Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CHROMIUM ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 559 records · Page 31

Understanding irradiation growth through atomistic simulations: Defect diffusion and clustering in α-zirconium and the influence of alloying elements - 2016-0093

Irradiation-induced structural changes of α-zirconium alloys and in particular the effect of iron were investigated by molecular dynamics simulations using embedded atom potentials derived from first-principles calculations. The simulations revealed that at temperatures between 500 and 600 K self-interstitial atoms (SIAs) diffuse rapidly in a cooperative movement, preferably parallel to basal planes (a directions; ), forming nano-clusters with an extension in and . Vacancies diffuse more slowly than SIAs and remain isolated for a longer period of time. Nano-clusters associated with SIAs cause a pronounced overall expansion in a directions, as well as local strains. Under compressive strain in the c direction, vacancy diffusivity increases in the c direction. In contrast, the diffusivity of SIAs increases in the c direction under a tensile strain in the c direction. SIA nano-clusters are highly mobile within basal planes. Vacancy clusters grow by merging, leading to a contraction in the a direction, compensating for the expansion caused by SIA nano-clusters and possibly contributing to the plateau in growth after the initial rapid expansion. At the onset of breakaway growth, possibly due to stress buildup, the vacancy nano-clusters can condense into c loops, thereby diminishing the compensation effect. The alloying elements iron, nickel, chromium, and niobium liberated from secondary phase particles under irradiation or already in solution are attracted to vacancies and SIAs and are found inside vacancy and SIA loops. The interaction of alloying elements with defect clusters is discussed, with a particular focus on iron. Iron has been found to promote cluster formation in zirconium, and the structures of zirconium-iron clusters have been analyzed. Tin is repelled by SIA clusters and only weakly attracted by vacancies. Niobium impedes the diffusion of SIAs (and therefore may increase annihilation rates with nearby vacancies) and does not destabilize vacancy or SIA clusters. Ab initio calculations of the dimensional and elastic coefficients of the intermetallic phases occurring in secondary phase particles, such as Zr{sub 2}Fe and Zr{sub 3}Fe, are presented, allowing an assessment of local strains in a zirconium matrix. Thus, novel results from extended molecular dynamics simulations provide new insights and contribute to a deeper understanding of the complex mechanisms causing irradiation-induced dimensional changes and the breakaway growth of zirconium alloys. (authors)

36 MATERIALS SCIENCE↗

High-temperature oxidation of advanced FeCrNi alloy in steam environments

Alloys of iron-chromium-nickel are being explored as alternative cladding materials to improve safety margins under severe accident conditions. Here, our research focuses on non-destructively investigating the oxidation behavior of the FeCrNi alloy “Alloy 33” using synchrotron-based methods. The evolution and structure of oxide layer formed in steam environments were characterized using X-ray diffraction, hard X-ray photoelectron spectroscopy, X-ray fluorescence methods and scanning electron microscopy. In conclusion, our results demonstrate that a compact and continuous oxide scale was formed consisting of two layers, chromium oxide and spinel phase (FeCr 2 O 4 ) oxides, wherein the concentration of the FeCr 2 O 4 phase decreased from the surface to the bulk-oxide interface.

36 MATERIALS SCIENCE↗

Reliability of thickness of oxide layer of stainless steels with chromium using cellular automaton model

A cellular automaton (CA) model based on the stochastic approach was proposed to simulate the process of oxidation and corrosion of stainless steels with different contents of chromium in-flowing lead bismuth eutectic (LBE). Chromium is a crucial alloying element added in stainless steels and nickel based alloys which have been proposed to be used in advanced nuclear reactors to improve resistance of the oxidation and corrosion. To verify the reliability of the thickness of the oxide layer by CA model, the influence of the stochastic character on the simulating results was investigated as changing parameter of chromium content of structure material in this study. Ten independent simulations were run for each specific environment. A stable and reasonable results were obtained according to the chi-square of goodness-of-fit test, the chi-square of the thickness of oxide layer for each case were significant smaller than critical chi-square value with a confidence level of 95% ({Chi}{sup 2}{alpha}, v = {Chi}{sup 2} 0.05,9 = 16.92). (authors)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

MS212--A Homogeneous Sputtered Solid Lubricant Coating for Use to 800 C

Composite coatings containing chromium carbide, stable fluorides and silver were prepared by magnetron sputtering. The microstructure of the coatings is very homogeneous compared to that of plasma sprayed and sintered versions of the same chemical composition. Friction and wear of MS212-coated and baseline uncoated aluminum and Inconel X-750 are compared. At room temperature, the friction and wear of coated aluminum is dramatically better compared to the baseline. The acceptable load is limited by deformation of the soft aluminum substrate. In the case of the nickel alloy, lower friction is observed for the coated alloy at all temperatures up to the maximum test temperature of 800 C. Pin wear factors for sliding against the coated alloy are lower than the baseline at room temperature and 350 C, and comparable to baseline wear at higher test temperatures. Low baseline wear at high temperatures is due to the lubricious nature of the natural oxides formed on nickel-chromium alloys in a hot, oxidizing atmosphere. No load limit was found for coated Inconel X-750 at loads up to five times the load limit for coated aluminum.

Sliney, Harold E.↗

The Influence of Modification on Crystal Lattice Stability of Austenite in Stainless Steel

Using the methods of electron diffraction microscopy and X-ray diffraction analysis, the influence of alloying of the austenitic steel, Grade 110H13, with chromium and vanadium, as well as high-melting, ultrafine-grained TiO{sub 2}, ZrO{sub 2} powders and Na{sub 3}AlF{sub 6} cryolite on its structural-phase state and microstructure is investigated. It is shown that the matrix of non-modified steel is completely austenitic and consists of an iron-based solid solution and the interstitial (C, N, O and other) and substitutional (Cr, V and other) atoms simultaneously. Alloying with chromium and vanadium changes neither its phase composition nor defect structure, while alloy modification results in qualitatively new structural features: γ → ε-transformation, high-intensity microtwinning, defect structure changes, and a sharp increase in the scalar dislocation density. The features of the deformation-induced microtwinning and ε-martensite plates identified in the modified steel promote revealing additional microtwin systems in the matrix γ-phase, which result in structural changes making it possible to classify it as a γ′-phase. It is found out that an introduction of modifying additions gives rise to the following sequence of structural-phase transformations: γ→γ′→(γ′ +ε). The experimental data obtained demonstrate that as a result of modification the crystal lattice transits into a low-stability state. This transition is accompanied by marked structural-phase changes consisting in the formation of several microtwin systems and γ → ε-transformation. These structural-phase changes in the modified steel are due to the crystal-lattice transition into the low-stability state, followed by new structural-phase alterations.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Tribological Behavior of Structural Materials in High Temperature Helium Gas-Cooled Reactor Environments

The High-Temperature Gas-cooled Reactor (HTGR) is a Generation IV concept designed to produce electricity and hydrogen at high efficiencies via high operating temperatures (700 °C or higher). Helium, the primary coolant for HTGRs, contains impurities (e.g., CO, H2O and CH4) that can induce corrosion reactions at high temperatures such as oxidation and (de)carburization, which in turn can affect the tribological behavior of components. Incoloy® 800HT (Ni-Fe-Cr austenitic solid-solution alloy) and Inconel® 617 (Ni-Cr-Co-Mo solid-solution alloy) are two high-temperature superalloys currently selected as candidate structural materials for the HTGR. The objective of this study is to evaluate the high-temperature tribological performance of these two candidate alloys after conditioning them in HTGR environments. Four regimes of corrosion were considered: a non-conditioned regime (Regime I), an oxidizing regime (Regime II), a carburizing and oxidizing regime (Regime III), and a carburizing regime (Regime IV). To simulate oxidation in HTGR, samples were conditioned for 22 days at elevated temperatures in a once-through helium loop with 4 ppmv H2O. Carburization of the samples was achieved by the commercial process, Kolsterising®. In addition, two surface treatments – shot peening and aluminization – were considered as potential routes of improving the alloys’ wear resistance. Surface-treated samples were tested both before and after conditioning in Regime II. Tribological testing of the samples was performed via a pin-on-disk tribometer at elevated temperatures in ambient environment – 650 and 750°C for 800HT; 850 and 900°C for 617 – with applied loads of 1N, 2N and 5N. The wear behavior of the alloys was assessed via wear volume and friction coefficient measurements, supported by morphological, structural and compositional analyses of the wear tracks. Conditioning the samples in Regime II led to the formation of a chromium oxide on both alloys. This protective scale increased the wear resistance compared to that of as-received samples (Regime I) due to the formation of a compacted ‘glaze’ oxide layer during sliding, rendering the wear track nearly undistinguishable from the unworn background and resulting in wear volumes below the detection limits of the measurement technique. The variability of the friction coefficients of the conditioned samples was also considerably reduced compared to that of the as-received samples due to the glaze layer. Additionally, the initial friction coefficients of the samples conditioned in Regime II were reduced by 45% and 54% compared to those of as-received samples for alloys 800HT and 617, respectively. Carburizing the samples (Regime IV) hardened the surfaces of both alloys and promoted the formation of an iron oxide on 800HT during tribological testing, thereby increasing the wear resistance and decreasing the initial friction coefficient by a factor of two compared to those of as-received 800HT. Alloy 617 exhibited an enhanced wear resistance but similar initial friction coefficient compared to those of as-received samples due to the increased surface hardness. The Mn-Cr oxide developed during Regime III conditioning of 800HT did not develop a glaze layer during tribotesting, even at lower loads. Thus, it was not as protective as the oxide produced during conditioning of Regime II samples, leading to lower wear resistance of 800HT in Regime III compared to that measured in the Regime II condition. 800HT benefited from the aluminization surface treatment, particularly before conditioning in Regime II, due to the promotion of a wear-resistant aluminum oxide layer during testing and the increase in surface hardness due to the presence of a FeAl intermetallic phase. The presence of this phase caused an order-of-magnitude reduction in wear volumes compared to those of as-received 800HT. Aluminization of 617 decreased its wear resistance, particularly after conditioning in Regime II, due to significant wear of the aluminum oxide via a ceramic wear mechanism. This aluminum oxide was removed during sliding, causing the wear volumes to increase by a factor of five compared to those of 617 conditioned in Regime II. Shot-peened 800HT exhibited a tribological behavior similar to that of as-received 800HT, despite an enhancement in the rate of chromium oxide formation. Shot-peened 800HT conditioned in Regime II showed lower wear resistance compared to that of 800HT conditioned in Regime II due to the poor adhesion between the oxide and the underlying metal, preventing the formation of the glaze layer during sliding. Shot peening of 617 increased its wear resistance at higher load, reducing worn volumes by 60% compared to that measured with as-received 617. Tribotesting of shot-peened 617 in Regime II revealed that the glaze-oxide layer was formed at every load, resulting in negligible wear, similar to what was observed from testing 617 after conditioning in Regime II. Overall, alloy 617 exhibited tribologically superior behavior compared to that of alloy 800HT, as demonstrated by its lower friction coefficients and its order-of-magnitude lower wear volumes when measurable.

36 MATERIALS SCIENCE↗

Cold spray chromium coating for nuclear fuel rods

A method is provided for coating the substrate of a component, such as a zirconium alloy cladding tube, for use in a water cooled nuclear reactor under normal operating conditions and under high temperature oxidation conditions. The method includes heating a pressurized carrier gas to a temperature between 200° C. and 1200° C., adding chromium or chromium-based alloy particles having an average diameter of 20 microns or less to the heated carrier gas, and spraying the carrier gas and particles onto the substrate at a velocity, preferably from 800 to 4000 ft./sec. (about 243.84 to 1219.20 meters/sec.), to form a chromium and/or chromium-based alloy coating on the substrate to a desired thickness.

36 MATERIALS SCIENCE↗

Evolution of Σ3n CSL boundaries in Ni-Cr-Mo alloy during aging treatment

Highlights: • Σ3{sup n} boundary distribution characteristics are changed during aging treatment at 600 °C. • The increase in fractions of Σ9 and Σ27 boundaries depends on interaction between Σ3{sup n} boundaries. • The consumption of Σ3{sub c} boundaries is modeled with migration of random HABs. • Generation mechanism of Σ3{sub ic} boundaries differs from traditional models. - Abstract: The evolution of Σ3{sup n} (n = 1,2,3) boundaries in a Ni-Cr-Mo alloy during an aging treatment at 600 °C was investigated based on electron backscatter diffraction (EBSD) measurements. Incoherent Σ3 (Σ3{sub ic}) and coherent Σ3 (Σ3{sub c}) boundaries were identified using the single-section trace analysis method. The results show that the Σ3{sup n} boundary distribution characteristics are changed and that a Pt{sub 2}Mo-type Ni{sub 2}(Cr,Mo) superlattice phase precipitates during the aging treatment. Through the analysis and comparison of the average grain diameters measured under the different conditions, the migration behaviors of both the Σ3{sub ic} boundaries and random high-angle boundaries (HABs) are found. The migration of the Σ3{sub ic} boundaries provides the probability of interaction between Σ3{sup n} boundaries. This interaction is responsible for some different types of triple junctions, the increase in Σ9 and Σ27 boundary fractions and interrupted connectivity of the network of random HABs. However, the Σ3{sub c} boundaries' consumption caused by the migration of random HABs and the difficulty of forming new Σ3{sub c} boundaries lead to the decreased fraction of Σ3{sub c} boundaries. The further discussion about the increase in the fraction of Σ3{sub ic} boundaries indicates that the generation mechanism of the Σ3{sub ic} boundaries during the aging treatment differs from the models applied to recrystallization and subsequent grain growth processes.

36 MATERIALS SCIENCE↗

Exploration of Sn 70 Li 30 alloy as possible material for flowing liquid metal plasma facing components

As an advanced alternative to solid materials, Liquid Metals (LM) may offer more resilient and feasible Plasma Facing Components (PFCs). Particularly, regarding the unavoidable material erosion/degradation produced by particle/heat fluxes in future fusion devices where much longer duty cycles are expected. Furthermore, configurations that propose a flowing LM surface can add the advantage of a continuously fresh and clean layer facing the plasma. Although lithium is the most widely tested option, tin-lithium (SnLi) alloys have been proposed to attempt to combine the positive characteristics of both pure elements and ameliorate the specific issues of lithium. In this work, the potential use of Sn70Li30 alloy in such flowing concepts has been explored by addressing several preliminary and mandatory aspects for its utilization. Key issues such as wettability and compatibility of the alloy with relevant substrates have been studied in a multidisciplinary approach. The data obtained from deposited liquid tin-lithium droplets indicates approximate wetting temperatures of 360 °C, 390 °C and 405 °C for the fresh alloy on 316 stainless steel, molybdenum, and tungsten, respectively. However, the alloy contamination appeared to strongly affect the wetting characteristics of materials, increasing their wetting temperature by ~130 °C in the worst observed cases. Interestingly, in some instances, the instability of the liquid alloy surface was observed in the form of sudden gaseous ejection. The deposited droplets were posteriorly characterized in terms of absolute composition and depth profile by Inductively Coupled PlasmaOptical Emission Spectroscopy (ICP-OES) and Secondary Ion Mass Spectrometry (SIMS-ToF). Additionally, the nature and composition of the boundaries between the substrates and alloy microparticles was investigated by Scanning Electron Microscopy (SEM), Energy Dispersive X-Ray Spectroscopy (EDS), and 3D Laser microscopy. The overall results of this post-mortem characterization revealed that first signs of corrosion induced by both alloy elements (lithium-chromium association and iron-tin intermetallic mixing) were present on 316 stainless steel after short exposures (≤3 h) at temperatures lower than 550 °C. Conversely, molybdenum and tungsten showed good compatibility with the alloy in equivalent conditions. The global implications of these results are finally addressed, focusing on the future perspectives and the more viable scenarios for the eventual utilization of these alloys in flowing liquid metal configurations.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Corrosion susceptibility and chromium loss in Austenitic steels and Nickel-based alloys in molten FLiNaK at 700 °C

A comparative study was conducted to evaluate the corrosion susceptibility of 316L, 316H, Ni 200, Inconel 625, and Hastelloy N in molten FLiNaK at 700 °C for 100 h. Top-view and cross-sectional scanning electron microscopy (SEM) imaging, combined with energy-dispersive X-ray spectroscopy (EDS) mapping, was performed to investigate microstructural and compositional changes. SEM images were further processed by introducing a contrast threshold to map cavity distribution. Using EDS mapping, intergranular and intragranular Cr loss were separately characterized. The ranking of mass loss after corrosion, from highest to lowest, is as follows: 316H > 316L > Inconel 625 > Hastelloy N > Ni 200. Cr loss was found to be correlated with Mo concentration, in agreement with many previous studies, with higher Mo content resulting in reduced Cr loss. On the other hand, there is no evidence that the high carbon content in 316H enhances corrosion resistance. The relatively low solubility of carbon in austenite at the testing temperature limits the amount of dissolved carbon. Therefore, the carbon-retarded vacancy diffusion, and consequently the reduced Cr diffusion, were not observed.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Development of Coatings for Tantalum Alloy Nozzle Vanes

A group of silicide coatings developed for the T222 tantalum-base alloy have afforded over 600 hours of protection at 1600 and 2400 F during cyclic exposure in air. These coatings were applied in two steps. A modifier alloy was applied by slurry techniques and was sintered in vacuum prior to siliciding by pack cementation in argon. Application of the modifier alloy by pack cementation was found to be much less effective. The addition of titanium and vanadium to molybdenum and tungsten yielded beneficial modifier alloys, whereas the addition of chromium showed no improvement. After siliciding, the 15Ti- 35W-15V-35Mo modifier alloy exhibited the best performance; one sample survived 1064 hours of oxidation at 2400 F. This same coating was the only coating to reproducibly provide 600 hours of protection at both 1600 and 2400 F; in the second and third of three experiments, involving oxidation of three to five specimens at each temperature in each experiment, no failures were observed in 600 hours of testing. The slurry coatings were also shown to protect the Cb752 and D43 columbium-base alloys.

PROTECTIVE COATING↗

Development of Fe-9Cr Alloy via High-Energy Ball Milling and Spark Plasma Sintering

Iron and chromium powders were mixed and mechanically alloyed via high-energy ball milling for different time durations (2–20 h) to produce an alloy powder with a nominal composition of Fe-9Cr (wt.%). The milled Fe-9Cr powders were analyzed using scanning electron microscopy (SEM), x-ray diffraction (XRD) and transmission electron microscopy (TEM) to understand the impact of ball milling (BM) time on the characteristics of the milled powder. The optimized milled powder samples were then consolidated via spark plasma sintering (SPS) for different dwell times and temperatures. The density of consolidated samples was found to reach a maximum of 98%. Microstructural characterization of the SPS samples were performed using XRD, SEM, TEM and electron backscatter diffraction. This study highlights the principles and importance of high-energy BM and SPS of Fe-9Cr model alloy for the future development of more complex oxide dispersion-strengthened alloys for various applications including advanced nuclear reactor applications.

36 MATERIALS SCIENCE↗

Enhancement in ordering of Fe{sub 50}Pt{sub 50} film caused by Cr and Cu additives

A 100-nm-thick Fe{sub 50}Pt{sub 50} film with high coercivity was fabricated by magnetron sputtering. On introducing a Cr top/bottom layer, the ordering temperature (T{sub or}) of the film decreased considerably from 500 to 380 deg. C. On introducing both Cr top/bottom layer and a 0.2-nm-thick Cu interlayer, the T{sub or} decreased even further to 340 deg. C. During the annealing process, the number of Cr atoms diffused into the Fe{sub 50}Pt{sub 50} layer increased. This increased the Fe diffusivity, lowering the T{sub or} in the process. The diffusion of the additive and the effects of annealing were verified by selected-area electron diffraction observations and by investigating the temperature dependence of the magnetization. The superlattice structure of the ordered Fe{sub 50}Pt{sub 50} film containing Cr and Cu additives was confirmed by the transmission electronic microscopy. Because of the Cr and Cu additives, the average grain size in the ordered Fe{sub 50}Pt{sub 50} film increased slightly; however, the coercivity of the ordered Fe{sub 50}Pt{sub 50} film is improved considerably.

36 MATERIALS SCIENCE↗

Durability and degradation of HT9 based alloy waste forms with variable Ni and Cr content

Short-term electrochemical and long-term hybrid electrochemical corrosion tests were performed on alloy waste forms in reference aqueous solutions that bound postulated repository conditions. The alloy waste forms investigated represent candidate formulations that can be produced with advanced electrochemical treatment of used nuclear fuel. The studies helped to better understand the alloy waste form durability with differing concentrations of nickel and chromium, species that can be added to alloy waste forms to potentially increase their durability and decrease radionuclide release into the environment.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Invar and Elinvar type amorphous Fe-Cr-B alloys with high corrosion resistance

Amorphous (Fe(1-x)Cr(x))85B15 alloys (x = 0 to 0.15) were prepared from the melts by rapid quenching using a single roller techinque, and their Invar and Elinvar characteristics and corrosion resistance were investigated. With an increase in chromium content the Curie temperature and the saturation magnetic moment per iron atom decreased monotonically, while the crystallization temperature incresed gradually. The thermal expansion coefficient alpha around room temperature became slightly larger with increasing chromium content. Nevertheless, these amorphous alloys exhibited excellent Invar characteristics below the Curie temperature. The value of Young's modulus increased remarkably in a relatively low magnetic field and then saturated at a field of about 80 kA/m, showing a large delta E effect. Its value as well as a longitudinal linear magnetostriction became smaller with an increase in chromium content. The temperature coefficient of Young's modulus changed from postive to negative, and the temperature range showing the Elinvar characteristics became narrower with chromium content. The temperature coefficient of delay time determined from the values of alpha and e was very small. The corrosion resistance of these alloys was extremely improved by chromium addition.

Kikuci, M.↗

Serrated Yielding in Alloy 709 at 500 deg. C

Gen-IV nuclear power reactors are being designed to improve the efficiency, safety, reliability, and lifetime in comparison with the current fleet of nuclear power reactors. Hence, candidate structural materials for Gen-IV reactors need to have superior mechanical properties to withstand harsh reactor conditions including higher operating temperature, higher radiation dose, and extremely corrosive environment. Sodium Fast Reactor (SFR) is one of the Gen-IV reactor concepts and it has a high technology readiness level for deployment. It uses liquid sodium as coolant and fast neutron spectrum to induce fission with core outlet temperature of no higher than 550 deg. C. In general, austenitic stainless steels have an excellent corrosion resistance and good creep properties due to high chromium and nickel contents. Alloy 709 is an austenitic stainless steel with base Fe-20Cr-25Ni stabilized with nitrogen and strengthened with niobium. Its excellent mechanical properties relative to similar steels (304 and 316) including high strength at elevated temperature, corrosion resistance, thermal stability, sodium compatibility and creep properties make it an excellent candidate material for the nth-of-a-kind SFR structural applications. Understanding the plastic deformation behavior at service temperature for Alloy 709 is essential to predict the performance of the material under the operating conditions. In this study, the effects of the temperature and strain-rate on the uniaxial quasi-static tensile plastic deformation of Alloy 709 are discussed with special emphasis on dynamic strain aging and work hardening behavior.

36 MATERIALS SCIENCE↗

Investigation of Additive Manufactured GRCop-42 Alloy Developed by Directed Energy Deposition Methods

GRCop is an alloy family constructed of copper, chromium, and niobium and was developed by NASA for high heat flux applications. GRCop-alloys were specifically formulated for the requirements in channel-cooled main combustion chambers allowing for repeat use in high heat flux environments[1]. GRCop-84 was evolved using additive manufacturing techniques under a NASA development program. To further increase thermal conductivity while maintaining material strength characteristics, the percentage of alloying elements were cut in half and GRCop-42 was developed. In recent years, NASA has successfully additively manufactured GRCop-42 with comparable material characteristics to extrudedGRCop-42 using a Laser Powder Bed Fusion (L-PBF) process. Benefits of this process include fabrication of intricate internal cooling channels as well as a decrease in manufacturing time. However, there are some large disadvantages in using this process. The nature of the powder bed process imposes a strict volume constraint as well as an excessive amount of material inventory required. A Directed Energy Deposition (DED) process addresses these limitations while also speeding up the manufacturing process. With little data on how DED performs with GRCop-42, an investigation into the mechanical properties was conducted. More specifically, Blown Powder Directed Energy Deposition (BPD), was used to compare material properties to that of the L-PBF manufactured GRCop-42. The DED manufactured material was found to have less than 0.1% porosity. Tensile tests concluded that the DED manufactured GRCop-42 had lower tensile strengths at room temperature. The results point towards a process capable of producing fully dense parts capable of meeting mechanical strength requirements with some possible refinement of printing parameters.

GRCop-42↗