DOE OSTI2017
Here, we report on the effect of molybdenum (Mo) incorporation on the crystal structure, surface morphology, Mo chemical valence state, and magnetic properties of cobalt ferrite (CoFe 2 O 4 , referred to CFO). Molybdenum incorporated cobalt ferrite (CoFe 2–x Mo x O 4 , referred to CFMO) ceramics were prepared by the conventional solid-state reaction method by varying the Mo concentration in the range of x = 0.0–0.3. X-ray diffraction studies indicate that the CFMO materials crystallize in inverse spinel cubic phase. Molybdenum incorporation induced lattice parameter increase from 8.322 to 8.343 Å coupled with a significant increase in density from 5.4 to 5.7 g/cm 3 was evident in structural analyses. Scanning electron microscopy imaging analyses indicate that the Mo incorporation induces agglomeration of particles leading to larger particle size with increasing x(Mo) values. Detailed X-ray photoelectron spectroscopic (XPS) analyses indicate the increasing Mo content with increasing x from 0.0 to 0.3. XPS confirms that the chemistry of Mo is complex in these CFMO compounds; Mo ions exist in the lower oxidation state (Mo 4+ ) for higher x while in a mixed chemical valence state (Mo 4+ , Mo 5+ , Mo 6+ ) for lower x values. From the temperature-dependent magnetization, the samples show ferrimagnetic behavior including the pristine CFO. From the isothermal magnetization measurements, we find almost 2-fold decrease in coercive field ( H c ) from 2143 to 1145 Oe with the increase in Mo doping up to 30%. This doping-dependent H c is consistently observed at all the temperatures measured (4, 100, 200, and 300 K). Furthermore, the saturation magnetization estimated at 4 K and at 1.5 T (from M–H loops) goes through a peak at 92 emu/g (at 15% Mo doping) from 81 emu/g (pristine CFO), and starts decreasing to 79 emu/g (at 30% Mo doping). The results demonstrate that the crystal structure, microstructure, and magnetic properties can be tuned by controlling the Mo-content in the CFMO materials.