At least 541 records · Page 30

Microstructural evolution during solution treatment of Co-Cr-Mo-C biocompatible alloys

Three different Co-Cr-Mo-C alloys conforming to ASTM F75 standard were poured in an industrial environment and subjected to a conventional solution treatment at 1225 Degree-Sign C for several time intervals. The microstructural changes and transformations were studied in each case in order to evaluate the way in which treatment time influences the secondary phase fraction and clarify the microstructural changes that could occur. To assess how treatment time affects microstructure, optical microscopy and image analyzer software, scanning electron microscopy and energy dispersion spectrometry analysis were employed. The main phases detected in the as-cast state were: {sigma}-phase, M{sub 6}C, and M{sub 23}C{sub 6} carbides. The latter presented two different morphologies, blocky type and lamellar type. Despite being considered the most detrimental feature to mechanical properties, {sigma}-phase and lamellar carbides dissolution took place in the early stages of solution treatment. M{sub 23}C{sub 6} carbides featured two different behaviors. In the alloy obtained by melting an appropriate quantity of alloyed commercial materials, a decrease in size, spheroidization and transformation into M{sub 6}C carbides were simultaneously observed. In the commercial ASTM F75 alloy, in turn, despite being the same phase, only a marked decrease in precipitates size was noticed. These different behaviors could be ascribed to the initial presence of other phases in the alloy obtained from alloyed materials, such as {sigma}-phase and 'pearlitic' carbides, or to the initial precipitate size which was much larger in the first than in the commercial ASTM F75 alloy studied. M{sub 6}C carbides dissolved directly in the matrix as they could not be detected in samples solution-treated for 15 min. - Highlights: Black-Right-Pointing-Pointer Three different Co-Cr-Mo alloys were poured under an industrial environment. Black-Right-Pointing-Pointer Transformation of existing phases followed during conventional solution treatment. Black-Right-Pointing-Pointer In as-cast/treated samples, phases were identified by color metallography, SEM and EDS. Black-Right-Pointing-Pointer M{sub 23}C{sub 6} {yields} M{sub 6}C transformation was corroborated by SEM and EDS analysis. Black-Right-Pointing-Pointer Carbide spheroidization was also detected prior a noticeably carbide size decreasing.

36 MATERIALS SCIENCE↗

Ca Addition Effects on the Microstructure, Tensile and Corrosion Properties of Mg Matrix Alloy Containing 8 wt.% Mg{sub 2}Si

The microstructure, tensile properties and corrosion behavior of the Mg-8 wt.% Mg{sub 2}Si-x%Ca alloy have been studied by the use of optical microscopy, scanning electron microscopy equipped with energy-dispersive spectroscopy, x-ray diffraction, standard tensile testing, polarization test and electrochemical impedance spectroscopy (EIS) measurements. Microstructural studies indicated that Ca modifies both primary and eutectic Mg{sub 2}Si phase. It was found that the average size of primary Mg{sub 2}Si particles is about 60 μm, which is dropped by about 82% in the alloy containing 0.05 wt.% Ca. By the addition of different Ca contents, Ca-rich intermetallics (i.e., CaSi{sub 2} and CaMgSi) were formed. The modification mechanism of adding Ca during solidification was found to be due to the strong effect of CaMgSi phase as a heterogonous nucleation site, apart from CaSi{sub 2} which was reported before, for Mg{sub 2}Si intermetallics. Tensile testing results ascertained that Ca addition enhances both ultimate tensile strength (UTS) and elongation values. The optimum amount of Ca was found to be 0.1 wt.%, which improved UTS and elongation values from about 130 MPa and 2% to 165 MPa and 5.5%, whereas more Ca addition (i.e., 3 wt.%) reduced the tensile properties of the alloy to about 105 MPa and 1.8%, which can be due to the formation of CaMgSi intermetallics with deteriorating needle-like morphology. Polarization and EIS tests also showed that the Mg-3%Si-0.5%Ca alloy pronounces as the best anti-corrosion alloy. Nevertheless, further added Ca (up to 3 wt.%) deteriorated the corrosion resistance due to predominance of worse galvanic coupling effect stemmed from the presence of stronger CaMgSi cathode in comparison with Mg{sub 2}Si. With higher Ca additions, an adverse effect was seen on corrosion resistance of the Mg-3%Si alloy, as a result of forming a weak film on the alloy specimen surface.

36 MATERIALS SCIENCE↗

Stainless steel corrosion by molten nitrates : analysis and lessons learned.

A secondary containment vessel, made of stainless 316, failed due to severe nitrate salt corrosion. Corrosion was in the form of pitting was observed during high temperature, chemical stability experiments. Optical microscopy, scanning electron microscopy and energy dispersive spectroscopy were all used to diagnose the cause of the failure. Failure was caused by potassium oxide that crept into the gap between the primary vessel (alumina) and the stainless steel vessel. Molten nitrate solar salt (89% KNO{sub 3}, 11% NaNO{sub 3} by weight) was used during chemical stability experiments, with an oxygen cover gas, at a salt temperature of 350-700 C. Nitrate salt was primarily contained in an alumina vessel; however salt crept into the gap between the alumina and 316 stainless steel. Corrosion occurred over a period of approximately 2000 hours, with the end result of full wall penetration through the stainless steel vessel; see Figures 1 and 2 for images of the corrosion damage to the vessel. Wall thickness was 0.0625 inches, which, based on previous data, should have been adequate to avoid corrosion-induced failure while in direct contact with salt temperature at 677 C (0.081-inch/year). Salt temperatures exceeding 650 C lasted for approximately 14 days. However, previous corrosion data was performed with air as the cover gas. High temperature combined with an oxygen cover gas obviously drove corrosion rates to a much higher value. Corrosion resulted in the form of uniform pitting. Based on SEM and EDS data, pits contained primarily potassium oxide and potassium chromate, reinforcing the link between oxides and severe corrosion. In addition to the pitting corrosion, a large blister formed on the side wall, which was mainly composed of potassium, chromium and oxygen. All data indicated that corrosion initiated internally and moved outward. There was no evidence of intergranular corrosion nor were there any indication of fast pathways along grain boundaries. Much of the pitting occurred near welds; however this was the hottest region in the chamber. Pitting was observed up to two inches above the weld, indicating independence from weld effects.

36 MATERIALS SCIENCE↗

A High Temperature Electrochemical Energy Storage System Based on Sodium Beta-Alumina Solid Electrolyte (Base)

This report summarizes the work done during the period September 1, 2005 and March 31, 2008. Work was conducted in the following areas: (1) Fabrication of sodium beta{double_prime} alumina solid electrolyte (BASE) using a vapor phase process. (2) Mechanistic studies on the conversion of {alpha}-alumina + zirconia into beta{double_prime}-alumina + zirconia by the vapor phase process. (3) Characterization of BASE by X-ray diffraction, SEM, and conductivity measurements. (4) Design, construction and electrochemical testing of a symmetric cell containing BASE as the electrolyte and NaCl + ZnCl{sub 2} as the electrodes. (5) Design, construction, and electrochemical evaluation of Na/BASE/ZnCl{sub 2} electrochemical cells. (6) Stability studies in ZnCl{sub 2}, SnCl{sub 2}, and SnI{sub 4} (7) Design, assembly and testing of planar stacks. (8) Investigation of the effect of porous surface layers on BASE on cell resistance. The conventional process for the fabrication of sodium ion conducting beta{double_prime}-alumina involves calcination of {alpha}-alumina + Na{sub 2}CO{sub 3} + LiNO{sub 3} at 1250 C, followed by sintering powder compacts in sealed containers (platinum or MgO) at {approx}1600 C. The novel vapor phase process involves first sintering a mixture of {alpha}-alumina + yttria-stabilized zirconia (YSZ) into a dense ceramic followed by exposure to soda vapor at {approx}1450 C to convert {alpha}-alumina into beta{double_prime}-alumina. The vapor phase process leads to a high strength BASE, which is also resistant to moisture attack, unlike BASE made by the conventional process. The PI is the lead inventor of the process. Discs and tubes of BASE were fabricated in the present work. In the conventional process, sintering of BASE is accomplished by a transient liquid phase mechanism wherein the liquid phase contains NaAlO{sub 2}. Some NaAlO{sub 2} continues to remain at grain boundaries; and is the root cause of its water sensitivity. In the vapor phase process, NaAlO{sub 2} is never formed. Conversion occurs by a coupled transport of Na{sup +} through BASE formed and of O{sup 2-} through YSZ to the reaction front. Transport to the reaction front is described in terms of a chemical diffusion coefficient of Na{sub 2}O. The conversion kinetics as a function of microstructure is under investigation. The mechanism of conversion is described in this report. A number of discs and tubes of BASE have been fabricated by the vapor phase process. The material was investigated by X-ray diffraction (XRD), optical microscopy and scanning electron microscopy (SEM), before and after conversion. Conductivity (which is almost exclusively due to sodium ion transport at the temperatures of interest) was measured. Conductivity was measured using sodium-sodium tests as well as by impedance spectroscopy. Various types of both planar and tubular electrochemical cells were assembled and tested. In some cases the objective was to determine if there was any interaction between the salt and BASE. The interaction of interest was mainly ion exchange (possible replacement of sodium ion by the salt cation). It was noted that Zn{sup 2+} did not replace Na+ over the conditions of interest. For this reason much of the work was conducted with ZnCl{sub 2} as the cathode salt. In the case of Sn-based, Sn{sup 2+} did ion exchange, but Sn{sup 4+} did not. This suggests that Sn{sup 4+} salts are viable candidates. These results and implications are discussed in the report. Cells made with Na as the anode and ZnCl{sub 2} as the cathode were successfully charged/discharged numerous times. The key advantages of the batteries under investigation here over the Na-S batteries are: (1) Steel wool can be used in the cathode compartment unlike Na-S batteries which require expensive graphite. (2) Planar cells can be constructed in addition to tubular, allowing for greater design flexibility and integration with other devices such as planar SOFC. (3) Comparable or higher open circuit voltage (OCV) than the Na-S battery. (4) Wider operating temperature range and higher temperature operation than the Na-S battery. (5) If a cell fails, it fails in the short circuit mode unlike Na-S batteries. Also, cells were successfully subjected to several freeze-thaw cycles. Finally, the feasibility of assembling a planar stack was explored. A two cell stack was assembled and tested. A five cell stack was assembled.

25 ENERGY STORAGE↗

MICROSTRUCTURE OF LONG-TERM AGED IN617 NI-BASE SUPERALLOY

The microstructure of the Ni-base superalloy IN617 that had undergone prolonged aging (approximately 65,000 hours) at a series of temperatures from 482 C to 871 C has been characterized by microhardness measurements, optical microscopy, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). Cr23C6, Mo-rich eta-M6C, and Ti(C,N) constitute the major primary coarse precipitates both within the grains and along the grain boundaries. The secondary carbides were mostly fine Cr23C6, which had a cube-on-cube orientation relationship (OR) with the fcc matrix, and at long times were present in cuboidal and plate-shape forms within the grains and as films along the grain boundaries. Fine, eta-M6C carbides were also observed at low to intermediate temperatures with an OR given by [011] carbide//[011] matrix, carbide// matrix. The coarse eta-M6C carbides increased in extent at 871 C, whereas the counterpart fine carbides were absent. The phase was found to be present at all aging temperatures up to 871 C, with a volume fraction ranging from very low to approximately 5 pct at 593 C, where the peak in microhardness occurs. The observations have also suggested that the presence of a very small amount of at temperatures as high as 871 C at long times may be associated with a reaction between the fine eta-carbides and the matrix. Ultrafine precipitates of the intermetallic phase Ni2(Cr,Mo) with the Pt2Mo-type structure was observed in addition to in samples aged for 28,300 hours at the lowest aging temperature of 482 C. These precipitates were absent in samples aged at higher temperatures. The various observations made have suggested that the long-term thermal stability of the IN617 alloy is reasonably good over a wide temperature range of 538 C to 704 C, whereas at higher temperatures (871 C), the substantial decrease in the volume fraction of and coarsening and clustering of the carbides lead to a large drop in the microhardness. A modified time-temperature-transformation (TTT) diagram was constructed based on the results of this study and comparison with previous reports.

36 MATERIALS SCIENCE↗

Elemental segregation and subsequent precipitation during solidification of continuous cast Nb–V–Ti high-strength low-alloy steels

In this study, elemental segregation during solidification and subsequent precipitation behaviour in a continuous cast Nb–V–Ti high-strength low-alloy steel was investigated by optical microscopy, scanning electron microscopy with energy dispersive X-ray spectroscopy and thermodynamic modelling. It is known that for steels with low carbon contents the pearlite that forms on slow cooling does so where the interdendritic liquid was present prior to final solidification. The alloying elements of Nb, Ti, Mn and V segregate into the interdendritic liquid during solidification, while Al preferentially segregates into the solidifying solid phase. The composition analysis on the slab samples verified the predicted element segregation behaviour, with a smaller difference in the concentrations of Mn and V in the pearlite and dendritic ferrite regions being observed compared to the Nb levels. Small (30–100 nm) spherical or irregular shaped Nb-rich precipitates (Nb(C, N) and (Nb, V)(C, N)) were mainly found in the pearlite regions, while angular Al-rich (60–300 nm) precipitates were found in the dendritic ferrite regions, in the form of AlN and complex AlN–V(C, N) precipitates. Small isolated ferrite regions surrounded by pearlite were observed in the microstructure and has two origins: one type is dendritic ferrite that appears as an isolated island due to a sectioning effect when observing the two-dimensional microstructure; the other is a ferrite idiomorph that forms in the interdendritic region due to the low carbon content of the steel. Accordingly, in these isolated ferrite islands two different precipitation behaviours are found; predominantly Al-rich particles in the dendritic regions or predominantly Nb-rich precipitates in the interdendritic ferrite idiomorphs. No Al-rich precipitates were observed in the interdendritic regions (pearlite or isolated ferrite idiomorphs) despite the Thermo-Calc predictions indicating a higher volume fraction of AlN in these regions compared to the dendritic regions. This is believed to be due to back diffusion of nitrogen after solidification reducing the available nitrogen, which reacts with the high Nb levels present. - Highlights: • Nb-rich precipitates (Nb(C, N) and (Nb, V)(C, N)) were mainly found in pearlite. • Angular Al-rich precipitates (AlN and AlN–V(C, N)) were found in dendritic ferrite. • Precipitation behaviour in isolated ferrite islands within pearlite was revealed. • Segregation of substitutional elements during solidification is retained. • Back diffusion of interstitial elements (C, N) occurred.

36 MATERIALS SCIENCE↗

0.22 THz wideband sheet electron beam traveling wave tube amplifier: Cold test measurements and beam wave interaction analysis

In this paper, we describe micro-fabrication, RF measurements, and particle-in-cell (PIC) simulation modeling analysis of the 0.22 THz double-vane half period staggered traveling wave tube amplifier (TWTA) circuit. The TWTA slow wave structure comprised of two sections separated by two sever ports loaded by loss material, with integrated broadband input/output couplers. The micro-metallic structures were fabricated using nano-CNC milling and diffusion bonded in a three layer process. The 3D optical microscopy and SEM analysis showed that the fabrication error was within 2-3 {mu}m and surface roughness was measured within 30-50 nm. The RF measurements were conducted with an Agilent PNA-X network analyzer employing WR5.1 T/R modules with a frequency range of 178-228 GHz. The in-band insertion loss (S{sub 21}) for both the short section and long section (separated by a sever) was measured as {approx}-5 dB while the return loss was generally around {approx}-15 dB or better. The measurements matched well with the S-matrix simulation analysis that predicted a 3 dB bandwidth of {approx}45 GHz with an operating frequency at 220 GHz. However, the measured S{sub 21} was {approx}3 dB less than the design values, and is attributed to surface roughness and alignment issues. The confirmation measurements were conducted over the full frequency band up to 270 GHz employing a backward wave oscillator (BWO) scalar network analyzer setup employing a BWO in the frequency range 190 GHz-270 GHz. PIC simulations were conducted for the realistic TWT output power performance analysis with incorporation of corner radius of 127 {mu}m, which is inevitably induced by nano-machining. Furthermore, the S{sub 21} value in both sections of the TWT structure was reduced to correspond to the measurements by using a degraded conductivity of 10% International Annealed Copper Standard. At 220 GHz, for an elliptic sheet electron beam of 20 kV and 0.25 A, the average output power of the tube was predicted to be reduced from 90 W (for ideal conductivity/design S-parameters) to 70 W (for the measured S-parameters/inferred conductivity) for an average input power of 50 mW. The gain of the tube remains reasonable: {approx}31.4 dB with an electronic efficiency of {approx}1.4%. The same analysis was also conducted for several frequencies between 190 GHz-260 GHz. This detailed realistic PIC analysis demonstrated that this nano-machined TWT circuit has slightly reduced S-parameters and output power from design, but within an acceptable range and still have promising output power, gain, and band width as required. Thus, we expect to meet the specifications of 1000 W-GHz for the darpa program goals.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Fe-24 wt.%Cr-4.1 wt.%C hardfacing alloy: Microstructure and carbide refinement mechanisms with ceria additive

The microstructure and carbide refinement mechanisms of Fe-24 wt.%Cr-4.1 wt.%C hardfacing alloys with 0 wt.%, 0.5 wt.%, 1.0 wt.%, 2 wt.%, and 4 wt.% ceria additives have been systematically investigated in this work. Optical microscopy, field emission scanning electron microscopy with energy dispersive spectrometer, and X-ray diffraction were collectively used to study the microstructure, the phase components, and the chemical formation of inclusion formed in the welding process. Wear-resistance of the alloys was comparatively studied using an abrasive wear testing machine. The structure analysis results show that the Fe-Cr-C hardfacing alloy mainly consists of martensite, retained austenite, MC carbide and M{sub 7}C{sub 3} carbide. With increasing ceria additive contents, the average size of the primary M{sub 7}C{sub 3} carbide decreases and reaches a most refined state in the alloy with 2 wt.% ceria additives. Comparative wear tests data shows that the wear resistance of the hardfacing alloys with ceria additives is better than that without ceria additive. In a good agreement with the carbide refinement results, the wear resistance of the alloy reaches an optimum level in the sample with 2 wt.% ceria additive. The main RE inclusion type identified with in-situ XRD analysis is RE inclusion Ce{sub 2}O{sub 2}S. Thermodynamics calculation confirms that this type of RE inclusion could precipitate prior to M{sub 7}C{sub 3} carbides, and act as a heterogeneous nucleus for M{sub 7}C{sub 3} in the welding process, which effectively provides a mechanism for significant refinement of the M{sub 7}C{sub 3} carbide and improves its wear resistance. - Graphical Abstract: Rare Earth inclusion (Ce{sub 2}O{sub 2}S) distributes in the primary M{sub 7}C{sub 3} carbide. Moreover, Ce{sub 2}O{sub 2}S, which acts as heterogeneous nuclei of the primary M{sub 7}C{sub 3} carbide, is medium effective. Therefore, the primary M{sub 7}C{sub 3} carbide has been refined. Highlights: Black-Right-Pointing-Pointer Micro-hardness of primary M{sub 7}C{sub 3} carbide in Fe-Cr-C hardfacing alloy is 1594 HV. Black-Right-Pointing-Pointer RE inclusion Ce{sub 2}O{sub 2}S can be observed in the primary M{sub 7}C{sub 3} carbide. Black-Right-Pointing-Pointer Ce{sub 2}O{sub 2}S as heterogeneous nuclei of the Cr{sub 7}C{sub 3} is medium effective. Black-Right-Pointing-Pointer Primary carbide is most refined with 2 wt.% ceria additive.

36 MATERIALS SCIENCE↗

Double patterning HSQ processes of zone plates for 10 nm diffraction limitedperformance

In e-beam lithography, fabrication of sub-20 nm dense structures is challenging. While there is a constant effort to develop higher resolution resist processes, the progress of increasing pattern density is slow. For zone plates, consisting of dense lines and spaces, the outermost zone width has been limited to slightly less than 20 nm due to effects such as low aerial image contrast, forward scattering, intrinsic resist resolution, and development issues. To circumvent these effects, we have successfully developed a new double patterning HSQ process, and as a result, we have fabricated zone plates of 10 and 12 nm using the process. We previously developed a double patterning process in which a dense zone plate pattern is sub-divided into two semi-isolated, complementary zone set patterns. These patterns are fabricated separately and then overlaid with high accuracy to yield the desired pattern. The key to success with this process is the accuracy of the overlay. For diffraction-limited zone plates, accuracy better than one-third of the smallest zone width is needed. In our previous work, the zone set patterns were formed using PMMA and gold electroplating, which were overlaid and aligned to the zero-level mark layer with sub-pixel accuracy using our internally developed algorithm. The complete zone plate fabrication was conducted in-house. With this process, we successfully fabricated zone plates of 15 nm outermost zone. Using this zone plate, we were able to achieve sub-15 nm resolution at 1.52 nm wavelength, the highest resolution ever demonstrated in optical microscopy at that time. We attempted to extend the process to fabricating 12 nm and smaller zones. However, the modest PMMA contrast, combined with a relatively large electron beam size compared to the target feature sized limited the process latitude. To overcome this problem, we developed a new overlay process based on high resolution negative tone resist of hydrogen silsesquioxane (HSQ). With the development in TMAH at 45 C, we can reliably achieve zone width as small as 8 nm with negligible line edge roughness in the semi-dense zone set. Such narrow zones in HSQ, however, detach easily from the gold plating base substrate needed for the electroplating step. We developed a process to condition the gold substrate with (3-mercaptopropyl) trimethoxysilane, or 3-MTP, which can form a homogeneous hydroxylation surface on gold surface and bond with hydroxyl in HSQ. Fig 2 shows the basic process steps of the double patterning HSQ process. Unlike the PMMA process, both zone sets are formed in HSQ and overlaid, and the complete zone plate pattern is converted to gold using electroplating in the final step. Using the new process, we successfully realized zone plates of 10 nm and 12 nm outermost zones. Fig. 3 shows the SEM micrographs of the zone plates outer regions. The zone plates are 30 nm thick in gold. To the best of our knowledge, these zone plates have the smallest zonal features ever fabricated using e-beam lithography. The complete zone plate fabrication was conducted in-house, using our vector scan electron beam lithography tool, the Nanowriter, which has a measured beam diameter of 6.5 nm (FWHM) at 100 keV. An internally developed, sub-pixel alignment algorithm, based on auto/cross-correlation methods, was used for the overlay. A 12 nm zone plate was tested with a full-field transmission x-ray microscope at the LBNL's Advanced Light Source. Fig. 4 shows an x-ray image of a 40 nm thick gold radial spoke pattern taken with the zone plate at 1.75 nm wavelength (707eV, FeL3 edge), along with the scanning transmission electron micrograph of same object. Numerous small features in the object can be seen in the x-ray image. Data analysis indicates that a near diffraction limited performance was achieved using the zone plate. In our presentation, we will discuss the details and subtleties of the overlay fabrication as well as the zone plate image results.

36 MATERIALS SCIENCE↗

Free-space confocal magneto-optical spectroscopies at milliKelvin temperatures

We describe the operation of a free-space confocal optical microscope operated in a dilution refrigerator. The microscope is installed on a cold insertable probe to enable fast sample exchange while the refrigerator is held at low temperatures. A vector magnet provides a 6 T field normal to the sample and 1 T fields at arbitrary angles. A variety of optical microscopies and spectroscopies, including photoluminescence, Raman, magneto-optical Kerr effect, and spin relaxometry measurements are described, and some of the challenges associated with performing these measurements at milliKelvin temperatures are explored.

Lawrie, B. J.↗

Free-space confocal magneto-optical spectroscopies at milliKelvin temperatures

We describe the operation of a free-space confocal optical microscope operated in a dilution refrigerator. The microscope is installed on a cold insertable probe to enable fast sample exchange while the refrigerator is held at low temperatures. A vector magnet provides a 6 T field normal to the sample and 1 T fields at arbitrary angles. A variety of optical microscopies and spectroscopies, including photoluminescence, Raman, magneto-optical Kerr effect, and spin relaxometry measurements are described, and some of the challenges associated with performing these measurements at milliKelvin temperatures are explored.

Lawrie, Benjamin↗

Modal focal adaptive optics for Bessel-focus two-photon fluorescence microscopy

Adaptive optics (AO) improves the spatial resolution of microscopy by correcting optical aberrations. While its application has been well established in microscopy modalities utilizing a circular pupil, its adaptation to systems with non-circular pupils, such as Bessel-focus two-photon fluorescence microscopy (2PFM) with an annular pupil, remains relatively uncharted. Herein, we present a modal focal AO (MFAO) method for Bessel-focus 2PFM. Measuring and correcting aberration using a spatial light modulator placed in conjugation with the focal plane of the microscope objective, MFAO employs Zernike annular polynomials — a first in AO implementation — to achieve performance on par with a previous zonal AO method, but with a notably simplified optical configuration. We validated the performance of MFAO in correcting artificial and sample-induced aberrations, as well as in in vivo imaging of zebrafish larvae and mouse brains. By expanding the application of modal AO to annular pupils as well as aberration measurement and correction to a wavefront modulator at the objective focal plane, MFAO represents a notable advancement in the implementation of AO in microscopy.

47 OTHER INSTRUMENTATION↗

Fast widefield imaging of neuronal structure and function with optical sectioning in vivo

Optical microscopy, owing to its noninvasiveness and subcellular resolution, enables in vivo visualization of neuronal structure and function in the physiological context. Optical-sectioning structured illumination microscopy (OS-SIM) is a widefield fluorescence imaging technique that uses structured illumination patterns to encode in-focus structures and optically sections 3D samples. However, its application to in vivo imaging has been limited. In this study, we optimized OS-SIM for in vivo neural imaging. We modified OS-SIM reconstruction algorithms to improve signal-to-noise ratio and correct motion-induced artifacts in live samples. Incorporating an adaptive optics (AO) module to OS-SIM, we found that correcting sample-induced optical aberrations was essential for achieving accurate structural and functional characterizations in vivo. With AO OS-SIM, we demonstrated fast, high-resolution in vivo imaging with optical sectioning for structural imaging of mouse cortical neurons and zebrafish larval motor neurons, and functional imaging of quantal synaptic transmission at Drosophila larval neuromuscular junctions.

42 ENGINEERING↗

Visualizing nanoscale excitonic relaxation properties of disordered edges and grain boundaries in monolayer molybdenum disulfide

The ideal building blocks for atomically thin, flexible optoelectronic and catalytic devices are two-dimensional monolayer transition metal dichalcogenide semiconductors. Although challenging for two-dimensional systems, sub-diffraction optical microscopy provides a nanoscale material understanding that is vital for optimizing their optoelectronic properties. We use the ‘Campanile’ nano-optical probe to spectroscopically image exciton recombination within monolayer MoS2 with sub-wavelength resolution (60 nm), at the length scale relevant to many critical optoelectronic processes. Moreover, synthetic monolayer MoS2 is found to be composed of two distinct optoelectronic regions: an interior, locally ordered but mesoscopically heterogeneous two-dimensional quantum well and an unexpected ~300-nm wide, energetically disordered edge region. Further, grain boundaries are imaged with sufficient resolution to quantify local exciton-quenching phenomena, and complimentary nano-Auger microscopy reveals that the optically defective grain boundary and edge regions are sulfur deficient. In conclusion, the nanoscale structure–property relationships established here are critical for the interpretation of edge- and boundary-related phenomena and the development of next-generation two-dimensional optoelectronic devices.

36 MATERIALS SCIENCE↗

Atomic Force Microscope Active Optical Probe for Single-Molecule Imaging and Time-Resolved Optical Spectroscopy (DOE SBIR Phase II/IIA Final Report)

Actoprobe LLC reports on the results of its DOE SBIR Phase II/IIA project on the development of Atomic Force Microscope Active Optical Probe for Single-Molecule Imaging and Time-Resolved Optical Spectroscopy. While chemistry science and technology greatly benefit from Atomic Force Microscopy in surface characterization, time-resolved chemical imaging on the single-molecule level lags far behind. Current scanning probe microscopy only obtains information about mechanical but not optical/chemical properties. To address this problem, the Actoprobe LLC research team has proposed a novel class of Atomic Force Microscopy probes, Ultra-Fast Pulsed Active Atomic Force Microscopy Optical Probes (UFP AAOPs), that will allow ultrafast time-resolved optical and chemical imaging at the nanoscale. As envisioned, these unique optical probes will perform the functions of conventional Atomic Force Microscopy probes and, in addition, will simultaneously provide chemical information about molecular scale interactions. This innovation is accomplished by integrating an ultrafast pulsed Quantum Dot laser source into an Atomic Force Microscopy probe. This report describes our progress with the fabrication of an ultrafast micrometer-size semiconductor laser, based on “artificial atoms” - Quantum Dots, integrated with an Atomic Force Microscopy probe. In this Phase II/IIA project, we have demonstrated the feasibility of the UFP AAOP concept by fabricating a first prototype of the UFP AAOP. The excellent performance of the probe has been proven in terms of AFM and optical spatial resolution through rigorous tests. The UFP AAOP provides pulses with less than 4 ps duration and higher than 11 GHz repetition rate, and spatial resolution better than 300 nm at 1240 nm wavelength. Technically, it is possible to reduce the pulse width to less than 1 ps and to improve lateral resolution to ~ 0.5 nm, which implies the potential capability for the probe to characterize chemical compounds with single-molecule resolution. The UFP AAOP fabrication procedure has been developed for wafer-scale production of multiple devices, with the yield of the process estimated to be lower than 1% with the limited fabrication capabilities and equipment available for use in the research project. However, using high-volume production tools and special GaAs processing equipment, the yield can be significantly improved, theoretically to ~ 50%. Finally, economic feasibility and scale-up manufacturing potential were analyzed for UFP AAOP and found to be very promising. In summary, the Actoprobe team has successfully demonstrated the feasibility of the UFP AAOP concept.

36 MATERIALS SCIENCE↗

Exploring the relationship between deposition method, microstructure, and performance of Nb/Si-based superconducting coplanar waveguide resonators

Superconducting quantum circuits (SQC) are one of the most promising hardware platforms for quantum computing, yet their performance is currently limited by the presence of various structural defects inside the circuit's structure. Despite impressive progress in the past decade, a precise understanding of the origin of these defects from various fabrication processes and their impact on coherence is still lacking. Here, in this study, we performed a comprehensive investigation on the microstructure, superconductivity, and resonator quality factor of Nb films deposited by high-power impulse magnetron sputtering (HiPIMS) and direct current (DC) magnetron sputtering. A suite of characterization techniques, including electron microscopy with spectroscopy, secondary ion mass spectrometry, magneto-optical microscopy, and pump-probe reflectivity spectroscopy is used. We reveal that niobium (Nb) resonators fabricated using HiPIMS exhibit a smaller average grain size, thicker surface oxide with larger thickness variations (rougher surface), and a thicker amorphous Nb/Si interface layer compared to samples deposited by DC sputtering. We identified that the amorphous Nb oxides (mainly located at the Nb surface and along the grain boundaries) and Nb-Si amorphous layers (at the Nb/Si interface) are major and potential sources of two-level system (TLS), while off-stochiometric oxides and suboxides of Nb close to the surface, crystalline defects (i.e., dislocations at grain boundary, point defects introduced during deposition) are main contributors of non-TLS sources. Our findings clarify the relationship between different defects and coherence loss mechanisms, highlighting the importance of material microstructure control on performance optimization in SQC.

36 MATERIALS SCIENCE↗

Effects of high temperature treatment on microstructure and mechanical properties of laser-clad NiCrBSi/WC coatings on titanium alloy substrate

Laser-clad composite coatings on the Ti6Al4V substrate were heat-treated at 700, 800, and 900 °C for 1 h. The effects of post-heat treatment on the microstructure, microhardness, and fracture toughness of the coatings were investigated by scanning electron microscopy, X-ray diffractometry, energy dispersive spectroscopy, and optical microscopy. The wear resistance of the coatings was evaluated under dry reciprocating sliding friction at room temperature. The coatings mainly comprised some coarse gray blocky (W,Ti)C particles accompanied by the fine white WC particles, a large number of black TiC cellular/dendrites, and the matrix composed of NiTi and Ni{sub 3}Ti; some unknown rich Ni- and Ti-rich particles with sizes ranging from 10 nm to 50 nm were precipitated and uniformly distributed in the Ni{sub 3}Ti phase to form a thin granular layer after heat treatment at 700 °C. The granular layer spread from the edge toward the center of the Ni{sub 3}Ti phase with increasing temperature. A large number of fine equiaxed Cr{sub 23}C{sub 6} particles with 0.2–0.5 μm sizes were observed around the edges of the NiTi supersaturated solid solution when the temperature was further increased to 900 °C. The microhardness and fracture toughness of the coatings were improved with increased temperature due to the dispersion-strengthening effect of the precipitates. Dominant wear mechanisms for all the coatings included abrasive and delamination wear. The post-heat treatment not only reduced wear volume and friction coefficient, but also decreased cracking susceptibility during sliding friction. Comparatively speaking, the heat-treated coating at 900 °C presented the most excellent wear resistance. - Highlights: • TiC + WC reinforced intermetallic compound matrix composite coatings were produced. • The formation mechanism of the reinforcements was analyzed. • Two precipitates were generated at elevated temperature. • Cracking susceptibility and microhardness of the coatings were improved. • Post-heat treatment enhances wear resistance of the coatings.

36 MATERIALS SCIENCE↗

Visualizing the bidirectional optical transfer function for near-field enhancement in waveguide coupled plasmonic transducers

Here, we report visualizations of the bidirectional near-field optical transfer function for a waveguide-coupled plasmonic transducer as a metrology technique essential for successful development for mass-fabricated near-field devices. Plasmonic devices have revolutionized the observation of nanoscale phenomena, enabling optical excitation and readout from nanoscale regions of fabricated devices instead of as limited by optical diffraction. Visualizations of the plasmonic transducer modes were acquired both by local near-field excitation of the antenna on the front facet of a waveguide using the focused electron beam of a scanning electron microscope as a probe of the near-field cathodoluminescence during far-field collection from the back facet of the waveguide, and by local mapping of the optical near-field for the same antenna design using scattering scanning near-field optical microscopy as a probe of the near-field optical mode density for far-field light focused into the back facet of the waveguide. Strong agreement between both measurement types and numerical modeling was observed, indicating that the method enables crucial metrological comparisons of as fabricated device performance to as-modeled device expectations for heat-assisted magnetic recording heads, which can be extended to successful development of future near-field-on-chip devices such as optical processor interconnects.

42 ENGINEERING↗