP#8 Series) and a sand only mix (SO Series) are provided in this report. Tank Farm Engineering and SRNL Project Management selected the 70070 mix as the base case for inclusion in Revision 0 of the Tanks 18-F and 19-F grout procurement specification and requested admixture recommendations and property confirmation for this formulation. Lower cementitious paste mixes were formulated because the 70070 mix is over designed with respect to strength and generates more heat from hydration reactions than is desirable for mass pour application. Work was also initiated on a modification of the recommended mix which included shrinkage compensation to mitigate fast pathways caused by shrinkage cracking and poor physical bonding to the tank and ancillary equipment. Testing of this option was postponed to FY12. Mix, LP#8-16 is recommended for inclusion in the specification for furnishing and delivering tank closure grout for Tanks 18-F and 19-F. A shrinkage compensating variation of this mix, LP#16C, has not been fully developed and characterized at this time.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of Sodium Carboxymethyl Celluloses on Water-catalyzed Self-degradation of 200°C-heated Alkali-Activated Cement

We investigated the usefulness of sodium carboxymethyl celluloses (CMC) in promoting self-degradation of 200°C-heated sodium silicate-activated slag/Class C fly ash cementitious material after contact with water. CMC emitted two major volatile compounds, CO 2 and acetic acid, creating a porous structure in cement. CMC also reacted with NaOH from sodium silicate to form three water-insensitive solid reaction products, disodium glycolate salt, sodium glucosidic salt, and sodium bicarbonate. Other water-sensitive solid reaction products, such as sodium polysilicate and sodium carbonate, were derived from hydrolysates of sodium silicate. Dissolution of these products upon contact with water generated heat that promoted cement’s self-degradation. Thus, CMC of high molecular weight rendered two important features to the water-catalyzed self-degradation of heated cement: One was the high heat energy generated in exothermic reactions in cement; the other was the introduction of extensive porosity into cement.

15 GEOTHERMAL ENERGY↗

Corrosion-resistant Foamed Cements for Carbon Steels

The cementitious material consisting of Secar #80, Class F fly ash, and sodium silicate designed as an alternative thermal-shock resistant cement for the Enhanced Geothermal System (EGS) wells was treated with cocamidopropyl dimethylamine oxide-based compound as foaming agent (FA) to prepare numerous air bubble-dispersed low density cement slurries of and ≤1.3 g/cm 3 . Then, the foamed slurry was modified with acrylic emulsion (AE) as corrosion inhibitor.

15 GEOTHERMAL ENERGY↗