Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ULTIMATE STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

Let it rip: The mechanics of self-bisection in asexual planarians determines their population reproductive strategies

Asexual freshwater planarians reproduce by transverse bisection (binary fission) into two pieces. This process produces a head and a tail, which fully regenerate within 1-2 weeks. How planarians split into two offspring - using only their musculature and substrate traction – is a challenging biomechanics problem. We found that three different species, Dugesia japonica, Girardia tigrina and Schmidtea mediterranea, have evolved three different mechanical solutions to self-bisect. Using time lapse imaging of the fission process, we quantitatively characterize the main steps of division in the three species and extract the distinct and shared key features. Across the three species, planarians actively alter their body shape, regulate substrate traction, and use their muscles to generate tensile stresses large enough to overcome the ultimate tensile strength of the tissue. Moreover, we show that how each planarian species divides dictates how resources are split among its offspring. This ultimately determines offspring survival and reproductive success. Furthermore, heterospecific differences in the mechanics of self-bisection of individual worms explain the observed differences in the population reproductive strategies of different planarian species.

59 BASIC BIOLOGICAL SCIENCES↗

The Effect of Impact Damage Next to Holes on the Bearing Strength of Carbon Fiber Laminates

This study was undertaken as a follow-on to a previous study that examined the effect of hole quality in the bearing strength of carbon fiber laminates. After the author of that previous study had established that hole quality had little effect on the ultimate bearing strength for carbon fiber laminates, the question was raised as to the effects of impact damage next to a hole on the bearing strength of that hole. While this is an unlikely scenario, it is still possible that this may occur on a launch vehicle structure and thus warranted study. After a literature review, results of a few studies on the hole-impact interaction with respect to resulting damage for carbon fiber laminates were found, but none that specifically addressed the resulting bearing strength. In reference 2, it was found that the holes and impact could interact to develop matrix splits. However, the lay-ups used in this study consisted of clumped plies [04/904]S, which are much more prone to matrix splitting than a laminate that would actually be used in practice (such as a lay-up of [0/90]4S). This study also focused on the analytical aspects of the problem rather than the experimental results. Reference 3 also used [04/904]S laminates (clumped plies) and examined the damage morphology, determining that, as the impact damage neared the hole, the damage zone became more asymmetrical. The effect this would have on bearing strength was not addressed. The experimental work presented in this study was to develop empirical data relating holeimpact damage effects on the resulting bearing strength of a commonly used (quasi-isotropic) lay-up of carbon fiber laminate. The emphasis was not on the morphology of the resulting damage, as it was in references 2 and 3, but rather on the practical aspects of how this damage affected the bearing strength and how this compared to the companion study1 on the effect of hole quality on the bearing strength of the laminate.

Nettles, A. T.↗

Quenching and Partitioning Process Development to Replace Hot Stamping of High Strength Automotive Steel

The present project investigated Quenching and Partitioning (Q&P) to process cold rolled steels to develop high strength sheet steels that exhibit superior ductility compared to available grades with the intent to allow forming of high strength parts at room temperature to provide an alternative to hot stamping of parts. Hot stamping of boron alloyed steel is the current technology to manufacture thinner gauge sections in automotive structures to guarantee anti-intrusion during collisions whilst improving fuel efficiency by decreasing vehicle weight. Hot stamping involves reheating steel to 900 °C or higher followed by deformation and quenching in the die to produce ultra-high strength materials. Hot stamping requires significant energy to reheat the steel and is less productive than traditional room temperature stamping operations. Stamping at elevated temperature was developed due to the lack of available steels with strength levels of interest possessing sufficient ductility enabling traditional room temperature forming. This process is seeing growing demand within the automotive industry and, given the reheating step in this operation, increased energy consumption during part manufacturing results. The present research program focused on the development of steel grades via Q&P processing that exhibit high strength and formability enabling room temperature forming to replace hot stamping. The main project objective consisted of developing sheet steels exhibiting minimum ultimate tensile strength levels of 1200 MPa in combination with minimum tensile elongation levels of 15 pct using Q&P processing through judicious alloy design and heat treating parameter definition. In addition, detailed microstructural characterization and study of properties, processing and microstructure interrelationships were pursued to develop strategies to further enhance tensile properties. In order to accomplish these objectives, alloy design was conducted towards achieving the target properties. Twelve alloys were designed and laboratory produced involving melting, alloying, casting, hot rolling, and cold rolling to obtain sheet steels of approximately 1 mm thickness. Q&P processing of the samples was then conducted. Target properties were achieved and substantially exceeded demonstrating success in the developed and employed alloy design approaches. The best combinations of tensile properties were found at approximately 1550 MPa with a total elongation in excess of 20 pct clearly showing the potential for replacement of hot stamping to produce advanced high strength steels.

36 MATERIALS SCIENCE↗

Report on Thermal Aging Effects on Tensile Properties of Advanced Austenitic Steels

This report provides an update on the evaluation of thermal-aging induced degradation of tensile properties of advanced HT-UPS austenitic stainless steels. The report is the second deliverable (level 3) in FY11 (M3A11AN04030103), under the Work Package A-11AN040301, “Advanced Alloy Testing” performed by Argonne National Laboratory, as part of Advanced Structural Materials Program for the Advanced Reactor Concepts. This work package supports the advanced structural materials development by providing tensile data on aged alloys and a mechanistic model, validated by experiments, with a predictive capability on long-term performance. The scope of work is to evaluate the effect of thermal aging on the tensile properties of advanced alloys such as ferritic-martensitic steels, mod.9Cr-1Mo (G91), G92, and advanced austenitic stainless steel, HT-UPS. The aging experiments have been conducted over a temperature of 550-750°C for various time periods to simulate the microstructural changes in the alloys. In addition, a mechanistic model based on thermodynamics and kinetics has been used to address the changes in microstructure of the alloys as a function of time and temperature, which is developed in the companion work package at ANL. The focus of this project is advanced alloy testing and understanding the effects of long-term thermal aging on the tensile properties. The first deliverable of FY11 reported the tensile testing results of thermally-aged G92 in the normalized and tempered condition (H1 G92), G92 in the cold-rolled condition (H2 G92), and reference alloy, G91 ferritic-martensitic steels. This report summarizes the tensile data of thermally aged HT-UPS austenitic stainless steel. Two heats of HT-UPS have been investigated, i.e., solution-annealed HT-UPS (SA HT-UPS) and hot-rolled HT-UPS (HR HT-UPS). Tensile data have been obtained for SA HT-UPS thermally-aged for up to 18031 h at 550°C and for up to 17595 h at 650°C, as well as for HR HT-UPS thermally aged for up to 6909 h at 550°C, 4293 h at 600°C, and 5407 h at 650°C. Major finding are: (1) the solution-annealed HT-UPS showed continued, moderate increase in strength and decrease in ductility with increasing aging time up to 18034 h at 550°C. Thermal aging at 650°C increased the yield stress and decreased the ultimate tensile strength and drastically reduced the ductility in the SA HT-UPS. For the HR HT-UPS, thermal aging at 550°C for up to 6909 h showed little influence on its tensile behavior. Thermal aging at 600°C for 4293 h increased the strength and decreased the ductility. The 650°C-thermally-aged HR HT-UPS specimens showed very different strengthening, strain hardening, and flow localization behavior. Thermal aging at 650°C increased the yield stress but decreased the ultimate tensile stress for the HR HT-UPS. (2) Dynamic strain aging (DSA) was observed in both the solution-annealed HT-UPS and the hot-rolled HT-UPS at temperatures between 550-650°C at a strain rate of 0.001 s -1 . Extensive precipitation in the matrix after thermal aging at 600 and 650°C significantly reduced serrated plastic flow observed in the stress-strain curves, i.e. less effect of DSA. Because the DSA phenomenon can have significant influence on tensile, creep strength, and fatigue resistance, and the DSA effects in HT-UPS steels were observed in the temperature range of interest to the SFR applications, the DSA phenomenon in the HT.

Li, Meimei↗

Tensile Behavior of Al2o3/feal + B and Al2o3/fecraly Composites

The feasibility of Al2O3/FeAl + B and Al2O3/FeCrAlY composites for high-temperature applications was assessed. The major emphasis was on tensile behavior of both the monolithics and composites from 298 to 1100 K. However, the study also included determining the chemical compatibility of the composites, measuring the interfacial shear strengths, and investigating the effect of processing on the strength of the single-crystal Al2O3 fibers. The interfacial shear strengths were low for Al203/FeAl + B and moderate to high for Al203/FeCrAlY. The difference in interfacial bond strengths between the two systems affected the tensile behavior of the composites. The strength of the Al203 fiber was significantly degraded after composite processing for both composite systems and resulted in poor composite tensile properties. The ultimate tensile strength (UTS) values of the composites could generally be predicted with either rule of mixtures (ROM) calculations or existing models when using the strength of the etched-out fiber. The Al2O3/FeAl + B composite system was determined to be unfeasible due to poor interfacial shear strengths and a large mismatch in coefficient of thermal expansion (CTE). Development of the Al2O3/FeCrAlY system would require an effective diffusion barrier to minimize the fiber strength degradation during processing and elevated temperature service.

Draper, S. L.↗

Method for estimating fracture strength of specially orthotropic composite laminates.

A method is presented for estimating the stress intensity factor characteristic of crack extension in a specially orthotropic advanced fiber composite laminate, based on the elastic properties and ultimate principal strengths of a lamina, the laminate construction, and the experimentally determined value of the characteristic stress intensity factor of an arbitrary angle-plied, midplane symmetric laminate. A comparison of the results obtained from this method with limited experimental data for graphite/epoxy laminates indicates that the method is quite accurate for this particular material system. The predictive method is also used, in conjunction with experimental data, to estimate the size of a damage zone surrounding the crack tip.

Konish, H. J., Jr.↗

Elevated temperature tensile tests on DU–10Mo rolled foils

We report that studies were completed to obtain tensile mechanical properties for uranium-10wt.% molybdenum (U-10Mo) foils which were subjected to four different thermomechanical processing conditions. U-Mo alloy foils are being investigated to support fuel conversion of high power research reactors from their current high enriched fuel form to a low enriched fuel form. Mechanical properties of the fuel foil have an effect on irradiation performance and fuel fabrication and therefore are required to support modeling and qualification of new low-enriched uranium monolithic fuel plate designs. The data contained in this document contributes to fuel qualification by fulfilling the requirement that physical properties related to fuel meat be established. It is expected that depleted uranium-10wt% Mo (DU–10Mo) mechanical behavior is representative of the low-enriched U10-Mo to be used in actual fuel plates; therefore DU–10Mo was studied to simplify material processing, handling, and testing requirements. In this report, the different thermomechanical treatments included variations of wrought hot and cold rolling reduction and post rolling annealing. Each of the four foils was hot rolled. After hot rolling reduction, three of the four foils were further reduced by cold rolling. One of the three was reduced a further 20% by cold rolling, and the remaining two were reduced 50% by cold rolling. Following cold rolling reduction, one of the two foils which had been reduced 50% by cold rolling was annealed at 650?°C. Performing this analysis allows assessment of the impact of foil fabrication history on the resultant tensile properties DU–10Mo fuel foils. Tensile properties of DU–10Mo at room temperature through approximately 400 °C determined from the tests conducted herein suggest the material is stronger and has lower ductility than what has been reported previously in the literature. The explanation for these differences has yet to be determined, but is likely related to differences in grain size and/or impurity content, and variation in fabrication history. At the highest temperatures tested (550 °C) better agreement between the values reported here and available literature was found. As expected, yield and ultimate tensile strength decreased with increasing test temperature. Generally, the yield stress for all foil processing conditions was found to be in the range of 1100 MPa for room temperature tests, and in the range of 200 MPa for tests conducted at 550 °C. Ultimate tensile stress was in the range of 1175 MPa at room temperature, decreasing to approximately 225 MPa at 550 °C. Lastly, elongation increased significantly, from 0 to 2% at room temperature to 50% or more for the tests at 550 °C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of spatial energy distribution-induced porosity on mechanical properties of laser powder bed fusion 316L stainless steel

Laser powder bed fusion (LPBF) additive manufacturing (AM) offers a variety of advantages over traditional manufacturing, however its usefulness for manufacturing of high-performance components is currently hampered by internal defects (porosity) created during the LPBF process that have an unknown impact on global mechanical performance. By inducing porosity distributions through variations in print energy density and inspecting the resulting tensile samples using computed tomography, nearly 50,000 pores across 75 samples were identified. Porosity characteristics were quantitatively extracted from inspection data and compared with mechanical properties to understand the strength of relationships between porosity and global tensile performance. Useful porosity characteristics were identified for prediction of part performance. Results indicate that ductility and strain at ultimate tensile strength are the global tensile properties most significantly impacted by porosity and can be predicted with reasonable accuracy using simple porosity shape descriptors such as volume, diameter, and surface area. Moreover, it was found that the largest pores influenced behavior most significantly. Specifically, pores in excess of 125 µm in diameter were found to be a sufficient threshold for property estimation. These results establish an initial understanding of the complex defect-performance relationship in AM 316L stainless steel and can be leveraged to develop certification standards and improve confidence in part quality and reliability for the broader set of engineering alloys.

36 MATERIALS SCIENCE↗

Microstructure evolution, enhanced aging kinetics, and mechanical properties of AA7075 alloy after friction extrusion

In the present study we utilized Friction Extrusion (FE) a solid phase processing technique to produce fully consolidated dense 5 mm rods of AA7075 alloy. The combination of large shear stresses and temperatures at the tool-billet interface during the FE process resulted in the formation of dynamically recrystallized ~2.0 μm equiaxed grains and fine uniformly distributed stable η (MgZn 2 ) precipitates ~25–100 nm in size. Formation of such a microstructure resulted in lower solutionizing temperature and times (flash annealing) as compared to the conventionally extruded counterparts. Here we demonstrate for the first time that the solutionizing times for the T6 heat treatment of AA7075 can be reduced by three times using this FE process. In addition to being an energy efficient process, FE also serves to improve the performance of AA7075 alloys by retaining their strength while enhancing the ductility of the material. The tensile data for samples that were flash annealed and artificially aged after FE processing showed exceptional increase in ultimate tensile strength by over 19% and yield strength by over 59%, compared with an as-FE-processed sample.

36 MATERIALS SCIENCE↗

Thermal stress effects in intermetallic matrix composites

Intermetallic matrix composites develop residual stresses from the large thermal expansion mismatch (delta-alpha) between the fibers and matrix. This work was undertaken to: establish improved techniques to measure these thermal stresses in IMC's; determine residual stresses in a variety of IMC systems by experiments and modeling; and, determine the effect of residual stresses on selected mechanical properties of an IMC. X ray diffraction (XRD), neutron diffraction (ND), synchrotron XRD (SXRD), and ultrasonics (US) techniques for measuring thermal stresses in IMC were examined and ND was selected as the most promising technique. ND was demonstrated on a variety of IMC systems encompassing Ti- and Ni-base matrices, SiC, W, and Al2O3 fibers, and different fiber fractions (Vf). Experimental results on these systems agreed with predictions of a concentric cylinder model. In SiC/Ti-base systems, little yielding was found and stresses were controlled primarily by delta-alpha and Vf. In Ni-base matrix systems, yield strength of the matrix and Vf controlled stress levels. The longitudinal residual stresses in SCS-6/Ti-24Al-llNb composite were modified by thermomechanical processing. Increasing residual stress decreased ultimate tensile strength in agreement with model predictions. Fiber pushout strength showed an unexpected inverse correlation with residual stress. In-plane shear yield strength showed no dependence on residual stress. Higher levels of residual tension led to higher fatigue crack growth rates, as suggested by matrix mean stress effects.

Wright, P. K.↗

Relevant biochar characteristics influencing compressive strength of biochar-cement mortars

To counteract the contribution of CO 2 emissions by cement production and utilization, biochar is being harnessed as a carbon-negative additive in concrete. Increasing the cement replacement and biochar dosage will increase the carbon offset, but there is large variability in methods being used and many researchers report strength decreases at cement replacements beyond 5%. This work presents a reliable method to replace 10% of the cement mass with a vast selection of biochars without decreasing ultimate compressive strength, and in many cases significantly improving it. By carefully quantifying the physical and chemical properties of each biochar used, machine learning algorithms were used to elucidate the three most influential biochar characteristics that control mortar strength: initial saturation percentage, oxygen-to-carbon ratio, and soluble silicon. These results provide additional research avenues for utilizing several potential biomass waste streams to increase the biochar dosage in cement mixes without decreasing mechanical properties.

97 MATHEMATICS AND COMPUTING↗

Tensile and fatigue characterization of multifunctional composites

This research is part of a larger effort to develop advanced self-sensing multifunctional polymer composites that are both lightweight and high-strength, while also enabling structural damage detection, fatigue cycle monitoring, and service life prediction. These multifunctional composites are particularly sought after in the automotive industry for their potential to significantly reduce vehicle weight and simultaneously provide additional functionality like condition monitoring to enhance safety. This study examines the tensile and fatigue properties of a composite material composed of acrylonitrile butadiene styrene (ABS) polymer embedded with piezoelectric barium titanate (BaTiO3) nanoparticles. The integration of BaTiO3 nanoparticles not only supplies the material with self-sensing capabilities but also influences its mechanical properties. While a high content of BaTiO3 nanoparticles is desired to enhance sensing capacity, the brittle nature of such materials causes concerns of decreased strength characteristics. To explore this, various composite samples were fabricated with nanoparticle contents ranging from 0 wt% to 20 wt%. These samples underwent tensile testing to measure their ultimate tensile strengths and Young’s moduli. Following this, fatigue tests were conducted to generate S-N curves, which are essential for understanding the material's durability under cyclic loading. The findings from these tests assess the impact of nanoparticle content on the composite’s tensile strength and fatigue life, providing essential insights that can guide the optimization and design of future self-sensing multifunctional composites. The results suggest that 5 wt% BaTiO3 provides an optimal balance between mechanical properties and nanoparticle concentration, making it a promising composition for semi-structural applications.

Bowland, Christopher [ORNL] (ORCID:000000021229431↗

Apple Strength Issues

Strength of the apple parts has been noticed to decrease, especially those installed by the new induction heating system since the LEP campaign started. Fig. 1 shows the ultimate tensile strength (UTS), yield strength (YS), and elongation of the installed or installation-simulated apples on various systems. One can clearly see the mean values of UTS and YS of the post-LEP parts decreased by about 8 ksi and 6 ksi respectively from those of the pre-LEP parts. The slight increase in elongation seen in Fig.1 can be understood from the weak inverse relationship between the strength and elongation in metals. Fig.2 shows the weak correlation between the YS and elongation of the parts listed in Fig. 1. Strength data listed in Figure 1 were re-plotted as histograms in Figs. 3 and 4. Figs. 3a and 4a show histograms of all UTS and YS data. Figs. 3b and 4b shows histograms of pre-LEP data and Figs. 3c and 4c of post-LEP data. Data on statistical scatter of tensile strengths have been rarely published by material suppliers. Instead, only the minimum 'guaranteed' strength data are typically presented. An example of strength distribution of aluminum 7075-T6 sheet material, listed in Fig. 5, show that its scatter width of both UTS and YS for a single sheet can be about 6 ksi and for multi-lot scatter can be as large as 11 ksi even though the sheets have been produced through well-controlled manufacturing process. By approximating the histograms shown in Figs. 3 and 4 by a Gaussian or similar type of distribution curves, one can plausibly see the strength reductions in the later or more recent apples. The pre-LEP data in Figs. 3b and 4b show wider scatter than the post-LEP data in Figs. 3c and 4c and seem to follow the binomial distribution of strength indicating that the apples might have been made from two different lots of material, either from two different vendors or from two different melts of perhaps slightly different chemical composition by a single vendor. The post-LEP apples seem to have been from a single batch of material. The pre-LEP apples of the weak strength and the post-LEP apples with even weaker strength could have been made of the same batch of material, and the small strength differential might be due to the difference in the induction heating system. If the pre-LEP apples with the lower strength and the post LEP apples are made from the same batch of material, their combined scatter of strength data would be wider and can be understood as a result of the additional processing steps of stress relief and induction heating as discussed.

36 MATERIALS SCIENCE↗

Properties of silicon carbide fiber-reinforced silicon nitride matrix composites

The mechanical properties of NASA Lewis developed SiC/RBSN composites and their thermal and environmental stability havd been studied. The composites consist of nearly 30 vol pct of aligned 142 micron diameter chemically vapor-deposited SiC fibers in a relatively porous silicon nitride matrix. In the as-fabricated condition, the unidirectional and 2-D composites exhibited metal-like stress-strain behavior, graceful failure, and showed improved properties when compared with unreinforced matrix of comparable density. Furthermore, the measured room temperature tensile properties were relativley independent of tested volume and were unaffected by artifical notches normal to the loading direction or by thermal shocking from temperatures up to 800 C. The four-point bend strength data measured as a function of temperature to 1400 C in air showed that as-fabricated strength was maintained to 1200 C. At 1400 C, however, nearly 15 pct loss in strength was observed. Measurement of room temperature tensile strength after 100 hr exposure at temperatures to 1400 C in a nitrogen environment indicated no loss from the as-fabricated composite strength. On the other hand, after 100 hr exposure in flowing oxygen at 1200 and 1400 C, the composites showed approximately 40 pct loss from their as-fabricated ultimate tensile strength. Those exposed between 400 to 1200 C showed nearly 60 pct strength loss. Oxidation of the fiber/matrix interface as well as internal oxidation of the porous Si3N4 matrix are likely mechanisms for strength degradation. The excellent strength reproducibility, notch insensitivity, and high temperature strength of the composite makes it an ideal candidate for advanced heat engine applications provided coating or densification methods are developed to avoid internal oxidation attack.

Bhatt, Ramakrishna T.↗

Characterization of commercial proton exchange membrane materials after exposure to beta and gamma radiation

Proton Exchange Membrane (PEM) type electrolysis cells have a potential use for tritium removal and heavy water upgrading. AECL is currently exposing various commercial PEM materials to both gamma (Cobalt-60 source) and beta (tritiated water) radiation to study the effects of radiation on these materials. This paper summarizes the testing methods and results that have been collected to date. The PEM materials that are or have been exposed to radiation are: Nafion 112, 212, 117 and 1110. Membrane characterization pre- and post- exposure consists of non-destructive inspection (FTIR, SEM/XPS), mechanical (tensile strength, percentage elongation, and modulus), electrical (resistance), or chemical (ion-exchange capacity - IEC). It has appeared that the best characterization techniques to compare exposed versus unexposed membranes were IEC, ultimate tensile strength and percent elongation. These testing techniques are easy and cheap to perform. The non-destructive tests, such as SEM and FTIR did not provide particularly useful information on radiation-induced degradation. Where changes in material properties were measured after radiation exposure, they would be expected to result in poorer cell performance. However, for modest γ-radiation exposure, all membranes showed a slight decrease in cell voltage (better performance). In contrast, the one β-radiation exposed membrane did show the expected increase in cell voltage. The counterintuitive trend for γ-radiation exposed membranes is not yet understood. Based on these preliminary results, it appears that γ- and β-radiation exposures have different effects.

07 ISOTOPE AND RADIATION SOURCES↗

Mechanisms of Oxide Formation in the Self-Reacting Friction Stir Weld Process

The initial objective of this study was to evaluate the effect of an extended delay time between preweld cleaning and the completion of a self-reacting friction stir welding (SRFSW) process on the resulting quality of various thickness panels of AA2219-T87. The current NASA standard specifies no more than a 48 hour delay between preweld cleaning and actual welding. The concern is whether increasing the cleaning delay time results in development of the residual oxide defect (ROD) in SRFSW. This concern emanates from the possibility of increased time correlating with increased oxide layer thickness on the faying surfaces. Oxide content on the faying surfaces has been reported to correlate with the occurrence of the ROD which reduces mechanical properties. When the SRFSW process was first adopted by the NASA Marshall Space Flight Center (MSFC), unexpected low tensile values that resulted were attributed to oxides within the weld that appeared to follow the former faying surface contours. Mitigation of the ROD was achieved through a combination of modifications to the processing parameters, tool designs, and incorporation of a weld seam offset. Two operations are involved in preweld cleaning: the first is removal of oil and grease, and the second is removal of surface oxides. In arc welding, improper cleaning of the faying surfaces of aluminum welded joints can increase the sensitivity toward development of defects. As the aluminum is locally melted, these contaminants contribute toward the development of porosity, inclusions, entrapped oxides, and other discontinuities which can degrade the strength of the weld joint. For weldment of large structures, the weld joint is typically cleaned, fit-up, and tack welded prior to the final full penetration welding pass. Because of the stringent joint fit-up requirements for mismatch and peaking for launch vehicle structures, the joint fit-up can sometimes contribute to lengthy delays between cleaning and tack welding, especially for circumferential weld joints on large diameter components. When the conventional friction stir welding (CFSW) process was introduced at the NASA MSFC, there was no procedure for cleaning prior to the solid-state joining process. As the process expanded to include SRFSW, preparation of the faying, crown, and root surfaces were implemented to overcome the ROD. Although the solid-state process is not expected to reach temperatures high enough for dissociation of the native oxide layer, concern remained regarding the redeposition of the native oxide layer within the stir zone. NASA has previously established the allowable time at 48 hours between preweld cleaning and a SRFSW process. The effect of potential 2 contamination resulting from an extended delay to 188 hours was subsequently evaluated for SRFSWs using tensile testing and metallographic imaging. Tensile specimens were tested at room temperature (RT), and at cryogenic conditions of liquid nitrogen (LN2) and liquid hydrogen. No detrimental effect on weld quality, as determined by weld strength, was reported for cleaning delays of 48, 120, 168, 240 or 288 hours. While no trends were established in this study, which extended the delay from 48 to 188 hours, there were a few outliers in terms of ultimate tensile strength (UTS). According to M. Fisher's 2014 Boeing Company Memo no. EYBF-MAF-14-029, all outliers were above the minimum acceptance criteria, but out of family with respect to the average values. As the robustness and reliability of any process ultimately depends on the average values as well as the outliers, an understanding of the cause of these outliers will ultimately improve the process. This report examines those outliers and their possible causes.

Schneider, J. A.↗

Sn and Nb modified ultrafine Ti-based bulk alloys with high-strength and enhanced ductility

Sn and Nb modified ultrafine eutectic Ti-Fe alloys with high strength and plasticity prepared by cold crucible levitation melting were tested in compression at room temperature. (Ti{sub 70.5}Fe{sub 29.5}){sub 93.15}Sn{sub 3.85}Nb{sub 3} alloy exhibited an ultimate compressive strength of 2.36 GPa at 15% plastic strain. Electron microscopy revealed that lamellar structures in Ti{sub 70.5}Fe{sub 29.5} alloy could be tailored by the addition of Sn and Nb to obtain a globular structure. The microstructural refinement, morphology of phase constituents, and their relationships to the mechanical properties are discussed.

36 MATERIALS SCIENCE↗

A parametric study of fracture toughness of fibrous composite materials

Impacts to fibrous composite laminates by objects with low velocities can break fibers giving crack-like damage. The damage may not extend completely through a thick laminate. The tension strength of these damage laminates is reduced much like that of cracked metals. The fracture toughness depends on fiber and matrix properties, fiber orientations, and stacking sequence. Accordingly, a parametric study was made to determine how fiber and matrix properties and fiber orientations affect fracture toughness and notch sensitivity. The values of fracture toughness were predicted from the elastic constants of the laminate and the failing strain of the fibers using a general fracture toughness parameter developed previously. For a variety of laminates, values of fracture toughness from tests of center-cracked specimens and values of residual strength from tests of thick laminates with surface cracks were compared to the predictions to give credibility to the study. In contrast to the usual behavior of metals, it is shown that both ultimate tensile strength and fracture toughness of composites can be increased without increasing notch sensitivity.

Poe, C. C., Jr.↗