Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FORGING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 559 records · Page 31

Wellbore Fracture Imaging Using Inflow Detection Measurements

One of the most striking measurements taken during DOE’s EGS Collab project at the 4850-foot depth location was the so-called ‘sewer cam’, which enabled direct visualization of the flow of water into the production well through fractures during the stimulation. The ability to see directly which fractures were flowing and (roughly) how much was a breakthrough in understanding the topology of the created fracture network. Achieving this kind of fracture flow imaging at FORGE would be more challenging because of the 225°C temperature, but equally or even more valuable if it could be achieved. In 2017, a joint project between Sandia and Stanford developed a downhole tool concept to measure the enthalpy of multiphase fluid entering a geothermal well from individual fractures (Gao et al., 2017). For the FORGE project, measuring enthalpy is of less interest because the fluid is expected to be single-phase liquid water. However, the foundation of the device was the measurement of chloride ion concentration, which could form the basis for a direct measurement of inflow from fractures. During the 2017 project, this novel chloride sensing system was implemented into a laboratory test instrument, and we confirmed the capability of the system to measure the ion concentration of fluid entering a model wellbore through a small entry port. The wellbore was a 6-inch diameter model well, and the port was approximately 0.08 inch (2mm) in diameter. The device could measure the chloride concentration accurately even when the well was flowing in a bubbly flow. Given its accuracy, the tool should be able to identify locations of water entering the wellbore even if the ion concentration differs only slightly from that of the water in the well. It is likely that different fractures may flow slightly different chloride concentrations, which would make it feasible to detect individual fractures as well as to estimate the volume of their flow. Ultimately, we could also recognize different fractures flowing back significantly different ion concentrations after fracturing in the FORGE wells. This could be realized by adding different ions in the fracturing fluids in different fractures created at different stages of stimulation (and modifying the tool to include different ion specificity). Sandia’s tool was shown during the study to have the capability to withstand the 225°C temperature, and the electrochemical sensing elements were tested in the laboratory to 225°C at 1500 psia for 24 hours. An early implementation of the fully integrated downhole electrochemical tool, including high-temperature electronics, robust housing, and wireline truck interface, had previously been constructed and tested successfully at Sandia; thus, hardware development tasks focused on advancing the technology readiness level (TRL) of this promising technology for FORGE deployment, rather than on developing a new scientific basis for its operation. The data collection electronics in this tool allowed for several other sensors (pressure, temperature, flow spinner) to be implemented in parallel as well. The research was a new collaboration between Stanford and Sandia to modify and refine the tool for FORGE deployment, to make the downhole measurements, and to characterize the evolving fractures.

15 GEOTHERMAL ENERGY↗

Powder metallurgy processing of high strength turbine disk alloys

Using vacuum-atomized AF2-1DA and Mar-M432 powders, full-scale gas turbine engine disks were fabricated by hot isostatically pressing (HIP) billets which were then isothermally forged using the Pratt & Whitney Aircraft GATORIZING forging process. While a sound forging was produced in the AF2-1DA, a container leak had occurred in the Mar-M432 billet during HIP. This resulted in billet cracking during forging. In-process control procedures were developed to identify such leaks. The AF2-1DA forging was heat treated and metallographic and mechanical property evaluation was performed. Mechanical properties exceeded those of Astroloy, one of the highest temperature capability turbine disk alloys presently used.

Evans, D. J.↗

The Lunar Lab Initiative

Analogous to terrestrial Antarctic basecamps at our south pole, space exploration outposts will be a combination of habitation and science-focused assets. The Artemis Exploration Roadmap endeavors to establish a sustained human presence on the lunar south pole starting in 2028. Within the planned Artemis Base Camp, most efforts to date have focused on the habitation assets or a mixture of science and habitation assets . With the recent advent of commercial lunar landing capabilities, the trade space can be further expanded to include dedicated science focused assets that ensure adequate science capability. To that end, the Forge, an innovation team initiative created at the Johnson Space Center (JSC), explored alternative ways to increase the science capabilities within the basecamp. The Forge uses structured brainstorming and facilitation to increase innovation within the assigned team, while executing its process in a rapid turnaround fashion for ideation and design study. As a pilot study for the Forge, a multi-disciplinary team investigated a lunar lab module to augment the lunar surface plans for Artemis. This formulation study evaluated the scientific and operational considerations for this dedicated crew space that would increase the capabilities of lunar surface science operations. The trade space evaluated single lunar lander delivery versus multiple lunar lander delivery for module assembly, alternative structural designs, the science instrument outfitting with mapping to scientific goals to maximize lunar science objectives, and how the lab would be operated. The lab operations options explored a stand-alone facility, as well as a facility integrated into a larger lunar surface complex, while evaluating crew usage and habitability considerations. The resulting alternatives were evaluated by the Forge team with a set of metrics to determine their originality, feasibility, and science performance, and thereby provide a recommendation to the lunar architecture planning team. Lessons learned from the lunar lab study were compiled to improve the process and tools for future Forge studies. Forward work, open issues, and challenges to further refine the design of the various science-focused asset options were also documented. By providing a robust science capability at humanity’s furthest outpost, we can plan for a sustained human lunar presence once the initial lunar surface access capability is well established.

Lunar outpost↗

Rapid Assessment of a Lunar Surface Laboratory Module

Johnson Space Center is piloting an innovation team known as the Forge to perform rapid turnaround, concurrent engineering studies. The Forge is intended to be able to pull together a team of strategically selected domain experts to innovatively solve a specified problem within a short period of time. The Forge’s inaugural project being the development of a Lunar Surface Laboratory Module concept. The lab module is intended as an option for the Artemis program’s Lunar Architecture Team. The lab module may allow for increased science productivity and return on investment than a surface architecture with only the habitat. This paper will discuss the configuration of the Lunar Laboratory module, including the pressure vessel, its placement relative to the Surface Habitat and Pressurized Rover, and internal architecture. In order to determine the suitability of such a design, a human factors evaluation is conducted. Historically, a human factors evaluation of a habitable volume could require a month or longer, including time needed to prepare a test plan, conduct the evaluation, compile the data, and produce a report. The entire Forge effort will only last for five weeks, forcing the creation of a rapid assessment process. This rapid assessment includes three evaluation studies, all conducted and processed in the space of a single day, to determine the acceptability of the resulting design. The first evaluation is a card sort evaluation of the laboratory instruments. A brief discussion of the card sort evaluation is provided. This card sort is focused on the relative positioning of the laboratory instruments, determining whether a given instrument should be adjacent to, or separated from, another. It will use human factors personnel and both life and physical scientists as subject matter experts. The second evaluation is a science productivity tabletop evaluation. This evaluation focuses on the selection of instruments and the number of instruments, attempting to assess the amount of work the crew will be able to use the facility to do. It uses life and physical science personnel as subject matter experts. The third evaluation is a CAD or Virtual Reality human factors walkthrough evaluation. This evaluation focuses on the layout of the lab module and its connectivity to the basecamp’s pressurized elements. If possible, astronauts will be used as subject matter experts. Each of these evaluations will focus primarily on objective data with limited subjective comments, reducing the time required for processing responses. The results of each evaluation and their implications will be discussed. Based on the evaluation data, an overall acceptability of the Lunar Surface Laboratory Module produced by the Forge study can be determined. Lessons learned and recommendations for future use of the human factors rapid assessment process in early design trades will also be provided.

Lunar Laboratory↗

Materials for Advanced Ultra-Supercritical (A-USC) Steam Turbines --- A-USC Component Demonstration

The U.S. Advanced Ultra-Supercritical (A-USC) Consortium was formed in 2001 as a government/industry program, sponsored by the U.S. Department of Energy (DOE) and the Ohio Coal Development Office (OCDO) and cost shared by industrial and not-for-profit partners. The purpose of the consortium was to advance the state of the art for power generation by evaluating and developing materials that allow the use of advanced steam cycles in coal-based power plants. These advanced cycles, with steam temperatures up to 1400°F (760°C), can increase the efficiency of coal-fired boilers from an average of 35% (current U.S. fleet) to more than 45% higher heating value (HHV) (>49% lower heating value [LHV]). The increase in a plant’s efficiency is limited unless new materials able to withstand these higher operating temperatures and pressures are identified and approved for use. The A-USC Consortium identified these needed materials during earlier phases of the program. It developed the welding and joining techniques along with manufacturing processes for casting and wrought products made from these new high-nickel alloys. It subjected these materials to extensive laboratory and steam loop testing. It then obtained ASME code approval for their use in U.S. boiler systems. The program’s successes leave this last remaining activity (ComTest Phase 2) that the U.S. utility industry has recommended to be accomplished prior to commercialization. The focus of the activity is the evaluation and demonstration of commercial readiness for “full scale” components to be made from these nickel-based alloy materials and provided by a U.S. domestic supply chain that is new to working with these alloys. According to studies completed by the Electric Power Research Institute (EPRI), the cost of an A-USC plant is approximately 20% higher than a non-A-USC plant because of its use of nickel-based alloys needed for the high temperature operating conditions. However, CO 2 reductions of approximately 30% from the current fleet average provide a strong incentive for its consideration. The actual costs and perceived value for CO 2 abatement will determine whether new or retrofitted plants are undertaken, although decisions to build A-USC plants in India would indicate its economic feasibility while also being part of a global carbon emissions strategy. The work by the A-USC Consortium, prior to the start of the ComTest project, has included lab scale and pilot scale materials testing, both in air and oxy-combustion. This testing has included air-cooled and steam-cooled “loops” that were installed into existing operating utility boilers to gain exposure of these materials to realistic conditions of high temperature and corrosion caused by the constituents in the coal ash. The A-USC Consortium also gained ASME Code approval of the Inconel 740 material, has cast and extruded the largest high nickel precipitation hardened alloys, and developed unique welding techniques to avoid problems identified by the competing European program. However, as valuable as these material test loops and accomplishments have been for obtaining information, their scale is below that required to minimize the risk associated for a U.S. utility to build a multibillion-dollar A-USC power plant. To reduce the final identified risk barrier to full-scale commercialization of these advanced materials and systems, the A-USC Consortium (guided by a utility industry advisory committee) has identified the key areas of the technology they desire to see as being capable of full-scale manufacturing and/or fabrication from an identified, capable U.S. domestic supplier base. A significant amount of work was accomplished during Phase 1 to identity the components, as well as the component size, that would be manufactured from advanced alloys such as Inconel 740H or Haynes 282 alloys. Pathways to supply these components for ComTest have been identified, as well as any further development that would be required. The Phase 2 effort used Phase 1 findings for designing these key full-scale components for A-USC boilers and turbines to include large castings; extrusions, forgings, fabrication of water walls and steam loops with headers from advanced materials, raw material (such as pipe extrusion billets) are at the commercial readiness level to permit advancement to a demonstration project. The Phase 2 work scope was addressed by a diverse team, including government, industry, and not-for-profit partners. The work scope under Phase 2 addressed fabrication of components identified as being outside of the proven capabilities of the existing supply chain, including the following: Steam turbine rotor forging and Haynes 282 nozzle carrier casting Superheater and reheater header and tube assemblies Large-diameter pipe extrusions and forgings Test valve articles to support ASME Code approval. In addition, key fabrication steps were completed, including boiler weld overlays and simulated field repairs. Throughout, extensive inspection and quality assurance testing of the components were performed. The team worked to advance ASME Code approval for key components and processes. Although much of the focus of ComTest Phase 2 was the high-temperature nickel-based alloy materials, a broader range of materials were incorporated, which would be representative of the materials used in full-scale A-USC power plant applications and have cross-cutting applicability on other high-temperature power generation options, such as advanced nuclear, supercritical CO 2 cycles, and central solar receivers. This report that has been submitted is organized in the following manner: Section 1 contains an Executive Summary. Section 2 discusses the ComTest project background and organization. Section 3 discusses project management and reporting. Section 4 discusses the procurement of nickel-based alloy and other A-USC materials and components. Section 5 discusses the fabrication of procurement of nickel-based alloy and other A-USC materials and components. Section 6 discusses the fabrication of cast nickel-based A-USC steam turbine components. Section 7 discusses the fabrication of forged nickel-based A-USC steam turbine piping and steam pipe components. Section 8 discusses the qualification of pressure relieve valves (PRVs) for A-USC power plants. Section 9 discusses proposed plans for future evaluation of A-USC components. Section 10 contains the summary and conclusion.

01 COAL, LIGNITE, AND PEAT↗

An innovative and alternative approach toward gear fabrication

In this paper, we present the first demonstration of single-step gear manufacturing via an innovative in-situ friction stir forging approach. This novel process is a natural extension to the friction stir processing technique and relies on shear and normal stresses to form the complex shapes. Friction stir welding pin tool with shoulder is plunged at high revolutions per minute (rpm) into the sample to heat it to the desired temperature and enable plastic flow. Then, the tool is forged at high plunge rate to form the desired structurally-sound and defect free complex shapes. To better visualize the process the experiments are complemented by a 3D thermomechanically coupled, smoothed particle hydrodynamics (SPH) model to understand the material flow pattern both radially and through thickness in the gear teeth, plastic strain distribution, and temperature profile. We have demonstrated application of I-FSF to inherently poor formable AZ31 Mg, AA 7075-T6, and AA5083–10 vol% TiB 2 composite and fabricated 14-tooth spur gears from these materials with minimal farther machining. In conclusion, microstructure of the forged gears exhibited a directional material flow pattern due to the normal forging action and refinement of grains to 6–13 μm through dynamically recrystallization across the radial, through-thickness direction, which is in good agreement with the corresponding SPH simulation results.

42 ENGINEERING↗

Enhanced thermoelectric properties of bismuth sulfide polycrystals prepared by mechanical alloying and spark plasma sintering

Bismuth sulfide powders were synthesized by mechanical alloying (MA) and then consolidated by spark plasma sintering (SPS) technique. In order to improve the electrical transport properties of bismuth sulfides, the carrier concentration was optimized by modifying chemical composition of sulfur through producing sulfur vacancies, and the carrier mobility was enhanced by a two-step SPS as a hot-forging process through increasing grain orientation. The electrical resistivity of bismuth sulfides was reduced to 10{sup -4} from 10{sup -2} {omega} m by optimizing sulfur content, and further lowered by hot-forging, whereby the power factor was significantly increased from 91 to 254 {mu}W/mK{sup 2}. The hot-forged Bi{sub 2}S{sub 2.90} sample showed the highest ZT=0.11 (at 523 K), which is higher than the reported value. The present work revealed that bismuth sulfide compounds as a promising candidate of thermoelectric materials can be synthesized by a simple process. - Abstract: Electrical properties of bismuth sulfides were improved by optimizing carrier concentration through modifying compositions of sulfur and enhancing carrier mobility through SPSed hot-forging. The ZT value of 0.11 was obtained, which is the maximum reported so far . Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Archaeometallurgical investigation of the iron anchor from the Tantura F shipwreck

The Tantura F shipwreck was a coaster or a fishing vessel about 15.7 m long, discovered in the Dor/Tantura lagoon, Israel in 1995. It was dated to between the mid-7th and the end of the 8th centuries CE. Among the finds excavated were two T-shaped type iron anchors. Of the two anchors, one (anchor A) was thoroughly studied by archaeometallurgical methods in order to identify forge-welding lines, to determine the welding quality and to understand the manufacturing technology. The examinations included X-ray radiography, XRF analysis, optical microscopy, SEM/EDS observation and analysis, OES analysis and microhardness tests. The investigation included characterization of the composition, microstructure, thermal treatments, forge-welding junctions and slag analysis. The results revealed a heterogeneous microstructure, rich in glassy, fayalite and wüstite slag. Iron based phases included ferrite, pearlite, cementite and Widmanstätten plates, all typical to wrought iron. The forge-welds of Anchor A were located. Each arm was made of one piece, weighing about 2.5–3 kg and the shank was made of a few 1.5–2 kg pieces. The second anchor (anchor B) was only briefly examined visually and with a few radiographs, which support the results from anchor A. The research results revealed significant information about T-shaped anchors and their manufacturing process, including hot-working processes without any additional heat treatments, and folding techniques. The microstructure was similar to other ancient simple tools such as saws, sickles, axes and mortise chisels, and though the technology to make complicated structures and objects, such as swords, existed at that time, the anchors did not require this sophistication; thus simpler techniques were used, presumably because they were more cost-effective. - Highlights: ► Tantura F was a coaster dated to mid-7th–end-8th centuries. ► Two iron anchors were discovered at the Tantura F shipwreck-site. ► Anchor A was manufactured from heterogeneous wrought iron blooms. ► Forge-welding lines were detected using archaeometallurgical methods.

36 MATERIALS SCIENCE↗

Effects of annealing parameters on microstructural evolution of a typical nickel-based superalloy during annealing treatment

Highlights: • Adopting an annealing treatment after deformation can improve the homogeneity of microstructure. • Heterogeneous grains become homogeneous firstly, and then heterogeneous with increasing annealing time. • The optimum annealing parameters are the temperature of 980 °C and the time of 10 min. - Abstract: It is usually one of important goals to obtain the homogeneous microstructure for forgings by hot working, such as hot die forging. However, there is always a large inhomogeneous deformation in die forgings during hot deformation. It often results in an inhomogeneous microstructure of forging due to the different dynamic recrystallization (DRX) fractions and grain sizes in different strain regions. In this study, a method was proposed to improve the homogeneity of deformed microstructure by annealing treatment. The microstructural evolution of a typical nickel-based superalloy during annealing treatment has been investigated. The Optical Microscope (OM), Electron Backscatter Diffraction (EBSD) and Scanning Electron Microscope (SEM) technologies were applied to observe microstructures. It is found that adopting an annealing treatment after deformation can effectively improve the homogeneity of microstructure due to the static recrystallization. There is an incubation period which is not less than 5 min for the occurrence of static recrystallization. The initial heterogeneous grains become homogeneous firstly, and then heterogeneous again when the annealing time is increased from 5 to 30 min. The deformation accelerates the dissolution of delta phase in annealing treatment. The fraction of delta phase decreases at the early stage of annealing whether the temperature exceeds the solution temperature. Based on a comprehensive consideration of all factors, the optimum annealing parameters, which are the temperature of 980 °C and the time of 10 min, have been obtained.

36 MATERIALS SCIENCE↗

Anomalous Annealing Response of Directed Energy Deposited Type 304L Austenitic Stainless Steel

Directed energy deposited (DED) and forged austenitic stainless steels possess dissimilar microstructures but can exhibit similar mechanical properties. In this study, annealing was used to evolve the microstructure of both conventional wrought and DED type 304L austenitic stainless steels, and significant differences were observed. In particular, the density of geometrically necessary dislocations and hardness were used to probe the evolution of the microstructure and properties. Forged type 304L exhibited the expected decrease in measured dislocation density and hardness as a function of annealing temperature. Here, the more complex microstructure–property relationship observed in the DED type 304L material is attributed to compositional heterogeneities in the solidification microstructure.

36 MATERIALS SCIENCE↗

Mapping Lipid Fragmentation for Tailored Mass Spectral Libraries

Libraries of simulated lipid fragmentation spectra enable the identification of hundreds of unique lipids from complex lipid extracts, even when the corresponding lipid reference standards do not exist. Often, these in silico libraries are generated through expert annotation of spectra to extract and model fragmentation rules common to a given lipid class. Although useful for a given sample source or instrumental platform, the time-consuming nature of this approach renders it impractical for the growing array of dissociation techniques and instrument platforms. Here, we introduce Library Forge, a unique algorithm capable of deriving lipid fragment mass-to-charge (m/z) and intensity patterns directly from high-resolution experimental spectra with minimal user input. Library Forge exploits the modular construction of lipids to generate m/z transformed spectra in silico which reveal the underlying fragmentation pathways common to a given lipid class. By learning these fragmentation patterns directly from observed spectra, the algorithm increases lipid spectral matching confidence while reducing spectral library development time from days to minutes. We embed the algorithm within the preexisting lipid analysis architecture of LipiDex to integrate automated and robust library generation within a comprehensive LC-MS/MS lipidomics workflow. .

74 ATOMIC AND MOLECULAR PHYSICS↗

Atom probe tomography characterization of neutron irradiated surveillance samples from the R. E. Ginna reactor pressure vessel

Surveillance samples of a low copper (nominally 0.05 wt.% Cu) forging and a higher copper (0.23 wt.% Cu) submerged arc weld from the R. E. Ginna reactor pressure vessel have been characterized by atom probe tomography (APT) after exposure to three levels of neutron irradiation, i.e., fluences of 1.7, 3.6 and 5.8 × 10 23 n.m –2 (E > 1 MeV), and inlet temperatures of ~289 °C (~552 °F). As no copper-enriched precipitates were observed in the low copper forging, and the measured copper content in the ferrite matrix was 0.04± <0.01 at.% Cu, after neutron irradiation to a fluence of 1.7 × 10 23 n.m –3 , this copper level was below the solubility limit. A number density of 2 × 10 22 m –3 of Ni–, Mn– Si-enriched precipitates with an equivalent radius of gyration of 1.7 ± 0.4 nm were detected in the sample. However, Cu-, Ni-, Mn-enriched precipitates were observed in specimens cut from different surveillance specimens from the same forging material in which the overall measured copper level was 0.08± <0.01 at.% (fluence of 3.6 × 10 23 n.m –3 ) and 0.09± <0.01 at.% Cu (fluence of 5.8 × 10 23 n.m –3 ). Therefore, these slightly higher copper contents were above the solubility limit of Cu under these irradiation conditions. A best fit of all the composition data indicated that the size and number density of the Cu-enriched precipitates increased slightly in both size and number density by additional exposure to neutron irradiation. High number densities of Cu-enriched precipitates were observed in the higher Cu submerged arc weld for all irradiated conditions. The size and number density of the precipitates in the welds were higher than in the same fluence forgings. Some Cu-enriched precipitates were found to have Ni-, Mn- Si-, and P-enriched regions on their surfaces suggesting a preferential nucleation site. Furthermore, atom maps revealed P, Ni, and Mn segregation to, and preferential precipitation of, Cu-enriched precipitates over the surface of a grain boundary in the low fluence weld.

36 MATERIALS SCIENCE↗

Self-Reacting Friction Stir Welding for Aluminum Alloy Circumferential Weld Applications

Friction stir welding is an innovative weld process that continues to grow in use, in the commercial, defense, and space sectors. It produces high quality and high strength welds in aluminum alloys. The process consists of a rotating weld pin tool that plasticizes material through friction. The plasticized material is welded by applying a high weld forge force through the weld pin tool against the material during pin tool rotation. The high weld forge force is reacted against an anvil and a stout tool structure. A variation of friction stir welding currently being evaluated is self-reacting friction stir welding. Self-reacting friction stir welding incorporates two opposing shoulders on the crown and root sides of the weld joint. In self-reacting friction stir welding, the weld forge force is reacted against the crown shoulder portion of the weld pin tool by the root shoulder. This eliminates the need for a stout tooling structure to react the high weld forge force required in the typical friction stir weld process. Therefore, the self-reacting feature reduces tooling requirements and, therefore, process implementation costs. This makes the process attractive for aluminum alloy circumferential weld applications. To evaluate the application of self-reacting friction stir welding for aluminum alloy circumferential welding, a feasibility study was performed. The study consisted of performing a fourteen-foot diameter aluminum alloy circumferential demonstration weld using typical fusion weld tooling. To accomplish the demonstration weld, weld and tack weld development were performed and fourteen-foot diameter rings were fabricated. Weld development consisted of weld pin tool selection and the generation of a process map and envelope. Tack weld development evaluated gas tungsten arc welding and friction stir welding for tack welding rings together for circumferential welding. As a result of the study, a successful circumferential demonstration weld was produced leading the way for future circumferential weld implementation.

Bjorkman, Gerry↗

Solid State Welding Development at Marshall Space Flight Center

What is TSW and USW? TSW is a solid state weld process consisting of an induction coil heating source, a stir rod, and non-rotating containment plates Independent heating, stirring and forging controls Decouples the heating, stirring and forging process elements of FSW. USW is a solid state weld process consisting of an induction coil heating source, a stir rod, and a non-rotating containment plate; Ultrasonic energy integrated into non-rotating containment plate and stir rod; Independent heating, stirring and forging controls; Decouples the heating, stirring and forging process elements of FSW.

Ding, Robert J.↗

THE EFFECTS OF HYDROGEN, TRITIUM, AND HEAT TREATMENT ON THE DEFORMATION AND FRACTURE TOUGHNESS PROPERTIES OF STAINLESS STEEL

The deformation and fracture toughness properties of forged stainless steels pre-charged with tritium were compared to the deformation and fracture toughness properties of the same steels heat treated at 773 K or 873 K and precharged with hydrogen. Forged stainless steels pre-charged with tritium exhibit an aging effect: Fracture toughness values decrease with aging time after precharging because of the increase in concentration of helium from tritium decay. This study shows that forged stainless steels given a prior heat treatment and then pre-charged with hydrogen also exhibit an aging effect: Fracture toughness values decrease with increasing time at temperature. A microstructural analysis showed that the fracture toughness reduction in the heat-treated steels was due to patches of recrystallized grains that form within the forged matrix during the heat treatment. The combination of hydrogen and the patches of recrystallized grains resulted in more deformation twinning. Heavy deformation twinning on multiple slip planes was typical for the hydrogen-charged samples; whereas, in the non-charged samples, less twinning was observed and was generally limited to one slip plane. Similar effects occur in tritium pre-charged steels, but the deformation twinning is brought on by the hardening associated with decay helium bubbles in the microstructure.

36 MATERIALS SCIENCE↗

Additive Manufactured Materials Studies

The production of additively manufactured (AM) materials, is a growing technology that potentially offers more cost effective ways to produce metallic components for various uses. Mechanical properties of some AM metals have been studied, but more work is needed to better understand their dynamic properties as a function of orientation. Due to the melting and reheating of molten metal during fabrication, these materials tend to have internal porosity and slightly different microstructures along the weldments and normal to the weldments that may cause the materials to behave differently than their forged counterparts. The AM process builds up a part layer by layer, which provides opportunities to tailor geometry and optimize structural performance in addition to minimizing the amount of material waste for oddly shaped parts, thereby reducing cost. These advanced materials hold great promise for revolutionizing design, fabrication, and assembly of engineered components and could be used for many NNSA-specific applications including armoring complex elements of nuclear weapons, and customized diagnostic components in subcritical experiments. We have conducted materials studies in collaboration with the University of Nevada, Las Vegas (UNLV) as well as Los Alamos National Laboratory (LANL) under our Site-Directed Research and Development program and the Nevada Science Initiative. We are currently placing emphasis on quantifying how dynamic properties are affected by directionality and porosity of the material. A study of dynamic failure events in forged, layered, and additive manufactured (AM) titanium alloy subject to hypervelocity impact was conducted in collaboration with UNLV. Experiments were conducted using a two stage light-gas gun, 0.22-caliber Lexan projectiles, and different types of titanium target plates. A four-channel Photonic Doppler Velocimetry (PDV) system was used to study the free surface velocities to provide an understanding of the different failure mechanisms in these materials. The experimental measurements were used to validate computational simulations, which describe the behavior of these materials under shock. It was determined that AM, forged titanium, and multi-layered stacks produce similar velocity profiles during the early stage of impact, with the AM targets exhibiting spall at lower velocities and the multi-layered stacks exhibiting vibrations between plates. Simulations of solid and layered forged materials provide a good match to experimental data.

36 MATERIALS SCIENCE↗

Effects of Controlled Cooling-Induced Ferrite–Pearlite Microstructure on the Cold Forgeability of XC45 Steel

The combination of hot/warm and cold forging with an intermediate controlled cooling process is a promising approach to saving costs in the manufacture of automobile parts. In this work, the effects of the ferrite–pearlite microstructure, which formed after controlled cooling, on the cold forgeability of a medium-carbon steel were investigated. Different specimens for both normal and notched tensile tests were directly heated to high temperature and then cooled down at different cooling rates, producing different ferrite volume fractions, ranging from 6.69 to 40.53%, in the ferrite–pearlite microstructure. The yield strength, ultimate tensile strength, elongation rate, percentage reduction of area, and fracture strain were measured by tensile testing. The yield strength, indicating deformation resistance, and fracture strain, indicating formability, were used to evaluate the cold forgeability. As the ferrite volume fraction increased, the cold forgeability of the dual-phase ferritic–pearlitic steel improved. A quantitatively relationship between the ferrite volume fraction and the evaluation indexes of cold forgeability for XC45 steel was obtained from the test data. To validate the mathematical relationship, different tensile specimens machined from real hot-forged workpieces were tested. There was good agreement between the predicted and measured values. Our predictions from the relationship for cold forgeability had an absolute error less than 5%, which is acceptable for industrial applications and will help to guide the design of combined forging processes.

36 MATERIALS SCIENCE↗

In situ NiTi/Nb(Ti) composite

Graphical abstract: - Highlights: • In situ NiTi/Nb(Ti) composites were fabricated. • The transformation temperature was affected by the mixing Ti:Ni atomic ratios. • The NiTi component became micron-scale lamella after forging and rolling. • The composite exhibited high strength and high damping capacity. - Abstract: This paper reports on the creation of a series of in situ NiTi/Nb(Ti) composites with controllable transformation temperatures based on the pseudo-binary hypereutectic transformation of NiTi–Nb system. The composite constituent morphology was controlled by forging and rolling. It is found that the thickness of the NiTi lamella in the composite reached micron level after the hot-forging and cold-rolling. The NiTi/Nb(Ti) composite exhibited high damping capacity as well as high yield strength.

36 MATERIALS SCIENCE↗