Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Solid dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

Geochemical modeling of leaching of Ca, Mg, Al, and Pb from cementitious waste forms

Results from extraction tests on cement-waste samples were simulated with a thermodynamic equilibrium model using a consistent database, to which lead data were added. Subsequent diffusion tests were modeled by means of a 3D diffusive transport model combined with the geochemical model derived from the extraction tests. Modeling results of the leached major element concentrations for both uncarbonated and (partially) carbonated samples agreed well with the extraction test using the set of pure minerals and solid solutions present in the database. The observed decrease in Ca leaching with increasing carbonation level was qualitatively predicted. Simulations also revealed that Pb leaching is not controlled by dissolution/precipitation only. The addition of the calcite-cerrusite solid solution and adsorption reactions on amorphous Fe- and Al-oxides improved the predictions and are considered to control the Pb leaching during the extractions tests. The dynamic diffusive leaching tests were appropriately modeled for Na, K, Ca and Pb.

36 MATERIALS SCIENCE↗

Mineralogy and pore water chemistry of a boiler ash from a MSW fluidized-bed incinerator

This paper presents an investigation of the mineralogy and pore water chemistry of a boiler ash sampled from a municipal solid waste fluidized-bed incinerator, subject to 18 months of dynamic leaching in a large percolation column experiment. A particular focus is on the redox behaviour of Cr(VI) in relation to metal aluminium Al{sup 0}, as chromium may represent an environmental or health hazard. The leaching behaviour and interaction between Cr(VI) and Al{sup 0} are interpreted on the basis of mineralogical evolutions observed over the 18-month period and of saturation indices calculated with the geochemical code PhreeqC and reviewed thermodynamic data. Results of mineralogical analyses show in particular the alteration of mineral phases during leaching (e.g. quartz and metal aluminium grains), while geochemical calculations suggest equilibria of percolating fluids with respect to specific mineral phases (e.g. monohydrocalcite and aluminium hydroxide). The combination of leaching data on a large scale and mineralogical analyses document the coupled leaching behaviour of aluminium and chromium, with chromium appearing in the pore fluids in its hexavalent and mobile state once metal aluminium is no longer available for chromium reduction.

54 ENVIRONMENTAL SCIENCES↗

Reactivity of Redox Cycled Fe-bearing Subsurface Sediments Towards Hexavalent Chromium Reduction

Structural Fe(II) in clay minerals and natural sediments is known to reduce Cr(VI) to Cr(III), but the effect of redox-cycled Febearing natural sediments on Cr(VI) reduction kinetics is poorly understood. The objective of this study was to understand the kinetics and mechanisms of Cr(VI) reduction by Fe(II) in redox cycled natural sediment. Fe-bearing sediment was collected from the Ringold formation in the 300 area of Hanford, Washington, United States. Fe redox cycling of the sediment was accomplished via four cycles of bioreduction of structural Fe(III) in Hanford sediment and air oxidation of the resulting Fe(II). Bio-produced Fe(II) in Hanford sediment from each redox cycle was utilized to reduce Cr(VI) at three temperatures (10, 20 and 30° C). The initial rate of Cr(VI) reduction generally increased with each redox cycle, which was more pronounced at high temperatures. The amount of Fe(II) oxidized to the amount of Cr(VI) reduced was close to the expected stoichiometric ratio of 3. Aqueous concentrations of Si, Al, and Fe revealed some dissolution of the sediment after reaction with Cr(VI). Xray diffraction (XRD) and scanning electron microscopy (SEM) detected secondary mineral formation. Mössbauer data showed that the oxidation of Fe(II) was coupled with the reduction of Cr(VI) but no Feoxides/ oxyhydroxides formed. Transmission electron microscopy (TEM), electron energy loss spectroscopy (EELS), XANES, and EXAFS were performed for representative reduced Cr solids that formed from reduction of Cr(VI) by sediment-associated Fe(II) at 30oC. TEM revealed that the d-spacing of Cr-reacted montmorillonite at 30° C, a dominant Fe-bearing mineral in Hanford sediment, expanded from 10 Å to 13 Å. This layer expansion was likely due to intercalation of reduced Cr(III) into the interlayer space of the montmorillonite structure. EELS exhibited an L2 absorption peak at 586.0 eV and an L3 absorption peak at 577.0 eV, suggestive of Cr(III) in a hydroxide mineral phase. Similarly, XANES and EXAFS analyses confirmed Cr(VI) reduction to Cr(OH)3 at 30° C and indicated an edge-sharing coordination of the Cr(III) octahedra to 2-3 other Cr or metal ions. This study has important implications for understanding the reactivity of clay-rich sediment towards Cr(VI) reduction at contaminated sites and the stability of the reduced Cr(III).

Bishop, Michael E.↗

Aluminum Coprecipitates with Fe (hydr)oxides: Does Isomorphous Substitution of Al3plus for Fe3plus in Goethite Occur

Iron (hydr)oxides are common in natural environments and typically contain large amounts of impurities, presumably the result of coprecipitation processes. Coprecipitation of Al with Fe (hydr)oxides occurs, for example, during alternating reduction-oxidation cycles that promote dissolution of Fe from Fe-containing phases and its re-precipitation as Fe-Al (hydr)oxides. We used chemical and spectroscopic analyses to study the formation and transformation of Al coprecipitates with Fe (hydr)oxides. In addition, periodic density functional theory (DFT) computations were performed to assess the structural and energetic effects of isolated or clustered Al atoms at 8 and 25 mol% Al substitution in the goethite structure. Coprecipitates were synthesized by raising the pH of dilute homogeneous solutions containing a range of Fe and Al concentrations (100% Fe to 100% Al) to 5. The formation of ferrihydrite in initial suspensions with {<=}20 mol% Al, and of ferrihydrite and gibbsite in initial suspensions with {>=}25 mol% Al was confirmed by infrared spectroscopic and synchrotron-based X-ray diffraction analyses. While base titrations showed a buffer region that corresponded to the hydrolysis of Fe in initial solutions with {<=}25 mol% Al, all of the Al present in these solutions was retained by the solid phases at pH 5, thus indicating Al coprecipitation with the primary Fe hydroxide precipitate. In contrast, two buffer regions were observed in solutions with 30 mol% Al (at pH {approx}2.25 for Fe{sup 3+} and at pH {approx}4 for Al{sup 3+}), suggesting the formation of Fe and Al (hydr)oxides as two separate phases. The Al content of initial coprecipitates influenced the extent of ferrihydrite transformation and of its transformation products as indicated by the presence of goethite, hematite and/or ferrihydrite in aged suspensions. DFT experiments showed that: (i) optimized unit cell parameters for Al-substituted goethites (8 and 25 Mol% Al) in clustered arrangement (i.e., the formation of diaspore-like clusters) were in good agreement with available experimental data whereas optimized unit cell parameters for isolated Al atoms were not, and (ii) Al-substituted goethites with Al in diaspore-like clusters resulted in more energetically favored structures. Combined experimental and DFT results are consistent with the coprecipitation of Al with Fe (hydr)oxides and with the formation of diaspore-like clusters, whereas DFT results suggest isomorphous Al for Fe substitution within goethite is unlike at 8 mol% Al substitution.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In situ Investigation of Water Interaction with Lead-Free All Inorganic Perovskite (Cs 2 SnI x Cl 6– x )

Hybrid halide perovskites display a great tunability of optoelectronic properties and environmental stability by controlling the halogen anions (e.g., I, Cl, and Br). Yet, their water interaction and degradation mechanisms are not completely elucidated. In this work, the interaction of Cs 2 SnCl 6 and Cl-enriched solid solution Cs 2 SnI 0.9 Cl 5.1 with water was systematically studied by in situ synchrotron X-ray diffraction and micro-Raman spectra and compared with the isostructural Cs 2 SnI 6 . Unlike Cs 2 SnI 6 , which experiences a direct dissolution in water, Cs 2 SnCl 6 displays an enhanced stability and the dissolution of the Cs 2 SnCl 6 accompanies with the formation of an amorphous alteration phase. Under controlled dehydration conditions, two-dimensional Cs 2 SnCl 6 flakes can be precipitated out from water solution. Moreover, the mixed halide perovskite (Cs 2 SnI 0.9 Cl 5.1 ) experiences fast iodide dissolution in water solution and transforms to a more chloride-enriched perovskite which shows a behavior similar to Cs 2 SnCl 6 . The mechanistic understanding of the dissolution–precipitation process of Cs 2 SnI x Cl 6–x perovskites is useful for developing new perovskites with varied halogen and controlled environmental stability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantification of Electrochemical Nanoscale Processes in Lithium Batteries By OperandoEC-(S)TEM

Lithium (Li)-ion batteries are currently used for a wide variety of portable electronic devices, electric vehicles and renewable energy applications. In addition, extensive worldwide research efforts are now being devoted to more advanced “beyond Li-ion” battery chemistries - such as lithium-sulfur (Li-S) and lithium-air (Li-O2) - in which the carbon anode is replaced with Li metal. However, the practical application of Li metal anode systems has been highly problematic. The main challenges involve controlling the formation of a solid-electrolyte interphase (SEI) layer and the suppression of Li dendrite growth during the charge/discharge process (achieving “dendrite-free” cycling). The SEI layer formation continuously consumes the electrolyte components creating highly resistive layer, which leads to the rapid decrease of cycling performance and degradation of the Li anode. The growth of Li metal dendrites at the anode contributes to rapid capacity fading (the presence of “dead Li” created during the discharge leads to an increased overpotential) and, in the case of continuous growth, leads to internal short circuits and extreme safety issues. Here we demonstrate the application of an operando electrochemical scanning transmission electron microscopy (ec-(S)TEM) cell to study the SEI layer formation and the initial stages of Li dendrite growth - the goal is to develop a mechanism for mitigating the degradation processes and increasing safety. Bright field (BF) STEM images in Figure 1 A-C show Li metal deposition and dissolution processes at the interface between the Pt working electrode and the lithium hexafluorophosphate (LiPF6) in propylene carbonate (PC) electrolyte during three charge/discharge cycles. A contrast reversal caused by Li metal being lighter/less dense than surrounding electrolyte (Li appears brighter than the background in BF STEM images) allows Li to be uniquely identified from the other components in the system - the only solid material that is less dense than the electrolyte is Li metal. Using these images, we can precisely quantify the total volume of Li deposition, the thickness of the SEI layer (observed as a ring of positive contrast around the electrode) and alloy formation due to Li+ ion insertion during each cycle. Furthermore, at the end of each discharge cycle we can quantify the presence of “dead Li” detached from the Pt electrode, thereby demonstrating the degree of irreversibility (and degradation of Pt electrode) associated with insertion/removal of Li+during this process with direct correlation to electrochemical performance. Such analyses provide significant insights into Li metal dendrite growth, which is critical to understand the complex interfacial reactions needed to be controlled for future Li-based and next generation energy storage systems.

batteries↗

DESORPTION OF SORBATES FROM MST, MMST, AND CST UNDER VARIOUS CONDITIONS

The Small Column Ion Exchange (SCIX) Program (formerly referred to as the Modular Salt Processing (MSP) Project) seeks to deploy equipment to remove the {sup 134,137}Cs, {sup 90}Sr, and alpha-emitting radionuclides (principally {sup 238,239,240}Pu and {sup 237}Np) from the high level waste salt solutions. The equipment is installed within a high level waste tank to take advantage of the shielding provided by the waste tank. The process will involve adding monosodium titanate (MST) to the waste tank (i.e., Tank 41H) to sorb the Sr and select actinides, removing the MST and entrained sludge with in-riser rotary microfilters, and subsequently using ion-exchange columns containing crystalline silicotitanate (CST) to remove the Cs. After being loaded with Cs, the CST will be ground to reduce the particle size and then transferred into another waste tank (e.g., Tank 40H). The MST and sludge solids stream will be transported to a sludge batch preparation tank (i.e., Tank 42H or Tank 51H) once the SCIX batch is processed. Both streams, MST/solids and CST, will ultimately be transported into and vitrified inside the Defense Waste Processing Facility (DWPF). A series of experiments were performed to examine desorption from monosodium titanate (MST), modified monosodium titanate (mMST), and crystalline silicotitanate (CST) under various conditions. The first two experiments examined desorption from MST and CST under two different sludge treatment processes, aluminum dissolution and sludge washing. Desorption of all sorbates was observed to varying degrees under the aluminum dissolution conditions. The extent of desorption ranged from < 3% to about 50% after 4 weeks, with Pu exhibiting the lowest desorption. At the end of the experiment, the temperature was reduced from 65 C to 25 C and the tests monitored for an additional two weeks. After reducing the temperature, partial resorption of the sorbates was observed with both MST and CST. Under the sludge washing conditions, no desorption of sorbates was observed with MST; however, some additional sorption did occur. For CST, a small amount of Cs leached from the material during the first day of testing, but no further leaching was observed over the remaining test period. The final test was designed to examine the possibility of desorption from both MST and mMST upon increasing the solid to liquid phase ratio. The results of these tests indicated some desorption of Pu from MST within the first two weeks after changing the phase ratio, then resorption of some of the leached Pu over the remaining 4 weeks of the experiment. No desorption of any sorbates was observed for mMST under these conditions.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Investigation of nanostructured Al-10 wt.% Zr material prepared by ball milling for high temperature applications

Ground chips of as-cast Al-10 wt.% Zr alloy were subjected to mechanical alloying (MA) with 5 vol.% of nanodiamond addition in a high energy planetary ball-mill. The aim of this work was to investigate the microstructure, phase transformation and mechanical properties of the material both after MA and after subsequent annealing. Optical and transmission electron microscopes were used for morphological and microstructural analysis. The effect of milling time on powder microhardness, Al lattice parameter, lattice microstrain and crystallite size was determined. It was shown that mechanical alloying of as-cast Al-10wt.%Zr alloy during 20 h leads to a complete dissolution of the primary tetragonal Al{sub 3}Zr crystals in aluminum. At the same time, the powder microhardness increases to 370 HV. Metastable cubic Al{sub 3}Zr phase nanoparticles precipitate from the Al solution due to its decomposition after annealing, however, the Al solid solution remains supersaturated and nanocrystalline. Compression tests at room temperature and at 300 °C showed that the strength values of the hot-pressed samples reach 822 MPa and 344 MPa, respectively. - Highlights: •As-cast Al-10 wt.% Zr alloy was mechanically alloyed with 5 vol.% nanodiamond. •The primary tetragonal Al{sub 3}Zr crystals were completely dissolved in Al after 20 h. •Cubic Al{sub 3}Zr phase nanoparticles precipitated from Al solution after aging. •The aged bulk material showed a high strength at room and elevated temperatures.

36 MATERIALS SCIENCE↗

On the dissolution of a borosilicate glass with the use of isotopic tracing – Insights into the mechanism for the long-term dissolution rate

An understanding of the mechanisms responsible for controlling the long-term corrosion rate of nuclear waste glass is paramount if reliable glass dissolution models are to be used to calculate the controlled release of radionuclides from nuclear waste glass under geologic disposal conditions. Additionally, understanding silicate glass dissolution is also important for natural glasses to understand the role from the dissolution of these glasses has on the composition of natural aquatic systems. Two general mechanisms appear to be responsible for the elemental release from glass to the surrounding biosphere - ion exchange (release principally of alkalis) and matrix dissolution (release of the structural components of the glass). Key unknowns related to these mechanisms are the impact of surface layers on the altered glass and how these layers participate in corrosion. To better understand the impact of these layers on glass corrosion, we made two glasses of the same elemental composition, but with selected elements enriched in specific isotopes, e.g. more 10 B than 11 B. We reacted these glasses for 1 y then the solutions from each were exchanged and the chemistry of the solutions and the solids were followed for another 2 y and in some cases 3 y. This allowed us to follow changes in the glasses with respect to these elements and how these elements were transported through the alteration layers with time and, for at least one element, into the glass. Results from these experiments demonstrate that the release behavior of different elements is strongly dependent on their structural role in the glass (e.g. network formers and modifiers), but, more importantly, the role of water transport and subsequent ion exchange has in the long-term dissolution of the glass studied here. In this article, we highlight the behavior of four elements: lithium, sodium, silicon, and boron. Lithium and sodium, network modifying elements, have similar chemistries. The behavior of Li could be tracked in more detail by following both 6 Li and 7 Li; Li penetrates through the gel layer in both directions without hinderance and into and released from the glass deeper than sodium. Silicon, a network forming element, reacts with the silica-rich alteration layer. Boron, a network forming element, does not accumulate in the gel or the pristine glass and has a very sharp elemental profile between the pristine glass and alteration layer. Boron, lithium, and sodium elemental profiles suggest that there is little if any transport control within the alteration layer. The correlation between the Li and Na profiles and that of a water species suggest that the limiting release is a steady state between the diffusion of a water species and matrix dissolution that results in a low release rate for alkali and this provides a steady driving force for the long-term dissolution of glass.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Technetium Stabilization in Low-Solubility Sulfide Phases: A Review

We report that technetium contamination remains a major environmental problem at nuclear reprocessing sites, e.g., the Hanford Site, Washington, USA. At these sites, Tc is present in liquid waste destined for immobilization in a waste form or has been released into the subsurface environment. The high environmental risk associated with Tc is due to its long half-life (214 000 years) and the mobility of the oxidized anionic species Tc(VII)O 4 - . Under reducing conditions, TcO 4 - is readily reduced to Tc(IV), which commonly exists as a relatively insoluble and therefore immobile, hydrous Tc-oxide (TcO 2 · n H 2 O). The stability of Tc(IV) sequestered as solid phases depends on the solubility of the solid and susceptibility to reoxidation to TcO 4 - , which in turn depend on the (biogeo)chemical conditions of the environment and/or nuclear waste streams. Unfortunately, the solubility of crystalline TcO 2 or amorphous TcO 2 ·H 2 O is still above the maximum contaminant level (MCL) established by the U.S. EPA (900 pCi/L), and the kinetics of TcO 2 oxidative dissolution can be on the order of days to years. In addition to oxygen, sulfur can form complexes that significantly affect the adsorption, solubility, and reoxidation potential of Tc, especially Tc(IV). The principal technetium sulfides are TcS 2 and Tc 2 S 7 , but much less is known about the mechanisms of formation, stabilization, and reoxidation of Tc-sulfides. A common assumption is that sulfides are less soluble than their oxyhydrous counterparts. Determination of the molecular structure of Tc 2 S 7 in particular has been hampered by the propensity of this phase to precipitate as an amorphous substance. Recent work indicates that the oxidation state of Tc in Tc 2 S 7 is Tc(IV), in apparent contradiction to its nominal stoichiometry. Technetium is relatively immobile in reduced sediments and soils, but in many cases the exact sink for Tc has not been identified. Experiments and modeling have demonstrated that both abiotic and biologic mechanisms can exert strong controls on Tc mobility and that Tc binding or uptake into sulfide phases can occur. These and similar investigations also show that extended exposure to oxidizing conditions results in transformation of sulfide-stabilized Tc(IV) to a Tc(IV)O 2 -like phase without formation of measurable dissolved TcO 4 - , suggesting a solid-state transformation in which Tc(IV)-associated sulfide is preferentially oxidized before the Tc(IV) cation. This transformation of Tc(IV)-sulfides to Tc(IV)-oxides may be the main process that limits remobilization of Tc as Tc(VII)O 4 - . The efficacy of the final waste form to retain Tc also strongly depends on the ability of oxidizing species to enter the waste and convert Tc(IV) to Tc(VII). Finally, many waste form designs are reducing (e.g., cementitious waste forms such as salt stone) and, therefore, attempt to restrict access of oxidizing species such that diffusion is the rate-limiting step in remobilization of Tc.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Understanding the Importance of Labile Fe(III) during Fe(II)-Catalyzed Transformation of Metastable Iron Oxyhydroxides

Transformation of metastable Fe(III) oxyhydroxides is a prominent process in natural environments and can be significantly accelerated by the coexisting aqueous Fe(II) (Fe(II) aq ). Recent evidence points to the solution mass transfer of labile Fe(III) (Fe(III) labile ) as the primary intermediate species of general importance. However, a mechanistic aspect that remains unclear is the dependence of phase outcomes on the identity of the metastable Fe(III) oxyhydroxide precursor. Here, we compared the coupled evolution of Fe(II) species, solid phases, and Fe(III) labile throughout the Fe(II)-catalyzed transformation of lepidocrocite (Lp) versus ferrihydrite (Fh) at equal Fe(III) mass loadings with 0.2–1.0 mM Fe(II) aq at pH = 7.0. Similar to Fh, the conversion of Lp to product phases occurs by a dissolution–reprecipitation mechanism mediated by Fe(III) labile that seeds the nucleation of products. Though for Fh we observed a transformation to goethite (Gt), accompanied by the transient emergence and decline of Lp, for initial Lp we observed magnetite (Mt) as the main product. Further, a linear correlation between the formation rate of Mt and the effective supersaturation in terms of Fe(III) labile concentration shows that Fe(II)-induced transformation of Lp into Mt is governed by the classical nucleation theory. When Lp is replaced by equimolar Gt, Mt formation is suppressed by opening a lower barrier pathway to Gt by heterogeneous nucleation and growth on the added Gt seeds. The collective findings add to the mechanistic understanding of factors governing phase selections that impact iron bioavailability, system redox potential, and the fate and transport of coupled elements.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Irradiation Effect on Noble Metal Particles in Water Using in situ Liquid Cell STEM Observation

During geologic disposal of spent nuclear fuel (SNF) in an engineered nuclear waste repository, once all other barriers have degraded, oxidizing may occur at the solid-water interface owing to a self-generated radiolytic field. The repository design includes large quantities of iron (Fe), that is anticipated to corrode under an anoxic environment, and generate hydrogen (H 2 ) gas. This H 2 gas is thought to be able to suppress the dissolution of SNF through a catalytic reaction with noble metal particles (NMP) that are pre-existing in the SNF. This interaction leads to the decomposition of the major oxidant, hydrogen peroxide (H 2 O 2 ). In conclusion, these processes are described in the Fuel Matrix Degradation (FMD) model that is being used to predict SNF degradation rates. The NMP, therefore, plays an important role within the FMD model.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Utilization of municipal solid waste incineration fly ash for sulfoaluminate cement clinker production

Highlights: > The replacement can be taken up to 30% of MSWI fly ash in the raw mix. > The novelty compositional parameters were defined, their optimum values were determined. > Expansive property of SAC is strongly depended on gypsum content. > Three leaching test methods are used to assess the environmental impact. - Abstract: The feasibility of partially substituting raw materials with municipal solid waste incineration (MSWI) fly ash in sulfoaluminate cement (SAC) clinker production was investigated by X-ray diffraction (XRD), compressive strength and free expansion ratio testing. Three different leaching tests were used to assess the environmental impact of the produced material. Experimental results show that the replacement of MSWI fly ash could be taken up to 30% in the raw mixes. The good quality SAC clinkers are obtained by controlling the compositional parameters at alkalinity modulus (C{sub m}) around 1.05, alumina-sulfur ratio (P) around 2.5, alumina-silica ratio (N) around 2.0{approx}3.0 and firing the raw mixes at 1250 deg. C for 2 h. The compressive strengths of SAC are high in early age while that develop slowly in later age. Results also show that the expansive properties of SAC are strongly depended on the gypsum content. Leaching studies of toxic elements in the hydrated SAC-based system reveal that all the investigated elements are well bounded in the clinker minerals or immobilized by the hydration products. Although some limited positive results indicate that the SAC prepared from MSWI fly ash would present no immediate thread to the environment, the long-term toxicity leaching behavior needs to be further studied.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Accelerated carbonation of steel slags in a landfill cover construction

Steel slags from high-alloyed tool steel production were used in a full scale cover construction of a municipal solid waste (MSW) landfill. In order to study the long-term stability of the steel slags within the final cover, a laboratory experiment was performed. The effect on the ageing process, due to i.e. carbonation, exerted by five different factors resembling both the material characteristics and the environmental conditions is investigated. Leaching behaviour, acid neutralization capacity and mineralogy (evaluated by means of X-ray diffraction, XRD, and thermogravimetry/differential thermal analysis, TG/DTA) are tested after different periods of ageing under different conditions. Samples aged for 3 and 10 months were evaluated in this paper. Multivariate data analysis was used for data evaluation. The results indicate that among the investigated factors, ageing time and carbon dioxide content of the atmosphere were able to exert the most relevant effect. However, further investigations are required in order to clarify the role of the temperature.

54 ENVIRONMENTAL SCIENCES↗

Manganese: The overlooked contaminant in the world largest mine tailings dam collapse

Manganese (Mn) is an abundant element in terrestrial and coastal ecosystems and an essential micronutrient in the metabolic processes of plants and animals. Mn is generally not considered a potentially toxic element due to its low content in both soil and water. However, in coastal ecosystems, the Mn dynamic (commonly associated with the Fe cycle) is mostly controlled by redox processes. Here, we assessed the potential contamination of the Rio Doce estuary (SE Brazil) by Mn after the world’s largest mine tailings dam collapse, potentially resulting in chronic exposure to local wildlife and humans. Estuarine soils, water, and fish were collected and analyzed seven days after the arrival of the tailings in 2015 and again two years after the dam collapse in 2017. Using a suite of solid-phase analyses including X-ray absorption spectroscopy and sequential extractions, our results indicated that a large quantity of Mn II arrived in the estuary in 2015 bound to Fe oxyhydroxides. Over time, dissolved Mn and Fe were released from soils when Fe III oxyhydroxides underwent reductive dissolution. Due to seasonal redox oscillations, both Fe and Mn were then re-oxidized to Fe III , Mn III , and Mn IV and re-precipitated as poorly crystalline Fe oxyhydroxides and poorly crystalline Mn oxides. In 2017, redox conditions (Eh: -47 ± 83 mV; pH: 6.7 ± 0.5) favorable to both Fe and Mn reduction led to an increase (~880%) of dissolved Mn (average for 2015: 66 ± 130 μg L -1 ; 2017: 582 ± 626 μg L -1 ) in water and a decrease (~75%, 2015: 547 ± 498 mg kg -1 ; 2017: 135 ± 80 mg kg -1 ) in the total Mn content in soils. The crystalline Fe oxyhydroxides content significantly decreased while the fraction of poorly ordered Fe oxides increased in the soils limiting the role of Fe in Mn retention. The high concentration of dissolved Mn found within the estuary two years after the arrival of mine tailings indicates a possible chronic contamination scenario, which is supported by the high levels of Mn in two species of fish living in the estuary. Our work suggests a high risk to estuarine biota and human health due to the rapid Fe and Mn biogeochemical dynamic within the impacted estuary.

54 ENVIRONMENTAL SCIENCES↗

Radiocarbon analysis as a method for verifying atmospheric CO 2 uptake during carbon mineralization

Sequestration of atmospheric CO 2 is required to constrain the warming of Earth’s climate. Carbon mineralization refers to the precipitation of carbonate minerals by reaction of CO 2 and Mg- and Ca-rich rocks; if the source of the CO 2 is atmospheric and the precipitated carbonate is protected from subsequent dissolution, this process at sufficient scale may be able to reliably draw down atmospheric greenhouse gas levels. Such reactions occur passively in ultramafic settings and previous work has demonstrated that they actively draw down local CO 2 (g) concentrations. However, a method for unambiguously attributing the sequestered carbon solid product to atmospheric sources is still lacking. Here, we test if radiocarbon can be used to verify that the carbon being incorporated into carbonate minerals during carbon mineralization is atmospheric in origin. Additionally, samples from recently exposed ultramafic sites are analyzed and the results demonstrate the utility of this technique for verifying true atmospheric carbon reduction.

58 GEOSCIENCES↗

Calcium Solubility and Cation Exchange Properties in Zeoponic Soil

An important aspect of a regenerative life support system at a Lunar or Martian outpost is the ability to produce food. Essential plant nutrients, as well as a solid support substrate, can be provided by: (1) treated Lunar or Martian regolith; (2) a synthetic soil or (3) some combination of both. A synthetic soil composed of ammonium- and potassium-saturated chinoptlolite (a zeolite mineral) and apatite, can provide slow-release fertilization of plants via dissolution and ion-exchange reactions. Previous equilibrium studies (Beiersdorfer, 1997) on mixtures of synthetic hydroxyapatite and saturated-clinoptilolite indicate that the concentrations of macro-nutrients such as ammonium, phosphorous, potassium, magnesium, and calcium are a function of the ratio of chinoptilolite to apatite in the sample and to the ratio of potassium to ammonium on the exchange sites in the clinoptilolite. Potassium, ammonium, phosphorous, and magnesium are available to plants at sufficient levels. However, calcium is deficient, due to the high degree of calcium adsorption by the clinoptilolite. Based on a series of batch-equilibration experiments, this calcium deficiency can be reduced by (1) treating the clinoptilolite with CaNO3 or (2) adding a second Ca-bearing mineral (calcite, dolomite or wollastonite) to the soil. Treating the Cp with CaNO3 results in increased Ca in solution, decreased P in solution and decreased NH4 in solution. Concentrations of K were not effected by the CaNO3 treatment. Additions of Cal, Dol and Wol changed the concentrations of Ca and P in solution in a systematic fashion. Cal has the greatest effect, Dol the least and Wol is intermediate. The changes are consistent with changes expected for a common ion effect with Ca. Higher concentrations of Ca in solution with added Cal, Dol or Wol do not result in changes in K or NH4 concentrations.

Beiersdorfer, Raymond E.↗

Effects of alloying elements on the formation of < c >-component loops in Zr alloy Excel under heavy ion irradiation.

We report here the microstructural changes occurring in the zirconium alloy Excel (Zr-3.5 wt% Sn-0.8Nb-0.8Mo-0.2Fe) during heavy ion irradiation. In situ irradiation experiments were conducted at reactor operating temperatures on two Zr Excel alloy microstructures with different states of alloying elements, with the states achieved by different solution heat treatments. In the first case, the alloying elements were mostly concentrated in the beta (beta) phase, whereas, in the second case, large Zr-3(Mo,Nb,Fe)(4) secondary phase precipitates (SPPs) were grown in the alpha (alpha) phase by long term aging. The heavy ion induced damage and resultant compositional changes were examined using transmission electron microscopy (TEM) in combination with scanning transmission electron microscope (STEM)-energy dispersive x-ray spectroscopy (EDS) mapping. Significant differences were seen in microstructural evolution between the two different microstructures that were irradiated under similar conditions. Nucleation and growth of < c >-component loops and their dependence on the alloying elements are a major focus of the current investigation. It was observed that the < c >-component loops nucleate readily at 100, 300, and 400 degrees C after a threshold incubation dose (TID), which varies with irradiation temperature and the state of alloying elements. It was found that the TID for the formation of < c >-component loops increases with decrease in irradiation temperature. Alloying elements that are present in the form of SPPs increase the TID compared to when they are in the beta phase solid solution. Dose and temperature dependence of loop size and density are presented. Radiation induced redistribution and clustering of alloying elements (Sn, Mo, and Fe) have been observed and related to the formation of < c >-component loops. It has been shown that at the higher temperature tests, irradiation induced dissolution of precipitates occurs whereas irradiation induced amorphization occurs at 100 degrees C. Furthermore, dose and temperature seem to be the main factors governing the dissolution of SPPs and redistribution of alloying elements, which in turn controls the nucleation and growth of < c >-component loops. The correlation between the microstructural evolution and microchemistry has been found by EDS and is discussed in detail.

Idrees, Yasir↗