Characterizing Early Damage Evolution in CMCs

Silicon carbide / silicon carbide ceramic matrix composites (SiC/SiC CMCs) are structural ceramics that are well-suited for the extreme environment conditions of space and aerospace applications largely due to their low weight, creep resistance, damage tolerance, and high specific strength. In CMCs, the initiation and accumulation of damage depends on characteristics of the constituent landscape including porosity, interfacial properties, and geometric distribution of CMC constituents. In order to accurately predict the lifetimes of these advanced composites, it is critical to understand the evolution of damage and to characterize which early damage mechanisms subsequently lead to crack coalescence and macroscopic failure. In this study, SiC/SiC minicomposites are characterized through an experimental approach combining acoustic emission (AE) with tensile testing in-SEM (scanning electron microscope), in order to examine early damage initiation (below the proportional limit) and its evolution at room temperature. The approach provides insight into the relative activity of early damage mechanisms in CMCs at both the surface and subsurface levels and sheds light on the impact of fabrication choices on the evolution of damage to final failure. The potential application of this combined approach towards the characterization of damage in SiC/SiC CMCs under more complex testing conditions will also be discussed.

damage evolution↗

Characterizing Damage Accumulation in CMCs

Silicon carbide / silicon carbide ceramic matrix composites (SiC/SiC CMCs) are structural ceramics that are well-suited for the extreme environment conditions of aerospace applications largely due to their low weight, creep resistance, damage tolerance, and high specific strength. In CMCs, the initiation and evolution of damage is influenced by a number of factors including characteristics of the constituent landscape (porosity, interfacial properties, and geometric distribution of CMC constituents), thermo-mechanical loading parameters, and environmental conditions. However, much is still unknown about these factors and the interactions between them. In order to accurately predict the lifetimes of these advanced composites, it is critical to understand the evolution of damage and to characterize which early damage mechanisms (and their relationship to key microstructural features) subsequently lead to crack coalescence and macroscopic failure. This research focuses on the use of a multi-modal, experimental approach to examine the relative activity of surface and subsurface damage mechanisms in CMCs. The impact of fabrication choices on the evolution of damage to final failure, and the influence of constituent architecture on early damage mechanisms, are investigated. This approach combines acoustic emission (AE) with microscale deformation tracking via digital image correlation inside a scanning electron microscope (SEM-DIC). The potential application of this combined approach towards characterization of damage in SiC/SiC CMCs under more complex testing conditions is explored.

Swaminathan, Bhavana↗

Repair process and a repaired component

Matrix composite component repair processes are disclosed. The matrix composite repair process includes applying a repair material to a matrix composite component, securing the repair material to the matrix composite component with an external securing mechanism and curing the repair material to bond the repair material to the matrix composite component during the securing by the external securing mechanism. The matrix composite component is selected from the group consisting of a ceramic matrix composite, a polymer matrix composite, and a metal matrix composite. In another embodiment, the repair process includes applying a partially-cured repair material to a matrix composite component, and curing the repair material to bond the repair material to the matrix composite component, an external securing mechanism securing the repair material throughout a curing period, In another embodiment, the external securing mechanism is consumed or decomposed during the repair process.

42 ENGINEERING↗

The Influence of SiC on the Ablation Response of Advanced Refractory Composite Materials

In continuing our studies of advanced refractory composite materials we have recently completed an arc-jet test series of a diverse group of ceramics and ceramic matrix composites. The compositions range from continuous fiber reinforced ceramics to monoliths. Many of these materials contain SiC and one objective of this test series was to identify the influence of SiC oxidation mechanisms on material performance. Hence the arc heater was operated at two conditions; one in which the passive oxidation of SiC would be dominant and the other where the active oxidation of SiC would be dominant. It is shown here that the active oxidation mechanism of SiC does not dominate material performance when it is present at levels equal to or below 20 volume percent.

Bull, Jeffrey D.↗

Joining and Assembly of Silicon Carbide-based Advanced Ceramics and Composites for High Temperature Applications

Silicon carbide based advanced ceramics and fiber reinforced composites are under active consideration for use in wide variety of high temperature applications within the aeronautics, space transportation, energy, and nuclear industries. The engineering designs of ceramic and composite component require fabrication and manufacturing of large and complex shaped parts of various thicknesses. In many instances, it is more economical to build up complex shapes by joining simple geometrical shapes. In addition these components have to be joined or assembled with metallic sub-components. Thus, joining and attachment have been recognized as enabling technologies for successful utilization of ceramic components in various demanding applications. In this presentation, various challenges and opportunities in design, fabrication, and testing o high temperature joints in ceramic matrix composites will be presented. Silicon carbide based advanced ceramics (CVD and hot pressed), and C/SiC and SiC/SiC composites, in different shapes and sizes, have been joined using an affordable, robust ceramic joining technology (ARCJoinT). Microstructure and high temperature mechanical properties of joints in silicon carbide ceramics and CVI and melt infiltrated SiC matrix composites will,be reported. Various joint design philosophies and design issues in joining of ceramics and composites well be discussed.

Singh, M.↗

Graphite/Polyimide Tabs For High-Temperature Tensile Tests

Delamination from ceramic composite specimens prevented. Tabs made from composite of graphite and PMR-15 polyimide enable high-temperature tensile testing of flat coupons of ceramic-matrix composites. Also used in high-temperature tensile testing of flat coupons of ceramics, metals, and metal-matrix composites.

Gyekenyesi, John Z.↗

Fabrication of Fiber-Reinforced Celsian Matrix Composites

A method has been developed for the fabrication of small diameter, multifilament tow fiber reinforced ceramic matrix composites. Its application has been successfully demonstrated for the Hi-Nicalon/celsian system. Strong and tough celsian matrix composites, reinforced with BN/SiC-coated Hi-Nicalon fibers, have been fabricated by infiltrating the fiber tows with the matrix slurry, winding the tows on a drum, cutting and stacking of the prepreg tapes in the desired orientation, and hot pressing. The monoclinic celsian phase in the matrix was produced in situ, during hot pressing, from the 0.75BaO-0.25SrO-Al2O3-2SiO2 mixed precursor synthesized by solid state reaction from metal oxides. Hot pressing resulted in almost fully dense fiber-reinforced composites. The unidirectional composites having approx. 42 vol% of fibers exhibited graceful failure with extensive fiber pullout in three-point bend tests at room temperature. Values of yield stress and strain were 435 +/- 35 MPa and 0.27 +/- 0.01 percent, respectively, and ultimate strengths of 900 +/- 60 MPa were observed. The Young's modulus of the composites was measured to be 165 +/- 5 GPa.

Bansal, Narottam P.↗

Development of Advanced Environmental Barrier Coatings for SiC/SiC Composites at NASA GRC: Prime-Reliant Design and Durability Perspectives

Environmental barrier coatings (EBCs) are considered technologically important because of the critical needs and their ability to effectively protect the turbine hot-section SiC/SiC ceramic matrix composite (CMC) components in harsh engine combustion environments. The development of NASA's advanced environmental barrier coatings have been aimed at significantly improved the coating system temperature capability, stability, erosion-impact, and CMAS resistance for SiC/SiC turbine airfoil and combustors component applications. The NASA environmental barrier coating developments have also emphasized thermo-mechanical creep and fatigue resistance in simulated engine heat flux and environments. Experimental results and models for advanced EBC systems will be presented to help establishing advanced EBC composition design methodologies, performance modeling and life predictions, for achieving prime-reliant, durable environmental coating systems for 2700-3000 F engine component applications. Major technical barriers in developing environmental barrier coating systems and the coating integration with next generation composites having further improved temperature capability, environmental stability, EBC-CMC fatigue-environment system durability will be discussed.

Environmental barrier coatings (EBCs)↗

A CMC database for use in the next generation launch vehicles (rockets)

Ceramic matrix composites (CMC's) are being envisioned as the state-of-the-art material capable of handling the tough structural and thermal demands of advanced high temperature structures for programs such as the SSTO (Single Stage to Orbit), HSCT (High Speed Civil Transport), etc. as well as for evolution of the industrial heating systems. Particulate, whisker and continuous fiber ceramic matrix (CFCC) composites have been designed to provide fracture toughness to the advanced ceramic materials which have a high degree of wear resistance, hardness, stiffness, and heat and corrosion resistance but are notorious for their brittleness and sensitivity to microscopic flaws such as cracks, voids and impurity.

Mahanta, Kamala↗

Hybrid Ceramic-CMC Vane with EBC for Future Coal Derived Syngas Fired 65% Efficient Turbine Combined Cycle

The efficiency of both simple cycle and combined cycle power generation systems scale with the peak temperature at which the gas exits the combustor to drive the turbine. In conventional systems, a substantial fraction of the total turbine core flow exiting the compressor is diverted downstream to cool metallic turbine hardware rather than power the turbine, much of which is used to cool the first-stage turbine vane. The use of coal derived syngas fuels provides an additional challenge to the lifetime of materials utilized in the turbine, as particulate byproducts created in the coal gasification process melt in the combustion gas, and can subsequently deposit and interact with the turbine hardware. The development of durable hot-section materials capable of operating at temperature well above that of single crystal superalloy airfoil/zirconia based thermal barrier coatings is critical to realizing 65% efficient coal derived syngas fired gas turbine based power systems. To enable higher turbine inlet temperatures while lowering cooling air requirements, United Technologies Research Center (UTRC), the central R&D laboratory supporting UT Pratt & Whitney, led the conceptual design of a new type of ceramic composite turbine hot section materials system. The design focused on a novel hybrid monolithic ceramic-fiber reinforced ceramic matrix composite (CMC) first stage turbine vane having an environmental barrier coating. By utilizing ceramic construction in the turbine hot-section, the core flow normally used to cool metallic components will be substantially reduced, increasing efficiency and reducing emissions. To provide the framework for future demonstration testing, UTRC partnered with University of North Dakota Energy and Environmental Research Center (UNDEERC) to provide a conceptual design for a gasified coal fed high-pressure turbine combustor system designed to mimic the conditions expected in a future 65% fuel to busbar efficient syngas fueled gas turbine based combined cycle. The UNDEERC and UTRC collaborated on characterizing dusts from coal gasifier filtration systems.

10 SYNTHETIC FUELS↗

Factors Controlling Stress Rupture of Fiber-Reinforced Ceramic Composites

The successful application of fiber-reinforced ceramic matrix composites (CMC) depends strongly on maximizing material rupture life over a wide range of temperatures and applied stresses. The objective of this paper is to examine the various intrinsic and extrinsic factors that control the high-temperature stress rupture of CMC for stresses below and above those required for cracking of the 0 C plies (Regions I and II, respectively). Using creep-rupture results for a variety of ceramic fibers and rupture data for CMC reinforced by these fibers, it is shown that in those cases where the matrix carries little structural load, CMC rupture conditions can be predicted very well from the fiber behavior measured under the appropriate test environment. As such, one can then examine the intrinsic characteristics of the fibers in order to develop design guidelines for selecting fibers and fiber microstructures in order to maximize CMC rupture life. For those cases where the fiber interfacial coatings are unstable in the test environment, CMC lives are generally worse than those predicted by fiber behavior alone. For those cases where the matrix can support structural load, CMC life can even be greater provided matrix creep behavior is properly controlled. Thus the achievement of long CMC rupture life requires understanding and optimizing the behavior of all constituents in the proper manner.

DiCarlo, J. A.↗

Joining and Integration of Silicon Carbide-Based Materials for High Temperature Applications

Advanced joining and integration technologies of silicon carbide-based ceramics and ceramic matrix composites are enabling for their implementation into wide scale aerospace and ground-based applications. The robust joining and integration technologies allow for large and complex shapes to be fabricated and integrated with the larger system. Potential aerospace applications include lean-direct fuel injectors, thermal actuators, turbine vanes, blades, shrouds, combustor liners and other hot section components. Ground based applications include components for energy and environmental systems. Performance requirements and processing challenges are identified for the successful implementation different joining technologies. An overview will be provided of several joining approaches which have been developed for high temperature applications. In addition, various characterization approaches were pursued to provide an understanding of the processing-microstructure-property relationships. Microstructural analysis of the joint interfaces was conducted using optical, scanning electron, and transmission electron microscopy to identify phases and evaluate the bond quality. Mechanical testing results will be presented along with the need for new standardized test methods. The critical need for tailoring interlayer compositions for optimum joint properties will also be highlighted.

Ceramic Matrix Composites↗

ASME Code Rules and ASTM Standards Integration for Ceramic Composite Core Materials and Components 1

Fiber-reinforced ceramic matrix composites have many desirable properties for high-temperature nuclear applications, including excellent thermal and mechanical properties and reasonable to outstanding radiation resistance. Over the last 20 years, the use of ceramic composite materials has already expanded in many commercial nonnuclear industries as fabrication and application technologies mature. The new ASME design and construction rules under Section III, Subsection HH, Subpart B lay out the requirements and criteria for materials, design, machining and installation, inspection, examination, testing, and the marking procedure for ceramic composite core components, which is similar to the established graphite code under Section III, Subsection HH, Subpart A. Moreover, the general requirements listed in Section III, Subsection HA, Subpart B are also expanded to include ceramic composite materials. The code rules rely heavily on the development and publication of standards for composite specification, classification, and testing of mechanical, thermal, and other properties. These test methods are developed in the American Society for Testing and Materials Committee C28 on Advanced Ceramics with a current focus on ceramic composite tubes. Details of the composites code, design methodology, and similarities to the graphite code, as well as guidance for the development of specifications for ceramic composites for nuclear application and recent standard developments, are discussed. The next step is to "close the gap" to support licensing aspects by validating the code with benchmarking data.

Geringer, Josina↗

Evaluation of CVI SiC/SiC Composites for High Temperature Applications

Silicon carbide fiber reinforced silicon carbide (SiC/SiC) composites are candidate materials for various high temperature turbine engine applications because of their high specific strength and good creep resistance at temperatures of 1400 C (2552 F) and higher. Chemical vapor infiltration (CVI) SiC/SiC ceramic matrix composites (CMC) incorporating Sylramic-iBN SiC fiber were evaluated via fast fracture tensile tests (acoustic emission damage characterization to assess cracking behavior), tensile creep testing, and microscopy. The results of this testing and observed material behavior degradation mechanisms are reviewed.

testing↗

NASA's high-temperature engine materials program for civil aeronautics

The Advanced High-Temperature Engine Materials Technology Program is described in terms of its research initiatives and its goal of developing propulsion systems for civil aeronautics with low levels of noise, pollution, and fuel consumption. The program emphasizes the analysis and implementation of structural materials such as polymer-matrix composites in fans, casings, and engine-control systems. Also investigated in the program are intermetallic- and metal-matrix composites for uses in compressors and turbine disks as well as ceramic-matrix composites for extremely high-temperature applications such as turbine vanes.

Gray, Hugh R.↗

Environmental Barrier Coating Fracture, Fatigue and High-Heat-Flux Durability Modeling and Stochastic Progressive Damage Simulation

Advanced environmental barrier coatings will play an increasingly important role in future gas turbine engines because of their ability to protect emerging light-weight SiC/SiC ceramic matrix composite (CMC) engine components, further raising engine operating temperatures and performance. Because the environmental barrier coating systems are critical to the performance, reliability and durability of these hot-section ceramic engine components, a prime-reliant coating system along with established life design methodology are required for the hot-section ceramic component insertion into engine service. In this paper, we have first summarized some observations of high temperature, high-heat-flux environmental degradation and failure mechanisms of environmental barrier coating systems in laboratory simulated engine environment tests. In particular, the coating surface cracking morphologies and associated subsequent delamination mechanisms under the engine level high-heat-flux, combustion steam, and mechanical creep and fatigue loading conditions will be discussed. The EBC compostion and archtechture improvements based on advanced high heat flux environmental testing, and the modeling advances based on the integrated Finite Element Analysis Micromechanics Analysis Code/Ceramics Analysis and Reliability Evaluation of Structures (FEAMAC/CARES) program will also be highlighted. The stochastic progressive damage simulation successfully predicts mud flat damage pattern in EBCs on coated 3-D specimens, and a 2-D model of through-the-thickness cross-section. A 2-parameter Weibull distribution was assumed in characterizing the coating layer stochastic strength response and the formation of damage was therefore modeled. The damage initiation and coalescence into progressively smaller mudflat crack cells was demonstrated. A coating life prediction framework may be realized by examining the surface crack initiation and delamination propagation in conjunction with environmental degradation under high-heat-flux and environment load test conditions.

Mechanical creep and fatigue loading condition↗

Expanding the Capability of A Legacy Combustion Flametube to Test High Temperature Engine Materials in Relevant Environments

New materials and component designs are needed to advance gas turbine engine technology and provide the performance and efficiency needs for future applications. In order to advance these materials, testing in combustion environments is a critical step prior to engine testing. In this work, we detail the design and the fabrication of a materials test sector in a flametube combustor facility. The facility simulates a combustion environment similar to that experienced by components in gas turbine engines. The flow regime is characterized by a combination of high-temperature, high-velocity, high-heat flux, and high-velocity that components experience in gas turbine engines. Exposure of components in this facility allows for the study of combined environmental effects and the impact on both coating and substrate durability. The test facility may operate across a wide range of pressures from 275-400 psig (1,896-2,758 kPa) and an air flow rate of 5 lb/s (2.27 kg/s). While combustion gas temperature is expected in excess of 3,000°F (1,649°C), 900°F (482°C) cooling air may be supplied to the backside of components or test articles. The flametube combustor was previously used to evaluate fuel injectors and combustion products, and the new test configuration will also allow for materials exposure to complex, engine-like conditions. The interior of the Test Section was additively manufactured from GRCop-84 and cryogenically fit and brazed to a stainless steel 304 housing. The use of a copper liner minimizes welds and with active cooling, is expected to provide better durability over traditional hardware using stainless steel or Inconel with a ceramic liner. The Test Section has two opposing removable windows approximately 230 mm x 80 mm that can accommodate articles up to 85 mm tall. This modular design allows for custom platforms to hold coupons, panels, or airfoil shapes to be tested with minimal re-engineering or fabrication. The bolted joint and sealing remains consistent, so any new testing only needs to work within the existing design footprint. This paper will provide an overview of the facility capabilities, design considerations, as well as thermal and structural analysis of the hardware. Future testing of ceramic matrix composite (CMC) airfoils and advanced environmental barrier coatings (EBCs) will also be discussed.

Combustion↗

Advanced Environmental Barrier Coatings Developed for SiC/SiC Composite Vanes

Ceramic components exhibit superior high-temperature strength and durability over conventional component materials in use today, signifying the potential to revolutionize gas turbine engine component technology. Silicon-carbide fiber-reinforced silicon carbide ceramic matrix composites (SiC/SiC CMCs) are prime candidates for the ceramic hotsection components of next-generation gas turbine engines. A key barrier to the realization of SiC/SiC CMC hot-section components is the environmental degradation of SiC/SiC CMCs in combustion environments. This is in the form of surface recession due to the volatilization of silica scale by water vapor. An external environmental barrier coating (EBC) is a logical approach to achieve protection and long-term durability.

Lee, Kang N.↗