Improvement of (004) texturing by slow growth of Nd doped TiO{sub 2} films
In this work, we present preferred (004) texturing of sputter deposited titanium dioxide (TiO{sub 2}) films on glass substrates as a consequence of Nd doping at very slow growth rate. Nd concentration was varied from 0.0 to 2.0 atomic percent (at. %) in TiO{sub 2} thin films deposited under identical growth conditions, i.e., the growth rate of 0.6 A/s and at 500 Degree-Sign C. At 2 at. % Nd, complete texturing along (004) plane was observed, as indicated by the X-ray diffraction analyses. Morphology of the deposited TiO{sub 2} films from pure to 2 at. % Nd doped TiO{sub 2} films showed faceted to planar growth. Visualization of electrical and structural analysis (VESTA) software revealed that the change in the morphology was due to preferential growth in (004) orientation. Raman spectroscopy highlighted the phonon confinement in the Eg mode, and a red shift was observed due to an increase in the anti-symmetry in bonding with increased Nd concentration. XPS results confirmed the variation in oxygen vacancy concentration along with the reduction of Ti and Nd valance states with the change in the dopant concentration. Our experiments confirmed that the substitution of Nd at Ti sites was responsible for texturing in (004) orientation and this was possible by growing films at a very slow rate.