Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STACKING FAULT”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

Mechanical behavior of a composite interface: Calcium-silicate-hydrates

The generalized stacking fault (GSF) is a conceptual procedure historically used to assess shear behavior of defect-free crystalline structures through molecular dynamics or density functional theory simulations. We apply the GSF technique to the spatially and chemically complex quasi-layered structure of calcium-silicate-hydrates (C-S-H), the fundamental nanoscale binder within cementitious materials. A failure plane is enforced to calculate the shear traction-displacement response along a composite interface containing highly confined water molecules, hydroxyl groups, and calcium ions. GSF simulations are compared with affine (homogeneous) shear simulations, which allow strain to localize naturally in response to the local atomic environment. Comparison of strength and deformation behavior for the two loading methods shows the composite interface controls bulk shear deformation. Both models indicate the maximum shear strength of C-S-H exhibits a normal-stress dependency typical of cohesive-frictional materials. These findings suggest the applicability of GSF techniques to inhomogeneous structures and bonding environments, including other layered systems such as biological materials containing organic and inorganic interfaces.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Bamboo-like 3C-SiC nanowires with periodical fluctuating diameter: Homogeneous synthesis, synergistic growth mechanism, and their luminescence properties

Herein, bamboo-like 3C-SiC nanowires have been successfully fabricated on homogeneous 6H-SiC substrate by a simple chemical vapor reaction (CVR) approach. The obtained 3C-SiC nanostructure with periodical fluctuating diameter, is composed of two alternating structure units, the typical normal-sized stem segment with perfect crystallinity and obvious projecting nodes segment having high-density stacking faults. The formation of the interesting morphology is significantly subjected to the peculiar growth condition provided by the homogeneous substrate as well as the varying growth elastic energy. Furthermore, the photoluminescence (PL) performance measured on the bamboo-like SiC nanowire shows an intensive emission peaks centered at 451 nm and 467 nm, which has been expected to make a positive progress toward the optical application of the SiC-based one-dimensional (1D) nanostructures, such as light emission diode (LED). - Graphical abstract: Based on the synergistic growth mechanism from homogeneous substrate and elastic energy, bamboo-like 3C-SiC nanowires with periodically fluctuating diameter have been synthesized on 6H-SiC. The blue-violet light emission properties of the bamboo-like nanowires have also been investigated for exploring their peculiar optical application. - Highlights: • Bamboo-like 3C-SiC nanowires with periodically fluctuating diameter have been synthesized on 6H-SiC. • A synergistic growth mechanism from homogeneous substrate and elastic energy has been proposed firstly. • The blue-violet light emission properties of the products displayed peculiar optical application.

36 MATERIALS SCIENCE↗

Characterization of Metamorphic GaAsP/Si Materials and Devices for Photovoltaic Applications

GaAsyP{sub 1-y} anion-sublattice compositionally graded buffers and device structures were grown directly on Si(100) substrates by way of a high-quality GaP integration layer, yielding GaAsP target layers having band gaps of photovoltaic interest (1.65-1.8 eV), free of antiphase domains/borders, stacking faults, and microtwins. GaAsyP{sub 1-y} growths on both Si and GaP substrates were compared via high-resolution X-ray diffractometry of the metamorphic buffers and deep-level transient spectroscopy (DLTS) of p{sup +}-n diodes that are lattice matched to the final buffer layer. Structural analysis indicates highly efficient epitaxial relaxation throughout the entire growth structure for both types of samples and suggests no significant difference in physical behavior between the two types of samples. DLTS measurements performed on GaAsP diodes fabricated on both Si and GaP substrates reveal the existence of identical sets of traps residing in the n-type GaAsP layers in both types of samples: a single majority carrier (electron) trap, which is located at EC - 0.18 eV, and a single minority carrier (hole) trap, which is located at EV + 0.71 eV. Prototype 1.75-eV GaAsP solar cell test devices grown on GaAsyP{sub 1-y}/Si buffers show good preliminary performance characteristics and offer great promise for future high-efficiency III-V photovoltaics integrated with Si substrates and devices.

14 SOLAR ENERGY↗

The influence of temperature on the strain-hardening behavior of Fe-22/25/28Mn-3Al-3Si TRIP/TWIP steels

In this work, the influence of temperature and stacking fault energy (SFE) on the strain-hardening behavior and critical resolved shear stress for twinning was investigated for three Fe–22/25/28Mn–3Al–3Si wt.% transformation- and twinning-induced plasticity (TRIP/TWIP) steels. The SFEs were calculated by two different methods, density functional theory and statistical thermodynamic modeling. The dislocation structure, observed at low levels of plastic deformation, transitions from “planar” to “wavy” dislocation glide with an increase in temperature, Mn content, and/or SFE. The change in dislocation glide mechanisms from planar to wavy reduces the strain hardening rate, in part due to fewer planar obstacles and greater cross slip activity. Additionally, the alloys exhibit a large decrease in strength and ductility with increasing temperature from 25 to 200 °C, attributed to a substantial reduction in the thermally activated component of the flow stress, predominate suppression of TRIP and TWIP, and a significant increase in the critical resolved shear stress for mechanical twinning. Interestingly, the increase in SFE with temperature had a rather minor influence on the critical resolved shear stress for mechanical twinning, and other temperature dependent factors which likely play a more dominant role are discussed.

36 MATERIALS SCIENCE↗

Effect of short-range order on microstructure, texture and strain hardening of cold drawn Cu-10 at.%Mn alloy

Highlights: • Excluding the effect of stacking fault energy, short-range order effect is discussed solely. • Short-range order is beneficial for twinning and slip planarity. • Short-range order promotes the formation of <111> fiber texture. • Strain hardening improving by short-range order. - Abstract: The aim of the present study is to investigate the effect of short-range order (SRO) on the microstructural evolution and mechanical property of Cu-10 at.%Mn alloy during cold drawing deformation. Characterization of the cold drawn Cu-10 at.%Mn alloy samples were performed using transmission electron microscope (TEM) and electron back scattering diffraction (EBSD), and their hardness were also tested. The results show that SRO is beneficial for both twinning and the transition of dislocation glide from wavy slip to planar slip at the low strains. At the high strains, the wavy slip generates due to the destruction of SRO. SRO increases the volume fraction of <111> texture component and the critical strain threshold. Moreover, the presence of SRO significantly improves strain hardening by combining the effects of dislocation, deformation twinning and texture hardening, which results in a significant increase of hardness.

36 MATERIALS SCIENCE↗

Phase transformation and optical properties of Cu-doped ZnS nanorods

ZnS nanorods doped with 0-15 mol% of Cu have been prepared by simple solvothermal process. With gradual increase in the Cu concentration, phase transformation of the doped ZnS nanorods from wurtzite to cubic was observed. Twins and stacking faults were developed due to atomic rearrangement in the heavily doped ZnS nanorods during phase transformation. UV-vis-NIR absorbance spectroscopy ruled out the presence of any impure Cu-S phase. The doped ZnS nanorods showed luminescence over a wide range from UV to near IR with peaks at 370, 492-498, 565 and 730 nm. The UV region peak is due to the near-band-edge transition, whereas, the green peak can be related to emission from elementary sulfur species on the surfaces of the nanorods. The orange emission at 565 nm may be linked to the recombination of electrons at deep defect levels and the Cu(t{sub 2}) states present near the valence band of ZnS. The near IR emission possibly originated from transitions due to deep-level defects. - Graphical abstract: ZnS nanorods doped with 0-15 mol% of Cu has been prepared by simple solvothermal route. Interestingly, phase transformation of the doped ZnS nanorods from wurtzite to cubic was observed with gradual increase in the Cu concentration. Doped ZnS nanorods showed luminescence over a wide range from UV to near IR, which is also a rare observation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Formation of deformation textures in face-centered-cubic materials studied by in-situ high-energy x-ray diffraction and self-consistent model.

The evolution of deformation textures in copper and a brass that are representative of fcc metals with different stacking fault energies (SFEs) during cold rolling is predicted using a self-consistent (SC) model. The material parameters used for describing the micromechanical behavior of each metal are determined from the high-energy X-ray (HEXRD) diffraction data. At small reductions, a reliable prediction of the evolution of the grain orientation distribution that is represented as the continuous increase of the copper and brass components is achieved for both metals when compared with the experimental textures. With increasing deformation, the model could characterize the textures of copper, i.e., the strengthening of the copper component, when dislocation slip is still the dominant mechanism. For a brass at moderate and large reductions, a reliable prediction of its unique feature of texture evolution, i.e., the weakening of the copper component and the strengthening of the brass component, could only be achieved when proper boundary conditions together with some specified slip/twin systems are considered in the continuum micromechanics mainly containing twinning and shear banding. The present investigation suggests that for fcc metals with a low SFE, the mechanism of shear banding is the dominant contribution to the texture development at large deformations.

36 MATERIALS SCIENCE↗

Understanding the deformation behavior of the γ rich transformative Fe 38.5 Mn 20 Co 20 Cr 15 Si 5 Cu 1.5 complex concentrated alloy using in situ synchrotron diffraction

In situ tensile testing coupled with synchrotron x-ray diffraction was used to study the deformation behavior of metastability-engineered Fe 38.5 Mn 20 Co 20 Cr 15 Si 5 Cu 1.5 complex concentrated alloy. Monitoring the evolution of phase fraction and strain hardening response allowed the determination of true critical stress for the onset of the transformation-induced plasticity (TRIP) to be ∼375 MPa, preceded by slip starting at ∼255 MPa. In situ EBSD was used to validate the critical stress for transformation at the microstructure level and observe slip traces to confirm prior slip activity before the transformation. Further, a modeling framework based on stacking fault energy (SFE) was developed to predict the critical stress for transformation. Modeling suggested the SFE of the alloy to fall nearly 15 mJ/m 2 , which agrees well with SFE values calculated using synchrotron peak shifting (12 mJ/m 2 ) and thermodynamic calculation (11 mJ/m 2 ). As a result of γ-fcc to ε-hcp phase transformation, new {0002} ε planes emerged parallel to unaligned {111} γ planes with the tensile loading following S-N orientation relationship. Such selective emergence of new diffraction rings corresponding to ε phase is understood based on the reorientation of γ crystals with reference to tensile axis. In conclusion, this approach can be extended to effectively design alloys based on critical stress required for activating different deformation mechanisms to further push the limits of the strength-ductility envelope.

Complex concentrated alloy↗

Quantitative description of microstructure defects in hexagonal boron nitrides using X-ray diffraction analysis

A routine for simultaneous quantification of turbostratic disorder, amount of puckering and the dislocation and stacking fault density in hexagonal materials was proposed and tested on boron nitride powder samples that were synthesised using different methods. The routine allows the individual microstructure defects to be recognised according to their effect on the anisotropy of the X-ray diffraction line broadening. For quantification of the microstructure defects, the total line broadening is regarded as a linear combination of the contributions from the particular defects. The total line broadening is obtained from the line profile fitting. As testing material, graphitic boron nitride (h-BN) was employed in the form of hot-isostatically pressed h-BN, pyrolytic h-BN or a h-BN, which was chemically vapour deposited at a low temperature. The kind of the dominant microstructure defects determined from the broadening of the X-ray diffraction lines was verified by high resolution transmission electron microscopy. Their amount was attempted to be verified by alternative methods. - Highlights: • Reliable method for quantification of microstructure defects in BN was suggested. • The method is based on the analysis of anisotropic XRD line broadening. • This XRD line broadening is unique and characteristic of the respective defect. • Thus, the quantification of coexistent microstructure defects is possible. • The method was tested on hexagonal BN, which was produced by different techniques.

36 MATERIALS SCIENCE↗

Influences of defects evolvement on the properties of sputtering deposited ZnO:Al films upon hydrogen annealing

Understanding how the defects interact with each other and affect the properties of ZnO:Al films is very important for improving their performance as a transparent conductive oxide (TCO). In the present work, we studied the effects of hydrogen annealing on the structural, optical and electrical properties of ZnO:Al films prepared by magnetron sputtering. High resolution transmission electron microscopy observations reveal that annealing at ∼300 {sup o}C induces the formation of partial dislocations (PD) and stacking faults (SF), which disrupt the lattice periodicity leading to decreased grain size. Annealing at temperatures above ∼500 {sup o}C can remove the PD and SF, but large number of zinc vacancies will be generated. Our results show that when films are annealed at ∼500 {sup o}C, the oxygen-related defects (interstitials O{sub i}, etc.) in the as-grown films can be remarkably removed or converted, which lead to increments in the carrier concentration, mobility, and the transmittance in the visible range. At annealing temperatures above 550 {sup o}C, the hydrogen etching effect becomes predominant, and Al donors are deactivated by zinc vacancies. We also find an abnormal endothermic process by thermal analysis and an abnormal increase in the resistivity during heating the sample under hydrogen atmosphere, based on which the interaction of O{sub i} with the defects (mainly Al donors and PD) is discussed. It is also demonstrated that by annealing the as-grown AZO films at ∼500 {sup o}C under hydrogen atmosphere, high performance TCO films with a low resistivity of 4.48 × 10{sup −4} Ωcm and high transmittance of above 90% in the visible light are obtained.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Temperature-Dependent Mechanical Properties of Ni-Based Concentrated Alloys: Insights from First-Principles Calculations

The present work focuses on predicting temperature-dependent mechanical properties of Ni-based concentrated alloys Ni 18 Cr 10 Co 10 Fe 6 M 4 (abbreviated by X 44 M 4 , with M = Al, V, Mn, Fe, Nb, Mo, and W) using density functional theory (DFT). These predictions are based on shear (plastic) and elastic deformations, utilizing the special quasirandom structure (SQS), the phonon-based quasiharmonic approach (QHA), and the quasistatic approach. The resulting properties include coefficient of thermal expansion via QHA, ideal shear strength (τ IS ), and stable and unstable stacking fault energies (γ SF and γ US ) through pure alias shear deformation, and elastic constants (c ij ), bulk modulus (B 0 ), and shear modules (G 0 ) via elastic deformation. Notably, predicting accurate γ SF is challenging due to uncertainties that can exceed the γ SF values. τ IS and γ US exhibit a strong linear relationship, enabling the accurate prediction of γ US based on the precisely determined τ IS . All mechanical properties of X 44 M 4 decrease with increasing temperature, except for some γ SF cases such as X 44 M 4 with M = V, Mn, Fe, Mo, and W. Among the X 44 M 4 alloys, X 44 Nb 4 exhibits the lowest τ IS , γ US , and G 0 values, and the highest B 0 /G 0 ratio, while X 44 Mn 4 has the lowest B 0 and B 0 /G 0 ratio. We found that volume is a crucial descriptor for understanding and modeling mechanical properties (except B0 and maybe also γ SF ) affected by alloying elements and temperature. Ni-based dilute alloys (e.g., Ni 11 M 1 and Ni 31 M 1 ) and concentrated alloys (e.g., X 44 M 4 ) show similar trends in mechanical properties influenced by alloying elements and temperature, simplifying the analysis and design of Ni-based alloys.

Elastic properties↗

Effects of strain rate on mechanical properties and deformation behavior of an austenitic Fe-25Mn-3Al-3Si TWIP-TRIP steel

The effects of quasi-static and low-dynamic strain rate (ε = 10 –4 /s to ε = 10 2 /s) on tensile properties and deformation mechanisms were studied in a Fe-25Mn-3Al-3Si (wt%) twinning and transformation-induced plasticity [TWIP-TRIP] steel. The fully austenitic microstructure deforms primarily by dislocation glide but due to the room temperature stacking fault energy [SFE] of 21 ± 3 mJ/m 2 for this alloy, secondary deformation mechanisms such as mechanical twinning (TWIP) and epsilon martensite formation (TRIP) also play an important role in the deformation behavior. The mechanical twins and epsilon-martensite platelets act as planar obstacles to subsequent dislocation motion on non-coplanar glide planes and reduce the dislocation mean free path. A high-speed thermal camera was used to measure the increase in specimen temperature as a function of strain, which enabled the use of a thermodynamic model to predict the increase in SFE. The influence of strain rate and strain on microstructural parameters such as the thickness and spacing of mechanical twins and epsilon-martensite laths was quantified using dark field transmission electron microscopy, electron channeling contrast imaging, and electron backscattered diffraction. The effect of sheet thickness on mechanical properties was also investigated. Increasing the tensile specimen thickness increased the product of ultimate tensile strength and total elongation, but had no significant effect on uniform elongation or yield strength. The yield strength exhibited a significant increase with increasing strain rate, indicating that dislocation glide becomes more difficult with increasing strain rate due to thermally-activated short-range barriers. Finally, a modest increase in ultimate tensile strength and minimal decrease in uniform elongation were noted at higher strain rates, suggesting adiabatic heating, slight changes in strain-hardening rate and observed strain localizations as root causes, rather than a significant change in the underlying TWIP-TRIP mechanisms at low values of strain.

36 MATERIALS SCIENCE↗

High-Efficiency Non-Polar GaN-Based LEDs

Inlustra Technologies with subcontractor U.C. Santa Barbara conducted a project with the principle goal of demonstrating high internal quantum efficiency blue (430 nm) and green (540nm) light emitting diodes (LEDs) on low-defect density non-polar GaN wafers. Inlustra pursued the fabrication of smooth thick a-plane and m-plane GaN films, as well as defect reduction techniques such as lateral epitaxial overgrowth (LEO) to uniformly lower dislocation density in these films. Limited free-standing wafers were produced as well. By the end of the reporting period, Inlustra had met its milestone of dislocation reduction to < 5 x 10{sup 6} cm{sup -2}. Stacking faults were still present in appreciable density ({approx} 1 x 10{sup 5} cm{sup -1}), but were not the primary focus of defect reduction since there have been no published studies establishing their detrimental effects on LED performance. Inlustra's LEO progress built a solid foundation upon which further commercial development of GaN substrates will occur. UCSB encountered multiple delays in its LED growth and fabrication efforts due to unavoidable facilities outages imposed by ongoing construction in an area adjacent to the metalorganic chemical vapor deposition (MOCVD) laboratory. This, combined with the large amount of ab initio optimization required for the MOCVD system used during the project, resulted in unsatisfactory LED progress. Although numerous blue-green photoluminescence results were obtained, only a few LED structures exhibited electroluminescence at appreciable levels. UCSB also conducting extensive modeling (led by Prof. Van de Walle) on the problem of non-radiative Auger recombination in GaN-based LED structures, which has been posited to contribute to LED efficiency 'droop' at elevated current density. Unlike previous modeling efforts, UCSB's approach was truly a first-principles ab initio methodology. Building on solid numerical foundations, the Auger recombination rates of In{sub x}Ga{sub 1-x}N alloys were calculated from first-principles density-functional and many-body-perturbation theory. The differing mechanisms of inter- and intra-band recombination were found to affect different parts of the emission spectrum. In the blue to green spectral region and at room temperature the Auger coefficient was calculated to be as large as 2 x 10{sup -30} cm{sup 6} s{sup -1}; in the infrared it is even larger. These results indicated that Auger recombination may be responsible for the loss of quantum efficiency that affects InGaN-based light emitters, whether on non-polar or polar crystal planes.

36 MATERIALS SCIENCE↗

Monoclinic crystal structure of α - RuCl 3 and the zigzag antiferromagnetic ground state

We have proposed the layered honeycomb magnet α - RuCl 3 as a candidate to realize a Kitaev spin model with strongly frustrated, bond-dependent, anisotropic interactions between spin-orbit entangled j eff = 1/2 Ru 3 + magnetic moments. We report a detailed study of the three-dimensional crystal structure using x-ray diffraction on untwinned crystals combined with structural relaxation calculations. We consider several models for the stacking of honeycomb layers and find evidence for a parent crystal structure with a monoclinic unit cell corresponding to a stacking of layers with a unidirectional in-plane offset, with occasional in-plane sliding stacking faults, in contrast with the currently assumed trigonal three-layer stacking periodicity. We also report electronic band-structure calculations for the monoclinic structure, which find support for the applicability of the j eff = 1/2 picture once spin-orbit coupling and electron correlations are included. Of the three nearest-neighbor Ru-Ru bonds that comprise the honeycomb lattice, the monoclinic structure makes the bond parallel to the b axis nonequivalent to the other two, and we propose that the resulting differences in the magnitude of the anisotropic exchange along these bonds could provide a natural mechanism to explain the previously reported spin gap in powder inelastic neutron scattering measurements, in contrast to spin models based on the three-fold symmetric trigonal structure, which predict a gapless spectrum within linear spin wave theory. Our susceptibility measurements on both powders and stacked crystals, as well as magnetic neutron powder diffraction, show a single magnetic transition upon cooling below T N ≈ 13 K. Our analysis of our neutron powder diffraction data provides evidence for zigzag magnetic order in the honeycomb layers with an antiferromagnetic stacking between layers. Magnetization measurements on stacked single crystals in pulsed field up to 60 T show a single transition around 8 T for in-plane fields followed by a gradual, asymptotic approach to magnetization saturation, as characteristic of strongly anisotropic exchange interactions.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of radiation damage in 3D printed SiC

The SiC fuel matrix for advanced gas-cooled high temperature reactors as part of the Transformational Challenge Reactor program serves as the fuel particle container structure, a barrier to fission gas release, and a heat transfer medium. Its performance is particularly important because the fuel matrix must demonstrate good structural stability and thermal behaviors. An additive manufacturing methodology combining a binder jet 3D printing process with chemical vapor infiltration (CVI) for the production of SiC was recently developed. In this study, post irradiation examination by transmission electron microscopy shows that defect accumulation within the printed particles is very similar to other forms of high-purity SiC. However, damage accumulation was not directly observed in the CVI matrix because black spot damage and dislocation loops are difficult to image within the nanoscale highly faulted CVI matrix and because interstitial defects may rapidly annihilate at the stacking faults. Therefore, electron energy loss spectroscopy (EELS) analysis was used to analyze defect swelling in both the printed particles and the CVI matrix. The EELS analysis helped reveal that the radiation-induced swelling in the CVI matrix is similar to that of the printed SiC particles. This work shows that 3D printed SiC has behavior that is comparable to SiC processed by other means and that 3D printing could serve as a suitable processing technique for high-purity SiC for nuclear applications.

36 MATERIALS SCIENCE↗

Phase transformations of Al-bearing high-entropy alloys Al x CoCrFeNi (x = 0, 0.1, 0.3, 0.75, 1.5) at high pressure

Pressure-induced structural modifications in high-entropy alloys with varying Al contents, Al x CoCrFeNi (x = 0, 0.1, 0.3, 0.75, 1.5), have been investigated at pressures up to ~50 GPa by synchrotron X-ray diffraction and, following depressurization, by transmission electron microscopy (TEM). In Al x CoCrFeNi compounds with x ≤ 0.3, all of which exhibit an initial single-phase face-centered cubic (fcc) structure, proportionality between the Al content and the critical pressure for transformation to hexagonal close-packed (hcp) phases, distinguished by a distinct planar stacking sequence, is observed. This is attributed to the structural distortion arising from the large size of Al atoms relative to those of the other constituent elements, which results in an increase in the formation energy of stacking faults and a decrease in compressibility. High-resolution TEM results demonstrate variation of the stacking sequence from ABCABC, typical of fcc materials, to ABABAB, typical of hcp materials, in CoCrFeNi following high pressure. In Al 0.75 CoCrFeNi, which exhibits an initial dual-phase structure [fcc and body-centered cubic (bcc)], the result again shows the formation of a (hcp) phase despite its higher Al content, suggesting that the bcc phase may be more amenable to pressure-induced phase modification than is the fcc phase, which is absent for lower Al contents. However, the trend of transformation inhibition by increasing the Al content is again observed, with Al 1.5 CoCrFeNi retaining its initial structure up to the highest pressure achieved. Furthermore the determination of these compositional trends in the high-pressure phase response of these materials may enable the production of new phase mixtures with precisely tuned phase proportions and potentially desirable properties.

36 MATERIALS SCIENCE↗

Multilevel atomic structural model for interstratified opal materials

The structure of opal has long fascinated scientists. It occurs in a number of structural states, ranging from amorphous to exhibiting features of stacking disorder. Opal-CT, where C and T signify cristobalite- and tridymite-like interstratification, represents an important link in the length scales between amorphous and crystalline states. However, details about local atomic (dis)order and arrangements extending to long-range stacking faults in opal polymorphs remain incompletely understood. Here, a multilevel modeling approach is reported that considers stacking states in correlation with the abundance of C and T segments as a high-level structural parameter (i.e. not each atom). Optimization accounting for inter-tetrahedral bond lengths and angles and the regularity of the silicate tetrahedra is included as lower levels of structural parameters. Together, a set of parameters with both coarse-grained and atomistic features for different levels of structural details is refined. Structural disorder at the ~10–100 Å distance scale is evaluated using experimental pair distribution function and diffraction datasets, comparing peak intensities, widths and asymmetry. Here this work presents a complete multilevel structural description of natural opal-CT and explains many of the unusual features observed in X-ray powder diffraction patterns. This modeling approach can be adopted generally for analyzing layered materials and their assembly into 3D structures.

36 MATERIALS SCIENCE↗

Design metastability in high-entropy alloys by tailoring unstable fault energies

Metastable alloys with transformation-/twinning-induced plasticity (TRIP/TWIP) can overcome the strength-ductility trade-off in structural materials. Originated from the development of traditional alloys, the intrinsic stacking fault energy (ISFE) has been applied to tailor TRIP/TWIP in high-entropy alloys (HEAs) but with limited quantitative success. Here, we demonstrate a strategy for designing metastable HEAs and validate its effectiveness by discovering seven alloys with experimentally observed metastability for TRIP/TWIP. We propose unstable fault energies as the more effective design metric and attribute the deformation mechanism of metastable face-centered cubic alloys to unstable martensite fault energy (UMFE)/unstable twin fault energy (UTFE) rather than ISFE. Among the studied HEAs and steels, the traditional ISFE criterion fails in more than half of the cases, while the UMFE/UTFE criterion accurately predicts the deformation mechanisms in all cases. The UMFE/UTFE criterion provides an effective paradigm for developing metastable alloys with TRIP/TWIP for an enhanced strength-ductility synergy.

36 MATERIALS SCIENCE↗