At least 559 records · Page 31

Influence of gaseous hydrogen on metals

Tensile, fracture toughness, threshold stress intensity for sustained-load crack growth, and cyclic and sustained load crack growth rate measurements were performed on a number of alloys in high-pressure hydrogen and helium environments. The results of tensile tests performed in 34.5 MN/m2 (5000 psi) hydrogen indicated that Inconel 625 was considerable embrittled at ambient temperature but was not embrittled at 144 K (-200 F). The tensile properties of AISI 321 stainless steel were slightly reduced at ambient temperature and 144 K (-200 F). The tensile properties of Ti-5Al-2.5 Sn ELI were essentially unaffected by hydrogen at 144 K (-200 F). OFHC copper was not embrittled by hydrogen at ambient temperature or at 144 K (-200 F).

Walter, R. J.↗

Residual Stress Reversal in Highly Strained Shot Peened Structural Elements

The purpose of this research was to further the understanding of a crack initiation problem in a highly strained pressure containment housing. Finite Element Analysis methods were used to model the behavior of shot peened materials undergoing plastic deformation. Analytical results are in agreement with laboratory tensile tests that simulated the actual housing load conditions. These results further validate the original investigation finding that the shot peened residual stress had reversed, changing from compressive to tensile, and demonstrate that analytical finite element methods can be used to predict this behavior.

Mitchell, William S.↗

Mechanical Properties of Triaxial Braided Carbon/Epoxy Composites

In an on-going effort to increase the safety and efficiency of turbine engines, the National Aeronautics and Space Administration is exploring lightweight alternatives to the metal containment structures that currently encase commercial jet engines. Epoxy reinforced with braided carbon fibers is a candidate structural material which may be suitable for an engine case. This paper reports flat-coupon mechanical-property experiments performed to compliment previously reported subcomponent impact testing and analytical simulation of containment structures. Triaxial-braid T700/5208 epoxy and triaxial-braid T700h436 toughened epoxy composites were evaluated. Also, two triaxial-braid architectures (0 degrees plus or minus 60 degrees, and 0 degrees plus or minus 45 degrees) with the M36 resin were evaluated through tension, compression, and shear testing. Tensile behavior was compared between standard straight-sided specimens (ASTM D3039) and bow-tie specimens. Both double-notch shear (ASTM D3846) and Iosepescu (ASTM D5379) tests were performed as well. The M36/O degrees plus or minus 45 degrees configuration yield the best response when measurements were made parallel to the axial tows. Conversely, the M36/0 degrees plus or minus 60 degrees configuration was best when measurements were made perpendicular to the axial tows. The results were used to identify critical properties and to augment the analysis of impact experiments.

Bowman, C. L.↗

Cryogenic Chamber for Servo-Hydraulic Materials Testing

A compact cryogenic test chamber can be cooled to approximately 5 to 6 Kelvin for materials testing. The system includes a temperature controller and multiple sensors to measure specimen temperature at different locations. The testing chamber provides a fast and easy method to perform materials testing at lower than liquid nitrogen temperature (77 K). The purpose of the chamber is to cool a composite lap shear specimen to approximately 20 K so that tensile test force and displacement data may be acquired at this cryogenic temperature range.

Francis, John J.↗

Using Digital Image Correlation for Material Testing at Cryogenic Temperatures

Recent efforts were made to parametrize an aluminum alloy at cryogenic temperatures to calibrate finite element models simulating material deformation. Digital image correlation (DIC) was used to measure material properties using front/back strains of specimens during tensile tests. Data acquired from DIC was compared to physical extensometer measurements. Two camera pairs (front and back) were mounted via aluminum extrusion to the exterior of an environmental chamber of a hydraulic test stand. Images were taken through single-pane optical glass windows of the environment chamber. Positive pressure bags encased the cameras, attaching to the perimeter of the glass to keep out moisture and prevent windows from frosting. Figure 1 shows the environmental setup and the camera setup during cryogenic testing. Some of the challenges during testing at cryogenic temperatures include the gaseous flow of liquid nitrogen in the optical path of the mounted cameras, frost buildup on the windows as seen in Figure 1b, and frost on the test coupon. The temperature gradient present during the introduction of liquid nitrogen into the chamber can increase the projection error of images captured of the specimen. Figure 2 shows the estimated projection error from DIC as a function of temperature during the cool down process. This presentation addresses some of the concerns and observations when using DIC for testing at cryogenic temperatures using methods of isolated camera system and techniques for maintaining the glass panel clear from frost.

Joseph Cochran↗

X ray attenuation measurements for high-temperature materials characterization and in-situ monitoring of damage accumulation

The scope of this dissertation is to develop and apply x ray attenuation measurement systems that are capable of: (1) characterizing density variations in high-temperature materials, e.g., monolithic ceramics, ceramic and intermetallic matrix composites, and (2) noninvasively monitoring damage accumulation and failure sequences in ceramic matrix composites under room temperature tensile testing. This dissertation results in the development of: (1) a point scan digital radiography system, and (2) an in-situ x ray material testing system. Radiographic evaluation before, during, and after loading shows the effect of preexisting volume flaws on the fracture behavior of composites. Results show that x ray film radiography can monitor damage accumulation during tensile loading. Matrix cracking, fiber matrix debonding, fiber bridging, and fiber pullout are imaged throughout the tensile loading of the specimens. Further in-situ radiography is found to be a practical technique for estimating interfacial shear strength between the silicon carbide fibers and the reaction bonded silicon nitride matrix. It is concluded that pretest, in-situ, and post test x ray imaging can provide for greater understanding of ceramic matrix composite mechanical behavior.

Baaklini, George Y.↗

Anisotropy of nickel-base superalloy single crystals

The influence of orientation on the tensile and stress rupture behavior of 52 Mar-M247 single crystals was studied. Tensile tests were performed at temperatures between 23 and 1093 C; stress rupture behavior was examined between 760 and 1038 C. The mechanical behavior of the single crystals was rationalized on the basis of the Schmid factor contours for the operative slip systems and the lattice rotations which the crystals underwent during deformation. The tensile properties correlated well with the appropriate Schmid factor contours. The stress rupture lives at lower testing temperatures were greatly influenced by the lattice rotations required to produce cross slip. A unified analysis was attained for the stress rupture life data generated for the Mar-M247 single crystals at 760 and 774 C under a stress of 724 MPa and the data reported for Mar-M200 single crystals tested at 760 C under a stress of 689 MPa. Based on this analysis, the stereographic triangle was divided into several regions which were rank ordered according to stress rupture life for this temperature regime.

Mackay, R. A.↗

The Effect of Heating on the Degradation of Ground Laboratory and Space Irradiated Teflon(r) FEP

The outer most layer of the multilayer insulation (MLI) blankets on the Hubble Space Telescope (HST) is back surface aluminized Teflon(R) FEP (fluorinated ethylene propylene). As seen by data collected after each of the three servicing missions and as observed during the second servicing mission (SM2), the FEP has become embrittled in the space environment, leading to degradation of the mechanical properties and severe on-orbit cracking of the FEP. During SM2, a sample of aluminized-FEP was retrieved from HST that had cracked and curled, exposing its aluminum backside to space. Because of the difference in optical properties between FEP and aluminum, this insulation piece reached 200 C on-orbit, which is significantly higher than the nominal MLI temperature extreme of 50 C. This piece was more brittle than other retrieved material from the first and third servicing missions (SM1 and SM3A, respectively). Due to this observation and the fact that Teflon thermal shields on the solar array bi-stems were heated on-orbit to 130 C, experiments have been conducted to determine the effect of heating on the degradation of FEP that has been irradiated in a ground laboratory facility or in space on HST. Teflon FEP samples were X-ray irradiated in a high vacuum facility in order to simulate the damage caused by radiation in the space environment. Samples of pristine FEP, X-ray irradiated FEP and FEP retrieved from the HST during SM3A were heat treated from 50 to 200 C at 25 intervals in a high vacuum facility and then tensile tested. In addition, samples were tested in a density gradient column to determine the effect of the radiation and heating on the density of FEP. Results indicate that although heating does not degrade the tensile properties of non-irradiated Teflon, there is a significant dependence of the percent elongation at failure of irradiated Teflon as a function of heating temperature. Irradiated Teflon was found to undergo increasing degradation in the elongation at failure as temperature was increased from room temperature to 200 C. Rate of degradation changes, which were consistent with the glass I transition temperatures for FEP, appeared to be present in both tensile and density data. The results indicate the significance of the on-orbit temperature of Teflon FEP with respect to its degradation in the low Earth orbital space environment.

deGroh, Kim K.↗

Comparison of High-Performance Fiber Materials Properties in Simulated and Actual Space Environments

A variety of high-performance fibers, including Kevlar, Nomex, Vectran, and Spectra, have been tested for durability in the space environment, mostly the low Earth orbital environment. These materials have been tested in yarn, tether/cable, and fabric forms. Some material samples were tested in a simulated space environment, such as the Atomic Oxygen Beam Facility and solar simulators in the laboratory. Other samples were flown on the International Space Station as part of the Materials on International Space Station Experiment. Mass loss due to atomic oxygen erosion and optical property changes due to ultraviolet radiation degradation are given. Tensile test results are also presented, including where moisture loss in a vacuum had an impact on tensile strength.

Finckenor, M. M.↗

Effects of particle inclusions on cracking in ultrathin barrier films

Here, the effects of particle inclusions with different mechanical properties on the development of cracks in ultra-thin barrier films have been studied. Two types of particles, alumina and poly(styrene-b-methyl methacrylate) with large differences in their elastic modulus were used, representing both hard and soft inclusions. Particles were seeded onto polyethylene naphthalate substrates and subsequently coated with atomic layer deposited Al 2 O 3 as a barrier film. Ca corrosion tests used to determine the performance of the barrier films revealed that soft polymer particle inclusions severely affect the development of cracking in barrier films as compared to stiff ceramic particles. Tensile tests also confirmed that the barrier films with polymer particle inclusions have the lowest value of critical onset strain. Parametric simulations, conducted by varying the elastic modulus of the particle inclusions over a wide range, resulted in a larger strain energy release rate near particle inclusions which promotes crack formation and negatively impacts the performance of barrier films with softer particle inclusions. Thus, the combination of high residual stresses in the barrier films with the presence of soft particle inclusions is found the most detrimental for the development of high-performance ultrathin barrier films.

36 MATERIALS SCIENCE↗

Characterization of Alloy 709 Commercial Heats

The creep-resistant austenitic stainless steel Alloy 709 (Fe-20Cr-25Ni (wt%) based steel) is being investigated as a candidate structural material for the next generation of advanced reactors. Unlike conventional solid solution strengthened austenitic stainless steels, Alloy 709 develops a variety of precipitates during aging at different temperatures and times. In this study, precipitate evolution during short-term aging at 775°C was characterized. The effect of aging time (e.g., 10 vs. 100 hours) and cooling after aging (e.g., water quench vs. air cool) on grain size and precipitates have been investigated using light optical microscopy (OM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM), and energy-dispersive X-ray spectroscopy (EDS). MX (Ni,Tb)(C,N) and M23C6 (Cr,Mo)C precipitates were observed in all the statically-aged samples. The grain size distribution in the sample aged for 10 hours and water quenched (10Q) versus the one aged for 100 hours and air cooled (100A) were comparable. This indicates that grain structure was fairly stable when aging at 775°C for up to 100 hours. In contrast, the sample aged for 10 hours and air cooled (10A) showed the smallest and the most uniform grain size distribution. This phenomenon was observed in only one sample. More studies on duplicate samples are needed to confirm the results obtained. The cooling medium (e.g., water quench vs. air cool) was not observed to impact the size nor the distribution of the MX and M23C6 precipitates. Increasing the aging time resulted in the following: (1) a decrease in dislocations as well as the number density of small precipitates; (2) an increase in the ratio of free precipitates that were not pinning dislocations; (3) relatively higher N, Nb, and Ti concentration in MX precipitate; (4) some increase in length of M23C6 carbides which were located on the coherent boundaries; and (5) the introduction of Sienriched M6X precipitates. The tensile tests at room temperature showed similar properties for each of the static aging treatments, indicating that the differences observed in the microstructural analysis did not have a significant impact on the tensile properties.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Tensile Properties of Molybdenum and Tungsten from 2500 to 3700 F

Specimens of commercially pure sintered tungsten, arc-cast unalloyed molybdenum, and two arc-cast molybdenum-base alloys (one with 0.5 percent titanium, the other with 0.46 percent titanium and 0.07 percent zirconium) were fabricated from 1/2-inch-diameter rolled or swaged bars. All specimens were evaluated in short-time tensile tests in the as-received condition, and all except the molybdenum-titanium-zirconium alloy were tested after a 30-minute recrystallization anneal at 3800 F in a vacuum of approximately 0.1 micron. Results showed that the tungsten was considerably stronger than either the arc-cast unalloyed molybdenum or the molybdenum-base alloys over the 2500 to 3700 F temperature range. Recrystallization of swaged tungsten at 3800 F considerably reduced its tensile strength at 2500 F. However, above 3100 F, the as-swaged tungsten specimens recrystallized during testing, and had about the same strength as when recrystallized at 3800 F before evaluation. The ductility of molybdenum-base materials was very high at all test temperatures; the ductility of tungsten decreased sharply above about 3120 F.

Hall, Robert W.↗

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating↗

Precipitation hardening of laser powder bed fusion Ti-6Al-4V

Here, the laser powder bed fusion (PBF-L) additive manufacturing (AM) community has dedicated significant efforts into process optimization and control for defect-free Ti-6Al-4V. As defects become less of an issue for PBF-L Ti-6Al-4V, the processing-structure-properties (PSP) relationships between AM microstructures can now be explored to optimize mechanical properties. Lower temperature aging treatments around 550 °C in wrought Ti-6A-4V have been historically understood to precipitation harden the α phase with an ordered, hexagonal close packed (HCP) α 2 phase. The α 2 phase existed as nanoscale Ti 3 Al precipitates coherent with the parent α phase. The goal of the present investigation was to implement a vacuum heat treatment of 545 °C for 100 hours on PBF-L Ti-6Al-4V. This vacuum heat treatment took place after an initial hot isostatic pressure (HIP) treatment that decomposed the as-built, martensitic microstructure. The vacuum aging successfully produced nanoscale precipitates of α 2 phase within α-laths, confirmed via atom probe tomography (APT). Microstructural-length scale and quasi-static mechanical properties were investigated by nanoindentation and uniaxial tensile tests of miniaturized test specimens. Given the sensitivity of Ti-6Al-4V mechanical properties to small changes in chemistry, all test specimens originated from the same build. The α 2 precipitation resulted in significantly harder α-laths (≈ 2 GPa) as measured via nanoindentation, as well as a relative yield and ultimate tensile strength increase of 60 MPa and 38 MPa, respectively. Analysis of Variance (ANOVA) of the datasets revealed no statistical differences in total elongation between the HIPed and HIPed + aged specimens, indicative of the aging treatment producing a net benefit of strength with no loss in ductility.

36 MATERIALS SCIENCE↗

Influence of plasticizers on thermal and mechanical properties of biocomposite filaments made from lignin and polylactic acid for 3D printing

Polylactic acid (PLA) and organosolv lignin were mixed at different ratios and extruded to obtain PLA-lignin composite filaments. PLA was replaced with lignin up to 20 wt%. Two plasticizers (polyethylene glycol (PEG) 2000 and struktol TR451) were added in varying concentrations to enhance the properties of PLA_L20 (20% lignin in PLA) composite filaments. Furthermore, the effect of lignin in PLA, and PEG, and struktol in PLA_L20 composites was investigated via tensile test, differential scanning calorimetry, thermogravimetric analysis, scanning electron microscopy, Fourier transform infrared spectroscopy of the filaments, and dynamic mechanical analysis of 3D printed samples. A 2 wt% PEG was able to enhance both tensile stress and elongation at maximum load of PLA_L20 composite by 19% and 35%, respectively, whereas struktol TR451 was able to improve elongation at maximum load by 24%.

3D printing↗

Material property for designing, analyzing, and fabricating space structures

An analytical study was made of plasma assisted bullet projectile. The finite element analysis and the micro-macromechanic analysis was applied to an optimum design technique for the multilayered graphite-epoxy composite projectile that will achieve hypervelocity of 6 to 10 Km/s. The feasibility was determined of dialectics to monitor cure of graphite-epoxies. Several panels were fabricated, cured, and tested with encouraging results of monitoring the cure of graphite-epoxies. The optimum cure process for large structures was determined. Different orientation were used and three different curing cycles were employed. A uniaxial tensile test was performed on all specimens. The optimum orientation with the optimum cure cycle were concluded.

Kolkailah, Faysal A.↗

Determination of cleavage planes and fracture characterization of Ni-based single crystal superalloys

The room temperature fracture behavior of the Ge Rene N-4, CMSX-2, and CMSX-4C single crystal Ni-based superalloys was studied. All crystals were grown along the (001) direction and tensile tested in both helium and hydrogen atmospheres. A stereoscopic technique developed for use with a scanning electron microscope was applied to determine cleavage planes. Planar gamma(') morphologies also were examined to help determine cleavage planes. Helium charged specimens failed on a number of planes including the (111), (110), and (320). In most cases planes of the (111)-type initiated at the notch region and became smaller and smaller as they moved in radially. Tensile strengths in helium averaged 1000 MPa higher than that of the hydrogen charged specimens. Specimens tested in hydrogen generally failed on (100)-type planes originating from the notch region. This (100) region comprised 60 to 80 percent of the total fracture surface on most samples and appeared as large flat planes perpendicular to the growth direction of the crystal. The interior regions contained (100)-type planes as well as (321), (320), (210), and (111)-types. Hydrogen charged specimens also showed a high percentage of large cracks oriented at 90 deg to one another, indicative of the (100)-type fracture. The Ge Rene N4 and the CMSX-4C samples contained 3-5 percent gamma/gamma(') eutectic, while the CMSX-2 samples had little or no gamma/gamma(') eutectic. The relationship between gamma/gamma(') eutectic and the fracture surface has not been fully determined, but it is thought that the gamma/gamma(') eutectic may serve as a possible trapping site for hydrogen.

Merrill, John M.↗

The Effects of Fiber Orientation and Adhesives on Tensile Properties of Carbon Fiber Reinforced Polymer Matrix Composite with Embedded Nickel-Titanium Shape Memory Alloys

Tensile tests of Nickel-titanium (NiTi) shape memory alloys (SMA) embedded within carbon fiber reinforced polymer matrix composite (CFRP/PMC) laminates were evaluated with simultaneous monitoring of modal acoustic emissions (MAE). Three different layup configurations utilizing two different thin film adhesives were applied to bond the materials. Ultimate tensile strengths, strains, and moduli were obtained along with cumulative AE energy of events and specimen failure location. Scanning electron microscopy was used to examine the break areas of the specimens post-test. Microscopy was used to validate failure locations revealed from MAE analysis. A unique finding within this research showed that 90° plies in the outer ply gave the strongest acoustic signals as well as the cleanest fracture of the specimens tested. Overlapping 0° ply layers surrounding the SMA was found to be the best scenario to prevent failure of the specimen itself.

Derek Quade↗