Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “EUTECTIC ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

Metal Fuel Implications on Severe Accident Scenarios

Superior steady-state irradiation performance of metal fuel has been demonstrated, and metal fuel has been the choice for recent sodium-cooled fast reactor designs, e.g. PRISM, SAFR, 4S, TWR, PGSFR, and so on. Metal fuel also has excellent transient capabilities. The metal fuel itself does not impose any restrictions on transient operations or load-following capabilities. Metal fuel has benign run beyond cladding breach (RBCB) performance characteristics. Because metal fuel is compatible with sodium, there is no reaction product and the fuel loss is practically zero. Metal fuel is expected to be very reliable. However, even if unforeseen fuel pin failure occurs, it will simply release gases and does not cause failure propagation to neighboring pins. The eutectic formation temperature between the fuel and the cladding has been considered a critical parameter for the metal fuel pin design. The onset of fuel-cladding eutectic formation starts in the 700-725 deg. C temperature range, depending on the fuel alloy and cladding types. However, at this onset temperature, not much interaction occurs. In fact, even at 100 deg. C above the eutectic temperature, the eutectic penetration into the cladding is minimal in one hour. Only at much higher temperatures, close to the fuel melting point itself, the eutectic penetration into cladding becomes rapid. Therefore, the eutectic formation is not a primary safety concern during transient overpower conditions. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Solidification of Au-Cu-Si alloys investigated by a combinatorial approach

Composition libraries of Au-Cu-Si films comprising 800 composition patches were fabricated through co-sputtering deposition from elemental targets. The gold composition varies between 47% (compositions are in atomic percentage) and 81%, copper between 8% and 40%, and silicon between 6% and 36% within the library. We designed and used a high-throughput optical characterization method to detect melting and solidification based on changes in the film's contrast; further microscopy characterization reveals the microstructure. This approach reveals the composition dependence of the nucleation temperature and primary phase, which allows us to draw conclusions about glass forming ability and to identify bulk metallic glass forming compositions. Our solidification results suggest that the best glass forming composition coincides with the composition at which a transition from one primary phase to another occurs. We show that in general this transition is not at the eutectic composition but at the lowest nucleation temperature.

36 MATERIALS SCIENCE↗

Triggered Nucleation in Ni60Nb40 Using an Electrostatic Levitator

External triggering of nucleation in an undercooled liquid metal has been performed for the first time in an electrostatically levitated sample of undercooled eutectic Ni60Nb40. With the Electrostatic Levitator (ESL) facility at NASA/MSFC, NiNb alloys were externally nucleated at various undercooling increments. Observation of the resulting microstructure indicates that only one nucleation site is initiated with a trigger if the undercooling is sufficiently high. Well-defined transition zones exist in all the samples. An "anomalous" fine structured eutectic is initially grown from the nucleation point into the undercooled liquid followed by an unexpected variable width transition zone leading to a coarse structured region of dendrites. Our study tends to corroborate the findings of other studies on highly undercooled eutectics regarding a coupled growth zone within which the lamellar structure is formed and outside of which the anomalous is found.

Rathz, T.↗

Identification of salt-alloy combinations for thermal energy storage applications in advanced solar dynamic power systems

Thermodynamic calculations based on the available data for flouride salt systems reveal that a number of congruently melting compositions and eutectics exist which have the potential to meet the lightweight, high energy storage requirements imposed for advanced solar dynamic systems operating between about 1000 and 1400 K. Compatibility studies to determine suitable containment alloys to be used with NaF-22CaF2-13MgF2, NaF-32CaF2, and NaF-23MgF2 have been conducted at the eutectic temperature + 25 K for each system. For these three NaF-based eutectics, none of the common, commercially available high temperature alloys appear to offer adequate corrosion resistance for a long lifetime; however mild steel, pure nickel and Nb-1Zr could prove useful. These latter materials suggest the possibility that a strong, corrosion resistant, nonrefractory, elevated temperature alloy based on the Ni-Ni3Nb system could be developed.

Whittenberger, J. D.↗

Elucidating the corrosion mechanism of commercial Ni-based Superalloys in UCl3 containing-chloride Molten Salt Systems

Molten salt reactors (MSRs) have gained renewed interest, providing several advantages over their predecessors, including the capability to consume spent fuels, enhancing the environmental sustainability of the uranium fuel cycle. For example, molten chloride fast reactors (MCFRs) can reach criticality with molten chloride spent fuel containing high concentrations of impurities, such as actinide products like uranium chloride (UCl3). However, the redox potential of chloride molten salt fuels may change in the presence of these impurities, dictating their corrosivity and in turn the corrosion performance of structural components, such as those constructed from nickel (Ni)-based alloys. The purpose of this investigation is to assess the extent of corrosion of Ni-based alloy, Inconel 617, when exposed to UCl3-LiCl-KCl eutectic salt. Inconel 617 one of only six structural materials that are fully qualified by the American Society for Mechanical Engineers (ASME) Boiler and Pressure Vessel Code for high-temperature nuclear reactor components, making it a technologically mature material to consider for constructing MCFRs. Inconel 617 specimens were submerged in a static LiCl-KCl-UCl3 eutectic salt mixture heated at 700 C for 1000 h under an inert atmosphere. Upon completion, the extent of corrosion was analyzed through a multi-modal characterization approach spanning the engineering to nanoscale, employing computed tomography, focused-ion beam, and transmission electron microscopy techniques. Results from this investigation will enhance our understanding of property-to-performance relationships of candidate structural materials for MSRs with respect to corrosion resistance and interactions between the salt and alloy interface.

36 MATERIALS SCIENCE↗

From irregular to regular eutectic growth in the Al-Al 3 Ni system: In situ observations during directional solidification

Here we investigate the irregular eutectic growth dynamics of the Al-Al 3 Ni alloy, in which one of the solid phases (Al 3 Ni) grows faceted from the liquid. Leveraging in situ optical microscopy and synchrotron transmission x-ray microscopy, we address the question of the degree of coupling between Al and Al 3 Ni at the growth front and that of the shape of the microstructures left behind in the bulk solid during directional solidification. Real-time optical observations bring evidence for a morphological transition from a eutectic-grain dependent, irregular eutectic growth at low solidification velocity V (typically 1 μm s -1 ), to a weakly anisotropic, regular growth at higher V ( reaching 10 μm s -1 ). Unprecedented x-ray nano-imaging of the solid–liquid interface, and 3D characterization of the growth patterns, were made possible by a new DS setup at Brookhaven National Laboratory’s NSLS-II. At low V, the leading tips of partly faceted Al 3 Ni crystals are observed to grow not far ahead of the Al growth front. Correlating in situ images and postmortem 3D tomographic reconstructions reveals that the presence of faceted and non-faceted regions of Al 3 Ni crystals in the solid is a direct consequence of coupling and decoupling during DS, respectively. Upon increasing V, the lead distance of Al 3 Ni vanishes, and the shape of Al 3 Ni ceases to be governed by faceted growth. These observations cast light onto the basic mechanisms (faceted growth, diffusive coupling, and the dynamics of trijunctions) governing a faceted to rod-like transition upon increasing V in the Al 3 Ni system, with broad implications to a large class of irregular eutectics.

36 MATERIALS SCIENCE↗

Extreme shear-deformation-induced modification of defect structures and hierarchical microstructure in an Al–Si alloy

Abstract Extreme shear deformation is used for several material processing methods and is unavoidable in many engineering applications in which two surfaces are in relative motion against each other while in physical contact. The mechanistic understanding of the microstructural evolution of multi-phase metallic alloys under extreme shear deformation is still in its infancy. Here, we highlight the influence of shear deformation on the microstructural hierarchy and mechanical properties of a binary as-cast Al-4 at.% Si alloy. Shear-deformation-induced grain refinement, multiscale fragmentation of the eutectic Si-lamellae, and metastable solute saturated phases with distinctive defect structures led to a two-fold increase in the flow stresses determined by micropillar compression testing. These results highlight that shear deformation can achieve non-equilibrium microstructures with enhanced mechanical properties in Al–Si alloys. The experimental and computational insights obtained here are especially crucial for developing predictive models for microstructural evolution of metals under extreme shear deformation.

36 MATERIALS SCIENCE↗

Compatibility of SiC with ODS FeCrAl in flowing Pb-Li at 600° - 700°C

To establish the maximum operating temperature for the dual coolant lead lithium (DCLL) blanket concept, thermal convection loop (TCL) experiments were conducted for 1000 h with a peak temperature of 700 °C to determine compatibility with commercial eutectic Pb~17at.%Li. Two TCLs were fabricated from alloy APMT (FeCrAlMo) and the baseline TCL experiment contained only APMT specimens. The second TCL experiment exposed more fusion relevant CVD SiC and ODS Fe-10Cr-6Al specimens in the hot and cold legs. In the second experiment, the mass losses were much larger for the ODS FeCrAl specimens and most of the CVD SiC specimens experienced a mass gain as SiC reacted to form an Fe- and Cr-rich carbide reaction product. Dissolved Fe and Cr reacted with the SiC and removing Fe and Cr from the liquid appeared to increase ODS FeCrAl dissolution. Such a dissimilar material interaction appears consistent with thermodynamic calculations. Significant attack at the top of the hot leg in both experiments suggests that the Pb-Li compatibility of FeCrAl alloys is inadequate at 700 °C in a flowing environment and the maximum PbLi temperature is < 675 °C.

36 MATERIALS SCIENCE↗

M551 metals melting experiment

Electron beam welding studies were conducted in the Skylab M551 metals melting experiment, on three different materials; namely 2219-T87 aluminum alloy, 304L stainless steel, and commercially pure tantalum (0.5 wt % columbium). Welds were made in both one gravity and zero gravity (Skylab) environments. Segments from each of the welds were investigated by microhardness, optical microscopy, scanning microscopy, and electron probe techniques. In the 2219-T87 aluminum alloy samples, macroscopic banding and the presence of an eutectic phase in the grain boundaries of the heat affected zone were observed. The stainless steel samples exhibited a sharp weld interface and macroscopic bands. The primary microstructural features found in the tantalum were the presence of either columnar grains (ground base) or equiaxed grains (Skylab). The factors contributing to these effects are discussed and the role of reduced gravity in welding is considered.

Busch, G.↗

Crystal nucleation in Pd-Si alloys

A study of the crystal phase nucleation in undercooled droplets of Pd-Si alloys with composition near the Pd(84.5)Si(15.5) eutectic composition is reported. Molten droplets are released at the top of a drop tube and solidify (to either a crystalline or glassy state) during descent. This provides a containerless (and nearly gravity free) environment so that nucleation due to container walls or vibrations is eliminated. It is found that crystallization, due to homogeneous nucleation, is bypassed in droplets of 1 mm diameter when cooled at 760 K/sec. From this an upper limit of the homogeneous nucleation rate is estimated. Results are compared with a previously published study of nucleation in 0.06 mm to 0.33 mm diameter droplets, which indicated that nucleation results from heterogeneous surface nucleation and that the number of these nuclei is dependent on the atmosphere in the drop tube.

Drehman, A. J.↗

The volume change during solidification

The liquid-solid phase transformation of solidifying metallic melts is accompanied by a volume change Delta-Vm. This volume change produces a gravity-independent microscopic flow near the solidification front. In a ground-based laboratory, solidification processes are also affected by convection due to temperature and concentration gradients. A quantitative evaluation of the effects of these flows on the formation of structure requires reproducible values of Delta-Vm. Alloys with Delta-Vm = 0 would be best suited for such an evaluation, while alloys with a constant value for Delta-Vm are still usable. Another requirement is related to a solidus-liquidus interval which is as small as possible. One-phase alloys, which would be particularly well suited, could not be found. For these reasons, alloys which solidify in two phases, as for example eutectics, have been considered, taking into account the Al-Ge system. Attention is given to the volume change at the melting point, the measurement of this change, the volume change at solidification, and applications to terrestrial technology.

Rittich, M.↗

Study of formation mechanism of incipient melting in thixo-cast Al–Si–Cu–Mg alloys

Mechanical properties of thixo-cast Al–Si–Cu–Mg alloys can be enhanced by T61 heat treatment. Copper and magnesium atoms in aluminum matrix can form homogeneously distributed precipitations after solution and aging treatment which harden the alloys. However, microsegregation of these alloying elements could form numerous tiny multi-compound phases during solidification. These phases could cause incipient melting defects in subsequent heat treatment process and degrade the macro-mechanical properties of productions. This study is to present heterogeneous distribution of Cu, Si, and Mg elements and formation of incipient melting defects (pores). In this study, incipient melting pores that occurred during solution treatment at various temperatures, even lower than common melting points of various intermetallic phases, were identified, in terms of a method of investigating the same surface area in the samples before and after solution treatment in a vacuum environment. The results also show that the incipient melting mostly originates at the clusters with fine intermetallic particles while also some at the edge of block-like Al{sub 2}Cu. The fine particles were determined being Al{sub 2}Cu, Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} and Al{sub 8}Mg{sub 3}FeSi{sub 2}. Tendency of the incipient melting decreases with decreases of the width of the clusters. The formation mechanism of incipient melting pores in solution treatment process was discussed using both the Fick law and the LSW theory. Finally, a criterion of solution treatment to avoid incipient melting pores for the thixo-cast alloys is proposed. - Highlights: • In-situ comparison technique was used to analysis the change of eutectic phases. • The ralationship between eutectic phase size and incipient melting was studied. • Teat treatment criterion for higher incipient melting resistance was proposed.

36 MATERIALS SCIENCE↗

Some possible filler alloys with low vapor pressures for refractory-metal brazing

A compilation of eutectics and melting-point minima for binary combinations of metals having vapor pressures below 10 to the minus 10th power torr at 1500 degrees K and .00005 torr at 2000 degree K is presented. These compositions and others near them on their phase diagrams are potential special brazing fillers for refractory metals. Some possible problems and advantages for fusion bonds of such mixtures are indicated. Evaluations of brazing fillers containing refractory metals are reported.

Morris, J. F.↗

Integrated three-dimensional characterization of reactive phase formation and coarsening during isothermal annealing of metastable Zn–3Mg–4Al eutectic

Microstructural instabilities associated with a metastable lamellar eutectic when exposed to an elevated temperature were analyzed in a Zn-3Mg-4Al alloy as a model system. X-ray diffraction and scanning electron microscopy showed that annealing at a temperature 43 K below the equilibrium eutectic temperature converted the metastable ternary MgZn 2 /η-Zn/β-ZnAl eutectic to a stable mixture of Mg 2 Zn 11 /η-Zn/α-Al. 3D EBSD suggested that supersaturation of η-Zn with Mg and Al eased difficulties in nucleation of Mg 2 Zn 11 and α-Al at the MgZn 2 /η-Zn phase interfaces. Quasi-in-situ X-ray nanotomography revealed that a reactive diffusion process prevailed in an early stage of annealing leading to rapid consumption of MgZn 2 for growth of Mg 2 Zn 11 and concomitant thinning and pinch-off of η-Zn lamellae. The reactive diffusion process also brought about significant and quantifiable changes in the topological characteristics of the η-Zn phase at remarkably shorter time scales compared to Rayleigh instability and Ostwald ripening mechanisms. Overall, the present results provide fresh insights on the short-term annealing effects on metastable eutectics, with relevance to structural evolution in additive manufacturing.

36 MATERIALS SCIENCE↗

Preparation of eutectic superalloys by EFG

An attempt was made to produce airfoil shaped bars of three different eutectic superalloys by means of the edge-defined, film-fed growth (EFG) method. The alloys used were a gamma + delta Ni-Cb alloy, a gamma/gamma prime + delta Ni-Cb-Al alloy and a Co-TaC alloy containing Ni and Cr. The development of a new die material was essential in the investigation since these alloys are reactive toward known die materials. Tantalum carbide was selected as a die material because it exhibited spontaneous capillary rise and slow rate of degradation in the liquid metals. Eutectic bars up to 1 mm thick and 6 mm wide were grown from TaC dies in order to determine the growth characteristics and the thermal gradient. Large bars of the gamma/gamma prime + delta alloy were grown and tensile tested. A die with a blind central cavity was designed and several hollow, tear-shaped bars were grown.

Hurley, G. F.↗

Thermal fatigue and oxidation data of superalloys including directionally solidified eutectics

Thermal fatigue and oxidation data were obtained on 61 specimens, representing 15 discrete alloy compositions or fabricating techniques and three coating systems. Conventionally fabricated alloys included V57, MM 200, Rene 77, Rene 125, MM 246, MM 509, IN-738, IN-792 + Hf, and MM 200 + Hf. The directionally solidified alloys were MM 200, MM 200 single crystal, MM 200 bicrystal, cellular gamma/gamma' - delta) and lamellar gamma/gamma' - delta. The coatings systems included NiCrAlY on IN-738, In-792 + Hf, MM 200 DS, MM 200 DS single crystal, and cellular gamma/gamma' - delta and NiCrAlY/Pt on lamellar gamma/gamma' - delta. Crack initiation survival rates were recorded for all alloys, with and without coatings. All uncoated alloys, except MM 509, exhibited significant oxidation weight loss in 75,000 to 15,000 cycles. MM 509 specimens had weight losses only slightly higher than coated specimens through 7,500 cycles. All coated specimens had low weight loss.

Hill, V. L.↗

The Development and Production of a Functionally Graded Composite for Pb-Bi Service

A material that resists lead-bismuth eutectic (LBE) attack and retains its strength at 700°C would be an enabling technology for LBE-cooled reactors. No single alloy currently exists that can economically meet the required performance criteria of high strength and corrosion resistance. A Functionally Graded Composite (FGC) was developed with layers engineered to perform these functions. F91 was chosen as the structural layer of the composite for its strength and radiation resistance. Fe-12Cr-2Si, an alloy developed from previous work in the Fe-Cr-Si system, was chosen as the corrosion-resistant cladding layer because of its chemical similarity to F91 and its superior corrosion resistance in both oxidizing and reducing environments. Fe-12Cr-2Si experienced minimal corrosion due to its self-passivation in oxidizing and reducing environments. Extrapolated corrosion rates are below one micron per year at 700ï°C. Corrosion of F91 was faster, but predictable and manageable. Diffusion studies showed that 17 microns of the cladding layer will be diffusionally diluted during the three year life of fuel cladding. 33 microns must be accounted for during the sixty year life of coolant piping. 5 cm coolant piping and 6.35 mm fuel cladding preforms were produced on a commercial scale by weld-overlaying Fe-12Cr-2Si onto F91 billets and co-extruding them. An ASME certified weld was performed followed by the prescribed quench-and-tempering heat treatment for F91. A minimal heat affected zone was observed, demonstrating field weldability. Finally, corrosion tests were performed on the fabricated FGC at 700ï°C after completely breaching the cladding in a small area to induce galvanic corrosion at the interface. None was observed. This FGC has significant impacts on LBE reactor design. The increases in outlet temperature and coolant velocity allow a large increase in power density, leading to either a smaller core for the same power rating or more power output for the same size core. This FGC represents an enabling technology for LBE cooled fast reactors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗