In-Plane Liftout and Push-to-Pull for In Situ Mechanical Testing of Irradiated Inconel X-750

A streamlined sample preparation method for nanomechanical testing is needed to improve the quality of specimens, reduce the cost, and increase the versatility of specimen fabrication. This work outlines an in-plane liftout focused ion beam (FIB) fabrication procedure to prepare electron-transparent specimens for in situ transmission electron microscopy (TEM) nanomechanical testing. Ion etching and electron backscatter diffraction (EBSD) techniques were used to lift out a [110] oriented grain from a neutron-irradiated bulk X-750 alloy. Careful control of voltages and currents ensured precision. Top surface thinning sweeps prevented resurfacing and redeposition while dog-bone geometries were shaped with a 1:4 gauge width-to-milling pattern diameter ratio. Nanotensile testing in the TEM with a picoindenter allowed for the estimation of an ultimate tensile strength of 2.41 GPa, and inspection revealed a high density of bubbles in the X-750 matrix. The proposed fabrication procedure is significant for preparing samples from radioactive materials, studying complex structures that are orientation-dependent, and analyzing desired planar areas.

36 MATERIALS SCIENCE↗

Microstructure and Properties of Inconel 718 Fabricated by Directed Energy Deposition with In-Situ Ultrasonic Impact Peening

Many inherent issues, such as the detrimental residual stress, columnar grains with anisotropy, and weak mechanical properties, have severely impeded the adoption of metal additive manufacturing (AM) techniques including powder bed fusion and directed energy deposition (DED) processes. In this study, a hybrid AM process that consists of layer-wise laser metal deposition (i.e., a DED process) and in-situ ultrasonic impact peening (UIP) was applied to obtain Inconel 718 superalloy workpieces. Also, for further property enhancement, a post-heat treatment was applied to the deposited material obtained by the hybrid AM process. Scanning electron microscopy and transmission electron microscope were used to investigate the microstructure morphology and reveal the underlying strengthening mechanism. Electron backscatter diffraction was employed to quantitatively study the microstructure resulted from the hybrid AM process and the post-heat treatment. The profile of residual stress along the depth direction was obtained through X-ray diffraction. The results demonstrate that this hybrid AM process is capable of producing high-quality metal parts with significantly refined microstructure, and beneficial compressive residual stress along the depth into surface. Severe plastic strains are introduced by UIP, and the resulted mechanical twinning and dynamic recrystallization play an important role in refining microstructure. The material microstructure is further refined down to 100 µm, and the texture anisotropy is significantly diminished after solution treatment at 980 °C for 1 hour. Under the as-built condition, in-situ ultrasonic peening alters the residual stress component from a tensile state to an overall compressive state with a maximum value of − 190 MPa within the range of measurement depth.

36 MATERIALS SCIENCE↗

The formation mechanisms of interlocked microstructures in low-carbon high-strength steel weld metals

Microstructural features and the formation mechanisms of interlocked microstructures of acicular ferrite in a low-carbon high-strength steel weld metal were investigated by means of computer-aided three-dimensional reconstruction technique and electron backscattered diffraction analysis. Multiple nucleation on inclusions, sympathetic nucleation or repeated nucleation, hard impingement, mutual intersection, and fixed orientation relationships of acicular ferrite grains were observed. They were all responsible for the formation of interlocked microstructures in the weld metal. During the process of isothermal transformation, the pre-formed acicular ferrite laths or plates partitioned austenite grains into many small and separate regions, and the growth of later formed acicular ferrite grains was confined in these small regions. Thus, the crystallographic grain size became smaller with the increasing holding time. Highlights: Black-Right-Pointing-Pointer Acicular ferrite is formed by multiple nucleation and sympathetic nucleation. Black-Right-Pointing-Pointer Hard impingement and intersection of ferrite grains occur at later stages. Black-Right-Pointing-Pointer The pre-formed ferrite laths partition austenite grains into smaller regions. Black-Right-Pointing-Pointer The growth of later formed ferrite grains is confined in the smaller regions.

36 MATERIALS SCIENCE↗

Structural characterization of “carbide-free” bainite in a Fe–0.2C–1.5Si–2.5Mn steel

Low-alloyed, low C containing carbide-free bainitic steels are attractive candidates for applications in the automotive industry due to their well-balanced combination of high strength and ductility achieved in an economic way. In this work, their complex microstructure consisting of a mixture of bainitic ferrite, austenite with different morphologies and stabilities, martensite, M/A constituent and a few carbides has been investigated with metallographic and high-resolution techniques. After specific isothermal heat treatments in a dilatometer, a combination of LePera and Nital etching was applied to distinguish between bainite and martensite. Site-specific atom probe tips were prepared by means of scanning electron microscopy, electron backscatter diffraction and focused ion beam, revealing that “carbide-free” bainite consists of C depleted bainitic ferrite, C enriched retained austenite and occasional ε-carbides. Furthermore, it was found that the M/A constituent is highly dislocated and mainly martensitic. Its C content is increased compared to the nominal composition, but below the values obtained for retained austenite, explaining the lower transformation resistance. - Highlights: • Detailed top-down characterization of low C “carbide-free” bainitic steel • APT of all constituents in “carbide-free” bainite • Identification of ε-carbide based on its C content determined by APT • M/A constituent is mainly martensitic with austenitic areas at the boundaries • Lower C content of M/A constituent explains its lower stability.

36 MATERIALS SCIENCE↗

Effect of Microstructure Refinement on Hardness Homogeneity of Aluminum Alloy 1100 Processed by Accumulative Roll Bonding

This work examines the effect of grain refinement via accumulative roll bonding (ARB) on the homogeneity of microstructure and hardness through the thickness of commercially pure aluminum AA1100 sheets. The use of 7 cycles of ARB was shown to produce homogeneous ultrafine-grained microstructure, reducing the grain size to 0.46 and 1.03 µm in normal direction and rolling direction, respectively. Examination by electron backscattered diffraction indicates that continuous dynamic recrystallization was the main mechanism for the formation of submicron equiaxed grains bounded with high-angle grain boundaries (HAGBs). The fraction of HAGBs increased gradually reaching a maximum of 71.6% after 7 cycles. Through-thickness hardness measurements using Vickers and nanoindentation tests show an increase from 43.5 Hv (0.85 GPa) for as-received sample to 63 Hv (1.1 GPa) after 7 cycles. The heterogeneity in hardness through the thickness of the as-received material was shown to restrain the evolution of uniform hardness across the sheet thickness with increasing ARB cycles. Tensile tests showed that the tensile strength is increased to 250 MPa, which is about 2 times its initial value. Owing to the high stacking fault energy of AA1100, strong dynamic recovery occurred with increasing ARB strain which was balanced with the strain hardening property of the material. This resulted in plastic instability at small strains and thus early necking during the tensile test.

36 MATERIALS SCIENCE↗

Microstructural and textural evolution of AZ61 magnesium alloy sheet during bidirectional cyclic bending

In this work, the microstructural and textural evolution in the sheets of AZ61 magnesium alloy was studied by means of bidirectional cyclic bending for 8 passes at 623 K. The bended samples were examined by optical microscopy and electron backscatter diffraction analysis. The results showed that a gradient structure with fine grains about 3 μm in the regions near two surfaces and, in contrast, coarse grains in the middle of the sheet were formed. The evident grain refinement was attributed to twin-assisted dynamic recrystallization and continuous dynamic recrystallization induced by kink bands. The texture intensity was clearly reduced, resulting in a negative gradient distribution, with the texture intensity decreases from the center of the sheet to two surfaces. The weakened texture greatly facilitated the reduction of the yield strength. A higher fracture elongation and a slightly improved ultimate tensile strength were achieved concurrently. - Highlights: • The AZ61 Mg alloy is deformed at 623 K by bidirectional cyclic bending. • A symmetric gradient distribution of fine grains along the thickness is formed. • The basal texture in the regions near two surfaces is weakened significantly.

36 MATERIALS SCIENCE↗

Non-isothermal Reduction Kinetics of Iron During Vacuum Carbothermal Reduction of Ilmenite Concentrate

The non-isothermal reduction kinetics and mechanism of iron during vacuum carbothermal reduction of ilmenite concentrate were investigated by X-ray diffraction, backscattered electron imaging, and energy-dispersive X-ray spectroscopy at temperatures from 1273 K to 1673 K (1000 °C to 1400 °C). The pressure dropped and the increasing trend of mass loss and metallization ratios slowed down when the temperature was higher than 1573 K (1300 °C). The reaction products were iron, Ti{sub 2}O{sub 3}, and silicate. Iron was mainly obtained by carbothermal reduction of FeTiO{sub 3} and FeTi{sub 2}O{sub 5}. The irons continued to nucleate, aggregate, and grow during the reduction process. Comprehensive consideration of Šatava–Šesták method and Coats–Redfern method, the apparent activation energy of the reduction process was 587.4 ± 2.98 kJ/mol, and the forms of both integral and differential for the mechanism function were G(a)= [(1−a){sup −1/3}−1]{sup 2} and f(a) = 3/2(1−a){sup 4/3}[(1−a)−{sup 1/3}−1]{sup −1}, respectively.

36 MATERIALS SCIENCE↗

Understanding and Predicting Metallic Whisker Growth and its Effects on Reliability (LDRD Final Report)

Tin (Sn) whiskers are conductive Sn filaments that grow from Sn-plated surfaces, such as surface finishes on electronic packages. The phenomenon of Sn whiskering has become a concern in recent years due to requirements for lead (Pb)-free soldering and surface finishes in commercial electronics. Pure Sn finishes are more prone to whisker growth than their Sn-Pb counterparts and high profile failures due to whisker formation (causing short circuits) in space applications have been documented. At Sandia, Sn whiskers are of interest due to increased use of Pb-free commercial off-the-shelf (COTS) parts and possible future requirements for Pb-free solders and surface finishes in high-reliability microelectronics. Lead-free solders and surface finishes are currently being used or considered for several Sandia applications. Despite the long history of Sn whisker research and the recently renewed interest in this topic, a comprehensive understanding of whisker growth remains elusive. This report describes recent research on characterization of Sn whiskers with the aim of understanding the underlying whisker growth mechanism(s). The report is divided into four sections and an Appendix. In Section 1, the Sn plating process is summarized. Specifically, the Sn plating parameters that were successful in producing samples with whiskers will be reviewed. In Section 2, the scanning electron microscopy (SEM) of Sn whiskers and time-lapse SEM studies of whisker growth will be discussed. This discussion includes the characterization of straight as well as kinked whiskers. In Section 3, a detailed discussion is given of SEM/EBSD (electron backscatter diffraction) techniques developed to determine the crystallography of Sn whiskers. In Section 4, these SEM/EBSD methods are employed to determine the crystallography of Sn whiskers, with a statistically significant number of whiskers analyzed. This is the largest study of Sn whisker crystallography ever reported. This section includes a review of previous literature on Sn whisker crystallography. The overall texture of the Sn films was also analyzed by EBSD. Finally, a short Appendix is included at the end of this report, in which the X-Ray diffraction (XRD) results are discussed and compared to the EBSD analyses of the overall textures of the Sn films. Sections 2, 3, and 4 have been or will be submitted as stand-alone papers in peer-reviewed technical journals. A bibliography of recent Sandia Sn whisker publications and presentations is included at the end of the report.

36 MATERIALS SCIENCE↗

Effect of the pre-existing carbides on the grain boundary network during grain boundary engineering in a nickel based alloy

Grain boundary engineering was carried out on an aging-treated nickel based Alloy 690, which has precipitated carbides at grain boundaries. Electron backscatter diffraction technique was used to investigate the grain boundary networks. Results show that, compared with the solution-annealed samples, the aging-treated samples with pre-existing carbides at grain boundaries need longer duration or higher temperature during annealing after low-strain tensile deformation for forming high proportion of low-Σ coincidence site lattice grain boundaries (more than 75%). The reason is that the primary recrystallization is inhibited or retarded owing to that the pre-existing carbides are barriers to grain boundaries migration. - Highlights: • Study of GBE as function of pre-existing GB carbides, tensile strain and annealing • Recrystallization of GBE is inhibited or retarded by the pre-existing carbides. • Retained carbides after annealing show the original GB positions. • More than 80% of special GBs were formed after the modification of GBE processing. • Multiple twinning during recrystallization is the key process of GBE.

36 MATERIALS SCIENCE↗

Synergetic Strengthening of Grain Refinement and Texture in Gradient Zircaloy-4 by Surface Mechanical Rolling Treatment

A Zircaloy-4 rod was subjected to surface mechanical rolling treatment (SMRT) to form a gradient structure, and the evolution of the resulting sub-grain-boundary property and texture across the gradient structure was characterized using electron backscattered diffraction. Dual-gradient structures in grain size and orientation were formed; the grain size was refined from several microns at the center to approximately 400 nm at the topmost surface. Texture analysis revealed that the c-axis gradually tilted from a random orientation toward the parallel-to-radial direction on the radial–tangential plane. The SMRT-induced formation of the dual-gradient microstructure is attributed to the formation of gradient distributions of stress and strain, which resulted in various deformation mechanisms (twinning and dislocation) being active at different depths. During the SMRT process, twinning and dislocations were activated to refine the grains. When the dual-gradient microstructure formed, twinning was mainly activated at the subsurface near the matrix, whereas dislocations were activated across the entire gradient. The geometrically necessary dislocation density increased with decreasing depth and then slightly decreased near the surface. The synergetic strengthening of the dual-gradient microstructure resulted in a gradient distribution of the microhardness near the surface. Thus, the Zircaloy-4 rod exhibited a good combination of strength and ductility.

36 MATERIALS SCIENCE↗

In-situ characterization of transformation plasticity during an isothermal austenite-to-bainite phase transformation

This paper elucidates the stress-induced variant selection process during the isothermal austenite-to-bainite phase transformation in a tool steel. Specifically, a thorough set of experiments combining electron backscatter diffraction and in-situ digital image correlation (DIC) was carried out to establish the role of superimposed stress level on the evolution of transformation plasticity (TP) strains. The important finding is that TP increases concomitant with the superimposed stress level, and strain localization accompanies phase transformation at all stress levels considered. Furthermore, TP strain distribution within the whole material becomes more homogeneous with increasing stress, such that fewer bainitic variants are selected to grow under higher stresses, yielding a more homogeneous strain distribution. In particular, the bainitic variants oriented along [101] and [201] directions are favored to grow parallel to the loading axis and are associated with large TP strains. Overall, this very first in-situ DIC investigation of the austenite-to-bainite phase transformation in steels evidences the clear relationship between the superimposed stress level, variant selection, and evolution of TP strains. - Highlights: Black-Right-Pointing-Pointer Local variations of strain were observed by DIC throughout the phase transformation. Black-Right-Pointing-Pointer The study clearly established the role of the stress-induced variant selection. Black-Right-Pointing-Pointer Variant selection is a key parameter that governs distortion.

36 MATERIALS SCIENCE↗

Characterization of coarse bainite transformation in low carbon steel during simulated welding thermal cycles

Coarse austenite to bainite transformation in low carbon steel under simulated welding thermal cycles was morphologically and crystallographically characterized by means of optical microscope, transmission electron microscope and electron backscattered diffraction technology. The results showed that the main microstructure changes from a mixture of lath martensite and bainitic ferrite to granular bainite with the increase in cooling time. The width of bainitic laths also increases gradually with the cooling time. For a welding thermal cycle with relatively short cooling time (e.g. t{sub 8/5} is 30 s), the main mode of variant grouping at the scale of individual prior austenite grains changes from Bain grouping to close-packed plane grouping with the progress of phase transformation, which results in inhomogeneous distribution of high angle boundaries. As the cooling time is increased, the Bain grouping of variants becomes predominant mode, which enlarges the effective grain size of product phase. - Highlights: • Main microstructure changes and the width of lath structure increases with cooling time. • Variant grouping changes from Bain zone to close-packed plane grouping with the transformation. • The change of variant grouping results in uneven distribution of high angle grain boundary. • Bain grouping is main mode for large heat input, which lowers the density of high angle boundary.

36 MATERIALS SCIENCE↗

A study on the creep behavior of alloy 709 using in-situ scanning electron microscopy

In this research, an experimental evaluation of creep properties of Alloy 709 in the temperature range of 750–850 °C was undertaken. Alloy 709 is a novel austenitic stainless steel with 20% Cr and 25% Ni by wt% that was developed for application in structural components of nuclear power plants. Creep rupture tests were conducted in an in-situ heating-loading and Scanning Electron Microscope (SEM) unit equipped with Electron Backscatter Diffraction (EBSD) detector and Energy Dispersive Spectroscopy (EDS). “Real-time” creep damage mechanisms of Alloy 709 at various stresses and temperatures using a flat, un-notched sample with continuously reducing cross-section is studied so that the failure and maximum creep damage occurred at the center of the sample where the in-situ SEM imaging could be focused. Accelerated creep tests at temperatures and stresses above service conditions were performed by employing multiple blocks of constant loads where the loads were increased once the sample attained constant creep rate, indicating a secondary creep regime. This technique ensures multiple data points can be obtained from the same test, saves the time required for an otherwise long-term creep test and usage of SEM. Further, Coincident Site Lattice (CSL) boundary maps were collected as control maps before testing, and the grain boundaries were observed during the creep test to understand the effect of grain boundary character on the creep damage mechanism. Void growth, grain boundary separation, and sliding were found to be the main creep mechanisms whose rate is dependent on stress and temperature. Failure mechanisms studied on the fracture surface using SEM fractography were correlated to the sample surface observations to create complementary information to better understand the underline creep mechanism of Alloy 709.

36 MATERIALS SCIENCE↗

Microstructures of ancient and modern cast silver–copper alloys

The microstructures of modern cast Sterling silver and of cast silver objects about 2500 years old have been compared using optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), scanning transmission electron microscopy (STEM), energy dispersive X-ray microanalysis (EDX) and electron backscatter diffraction (EBSD). Microstructures of both ancient and modern alloys were typified by silver-rich dendrites with a few pools of eutectic and occasional cuprite particles with an oxidised rim on the outer surface. EBSD showed the dendrites to have a complex internal structure, often involving extensive twinning. There was copious intragranular precipitation within the dendrites, in the form of very fine copper-rich rods which TEM, X-ray diffraction (XRD), SEM and STEM suggest to be of a metastable face-centred-cubic (FCC) phase with a cube–cube orientation relationship to the silver-rich matrix but a higher silver content than the copper-rich β in the eutectic. Samples from ancient objects displayed a wider range of microstructures including a fine scale interpenetration of the adjoining grains not seen in the modern material. Although this study found no unambiguous evidence that this resulted from microstructural change produced over archaeological time, the copper supersaturation remaining after intragranular precipitation suggests that such changes, previously proposed for wrought and annealed material, may indeed occur in ancient silver castings. - Highlights: • Similar twinned structures and oxidised surfaces seen in ancient and modern cast silver • General precipitation of fine Cu-rich rods apparently formed by discontinuous precipitation is characteristic of as-cast silver. • The fine rods are cube-cube related to the matrix in contrast with the eutectic. • The silver-rich phase remains supersaturated with copper. • Possibly age-related grain boundary features seen in ancient cast silver.

36 MATERIALS SCIENCE↗

Multi-objective surrogate-assisted calibration of CPFEM models using macroscopic response and in situ EBSD measurements of grain reorientation trajectories

Crystal plasticity finite element method (CPFEM) models are widely used to simulate the deformation behaviour of polycrystalline materials, but their calibration is often limited by their high computational cost and the non-convexity of the optimisation landscape. Here, this study develops a multi-objective surrogate-assisted calibration workflow that couples a multi-objective genetic algorithm (MOGA) with an adaptively trained deep neural network (DNN) surrogate model to efficiently identify CPFEM parameters from experimental data. The workflow is demonstrated on three crystal plasticity (CP) formulations of increasing complexity — Voce hardening (VH), two-coefficient latent hardening (LH2), and six-coefficient latent hardening (LH6) — using in situ electron backscatter diffraction (EBSD) measurements of Alloy 617 under uniaxial tensile loading. The CPFEM models are calibrated against the experimentally observed stress–strain response and reorientation trajectories of eight grains, then validated against eight additional trajectories and overall texture evolution. Across the CP formulations, the macroscopic response was reproduced reliably, while differences emerged in the robustness and accuracy of the grain-scale predictions. Including grain reorientation trajectories in the multi-objective calibration improved texture evolution predictions and filtered out physically inconsistent parameter sets that can arise from calibrating against only the stress–strain data. The workflow also demonstrates good transferability of calibrated parameters from a low- to a high-fidelity microstructural model. These results provide practical guidance for integrating in situ microstructural data into CPFEM through efficient, repeatable, and physically meaningful multi-objective calibration.

Crystal plasticity finite element method↗

Effects of Solution Treatment on Microstructure Transformation, Tensile and Exfoliation Corrosion Properties of 7136 Aluminum Alloy

The effects of solution treatment on microstructure transformation and tensile properties of 7136 aluminum alloys were investigated by means of scanning electron microscopy, electron backscatter diffraction, differential scanning calorimeter, x-ray diffraction and tensile test, electrochemical evaluations, exfoliation corrosion tests, respectively. The results indicate that solution treatment had a significant effect on the microstructure transformation and tensile properties. Soluble constituents of 7136 aluminum alloys were more likely to form the η(MgZn{sub 2}) phase rather than the S(Al{sub 2}CuMg) phase. With increasing the solution temperature, the η phase was re-dissolved into the α(Al) matrix gradually. After solution treatment of 475 °C/1 h, the η phase was completely dissolved into the matrix, with insoluble Fe-rich phases remained. The dissolution of η phase would increase the strength and the corrosion resistance of the alloys. When continuing to increase the solution temperature, the recrystallized fraction increased obviously, resulting in the decrease in the strength and the corrosion resistance. Consequently, the strength and the corrosion resistance of the alloys increased firstly and then decreased with the increase in solution temperature. After solution treatment of 475 °C/1 h, the tensile strength and yield strength of the aged alloy reached their peaks, 738 and 715 MPa, respectively. The elongation of the alloy solution treated at 475 °C/1 h reached 11.2%, and its exfoliation corrosion rating got EB level. Furthermore, after the double-stage solution treatment of 450 °C/1 h + 475 °C/1 h, the recrystallized fraction decreased, resulting in a slight increase to 12.6% of the elongation, a slight increase in the corrosion resistance and a slight decrease in the strength.

36 MATERIALS SCIENCE↗

Evolution of microstructure and grain boundary character distribution of a tin bronze annealed at different temperatures

Specimens cut from a rolled tin bronze sheet were annealed at 400–800 °C for 1 h and evolution of their microstructures was then characterized in details by electron channeling contrast imaging and electron backscatter diffraction techniques. Particularly, statistics on special boundaries (SBs) with Σ ≤ 29 and network connectivity of random high angle boundaries (HABs) in the annealed specimens were examined to probe optimization potentials of grain boundary character distribution (GBCD) for this material. Results show that the deformed microstructure in the as-received material begins to be recrystallized when the annealing temperature increase to 500 °C and average grain sizes surge with further increasing temperatures. As a result of the recrystallization, a large number of annealing twins (with Σ3 misorientation) are produced, leading to remarkably increased fractions of SBs (f{sub SBs}). Thanks to preexisting dense low angle boundaries, the majority of SBs in the 500 °C specimen with only partial recrystallization are Σ3{sub ic} (incoherent) boundaries, which effectively disrupt connectivity of random HABs network. Although the f{sub SBs} can be further increased (up to 72.5%) in specimens with full recrystallization (at higher temperatures), the Σ3{sub ic} boundaries would be replaced to some extent by Σ3{sub c} (coherent) boundaries which do not contribute directly to optimizing the GBCD. This work should be able to provide clear suggestions on applying the concept of grain boundary engineering to tin bronze alloys. - Highlights: • The rolled tin bronze begins to be recrystallized as temperature increases to 500 °C. • A lot of SBs are produced after recrystallization and the highest f{sub SBs} is 72.5%. • Partially recrystallized specimen has the optimum GBCD due to more Σ3{sub ic} boundaries. • The Σ3{sub ic} boundaries are replaced by Σ3{sub c} boundaries after full recrystallization.

36 MATERIALS SCIENCE↗

Quasi in-situ analysis of geometrically necessary dislocation density in α-fibre and γ-fibre during static recrystallization in cold-rolled low-carbon Ti-V bearing microalloyed steel

Highlights: • Average GND density is higher in gamma fibre than alpha fibre. • Higher drop in average GND density in un-recrystallized portion of gamma fibre • Fine precipitates pin the grain boundary at 700 °C 0 s. • Precipitates are coarse at 800 °C and present inside strain-free grains. - Abstract: In the present study, cold-rolled low-carbon steel is annealed at three different conditions: 700 °C for 0 s, 800 °C for 0 s and 800 °C for 2 min at the heating rate of ~10 °C/s. Recrystallization behaviour on sample surface is studied using a heated stage Scanning Electron Microscopy and Electron Backscattered Diffraction. For the lower annealing temperature of 700 °C with no dwell, almost no recrystallization is observed and microstructure resembles the as-received deformed material with the exception of occasional sub-micron sized nuclei. For the annealing conditions of 800 °C 0 s and 800 °C 2 min, onset and evolution of recrystallization is observed in-situ as a function of the initial as-cold rolled texture. Slower recovery rate of alpha fibre than gamma fibre is observed and confirmed by lower drop in average geometrically necessary dislocation (GND) density for un-recrystallized alpha fibres (1.1E+14 m{sup −2} for 700 °C 0 s, 1.4E+14 m{sup −2} for 800 °C 0 s and 4.5E+14 m{sup −2} for 800 °C 2 min) than for un-recrystallized gamma fibre grains (3.0E+14 m{sup −2} for 700 °C 0 s, 6.2E+14 m{sup −2} for 800 °C 0 s and 9.8E+14 m{sup −2} for 800 °C 2 min) during annealing. Strong gamma texture in recrystallized matrix is found for annealing conditions of 800 °C 0 s and 800 °C 2 min. From TEM characterisation it was shown that sub-grain boundaries are decorated with fine precipitates (diameter d < 15 nm) of titanium‑vanadium carbides (Ti,V)C for the annealing condition of 700 °C 0 s, which suggests that these precipitates play a major overall role in retardation of the recrystallization kinetics.