Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “welding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

Abnormal macropore formation during double-sided gas tungsten arc welding of magnesium AZ91D alloy

One of the major concerns during gas tungsten arc (GTA) welding of cast magnesium alloys is the presence of large macroporosity in weldments, normally thought to occur from the presence of gas in the castings. In this study, a double-sided GTA welding process was adopted to join wrought magnesium AZ91D alloy plates. Micropores were formed in the weld zone of the first side that was welded, due to precipitation of H{sub 2} as the mushy zone freezes. When the reverse side was welded, the heat generated caused the mushy zone in the initial weld to reform. The micropores in the initial weld then coalesced and expanded to form macropores by means of gas expansion through small holes that are present at the grain boundaries in the partially melted zone. Macropores in the partially melted zone increase with increased heat input, so that when a filler metal is used the macropores are smaller in number and in size.

36 MATERIALS SCIENCE↗

A model of material flow during friction stir welding

Tin plated 6061-T6 aluminum extrusions were friction stir welded in a 90 deg. butt-weld configuration. A banded microstructure of interleaved layers of particle-rich and particle-poor material comprised the weld nugget. Scanning and transmission electron microscopy revealed the strong presence of tin within the particle-rich bands, but TEM foils taken from the TMAZ, HAZ and base material showed no indication of Sn-containing phases. Since tin is limited to the surface of the pre-weld extrusions, surface material flowed into the nugget region, forming the particle-rich bands. Similarly, the particle-poor bands with no tin originated from within the thickness of the extrusions. A model of material flow during friction stir welding is proposed for which the weld nugget forms as surface material extrudes from the retreating side into a plasticized zone surrounding the FSW pin. The extruded column buckles between the extrusion force driving the material into the zone and the drag force of the in-situ material resisting its entry. A banded microstructure of interleaved surface material and in-situ material, therefore, develops. The model successfully describes several of the experimentally observed weld characteristics, but the model is limited to specific conditions of material flow and assumptions regarding steady-state.

36 MATERIALS SCIENCE↗

Effects of heat input on microstructure and tensile properties of laser welded magnesium alloy AZ31

A 3 kW CO{sub 2} laser beam was used to join wrought magnesium alloy AZ31 sheets, and the effects of heat input on the quality of butt welding joints were studied. By macro and microanalysis, it is found that the welding heat input plays an important role in laser welding process for AZ31 wrought sheets. After welding, the grains far from the weld centre present the typical rolled structure. But the microstructure out of the fusion zone gradually changes to complete equiaxed crystals as the distance from the weld centre decreases. Adjacent to the fusion boundary, there is a band region with columnar grains, and its growth direction is obviously perpendicular to the solid/liquid line. The microstructure in fusion centre consists of fine equiaxed grains and the many precipitated particles are brittle phase Mg{sub 17}Al{sub 12} or Mg{sub 17}(Al,Zn){sub 12}. With increasing the heat input, the band width of columnar grains varies, the grains in fusion zone get coarser, and the distribution of precipitates changes from intragranularly scattered particles to intergranularly packed ones. The results of tensile test show that the change trend of ultimate tensile strength (UTS) and elongation of the welded joints is to increase at first and then decrease with the heat input increasing. When the heat input reaches 24 J mm{sup -1}, the maximum value of the UTS is up to 96.8% of the base metal.

36 MATERIALS SCIENCE↗

Abnormal distribution of microhardness in tungsten inert gas arc butt-welded AZ61 magnesium alloy plates

In this study, the effects of heat input on the distribution of microhardness of tungsten inert gas (TIG) arc welded hot-extruded AZ61 magnesium alloy joints were investigated. The results show that with an increase of heat input, the distributions of microhardness at the top and bottom of the welded joints are different because they are determined by both the effect of grain coarsening and the effect of dispersion strengthening. With an increase of the heat input, the microhardness of the heat-affected zone (HAZ) at the top and bottom of welded joints and the fusion zone (FZ) at the bottom of welded joints decreased gradually, while the microhardness of the FZ at the top of welded joints decreased initially and then increased sharply. The reason for the abnormal distribution of microhardness of the FZ at the top of the welded joints is that this area is close to the heat source during welding and then large numbers of hard {beta}-Mg{sub 17}(Al,Zn){sub 12} particles are precipitated. Hence, in this case, the effect of dispersion strengthening dominated the microhardness.

36 MATERIALS SCIENCE↗

Effect of heat input on dissimilar welds of ultra high strength steel and duplex stainless steel: Microstructural and compositional analysis

The effect of heat input on the microstructure and compositional heterogeneity of welds of direct-quenched ultra high strength steel (Optim 960 QC) and duplex stainless steel (UNS S32205) was studied. The dissimilar welds were made using GMAW with a fully austenitic filler wire. In addition to grain coarsening in the heat affected zone (HAZ) of the ferritic side, it was found that an increase in heat input correlatively increased the proportional volume of bainitic to martensitic phases. Coarse ferritic grains were observed in the duplex HAZ. Higher heat input, however, had a beneficial effect on the nucleation of austenite in the HAZ. Heat input had a regulatory effect on grain growth within the austenitic weld and more favorable equiaxed austenite was obtained with higher heat input. On the ferritic side of the welds, macrosegregation in the form of a martensitic intermediate zone was observed for all the cooling rates studied. However, on the duplex side, macrosegregation in the fusion boundary was only noticed with higher cooling rates. Microstructural observations and compositional analysis suggest that higher heat input could be beneficial for the structural integrity of the weld despite higher heat input increasing the extent of adverse coarse grains in the HAZ, especially on the ferritic side. - Highlights: •The effect of heat input on dissimilar welds of UHSS and DSS was studied. •Transmutation of the microstructure was discussed in detail. •The influence of heat input on compositional heterogeneity of welds was described. •Higher heat input enhanced bainitic transformation on the ferritic side. •Macrosegregation was affected by the amount of heat input on the DSS side.

36 MATERIALS SCIENCE↗

Impact of initial temper of base metal on microstructure and mechanical properties of friction stir welded AA 7055 alloy

Highlights: • Friction stir welded 7055-T4 alloy exhibits higher tensile properties than T6 alloy. • Friction stir welded 7055-T4 alloy exhibits more uniform hardness distribution. • Some regions in heat affected zone have higher hardness than base metal in T4-joint. • Effect of initial temper on precipitate evolution in different zones is discussed. AA 7055-T6 and AA 7055-T4 aluminium alloy sheets were friction stir welded to investigate the impact of initial base metal temper on microstructure, hardness and tensile properties of the joints. In the joint of alloy in T6 temper (T6-joint), the hardness of the weld zone is lower than that of base metal; in the joint of alloy in T4 temper (T4-joint), however, some regions in the heat affected zone exhibit higher hardness than base metal. The weld nugget zone in T6-joint exhibits slightly lower hardness compared with that in T4-joint. The hardness minima is slightly higher in T4-joint than in T6-joint. T4-joint exhibits higher yield strength, ultimate tensile strength and elongation compared with T6-joint. Based on microstructure examination by transmission electron microscopy, the impact of initial precipitate state on precipitation behavior in the weld nugget zone, thermo-mechanically affected zone and heat affected zone during friction stir welding and mechanical properties of the joints is discussed.

36 MATERIALS SCIENCE↗

APPLICATION OF LARGE APERTURE EMATS TO WELD INSPECTION

One of the most significant developments in EMAT operation is the incorporation of phased array techniques. Phased array EMATs enable electronic beam steering and focusing while operating with temporally short pulses for good range resolution. Using phased array EMAT operation, multiple high powered pulsers are combined in the generation of the ultrasonic wave and multiple elements are combined in the reception of the ultrasonic wave, for improved sensitivity. EMATs make it practical to operate with shear horizontal (SH) waves and scan over a metal part's surface. An EMAT generated line force at the surface launches shear horizontal waves with uniform amplitude for beam angles from -90 deg. to 90 deg. Shear horizontal waves also reflect without mode conversion from surfaces that are parallel to the polarization of the shear wave displacements. The combination of these advantages makes phased array EMATs well suited for weld inspection. Recently, BWXT Services has developed a 32 active channel EMAT phased array system for operation up to 5 MHz. In addition, each element can be constructed with several sub-elements, alternating in polarity, to effectively multiply the number of active elements for a restricted range of beam angles. For example by using elements comprised of 4 sub elements, a 128 active element aperture designed for operation with a nominal 60 deg. beam angle provides good beam steering and focusing performance for 45 deg. to 70 deg. beam angles. The large active apertures allow the use of highly focused beams for good defect detection and high resolution imaging of weld defects. Application of this system to weld inspections has verified that good defect detection and imaging is possible. In addition, operation with SH waves has proven to provide improved detection of lack of fusion at the cap and root of the weld for certain weld geometries. The system has also been used to demonstrate the inspection of submerged metal arc welds while welding.

36 MATERIALS SCIENCE↗

Dissimilar Friction Stir Welds in Al5186-Al2024: The Effect of Process Parameters on Microstructures and Mechanical Properties

The effect of tool traverse and rotation speeds on the microstructures and mechanical properties are quantified for welds between non-age-hardening Al5083 and age hardening Al2024 and compared to single alloy joints made from each of the two constituents. In this paper, we report the results of microstructural, mechanical property investigations of Al5186-Al2024 friction stir welds produced using various rotations and traveling speeds of the tool to investigate the effects of the welding parameters on the joint strength. Metallographic studies by optical microscopy, electron probe microscopy, and the utilization of the X-ray diffraction technique have been conducted. It was found that the weld properties were dominated by the thermal input rather than the mechanical deformation by the tool. In particular the larger stresses under the weld tool on the AA5186 side compared to the AA2024 side are related to a transient reduction in yield stress due to dissolution of the hardening precipitates during welding prior to natural aging after welding.

36 MATERIALS SCIENCE↗

Development of a pseudo phased array technique using EMATs for DM weld testing

Ultrasonic inspection of dissimilar metal (DM) welds in piping with cast austenitic stainless steel (CASS) has been an area ongoing research for many years given its prevalence in the petrochemical and nuclear industries. A typical inspection strategy for pipe welds is to use an ultrasonic phased array system to scan the weld from a sensor located on the outer surface of the pipe. These inspection systems generally refract either longitudinal or shear vertical (SV) waves at varying angles to inspect the weld radially. In DM welds, however, the welding process can produce a columnar grain structure in the CASS material in a specific orientation. This columnar grain structure can skew ultrasonic waves away from their intended path, especially for SV and longitudinal wave modes. Studies have shown that inspection using the shear horizontal (SH) wave mode significantly reduces the effect of skewing. Electromagnetic acoustic transducers (EMATs) are known to be effective for producing SH waves in field settings. This paper presents an inspection strategy that seeks to reproduce the scanning and imaging capabilities of a commercial phase array system using EMATs. A custom-built EMAT was used to collect data at multiple propagation angles, and a processing strategy known as the synthetic aperture focusing technique (SAFT) was used to combine the data to produce an image. Results are shown using this pseudo phased array technique to inspect samples with a DM weld and artificial defects, demonstrating the potential of this approach in a laboratory setting. Recommendations for future work to transition the technique to the field are also provided.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Non-circular electron beam spot welds in stainless steel alloys

Circularly symmetric-shaped spot welds are desirable for welding applications as they relate to heat and fluid flow conditions in the melt pool with predictable weld penetrations and repeatable results. Non-circular spot welds on the other hand result in undesirable and unpredictable weld penetrations or non-bridging of the liquid melt pool across the joint. Two known causes for non-circular melt pools occur when welding dissimilar metals, or when welding with skewed electron or laser beams that are not perpendicular to the surface. A largely unexplored additional factor, shown here, is an asymmetric power density distribution within the beam that can create non-circular melt pools even though the beam dimensions are much smaller than the melt pool itself.

36 MATERIALS SCIENCE↗

Friction Stir Spot Welding of DP780 Carbon Steel

Friction stir spot welds were made in uncoated and galvannealed DP780 sheets using polycrystalline boron nitride stir tools. The tools were plunged at either a single continuous rate or in two segments consisting of a relatively high rate followed by a slower rate of shorter depth. Welding times ranged from 1 to 10 s. Increasing tool rotation speed from 800 to 1600 rev min{sup -1} increased strength values. The 2-segment welding procedures also produced higher strength joints. Average lap shear strengths exceeding 10 {center_dot} 3 kN were consistently obtained in 4 s on both the uncoated and the galvannealed DP780. The likelihood of diffusion and mechanical interlocking contributing to bond formation was supported by metallographic examinations. A cost analysis based on spot welding in automobile assembly showed that for friction stir spot welding to be economically competitive with resistance spot welding the cost of stir tools must approach that of resistance spot welding electrode tips.

36 MATERIALS SCIENCE↗

Progress Report for Diffusion Welding of the NGNP Process Application Heat Exchangers (Revision 1)

The U.S. Department of Energy selected the high temperature gas-cooled reactor as the basis for the Next Generation Nuclear Plant (NGNP). The NGNP will demonstrate the use of nuclear power for electricity, hydrogen production, and process heat applications. The NGNP Project is currently investigating the use of metallic, diffusion welded, compact heat exchangers to transfer heat from the primary (reactor side) heat transport system to the secondary heat transport system. An intermediate heat exchanger will transfer this heat to downstream applications such as hydrogen production, process heat, and electricity generation. The channeled plates that make up the heat transfer surfaces of the intermediate heat exchanger will have to be assembled into an array by diffusion welding. This report describes the preliminary results of a scoping study that evaluated the diffusion welding process parameters and the resultant mechanical properties of diffusion welded joints using Alloy 800H. The long-term goal of the program is to progress towards demonstration of small heat exchanger unit cells fabricated with diffusion welds. Demonstration through mechanical testing of the unit cells will support American Society of Mechanical Engineers rules and standards development, reduce technical risk, and provide proof of concept for heat exchanger fabrication methods needed to deploy heat exchangers in several potential NGNP configurations.1 Researchers also evaluated the usefulness of modern thermodynamic and diffusion computational tools (Thermo-Calc and Dictra) in optimizing the parameters for diffusion welding of Alloy 800H. The modeling efforts suggested a temperature of 1150°C for 1 hour with an applied pressure of 5 MPa using 15 μm nickel foil as joint filler to reduce chromium oxidation on the welded surfaces. Good agreement between modeled and experimentally determined concentration gradients was achieved

08 HYDROGEN↗

Review of Dissimilar Metal Welding for the NGNP Helical-Coil Steam Generator

The U.S. Department of Energy (DOE) is currently funding research and development of a new high temperature gas cooled reactor (HTGR) that is capable of providing high temperature process heat for industry. The steam generator of the HTGR will consist of an evaporator economizer section in the lower portion and a finishing superheater section in the upper portion. Alloy 800H is expected to be used for the superheater section, and 2.25Cr 1Mo steel is expected to be used for the evaporator economizer section. Dissimilar metal welds (DMW) will be needed to join these two materials. It is well known that failure of DMWs can occur well below the expected creep life of either base metal and well below the design life of the plant. The failure time depends on a wide range of factors related to service conditions, welding parameters, and alloys involved in the DMW. The overall objective of this report is to review factors associated with premature failure of DMWs operating at elevated temperatures and identify methods for extending the life of the 2.25Cr 1Mo steel to alloy 800H welds required in the new HTGR. Information is provided on a variety of topics pertinent to DMW failures, including microstructural evolution, failure mechanisms, creep rupture properties, aging behavior, remaining life estimation techniques, effect of environment on creep rupture properties, best practices, and research in progress to improve DMW performance. The microstructure of DMWs in the as welded condition consists of a sharp chemical concentration gradient across the fusion line that separates the ferritic and austenitic alloys. Upon cooling from the weld thermal cycle, a band of martensite forms within this concentration gradient due to high hardenability and the relatively rapid cooling rates associated with welding. Upon aging, during post weld heat treatment (PWHT), and/or during high temperature service, C diffuses down the chemical potential gradient from the ferritic 2.25Cr 1Mo steel toward the austenitic alloy. This can lead to formation of a soft C denuded zone near the interface on the ferritic steel, and nucleation and growth of carbides on the austenitic side that are associated with very high hardness. These large differences in microstructure and hardness occur over very short distances across the fusion line (~ 50 100 ?m). A band of carbides also forms along the fusion line in the ferritic side of the joint. The difference in hardness across the fusion line increases with increasing aging time due to nucleation and growth of the interfacial carbides. Premature failure of DMWs is generally attributed to several primary factors, including: the sharp change in microstructure and mechanical properties across the fusion line, the large difference in coefficient of thermal expansion (CTE) between the ferritic and austenitic alloys, formation of interfacial carbides that lead to creep cavity formation, and preferential oxidation of the ferritic steel near the fusion line. In general, the large gradient in mechanical properties and CTE serve to significantly concentrate the stress along the fusion where a creep susceptible microstructure has evolved during aging. Presence of an oxide notch can concentrate the stress even further. Details of the failure mechanism and the relative importance of each factor varies.

2.25Cr-1Mo↗

Enhancing NDE Reliability for Grade 91 Steel Welds: Ultrasonic Imaging and Microstructural Correlations

Ensuring the integrity of Grade 91 (9Cr-1Mo-V) steel welds is vital for the safe and reliable operation of fossil fuel–fired and nuclear power plants. Here, this study applies an imaging technique for the ultrasonic characterization of two Grade 91 steel welds created with cold metal transfer and flux-cored arc welding processes. Ultrasonic immersion testing in the through-transmission configuration was employed to generate shear waves, which helped identify the weld metal, heat-affected zone, and base metal regions. These weld microstructures were also correlated to their ultrasonic images using metallography, ultrasonic amplitude, hardness measurements, and grain size. The findings from this study can assist practitioners in developing new nondestructive evaluation technologies, improving the inspection reliability of creep strength–enhanced ferritic steel welds by potentially identifying weld microstructure regions susceptible to creep-type failures.

Grade 91 steel↗

Friction Stir Spot Welding (FSSW) of Advanced High Strength Steel (AHSS)

Friction stir spot welding (FSSW) is applied to join advanced high strength steels (AHSS): galvannealed dual phase 780 MPa steel (DP780GA), transformation induced plasticity 780 MPa steel (TRIP780), and hot-stamped boron steel (HSBS). A low-cost Si3N4 ceramic tool was developed and used for making welds in this study instead of polycrystalline cubic boron nitride (PCBN) material used in earlier studies. FSSW has the advantages of solid-state, low-temperature process, and the ability of joining dissimilar grade of steels and thicknesses. Two different tool shoulder geometries, concave with smooth surface and convex with spiral pattern, were used in the study. Welds were made by a 2-step displacement control process with weld time of 4, 6, and 10 seconds. Static tensile lap-shear strength achieved 16.4 kN for DP780GA-HSBS and 13.2kN for TRIP780-HSBS, above the spot weld strength requirements by AWS. Nugget pull-out was the failure mode of the joint. The joining mechanism was illustrated from the cross-section micrographs. Microhardness measurement showed hardening in the upper sheet steel (DP780GA or TRIP780) in the weld, but softening of HSBS in the heat-affect zone (HAZ). The study demonstrated the feasibility of making high-strength AHSS spot welds with low-cost tools.

36 MATERIALS SCIENCE↗

Maturation of In-space Welding in Reduced Gravity and Reduced Pressure Environments Through Progression to Suborbital Flight Experiments

Development of in-space welding (ISW) is a key and enabling manufacturing technology as welding is currently involved in producing approximately 90% of durable goods, and this trend is expected to hold for in-space manufacturing as well. ISW is critical to a sustainable space economy. To mature in-space welding, numerous gaps must be closed since NASA has not made a weld in space in 50 years. Advancing laser beam welding (LBW) towards a suborbital flight demonstration will help mature the process for in-space assembly & manufacturing (ISAM) through demonstration in relevant environments and achieving technology readiness milestones. LBW technologies and science improved by this work will benefit in-space manufacturing, long-term sustainability of space structures & operations, and the overall space economy. Ground-based welding of aerospace hardware requires an Edisonian approach to qualify a welding process; however, this approach is infeasible for ISW qualification due to mass, volume, logistic, and cost challenges inherent to the space environment. To address this challenge, we are conducting ground and suborbital tests with partners performing parabolic flights to gather data on LBW processes and infuse them into NASA & partner missions. This progression from ground to flight experiments will elucidate relevant physics during LBW: 1) reduced gravity, 2) reduced pressure, and 3) extreme temperature. Data from post-flight evaluation and in situ instrumentation will feed integrated computational materials engineering (ICME) tools to reduce the burden of ISW infusion by establishing a link between space and terrestrial environments, ultimately accelerating the qualification of LBW in space.

in-space welding↗

A New Path Forward for Understanding Microstructural Evolution during Welding

Over the past century, the principal method for estimating the sequence of microstructural events that produce the final weld microstructure has been postweld microstructure analysis, and it's the interpretation of these microstructures that sets welding metallurgy apart from other related endeavors. In conjunction with heat flow analysis and thermodynamic principles, the postweld microstructural interpretation of grain sizes and shapes, second-phase particles, interphase boundaries, and composition gradients provide the framework for interpreting the events that lead to the final microstructure. However, without direct and confirming evidence of the actual phases that exist during welding, multiple interpretations for microstructural evolution of welds often occur. For this reason, methods for the direct observation of the phases and phase transformations that occur during welding was developed. This paper summarizes the 2007 Adams Lecture titled 'A New Path for Understanding Microstructural Evolution during Welding Using Synchrotron Radiation,' where real-time X-ray diffraction methods were presented as a means for the direct observation of phase transformations during welding.

36 MATERIALS SCIENCE↗

Friction Stir Spot Welding of DP780 Carbon Steel

Friction stir spot welds were made in uncoated and galvannneled DP780 sheets using polycrystalline boron nitride stir tools. The tools were plunged at either a single continuous rate or in two segments consisting of a relatively high rate followed by a slower rate of shorter depth. Welding times ranged from 1-10 s. Increasing tool rotation speed from 800 to 1600 rpm increased strength values. The 2-segment welding procedures also produced higher strength joints. Average lap-shear strengths exceeding 10.3 kN were consistently obtained in 4 s on both the uncoated and the galvannealed DP780. The likelihood of diffusion and mechanical interlocking contributing to bond formation was supported by metallographic examinations. A cost analysis based on spot welding in automobile assembly showed that for friction stir spot welding to be economically competitive with resistance spot welding the cost of stir tools must approach that of resistance spot welding electrode tips.

36 MATERIALS SCIENCE↗