At least 55 records · Page 3

Realizing crack-free high-aluminum-mole-fraction AlGaN on patterned GaN beyond the critical layer thickness

Wide-bandgap III-nitride heterostructures are required for a variety of device applications. However, this alloy system has a large lattice constant and thermal expansion coefficient mismatch that limits the alloy composition and layer thickness for many heteroepitaxial device structures. Consequently, various methods have been devised to allow the heteroepitaxial growth of AlInGaN heterostructures to accommodate this inherent strain. In this work, we describe a non-planar-growth approach that enables the deposition of crack-free high-Al-mole-fraction Al x Ga 1-x N on patterned GaN/sapphire templates and bulk GaN substrates with large-area mesas. We have studied the effects of the patterned mesa width, the mesa etch depth, and the gap between the mesas on the heteroepitaxy of Al x Ga 1-x N superlattices with an average Al molar fraction 0.11 < x¯ < 0.21 and non-planar overgrowth growth thicknesses up to 3.5 μm. Similar to the planar growth approach, increasing the thickness and Al mole fraction of the Al x Ga 1-x N superlattices leads to surface cracking when exceeding the critical layer thickness. However, limiting the mesa dimension in one direction enables strain mitigation and drastically increases the critical layer thickness. Additionally, larger etch depths of the mesas increase the Al alloy composition and thickness for crack-free AlGaN heteroepitaxy whereas the gap in between the mesas seems to have no crucial influence. We demonstrate that the Al alloy composition and layer thicknesses of such heterostructures can be increased far beyond the critical layer thickness for planar growth and demonstrate the growth of a crack-free full AlxGa 1-x N/GaN quantum-well laser heterostructure designed for operation at ~370 nm.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Fracture-based shape optimization built upon the topological derivative

In Silva et al. (2011) and Alidoost et al. (2020), the authors developed an approximation of the energy release rate field associated with a small edge or surface crack at any boundary location and with any orientation using the topological derivative. The approximation is computationally attractive because it requires only a single analysis on the non-cracked domain in contrast with conventional boundary-element and finite-element-based methods, which require a separate and costlier analysis for each crack length-location-orientation combination. Here, a shape optimization scheme for fracture-resistant structures is developed using the energy release rate approximation. In the gradient-based optimization scheme, the domain and its boundary are defined implicitly using level-set functions. The level-set functions of arbitrary geometries are constructed using Boolean operations from the level-set functions of simple primitives. This geometrical representation has the dual advantage of (i) allowing shapes to intersect and/or separate during the optimization and (ii) simplifying the computation of the shape sensitivities.

42 ENGINEERING↗

Modeling brittle fracture due to anisotropic thermal expansion in polycrystalline materials

Here, this work investigated brittle fracture of polycrystalline materials due to thermal stresses arising from anisotropic thermal expansion. We used phase-field fracture simulations with the properties of alpha-uranium (α-U) and assumed a linear elastic mechanical response. Three-dimensional simulations were used to predict fracture for various conditions and crystallographic textures. We found that fracture was more pronounced during cooling than during heating because the anisotropy increased with temperature. We also found that the total crack surface area increased with increasing average misorientation, while the net shape change of the material decreased with increasing misorientation. Two-dimensional simulations in which one crystallographic coefficient of thermal expansion (CTE) was set to zero indicated that the expansion behavior in the crystallographic direction with the smallest CTE was the primary cause of fracture.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Efficient high-fidelity TRISO statistical failure analysis using Bison: Applications to AGR-2 irradiation testing

The ability of tri-structural isotropic (TRISO) fuel to contain fission products is largely dictated by the quality of the manufacturing process, since most of the fission product release is expected to occur due to coating layer failure in a small number of particles containing defects. The Bison fuel performance code has capabilities to predict failure in individual particles, accounting for the presence of defects, and to apply statistical analysis methods to compute the probability of failure in a set of fuel particles. Bison has recently undergone significant development both to improve its physical representations of fuel particle behavior and to improve the efficiency of its statistical failure calculations. Physical model improvements include new capabilities to account for the pressure generated by fission gases on inner pyrolytic carbon (IPyC) crack surfaces and to use local material coordinate orientation to accurately incorporate the anisotropy in the material properties in aspherical particles. To improve statistical modeling efficiency, a direct integration approach which involves directly integrating the failure probability function associated with statistically varying parameters has been developed. The direct integration approach is much more efficient than the Monte Carlo (MC) schemes commonly employed, and allows Bison to directly run high-dimensional fuel performance models, which improves the accuracy of failure probability calculations. Finally, a set of benchmark problems is considered here to compare the MC and direct integration approaches, and a statistical failure analysis of compacts in the Advanced Gas Reactor (AGR)-2 experiments is performed using the direct integration approach.

36 MATERIALS SCIENCE↗

Implications of carbon content for the processing, stability, and mechanical properties of cast and wrought Ni-based superalloy Nimonic 105

As the temperature and pressure requirements in land-based turbines for power generation increase, the shift towards more advanced alloys, e.g., Ni-based superalloys, requires improved understanding of their long-term stability and mechanical properties. Additionally, the larger size of the components also presents fabrication and cost-reduction problems. In this study, we investigated Nimonic 105 as a potential rotor material at two carbon content levels – the commonly used maximum of the alloy specification and a lower carbon content variant. Reducing the carbon content presented fabrication challenges, resulting in surface crack formation during hot working. Additionally, a lower M 6 C carbide fraction was present after fabrication/solutioning, leading to a significantly larger grain size. After the standard aging treatment, similar γ' populations formed in the two variants, however the M 6 C carbides in the high-carbon variant already started transforming to intergranular M 23 C 6 . Although we did not observe a noticeable effect on the tensile properties of the two variants, the lower carbon content alloy possessed a superior creep property – mainly due to the larger grain size as the microstructural stability was inferior. Further, upon prolonged thermal exposure, the M 6 C carbides in the low-carbon variant further decomposed to intergranular and intragranular σ and μ precipitates, as opposed to mainly M 23 C 6 as in the high-carbon variant.

36 MATERIALS SCIENCE↗

Combustion-assisted ink-jet printing of nuclear targets

Advances in target fabrication are critical to high-precision measurements in nuclear physics. This work details the preparation of patterned CeO 2 and ThO 2 architectures and thin-film targets via ink-jet deposition of combustible solutions. The produced targets were characterized by scanning electron microscopy (SEM), and by alpha-particle spectroscopy for radioactive targets to determine densities. Ink jet printing of the targets, used both ethanol and 2-methoxyethanol as solvents, with cerium or thorium nitrate as the oxidizer and acetylacetone as the fuel. Additionally, we found that the distance between each droplet dispersion (step size) played the most significant role in determining the final pattern uniformity and thickness. A 50 μm step size leads to relatively thick targets with a density of 350 μg/cm 2 . Significant overlap in droplet sizes leads to a heterogeneous target with an undesirable cracked surface structure. In contrast, 150 μm spacing yields thinner (20 μg/cm 2 ) patterned structures with excellent surface coverage. This method of Ink-jet printing provides a straightforward, scalable, and high-efficiency pathway to prepare custom made, high-quality targets for nuclear physics experiments.

CeO2↗

The comparative strength and fracture toughness properties of commercial 95W-3.5Ni1.5Fe and 95W-3.5Ni1.5Cu tungsten heavy alloys

Due to the sharp surface cracks resulting from high and cyclic thermal loads, fracture toughness is a crucial property for fusion divertor materials. Tungsten heavy alloys (WHA) have emerged as a leading candidate for plasma facing component applications. Both the WNiFe and WNiCu WHAs have been considered. However, there is no fracture toughness data in the literature on the WNiCu WHA. Therefore, maximum load elastic–plastic fracture toughness (K Jm ) of a commercial 95W-3.5Ni1.5Cu (NiCu) WHA plate is reported here for the first time. The NiCu WHA K Jm is compared to a corresponding K Jm for commercial 95W-3.5Ni1.5Fe (NiFe) WHA, along with comparisons of their respective microstructures, microhardness, and tensile properties. Although their room temperature yield strengths are similar (≈ 600 MPa), the NiFe WHA has higher ultimate stress (818 MPa vs. 642 MPa) and total elongation (8% vs. 1.2%) compared to the NiCu WHA. Most notably, the room temperature elastic–plastic K Jm for the NiFe WHA of ≈ 80 ± 8 MPa$\sqrt{m}$, is nearly twice that of the NiCu WHA at ≈ 47 ± 4 MPa$\sqrt{m}$. Further, while the NiFe WHA experienced stable ductile tearing, the crack propagated unstably (approximately elastically) after reaching the maximum load in the NiCu WHA. The higher K Jm of the NiFe WHA is attributed to its higher flow stress and ductility, along with the energy dissipation and microcrack dilatational stress shielding, provided by a wide distribution of arrested process-zone microcracks, which are largely absent in the NiCu WHA. Since, the 95W-NiFe WHA has distinctly better mechanical properties than 95W-NiCu WHA, it is a more suitable candidate for the fusion reactor application.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Understanding Reactivities of Ni-rich Li[NixMnyCo1-x-y]O2 Single-Crystal Cathode Materials

While Ni-rich Li[NixMnyCo1-x-y]O2 (NMC, x ? 0.8) compounds are considered the most promising cathode materials for high-energy lithium-ion batteries (LIBs), a significant challenge is the higher reactivities caused by the increased Ni content, especially under high-voltage operation conditions. In the present study, we synthesize three single-crystal NMC (SC-NMC) samples with the same particle size and morphology: LiNi0.8Mn0.1Co0.1O2 (NMC811), LiNi0.80Mn0.15Co0.05O2 (NMC80155) and LiNi0.85Mn0.10Co0.05O2 (NMC85105). By systematically varying the composition while controlling other properties, the role of each transition metal during air exposure, thermal treatment and long-term cycling is clearly demonstrated. We reveal that while higher Ni content leads to an overall increased reactivities, the presence of Mn provides a stabilizing effect on thermal, structural and chemical properties. In the absence of cycling-induced particle cracking, surface reconstruction is shown to be the dominating contributor to cathode capacity fade. Our study provides key insights needed for the development of better-performing Ni-rich NMC cathode materials.

Kim, Minkyung↗

Approaches for the Simulation of Coupled Processes in Evolving Fractured Porous Media Enabled by Exascale Computing

Models have historically represented fractured porous media with continuum descriptions that characterize the media using bulk parameters. The impact of small-scale features is not captured in these models, although they may be controlling the performance of subsurface applications. Pore-scale models can simulate processes in small-scale features by representing the pore space geometry explicitly but are computationally expensive for large domains. The alternative multiscale approach entails the combination of pore-scale and continuum-scale descriptions in a single framework. We use Chombo-Crunch, a computational capability that discretizes complex geometries with an adaptive, embedded boundary method to contrast these two approaches. Chombo-Crunch takes advantage of recent computational performance and memory bandwidth improvements resulting from the emergence of exascale computing resources. These combined improvements enable the efficient simulation of reactive transport in fractured media with a high degree of fidelity and the ability to capture the control small-scale processes exert on the overall medium evolution.

42 ENGINEERING↗

In-Situ Calibrated Digital Process Twin Models for Resource Efficient Manufacturing

The chief objective of manufacturing process improvement efforts is to significantly minimize process resources such as time, cost, waste, and consumed energy while improving product quality and process productivity. This paper presents a novel physics-informed optimization approach based on artificial intelligence (AI) to generate digital process twins (DPTs). The utility of the DPT approach is demonstrated in the case of finish machining of aerospace components made from gamma titanium aluminide alloy (γ-TiAl). This particular component has been plagued with persistent quality defects, including surface and sub-surface cracks, which adversely affect resource efficiency. Previous process improvement efforts have been restricted to anecdotal post-mortem investigation and empirical modeling, which fail to address the fundamental issue of how and when cracks occur during cutting. In this work, the integration of in-situ process characterization with modular physics-based models is presented, and machine learning algorithms are used to create a DPT capable of reducing environmental and energy impacts while significantly increasing yield and profitability. Based on the preliminary results presented here, we report an improvement in the overall embodied energy efficiency of over 84%, 93% in process queuing time, 2% in scrap cost, and 93% in queuing cost has been realized for γ-TiAl machining using our novel approach.

42 ENGINEERING↗

Capacity Fade of Graphite/NMC811: Influence of Particle Morphology, Electrolyte, and Charge Voltage

LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) is an important Li-ion battery cathode material; however, there is a tradeoff between delivered capacity and capacity retention. As the charge potential increases the capacity rises but at the expense of capacity retention. The decrease in capacity retention has been ascribed to several factors including particle cracking, surface reconstruction, transition metal dissolution, and electrolyte reactivity. The present study compares 4.1 and 4.3 V charging limits in commercially relevant graphite/NMC811 pouch cells for single crystal (SC) and polycrystalline (PC) NMC811 with ethylene carbonate (EC)-containing or EC-free electrolytes. The electrochemistry is rationalized through analysis of electrochemical impedance spectroscopy, positive electrode X-ray photoelectron spectroscopy, soft X-ray absorption spectroscopy, X-ray diffraction, and negative electrode mapping by X-ray fluorescence. Graphite/SC-NMC811 cells show high-capacity retention at 4.1 V but exhibit degradation at 4.3 V charging potentials. The EC-free electrolyte cells led to higher capacity fade, especially when charged to 4.3 V. Cathode dissolution and deposition on the negative electrode from PC-NMC811 cells was higher than for samples from SC-NMC811 cells. This study reveals the impact of material type, charge voltage, and electrolyte composition on the reactions at the positive electrode, their influence on the negative electrode, and evolution with cycle number.

36 MATERIALS SCIENCE↗

A simplified framework for prediction of sensor network coverage in real-time structural health monitoring of plate-like structures

In this article, the coverage area prediction of piezoelectric sensor network for detecting a specific type of under-surface crack in plate-like structures is addressed. In particular, this article proposes a simplified framework to estimate the coverage of any given sensor network arrangement when a critical defect is known. Based on numerical results from finite element methods (FEM), a simplified framework to estimate coverage area of any given network arrangement is developed. Using such a simplified framework, one can avoid time-consuming procedure of evaluating numerous FEM models in estimating sensor network coverage. Back-scatter fields of partial cracks are estimated using a proposed function, whose parameters are estimated from the results of a limited number of FEM simulations. The proposed function efficiently predicts the back-scattered field of any combination of transmitters and receivers for a given crack geometry. Superposition is used to estimate the coverage area of an arbitrary piezoelectric (e.g., PZT) sensor network. It is shown that the coverage area of a sensor network depends on both sensor network geometry and defect properties (e.g., crack inclination) and it is not necessarily a linear function of the number of sensors. Furthermore, it is shown that the network arrangement has an important effect on the geometry of the coverage area. Experimental results of a network of 14 PZTs in two clusters confirm the accuracy of the method.

Engineering↗

Residual Stresses in Spent Nuclear Fuel Storage Canisters with Cold Spray Coatings

This report describes the development of cold spray (CS) process and its application to provide on overlay coating of metal welds with a surface crack in a spent nuclear fuel (SNF) storage canister and thereby remediate the canister from further propagation of the crack. This work informs aging management programs for the SNF canisters.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

ATF Cladding Mechanical Properties Report: Capability Demonstration

This report documents mechanical testing capability demonstration activities performed in fiscal year (FY)2025 at Oak Ridge National Laboratory(ORNL)on chromium-coated (Cr-coated) and uncoated advanced zirconium alloy claddings irradiated in the High Flux Isotope Reactor (HFIR) to approximately 4 displacements per atom (dpa), corresponding to ~13GWd/t burnup. Specimens were prepared in axial tension (ATT) and ring tension (RTT) geometries, and passive silicon carbide(SiC)thermometry (TM) was employed to determine irradiation temperatures, which averaged 38–43 °C below the 330 °C design target. Mechanical testing at ambient temperature demonstrated the expected irradiation-induced hardening, with yield strength(YS)and ultimate tensile strength(UTS)values increasing substantially relative to unirradiated counterparts. However, this strengthening was accompanied by a reduction in ductility, as indicated by lower uniform and total elongations(UE and TE). Both coated and uncoated claddings exhibited similar mechanical response, though Cr-coated specimens showed surface cracking perpendicular to the loading direction, attributable to the hardness mismatch between the coating and substrate. Fracture in all cases remained ductile, and no coating spallation was observed following HFIR irradiation. Complementary efforts were directed toward the fabrication of test specimens from commercially irradiated cladding (rod 47I, ~31.1 GWd/t average burnup). Axial sectioning and computer numerical control(CNC)machining successfully produced ATT geometries suitable for benchmarking against HFIR-irradiated specimens. This capability enables direct comparison of cladding behavior between test reactor and commercial reactor environments, thereby supporting the validation of HFIR as a surrogate irradiation platform for accident tolerant fuel (ATF) development. Once HFIR irradiations are completed in FY26,the relevant comparison tests will be completed. Collectively, the FY 2025 PIE campaign has provided mechanical performance data for irradiated advanced claddings The demonstrated capabilities support the framework for mechanical testing and further evaluations in subsequent years. These efforts will represent an important contribution toward the licensing and deployment of Cr-coated zirconium alloy cladding as a near-term ATF solution.

36 MATERIALS SCIENCE↗

Degradability of Biodegradable Soil Moisture Sensor Components and Their Effect on Maize (Zea mays L.) Growth

Inexpensive and no-maintenance biodegradable soil moisture sensors could improve existing knowledge on spatial and temporal variability of available soil water at field-scale. Such sensors can unlock the full potential of variable-rate irrigation (VRI) systems to optimize water applications in irrigated cropping systems. The objectives of this study were to assess (i) the degradation of soil moisture sensor component materials and (ii) the effects of material degradation on maize (Zea Mays L.) growth and development. This study was conducted in a greenhouse at Colorado State University, Colorado, USA, by planting maize seeds in pots filled with three growing media (field soil, silica sand, and Promix commercial potting media). The degradation rate of five candidate sensor materials (three blends of beeswax and soy wax, balsa wood, and PHBV (poly(3-hydroxybutyrate-co-3-hydroxyvalerate))) was assessed by harvesting sensor materials at four maize growth stages (30, 60, 90, and 120 days after transplanting). All materials under consideration showed stability in terms of mass and dimension except PHBV. PHBV was degraded entirely within 30 days in soil and Promix, and within 60 days in sand. Balsa wood did now show any significant reduction in mass and dimensions in all growth media. Similarly, there was no significant mass loss across wax blends (p = 0.05) at any growth stage, with a few exceptions. Among the wax blends, 3:1 (beeswax:soy wax) was the most stable blend in terms of mass and dimension with no surface cracks, making it a suitable encapsulant for soil sensor. All materials under consideration did not have any significant effect on maize growth (dry biomass, green biomass, and height) as compared to control plants. These results indicated that 3:1 beeswax:soy wax blend, PHBV, and balsa wood could be suitable candidates for various components of biodegradable soil moisture sensors.

Dahal, Subash (ORCID:0000000205489103)↗

Corrosion Mitigation and Increased Discharge Capacity in Aqueous Processed Thick Cathodes using Phosphoric Acid Additives

Aqueous processed cathodes for lithium-ion batteries are favorable for both cost and environmental reasons; however, these electrodes still face significant problems with increasing areal capacities (i.e. thickness). Highly basic slurry conditions (pH in excess of 12) corrode the current collector surface and evolve hydrogen gas. Consequently, bubbling at the electrode interface causes substantial damage to the dried electrode. As the loading of these electrodes is increased, damage becomes severe and results in lack of adhesion and cohesion. Here introduction of phosphoric acid to combat the rise in pH and suppress the corrosion at the current collector surface is investigated. Phosphoric acid was added in increments of 0.5, 1.0, and 1.5 wt% and the subsequent effects on slurry rheology, particle size, adhesion, and electrochemical cycling were investigated. A technique is reported for obtaining thick (6-8 mAh/cm2) cathodes that exhibit reduced surface cracking and improved rate performance as compared to control samples.

Kukay, Alexander↗

Modeling Chemo-Mechanics with Electrolyte Infiltration to Quantify Degradation of Cathode Particles

One of the main goals in modeling lithium-ion batteries is to improve/predict longevity and resilience of new chemistries. To that end, this talk investigates the formation of stress-induced fracture within polycrystalline cathode particles and the impact on capacity loss. Physically based cathode aging dynamics is simulated in a 3D, continuum-level chemo-mechanical model. The model captures anisotropic Li diffusion within a single polycrystalline particle comprised of hundreds to thousands of randomly oriented grains. A recent addition to this model includes electrolyte infiltration, which occurs when the electrolyte seeps into surface cracks within the particle. The model predicts that particle fracture is primarily due to non-ideal grain interactions with slight dependence on high-rate charge demands. Essentially, when neighboring grains are misaligned, they expand a different rates relative to one another leading to high stresses and ultimately the formation of intraparticle cracks. The model predicts that small particles with large grains develop significantly less damage than larger particles with small grains. Finally, the model predicts most of the chemo-mechanical damage accumulates in the first charge after formation. This chemo-mechanical "damage saturation" effect indicates that initial particle fracture occurs within the first few cycles, while long-term cathode degradation is not solely chemo-mechanically induced. The principle contribution of this research is the use of an anisotropic chemo-mechanical model to test how particle geometry affect capacity fade, which predicts that particle size has a stronger effect on capacity fade than grain size and ultimately that small particles with large grains have the least capacity fade.

cathode↗

Influence of acid leaching surface treatment on indentation cracking of soda lime silicate glass

Past work has shown that water or acid soaking treatments can increase the mechanical strength of soda lime silicate (SLS) glasses. In this work, we show that acid leaching treatments result in an increase in the apparent crack resistance of the acid-leached surface of SLS glass during indentation. Vickers indentation tests in controlled environments show a humidity dependence of radial cracking, suggesting that the transport of water through the leached layer plays a critical role in the propagation of cracks to the glass surface. Here, molecular dynamics simulations with reactive force fields indicate that the leached surface layer can undergo pressure-induced mechanochemical reactions during indentation, which increases the bridging oxygen connectivity in the silica network of the leached layer. Such structural changes can hinder transport of water molecules from the environment to the subsurface crack tip. Based on experimental observations and simulation results, a new hypothesis is proposed that mechanochemical restructuring in the leached layer in response to the applied load may lower the transport kinetics of molecular water to critical flaws, resulting in an apparent enhancement in the crack resistance of the acid-leached surface of SLS glass.

36 MATERIALS SCIENCE↗