Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Alkali”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 559 records · Page 31

Understanding the Crystallographic Phase Relations in Alkali-Trihalogeno-Germanates in Terms of Ferroelectric or Antiferroelectric Arrangements of the Tetrahedral GeX 3 Units

The alkali-trihalogeno-germanates AGeX 3 with A: Rb or Cs and X a halogen (I, Br, Cl) along with the corresponding stannates (ASnX 3 ) and plumbates (APbX 3 ) reflect a large variety of crystal structures, some of which are of the perovskite type. These materials, better known as “halide perovskites” have recently gained worldwide attention as promising photovoltaic and more broadly opto-electronic materials. Yet, their stability problems relative to the non-perovskite phases are a major issue. It is shown that some of the phase relations in these materials can be understood in terms of the relative orientation of the GeX 3 tetrahedral units, which is ferroelectric (FE) in the perovskite phase but antiferroelectric (AFE) in the competing monoclinic phase. Electrostatic dipole interactions favor the AFE phase and the additional bond formation favors the FE phase. The change in phase is accompanied by a large change in band gap.

36 MATERIALS SCIENCE↗

The Effect of Mechanical State on the Equilibrium Potential of Alkali Metal/Ceramic Single–Ion Conductor Systems

The relationship between mechanical stress states and interfacial electrochemical thermodynamics of Li metal/Li 6.5 La 3 Zr 1.5 Ta 0.5 O 12 and Na metal/ Na-β”-Al 2 O 3 systems are examined in two experimental configurations with an applied uniaxial load; the solid electrolytes are pellets and the metal electrodes high-aspect-ratio electrodes. The experimental results demonstrate that 1) the change in equilibrium potential at the metal/electrolyte interface, when stress is applied to the metal electrode, is linearly proportional to the molar volume of the metal electrode, and 2) the mechanical stress in the electrolyte has a negligible effect on the equilibrium potential for an experimental setup in which the electrolyte is stressed and the electrode is left unstressed. Solid mechanics modeling of a metal electrode on a solid electrolyte pellet indicates that pressure and normal stress are within ≈0.5 MPa of each other for the high aspect ratio (≈1:100 thickness:diameter in our study) Li metal electrodes under loads that exceed yield conditions. Furthermore, this work should aid in advancing the quantitative understanding of alkali metal dendrite formation within incipient cracks and their subsequent growth, and pore formation upon stripping, both situations where properly accounting for the impact of mechanical state on the equilibrium potential is of critical importance for calculating the current distribution.

25 ENERGY STORAGE↗

Ultrasmall Zeolite L Crystals Prepared from Highly Interdispersed Alkali‐Silicate Precursors

Abstract The preparation of nanosized zeolites is critical for applications where mass‐transport limitations within microporous networks hinder their performance. Often the ability to generate ultrasmall zeolite crystals is dependent upon the use of expensive organics with limited commercial relevance. Herein, we report the generation of zeolite L crystals with uniform sizes less than 30 nm using a facile, organic‐free method. Time‐resolved analysis of precursor assembly and evolution during nonclassical crystallization highlights key differences among silicon sources. Our findings reveal that a homogenous dispersion of potassium ions throughout silicate precursors leads to the formation of a metastable nonporous phase, which undergoes an intercrystalline transformation to zeolite L. The generation of highly interdispersed alkali‐silicate precursors is seemingly critical to enhancing the rate of nucleation and facilitating the formation of ultrasmall crystal.

Li, Rui↗

Effect of Alkali Treatment on Mechanical and Morphological Properties of Pineapple Leaf Fibre/Polyester Composites

In this study, our aim is to analyze the influence of fibre treatments and different fibre loading on mechanical, physical and chemical properties of pineapple leaf fibre reinforced polyester composites (PALF/PE). Fibre treatments were carried out with 1 N NaOH and KOH for 1 h. The untreated and treated PALF/PE composites were fabricated with 25 wt%, 35 wt% and 45 wt% fibre loadings by compression molding technique. Fourier Transform Infrared Spectroscopy (FTIR) was used to understand the effects of chemical treatment on PALF mechanical test results revealed that 45 wt% of PALF/PE composites treated with NaOH showed a 35% increase in tensile strength compared to untreated PALF/PE composites. The tensile modulus and the flexural module are also the highest at 45 wt% of KOH treated composites. The highest impact strength of 70 J/m was obtained for PALF/PE composites with NaOH treated fibres at 25% fibre loading. The results show that the fibre treatments in terms of the flexural and inter-laminar shear strength of composites were not effective. SEM of the tensile fractured specimen of PALF/PE composites revealed the changes in fibre characteristics due to the alkali treatment and less fibre pull-out at higher fibre loading. Overall we conclude that 1 N NaOH, 45 wt% treated PALF/PE composites satisfactorily and effectively improved both the mechanical and morphological properties. Obtained composites would be promising for construction materials, furniture and automotive components due to their superior strength and modulus at higher fibre loading.

36 MATERIALS SCIENCE↗

Transformations of cyclohexa-1,4-diene under the action of biphenyl—alkali metal systems in THF. Synergistic acceleration by mixtures of lithium and sodium

In the interaction of cyclohexa-1,4-diene (1,4-CHD) with a mixture of biphenyl and metallic lithium or sodium in THF at 20 °C, three processes occur, viz., disproportionation of 1,4-CHD to form benzene and cyclohexene, dehydrogenation of 1,4-CHD to form benzene and molecular hydrogen, and dehydrogenation of 1,4-CHD to form benzene and lithium or sodium hydride. In the case of lithium on the use of an equimolar amount of biphenyl, the isomerization of 1,4-CHD to cyclohexa-1,3-diene is also observed. When the molar ratio Li(Na): Ph{sub 2} increases from 1 : 1 to 2 : 1, i.e., when the reaction is carried out in the presence of an alkali metal solid phase, the overall conversion of 1,4-CHD into benzene and cyclohexene increases. The use of mixtures of lithium and sodium leads to acceleration of the processes of the formation of benzene and cyclohexene. The possible mechanism of the synergistic effect found is discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Alkali-free bioactive glasses for bone tissue engineering: A preliminary investigation

An alkali-free series of bioactive glasses has been designed and developed in the glass system CaO-MgO-SiO2-P2O5-CaF2 along diopside (CaMgSi2O6) – fluorapatite [Ca5(PO4)3F] – tricalcium phosphate (3CaO•P2O5) join. The silicate network in all the investigated glasses is predominantly coordinated in Q2 (Si) units while phosphorus tends to remain in orthophosphate (Q0) environment. The in vitro bioactivity analysis of glasses has been made by immersion of glass powders in simulated body fluid (SBF) while chemical degradation has been studied in Tris-HCl in accordance with ISO-10993-14. Some of the investigated glasses exhibit hydroxyapatite (HA) formation on their surface with in 1-12 h of their immersion in SBF solution. The sintering and crystallization kinetics of glasses has been investigated by differential thermal analysis (DTA) and hot-stage microscopy (HSM), respectively while the crystalline phase evolution in resultant glass-ceramics (GCs) has been studied in the temperature range of 800-900 oC using powder X-ray diffraction (XRD) and scanning electron microscope (SEM). The cell growth and osteogenic differentiation for glasses has been studied in vitro on sintered glass powder compacts using rat bone marrow mesenchymal stem cells. The as designed glasses are ideal candidates for their potential applications in bone tissue engineering in the form of bioactive glasses as well as glass/GC scaffolds.

59 BASIC BIOLOGICAL SCIENCES↗

Adsorption of superplasticizer admixtures on alkali-activated slag pastes

Alkali-activated slag (AAS) binders are obtained by a manufacturing process less energy-intensive than ordinary Portland cement (OPC) and involves lower greenhouse gasses emission. These alkaline cements allow the production of high mechanical strength and durable concretes. In the present work, the adsorption of different superplasticizer admixtures (naphthalene-based, melamine-based and a vinyl copolymer) on the slag particles in AAS pastes using alkaline solutions with different pH values have been studied in detail. The effect of the superplasticizers on the yield stress and plastic viscosity of the AAS and OPC pastes have been also evaluated. The results obtained allowed us to conclude that the adsorption of the superplasticizers on AAS pastes is independent of the pH of the alkaline solutions used and lower than on OPC pastes. However, the effect of the admixtures on the rheological parameters depends directly on the type and dosage of the superplasticizer as well as of the binder used and, in the case of the AAS, on the pH of the alkaline activator solution. In 11.7-pH NaOH-AAS pastes the dosages of the superplasticizers required to attain similar reduction in the yield stress are ten-fold lower than for Portland cement. In this case the superplasticizers studied show a fluidizing effect considerably higher in 11.7-pH NaOH-AAS pastes than in OPC pastes. In 13.6-pH NaOH-AAS pastes, the only admixture observed to affect the rheological parameters is the naphthalene-based admixture due to its higher chemical stability in such extremely alkaline media.

36 MATERIALS SCIENCE↗

Concrete modelling for expertise of structures affected by alkali aggregate reaction

Alkali aggregate reaction (AAR) affects numerous civil engineering structures and causes irreversible expansion and cracking. In order to control the safety level and the maintenance cost of its hydraulic dams, Electricite de France (EDF) must reach better comprehension and better prediction of the expansion phenomena. For this purpose, EDF has developed a numerical model based on the finite element method in order to assess the mechanical behaviour of damaged structures. The model takes the following phenomena into account: concrete creep, the stress induced by the formation of AAR gel and the mechanical damage. A rheological model was developed to assess the coupling between the different phenomena (creep, AAR and anisotropic damage). Experimental results were used to test the model. The results show the capability of the model to predict the experimental behaviour of beams subjected to AAR. In order to obtain such prediction, it is necessary to take all the phenomena occurring in the concrete into consideration.

36 MATERIALS SCIENCE↗

Influence of steel fibers on the development of alkali-aggregate reaction

This work presents the results of an experimental research concerning the use of fibers in mortar specimens subjected to alkali-aggregate reaction (AAR). Two types of steel fibers (0.16 mm diameter and 6.0 mm length, and 0.20 mm diameter and 13.0 mm length) were used with fiber volume contents of 1% and 2%. Besides the expansion accelerated tests, compressive tests and flexural tests have also been carried out to display the main mechanical characteristics of the fiber-reinforced mortars after being subjected to AAR. Moreover, the microstructure of the specimens was analyzed by scanning electron microscopy and energy dispersive X-ray. The results shown that the addition of steel fibers reduced the expansion due to AAR for the experimental conditions studied in this paper. The most expressive benefit corresponded to the addition of 13.0 mm fibers in the mixture containing 2% fiber content. This fiber volume content also corresponded to the maximum increment in the mechanical properties compared to the reference mortar, mainly for the post-cracking strength and for the toughness in bending. It was observed that the fibers have a beneficial effect on the material, without compromising its main mechanical properties.

36 MATERIALS SCIENCE↗

Effect of moisture conditions and transfers on alkali silica reaction damaged structures

The aim of this paper is to point out the water driving effect on the alkali silica reaction (ASR) expansion and particularly when modifications of moisture conditions occur. After being submitted to a unidirectional moisture gradient during 14 months, the upper faces of ASR reactive beams were covered by water for 9 months. This late water supply on the upper face rapidly produced large expansions, which mainly occurred along the transverse and the vertical directions resulting in large longitudinal cracks. Companion nonreactive specimens were kept in the same environmental conditions in order to quantify the basic characteristics of moisture-dependent expansive behaviour of the material. The paper focuses on the effects of late water supply or late drying on already ASR-damaged concrete, which is a significant concern for real-life structures. Both structural effects of late water supply on ASR progress in already damaged structures and interpretation of such phenomena are described.

36 MATERIALS SCIENCE↗

Density and water content of nanoscale solid C-S-H formed in alkali-activated slag (AAS) paste and implications for chemical shrinkage

Alkali-activated slag (AAS) paste was analyzed using small-angle neutron scattering (SANS). The scattering response indicates that the microstructure consists of a uniform matrix of hydration product with a high surface area studded with unhydrated cores of slag particles. In contrast with portland cement paste, no surface fractal scattering regime was detected, and elevated temperature curing (at 60 Degree-Sign C) had no detectable effect on the microstructure at any length scale studied. The specific surface area of the AAS pastes is about 25% higher than that of a portland cement paste cured under the same conditions. The composition and mass density of the nanoscale solid C-S-H phase formed in the AAS paste was determined using a previously developed neutron scattering method, in conjunction with a hydration model. The result ((CaO){sub 0.99}-SiO{sub 2}-(Al{sub 2}O{sub 3}){sub 0.06}-(H{sub 2}O){sub 0.97}, d = (2.73 {+-} 0.02) g/cm{sup 3}) is significantly lower in calcium and in water as compared to portland cement or pure tricalcium silicate paste. These values were used to calculate the chemical shrinkage that would result from complete hydration of the AAS paste. The result, (12.2 {+-} 1.5) cm{sup 3} of volumetric shrinkage per 100 g of unhydrated cement, is about twice the amount of chemical shrinkage exhibited by normal cement pastes.

36 MATERIALS SCIENCE↗

Stability of cenospheres in lightweight cement composites in terms of alkali-silica reaction

This paper presents an experimental study on characteristics and stability of cenospheres used in lightweight cement composites. ASTM C227 and C1260 tests were used to evaluate if cenospheres are potentially deleterious due to alkali-silica reaction (ASR). Natural sand was used as control. Examination by scanning electron microscope with energy-dispersive X-ray spectroscopy and analyses by X-ray diffractometer and thermogravimetry were conducted on samples with cenospheres after 9-month C227 and C1260 tests to better understand the behavior of cenospheres exposed to high alkaline environments and higher temperatures in these tests. Results indicate that cenospheres are not potentially deleterious due to ASR. Expansion of the mortar specimens tested to ASTM C227 and C1260 seems to be affected by the pozzolanic reactivity of cenospheres. Fine cenospheres showed limited pozzolanic reactivity at 28-30 Degree-Sign C and 38 Degree-Sign C, but exhibited significant pozzolanic reactivity at 80 Degree-Sign C with aluminum tobermorite [Ca{sub 5}Si{sub 5}Al(OH)O{sub 17} Bullet-Operator 5H{sub 2}O] identified as the main reaction product.

36 MATERIALS SCIENCE↗

Retention of alkali ions by hydrated low-pH cements: Mechanism and Na{sup +}/K{sup +} selectivity

Low-pH cements, also referred to as low-alkalinity cements, can be designed by replacing significant amounts of Portland cement by pozzolanic materials. Their pore solution is characterized by a pH near 11, and an alkali concentration much lower than that of Portland cement. This work investigates the retention of sodium and potassium by a hydrated low-pH cement comprising 60% Portland cement and 40% silica fume. It is shown that sorption of potassium is higher than that of sodium and mainly results from counterion charge balancing of the C-S-H negative surface charge. To explain the greater retention of potassium compared to sodium, it is postulated that potassium, unlike sodium, may enter the interlayer of C-S-H to compensate the negative charges in the interlayer, in addition to the external surfaces. This assumption is supported by structural characterization of C-S-H using X-ray diffraction.

36 MATERIALS SCIENCE↗

A coupled mechanical and chemical damage model for concrete affected by alkali–silica reaction

To model the complex degradation phenomena occurring in concrete affected by alkali–silica reaction (ASR), we formulate a poro-mechanical model with two isotropic internal variables: the chemical and the mechanical damage. The chemical damage, related to the evolution of the reaction, is caused by the pressure generated by the expanding ASR gel on the solid concrete skeleton. The mechanical damage describes the strength and stiffness degradation induced by the external loads. As suggested by experimental results, degradation due to ASR is considered to be localized around reactive sites. The effect of the degree of saturation and of the temperature on the reaction development is also modeled. The chemical damage evolution is calibrated using the value of the gel pressure estimated by applying the electrical diffuse double-layer theory to experimental values of the surface charge density in ASR gel specimens reported in the literature. The chemo-damage model is first validated by simulating expansion tests on reactive specimens and beams; the coupled chemo-mechanical damage model is then employed to simulate compression and flexure tests results also taken from the literature. -- Highlights: •Concrete degradation due to ASR in variable environmental conditions is modeled. •Two isotropic internal variables – chemical and mechanical damage – are introduced. •The value of the swelling pressure is estimated by the diffuse double layer theory. •A simplified scheme is proposed to relate macro- and microscopic properties. •The chemo-mechanical damage model is validated by simulating tests in literature.

36 MATERIALS SCIENCE↗

The effects of lithium ions on chemical sequence of alkali-silica reaction

This paper presents the results of the investigation on the effects of Li{sup +} ions on the chemical and physical changes in the cementitious system undergoing alkali-silica reaction (ASR). Specifically, this paper focuses on determining which chemical steps of ASR processes are affected by the presence of Li{sup +} ions in the pore solution in order to provide better understanding of the role of Li{sup +} ions in the mitigation process of ASR. The results presented in this paper strongly support the hypothesis that the Li{sup +} ions facilitate the formation of a physical barrier on the surface of reactive silica, and thus prevent further attack on the reactive sites by hydroxyl ions.

36 MATERIALS SCIENCE↗

Influence of fiber inclination angle on bond-slip behavior of different alkali-activated composites under dynamic and quasi-static loadings

This study investigates the influence of inclination angle (0° and 45°) on the interfacial bond-slip behavior of macro steel fibers (straight, hooked end-deformed and length-deformed) and length-deformed polypropylene fibers reinforced in fly-ash and metakaolin based alkali-activated composites (AACs) under quasi-static and dynamic loadings. AACs demonstrate superior peak bond strength and toughness compared to cement composites regardless of fiber type and loading rate. Results also show that straight steel fiber exhibits a complete pullout in AACs. The amount of deformation of the fibers (deformation ratio) determined the failure type at different inclination angle and loading rate, thus governing the peak load and energy absorption. Depending on the fiber orientation, premature fiber rupture or matrix cracking is observed under dynamic loading in AACs due to matrix brittleness. The fiber failure modes in dynamic pullout are no different from those observed in the quasi-static pullout in AACs.

36 MATERIALS SCIENCE↗

Sulfuric acid resistance of one-part alkali-activated mortars

One-part alkali-activated (geopolymer) mortars based on three different silica-rich starting materials and sodium aluminate, with and without ground granulated blast furnace slag (GGBFS) addition, were tested regarding sulfuric acid resistance according to DIN 19573:2016-03 (70 days at pH = 1). Corresponding pastes were characterized by XRD, SEM, chemical analysis, {sup 29}Si MAS NMR and {sup 1}H-{sup 29}Si CPMAS NMR after water storage and after acid exposure. The mortars exhibited a high resistance against sulfuric acid attack, with the best ones conforming to the requirements of DIN 19573:2016-03. The analytical results showed that this was due to precipitation of silica gel at the acid-mortar interface, which formed a mechanically stable layer that protected the subjacent mortar and thus inhibited further degradation. The addition of GGBFS decreased the acid resistance via formation of expansive calcium sulfate phases.

36 MATERIALS SCIENCE↗

Performance of fly ash concrete with ferronickel slag fine aggregate against alkali-silica reaction and chloride diffusion

Ferronickel slag (FNS) is an industrial by-product of ferronickel alloy production at a high temperature which can be a promising potential to be used as fine aggregate to produce more sustainable concrete. In this study, the performance of concrete containing ferronickel slag sand and fly ash relating to alkali-silica reaction (ASR) and chloride contamination was investigated. ASR-induced expansion, chloride diffusion resistance, and chloride binding capacity of FNS concrete were determined through concrete prism tests (CPT), accelerated diffusion test, and bulk diffusion test. Thermogravimetric analysis (TGA) was conducted to measure the amount of Portlandite and Friedel's salt in concrete. Concrete with 50 wt% FNS sand as fine natural aggregate replacement and 25 wt% of cement replacement by fly ash showed a remarkable potential to be used not only as a low-carbon concrete with comparable mechanical properties to conventional concrete but also with a better performance against ASR and chloride contamination.

36 MATERIALS SCIENCE↗