Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FERRITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

A Comparative Study of Physical Properties of Er and Yb Nanophase Ferrite for Industrial Application

Nano ferrites CuCr{sub 0.3}Er{sub 0.03}Fe{sub 1.67}O{sub 4} and CuCr{sub 0.3}Yb{sub 0.03}Fe{sub 1.67}O{sub 4} were synthesized using standard ceramic technique. X-ray diffraction (XRD) patterns confirmed that the samples had cubic spinel structures. The average crystallite sizes of Er and Yb samples were in the range of 104.2–100 nm. The morphology analyses using field emission scanning electron microscopy (FESEM), high-resolution transmission electron microscopy (HRTEM) and atomic force microscopy (AFM) confirmed that the samples were in the nanoscale range. The compositional analyses using energy-dispersive x-ray (EDX) showed the atomic percentage (at.%) and weight percentage (wt%) of the investigated samples. The magnetic properties were carried out at room (300 K) and at low (100 K) temperatures magnetic hysteresis loop. The data showed that Er sample had higher saturation magnetization (M{sub s}) and lower coercivity (H{sub c}) than that of Yb sample suggesting that Er sample can be applied in magnetic applications. Moreover, Er sample had higher dielectric constant (ε’), dielectric loss (ε”) and dielectric loss tangent (tan δ) than that of Yb sample. However, Yb sample had higher resistivity than that of Er sample suggesting that Yb sample can be applied in electrical applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Enhanced Magneto-optical and Photocatalytic Properties of Ferromagnetic Mg{sub 1−y}Ni{sub y}Fe{sub 2}O{sub 4} (0.0 ≤ y ≤ 1.0) Spinel Nano-ferrites

Spinel Mg{sub 1−y}Ni{sub y}Fe{sub 2}O{sub 4} (0.0 ≤ y ≤ 1.0) ferrite magnetic nanoparticles (MNPs) were synthesized by a sol-gel combustion method using urea as the reducing agent/fuel. Powder X-ray diffraction (XRD) analysis revealed the formation of cubic spinel Mg{sub 1−y}Ni{sub y}Fe{sub 2}O{sub 4} powders and confirmed pure crystalline phase and the average crystalline size of 21.25 to 17.04 nm. Functional group bonds between metal and oxygen (M–O) were confirmed by Fourier transform infrared (FT-IR) spectra. The microstructure of the powders was recorded by high-resolution scanning electron microscope (HR-SEM) and confirmed the particle-like surface morphology with smaller agglomeration, due to the magnetic interaction of the particles. Energy-dispersive X-ray (EDX) results showed the composition of the expected elements and confirmed the phase purity of the products. Vibrating sample magnetometer (VSM) technique recorded at room temperature was used to analyse the magnetic properties of the samples and the hysteresis loops showed the ferromagnetic behaviour. Moreover, the samples Mg{sub 1−y}Ni{sub y}Fe{sub 2}O{sub 4} NPs were tested for the photocatalytic degradation (PCD) of methylene blue (MB) dye and the sample y = 0.6 showed maximum degradation efficiency (96.83 %), due to the smaller particle size with higher surface area than other compositions. Furthermore, spinel Mg{sub 1−y}Ni{sub y}Fe{sub 2}O{sub 4} nano-photocatalysts can be reused several times without change of its catalytic activity.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic and Structural Properties of Novel Neodymium-Tin Spinel Ferrite Nanoparticles

Novel spinel neodymium-tin ferrite nanoparticles (Nd{sub 0.5}Sn{sub 0.5}Fe{sub 2}O{sub 4}) have been synthesized by the coprecipitation method; x-ray diffraction (XRD), transmission electron microscopy (TEM), and superconducting quantum interference device magnetometer (SQUID) techniques were used to characterize the crystal structure, morphology, and magnetic properties. The spinel structure of a single phase is obtained according to XRD results. From TEM characterization results, we obtained a spherical morphology with an average of 13 nm. Magnetic measurement indicates that the nanoparticles have a superparamagnetic phase with a corresponding blocking temperature (T{sub B}) of about 360 K. These new nanomaterials can potentially be used in nanoelectronic devices, magnetic sensors, and hyperthermia application.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Tuning of Magnetic and Optical Properties of Co{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4} Spinel Ferrite Thin Films Based on Post Annealing Temperature

This paper is dedicated to deposit zinc substituted cobalt ferrite (Co{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4}) thin films on glass substrate using electron beam deposition technique. The effect of post annealing temperature on structural, magnetic, and optical properties of thin films has been investigated. Thin films have been characterized using x-ray diffraction (XRD), Raman spectroscopy, atomic force microscopy (AFM), vibrating sample magnetometer (VSM), UV-VIS spectroscopy, and spectroscopic ellipsometry (SE) analysis. The as-deposited thin films are amorphous in nature. After deposition, these thin films post annealed at different temperature ranges from 200 to 500 {sup ∘}C to enhance the crystallinity of films. The film post annealed at 200 {sup ∘}C is also amorphous in nature. As the post annealing temperature increases, the thin films become more crystalline. X-ray diffractometer and Raman analysis confirm the formation of cubical inverse spinel structure of thin films. The saturation magnetization of the thin films decreases with the annealing temperature due to the sites occupancy of cations between tetrahedral and octahedral. The reduction in coercivity is correlated with the anisotropy constant, but the anisotropy value is still high which is suitable to form stable magnetic storage memories. The band gap energy are decreased which is mainly attributed due to increase in grain size of the film. It is noted that the band gap energy of these thin films are higher than that of bulk material, so these may be suggested for use in wide band gap applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Enhancement of Magnetization and Tailoring of Blocking Temperatures of Nano-Ni–Zn Ferrite Powder Synthesized Using Microwave-assisted Combustion Method

Single-phase nano-Ni–Zn ferrite samples in the range of 6 to 75 nm were synthesized using microwave-assisted combustion method. Enhancement of saturation magnetization (M{sub s}) was observed in comparison with previously reported results. Minor variation of (M{sub s}) due to composition change can be explained on the basis of strengthening of A–B exchange interaction due to replacement of nonmagnetic Zn ions by Ni ions. Low coercivity (H{sub c}) and retentivity (M{sub r}) indicate low loss in the samples. SQUID analysis showed that the blocking temperature (T{sub B}) of the samples can be tailored in the present work.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and Magnetic Properties of La-Substituted M-Type Hexagonal Sr–Ni Ferrites Synthesized by Ball-Milling-Assisted Ceramic Process

Sr{sub 0.5}Ni{sub 0.5}La{sub x}Fe{sub 12 − x}O{sub 19} (x = 0, 0.08, 0.16, and 0.24) hexaferrites have been synthesized by ball-milling-assisted ceramic process. The calcined samples are characterized by X-ray powder diffraction (XRD), scanning electron microscopy (SEM), Fourier transform infrared spectra (FTIR), and vibrating sample magnetometry (VSM). XRD reveals that all samples consist of the main M-type hexagonal Sr ferrite phase and a low amount of rhombohedral Fe{sub 2}O{sub 3} as secondary phase, and a continuous increase of the hexagonal lattice parameters with substitution content (x). Magnetic characterization indicates that all Sr{sub 0.5}Ni{sub 0.5}La{sub x}Fe{sub 12 − x}O{sub 19} samples have a hard magnetic property. Substitution of Fe{sup 3+} ions by La{sup 3+} ions can obviously improve the specific saturation magnetization, remanence, magnetic moment, and effective anisotropy constant. Specific saturation magnetization, remanence, and the magnetic moment reach a maximum at x= 0.24 and calcination temperature of 1050 {sup ∘}C.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Single- and Double-Layer Microwave Absorbers of Cobalt Ferrite and Graphite Composite at Gigahertz Frequency

Microwave absorbers of cobalt ferrite and graphite composite have been fabricated to investigate the broadening of absorption frequency by mixing small and large particles and comparing single- and double-layer composites in order to broaden the absorption frequency and to enhance multireflection and scattering of electromagnetic wave. CoO and Fe{sub 2}O{sub 3} precursors were mechanically alloyed and sintered at 800, 900, 1000 and 1100 {sup ∘}C in order to synthesise various particle sizes and shapes. A mixed sample of powders sintered at the above mentioned temperatures was also formed. The morphological, phase, and magnetic properties of these samples were studied. Two series of samples have been synthesised which were single- and double-layer composites. Single-layer composite consisted of mixed particles, and their thickness parameters were varied. Double-layer composite was also prepared with various particle sizes of CoFe{sub 2}O{sub 4} as a layer and graphene as another layer. The effect of these layers as matching and absorbing layer was studied. The degree of crystallinity of CoFe{sub 2}O{sub 4} was increased with increase of sintering temperature. Microstructural study showed the evolution of particle size and shape subjected to sintering temperature. Arrhenius plot showed two stages of growth process with activation energy calculated at 26.85 and 83.091 kJ/mol. The critical size of single domain of this sample plotted from the coercivity against particle size was 63.44 nm. Single-layer composite with mixed particle size was not able to show good electromagnetic (EM)-wave absorption; however double-layer composite showed good return loss. The mechanism of the EM-wave absorption of double-layer composite was discussed in this paper.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of the Effect of Pr Doping on Structural, Morphological and Magnetic Properties of Nickel Ferrite

Praseodymium rare earth ion (Pr{sup 3+}) doped nickel ferrite (NiFe{sub 2−x}Pr{sub x}O{sub 4}, 0 < x< 0.1) nanocrystals (NFPO) were synthesized by hydrothermal method. The structural, morphological and magnetic properties of the prepared samples have been studied. The x-ray diffraction (XRD) and fourier transform infrared (FTIR) techniques confirmed the phase formation of the NFPO nanocrystals. The average crystallite size of NFPO nanoparticles found to be in the range 39 to 44 nm. The presence of Pr ions in NFPO was confirmed by energy-dispersive x-ray (EDX) analysis. It has been observed that after a certain amount of Pr doping, the morphology of the nanocrystals starts changing from nano-octahedrons to nanorods shape, as confirmed by transmission electron microscopy (TEM). Also, the magnetic properties of the prepared nanocrystals were measured using physical properties measurement system (PPMS) at 10 K and 300 K. The saturation magnetization (Ms) first decreases with the increasing loading amount of Pr ions up to (x = 0.025) and later it increases at both the temperatures. However, the value of coercivity shows an increasing trend with the increasing amount of Pr ions in NFPO at room temperature.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microstructural, Magnetic, Magnetocaloric, and Electrical Properties of Ni{sub 0.4}Mg{sub 0.3}Cu{sub 0.3}Fe{sub 2}O{sub 4} Ferrite Prepared Using Sol–Gel Method

Detailed investigations of the microstructural, magnetic, magnetocaloric, and electrical properties of Ni{sub 0.4}Mg{sub 0.3}Cu{sub 0.3}Fe{sub 2}O{sub 4} ferrite synthesized by sol-gel method have been investigated. XRD pattern indicates that sample has cubic spinel structure with Fd 3-bar m symmetry. The cation distribution of the sample has been determined by Rietveld refinement. Temperature dependence of magnetization shows that sample exhibits a second-order PM to FM phase transition at the Curie temperature T{sub C} = 690 K. From the M(μ{sub 0}H,T) data, we found that the maximum entropy change |ΔS{sub M}{sup max}| reaches value of about 1.56 J kg{sup − 1} K{sup − 1} and relative cooling power (RCP) of 136 J kg{sup − 1} at μ{sub 0}H = 5 T. From electrical conductivity curves, the estimated value of the activation energy is equal to 0.349 eV. The Nequist diagram at different temperatures reveals that the grain boundary contribution is responsible to the conduction process for the studied sample.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Mössbauer Study and Curie Temperature Configuration on Sintering Nano-Ni-Zn Ferrite Powder

Variations of Curie temperature and strength of magnetic phases with sintering temperature and Ni concentration is investigated in the present work. The AC susceptibility studies show a decrease in Curie temperature (TC) with an increase in Ni concentration in the samples. Comparison of Curie temperatures with the reported results reveals that samples in the present work show higher TC enabling high thermal stability. The Mössbauer spectra of nano- and sintered Ni-Zn ferrite samples were recorded at room temperature to monitor the local environment around Fe cations through Mössbauer hyperfine parameters as a function of composition and sintering temperatures. The increase in sharpness of the Mössbauer sextet with an increase in Ni concentration and sintering temperature corroborate improvement in homogeneity and ferrimagnetic ordering. The results of hyperfine parameters offer the possibility of having close view on configuring Curie temperature through monitoring hyperfine field by altering sintering temperature and/or Ni concentration. As the temperature dependence of magnetic and magnetoelastic properties is strongly influenced by the Curie temperature, the successful possible configuration of Curie temperature in the present work can be further investigated for desired sensor applications.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Structural and Magnetic Behavior of BaAl{sub x}Cr{sub y}Fe{sub 11}O{sub 19} (x + y = 1) Hexagonal Ferrites

The present study aims to analyze barium hexagonal ferrite and its derivation behavior using sol-gel auto-combustion co-doped with Al{sup 3+}/Cr{sup 3+}ions. Also, the effects of dopants on structural and magnetic properties of prepared samples were investigated. To this purpose, the finest powders were preheated at 500 °C for 1 h and calcinated at 900 °C about 2 h. Then, the magnetic powders were characterized by Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), field emission scanning electron microscope (FESEM), and vibrating sample magnetometer (VSM). The XRD patterns show the magnetoplumbite phase. According to the Scherrer equation applied, inserting ions led to a decrease in lattice parameters (a and c) and crystallite size. The morphology of synthesized samples was observed by FESEM and proved the hexagonal shapes of the prepared samples. The nanoparticles sizes were recorded between 59 and 79 nm. Moreover, the magnetic properties of prepared samples were specified by VSM. The saturation magnetization (M{sub s}) and remnant magnetization (M{sub r}) of the synthesized magnetic powders were decreased by inserting Al{sup 3+}/Cr{sup 3+} ions, while coercivity (H{sub c}) increased from 5215 to 7178 Oe. .

77 NANOSCIENCE AND NANOTECHNOLOGY↗

FMR and Magnetic Studies of RF-Sputtered Mn-Zn Ferrite Thin Films

The Manganese–Zinc ferrite (MZF) thin films were deposited on quartz substrates by radio frequency (RF) magnetron sputtering at 10 mTorr of argon gas pressure. The FMR and magnetization measurement were carried out to understand magnetic properties of the as-deposited and annealed MZF films. The resonance field (H{sub r}) of the FMR spectra shifts towards higher magnetic field when angle between applied field and thin film plane is changed from 0 to 90° indicating the existence of uniaxial anisotropy in the film. Whereas, H{sub r} shifts towards lower magnetic field with decrease in temperature of the film. This is due to ferrimagnetic ordering in the films at low temperatures. The magnetization versus field (M-H) plots reveal the soft ferrimagnetic behavior of the films. The post-deposition annealing of the film leads to increase in crystallite size with more uniform film surface and dense columnar growth compared to the as-deposited film. The increase in magnetization and decreases in H{sub r}-values compared to that of as-deposited film are observed for annealed film. The optical band gap of the film is also found to increase with annealing.

36 MATERIALS SCIENCE↗

Internal Oxidation-Nitridation of Ferritic Fe(Al) Alloys in Air

Exposure of undoped Fe(Al) and Fe(Al)+Cr ferritic alloys in laboratory air at 900-1,000 C resulted in significant internal attack after 5,000 h, including oxides and underlying nitrides. In the most severely attacked alloys, kinetics based on mass gain and maximum penetration depth were linear; also, the deepest penetrations were a significant fraction of the specimen thickness, and were thickness-dependent. Little internal attack was observed at 700-800 C where these compositions may be used as coatings. The extent of internal attack did not decrease with increasing Al or Cr content which may indicate that rather than classical internal oxidation this attack is related to the permeation of N through a defective external scale. No internal attack was observed in alloys doped with Y, Zr, Hf or Ti where the substrate-alumina scale interface was flatter.

36 MATERIALS SCIENCE↗

Enhancement of Nanostructured Ferritic Alloy 14YWT Properties via Heat Treatment for Post-Consolidation Processing

The nanostructured ferritic alloy 14YWT is a promising candidate for in-core use in generation IV nuclear reactors, due to a dense dispersion of insoluble, ultrafine-scale Y-Ti-O nano-oxides, which provide a high degree of irradiation tolerance and thermal stability. This work investigates the effects of heat treatment on the workability of 14YWT, along with the effect of processing history on abnormal grain structures and radial microstructural uniformity. In this study, a 14YWT rod consolidated at 850 °C was heat treated in argon at 1100 °C, 1150 °C, 1200 °C, or 1250 °C for 1 or 8 hours and changes in mechanical properties and microstructure were examined using microhardness and electron backscattered diffraction (EBSD). Two distinct types of large abnormal grains were observed, each with unique processing origins, including one with high and the other with low strain energy. Consolidation via direct extrusion resulted in radial microstructural gradients, where the center of the rod was softer with larger grain sizes and lower strain energies. These gradients persisted and intensified throughout heat treatment. Based upon this work, the recommended heat treatment for increased workability with minimal microstructural change is 1150 °C for 1 hours.

36 MATERIALS SCIENCE↗

Effects of Static Recrystallization and Precipitation on Mechanical Properties of 00Cr12 Ferritic Stainless Steel

The 00Cr12 ferritic stainless steel samples were isothermally held at different temperatures in the range of 700 °C to 1000 °C to investigate the effect of static recrystallization and precipitation on mechanical properties, such as microhardness, tensile strength, and yield strength. The results show that the formation of the fine recrystallized grain, as well as precipitation, coarsening, and dissolution of the second-phase particles, influences the mechanical properties remarkably. The fine recrystallized grain can provide a positive grain boundary-strengthening effect in the sample under a relatively high holding temperature. Coarsening and dissolution of M{sub 23}C{sub 6} result in partial depletion of precipitate hardening. In contrast, the size and number density of MX particles are almost constant, regardless of the holding temperature; therefore, it can provide a better precipitation-hardening effect.

36 MATERIALS SCIENCE↗

Solidification of Calcium Ferrite Melt Using Ultrasonic Vibration: Effect and Mechanism

Calcium ferrite (CF) is a very important binder phase in iron ore sintering processes. To improve the microstructure of CF, power ultrasound was introduced during its solidification process, and the effect of immersion depth of ultrasonic probe (IDUP) on the properties of CF was investigated in detail. The results indicated that the microstructure of CF was greatly refined; the grain size decreased from 2864 μm without ultrasonic vibration to 841 μm with ultrasonic vibration at an immersion depth of 30 mm. Without ultrasonic vibration, the density and compressive strength of CF slag were 3904 kg/m{sup 3} and 38.3 MPa, respectively. When the IDUP was increased from 10 to 30 mm, the density and compressive strength of CF increased from 4049 to 4452 kg/m{sup 3} and 52.5 to 87.3 MPa, respectively. Further, the reducibility of CF was examined. The reduction time, at the same reduction rate, decreased from 347 minutes without ultrasonic vibration to 200 minutes with ultrasonic vibration at an IDUP of 30 mm. The rate-limiting step was obviously improved, which may be attributable to the grain refinement of CF and composition segregation in the slag. In general, the properties of CF were greatly improved due to the cavitation and acoustic streaming of ultrasonic waves.

36 MATERIALS SCIENCE↗

Wetting Behavior of TiO{sub 2} by Calcium Ferrite Slag at 1523 K

The wetting behaviors of a TiO{sub 2} substrate by calcium ferrite (CF) series slags were investigated using an improved sessile drop method at 1523 K (1250 °C). The initial contact angles were in the range 35 to 50 deg, the final equilibrium apparent contact angles were < 20 deg, and the spreading durations were in the range 75 to 180 seconds. The CF-TiO{sub 2} system showed reactive wetting, which was categorized into four dynamic stages. Stage I: physical spreading, stage II: slow linear spreading, stage III: fast linear spreading, and stage IV: equilibrium. Interfacial reactions yielded CaTiO{sub 3} during reactive spreading, thereby transitioning TiO{sub 2} wetting into CaTiO{sub 3} wetting and then forming Fe{sub 2}TiO{sub 5} and FeTiO{sub 3} owing to the excess Fe{sub 2}O{sub 3} and FeO that had accumulated in the interfacial zone. Although stage III spreading was faster than stage II spreading, adding MgO to the slag slowed stage III spreading. The interfacial microstructure of the residual slag was roughly divided into three layers owing to the different densities of the slag and solid products. The top layer was composed of CaTiO{sub 3} and Fe{sub 2}O{sub 3}, the middle one was composed of CaTiO{sub 3} and Fe{sub 2}TiO{sub 5}, and the bottom one was composed of Fe{sub 2}TiO{sub 5} and FeTiO{sub 3}. Adding TiO{sub 2} to the slag produced a dense CaTiO{sub 3}-containing interfacial layer, resulting in CF being detected in the residual slag.

36 MATERIALS SCIENCE↗

Solidification Behavior of Calcium Ferrite Under Ultrasonic Vibration

Ultrasonic vibration was applied to the solidification process of calcium ferrite (CF) to modify the grain size and improve the homogeneity of the solidified microstructure. The effects of ultrasound on microstructure, density, compressive strength, and reducibility were studied. The acoustic pressure decreased and then increased along the axis symmetry due to the attenuation of acoustic pressure and reflection of ultrasonic waves in the melt under a fixed power. When the ultrasonic power was increased, the general acoustic pressure increased, which was beneficial to the avoidance of macropores and to improvement of the microstructure. Coarse acicular CF grains were significantly refined; the grain size decreased from 1967 to 442 μm when the ultrasonic power was increased from 0 to 300 W. The density of the samples increased from 4370 to 4680 kg/m{sup 3} due to cavitation and acoustic streaming effects. Ultrasonic vibration greatly improved the ultimate compressive strength of CF; the values were 41.8 ± 2.1 to 67.3 ± 3.4 MPa for ultrasonic powers of 100 to 300 W, respectively. Without ultrasonic treatment, it was only 37.4 ± 1.9 MPa. Ultrasonic vibration also influenced the reduction time of CF due to the composition segregation in the slag during solidification.

36 MATERIALS SCIENCE↗