Type I clathrates as novel silicon anodes: An electrochemical and structural investigation

In this study, silicon clathrates contain cage-like structures that can encapsulate various guest atoms or molecules. Here we present an electrochemical evaluation of type I silicon clathrates based on Ba 8 Al y Si 46-y for the anode material in lithium-ion batteries. Post-cycling characterization with NMR and XRD show no discernible structural or volume changes even after electrochemical insertion of 44 Li into the clathrate structure. The observed properties are in stark contrast with lithiation of other silicon anodes, which become amorphous and suffer from larger volume changes. The lithiation/delithiation processes are proposed to occur in single phase reactions at approximately 0.2 and 0.4 V vs. Li/Li + , respectively, distinct from other diamond cubic or amorphous silicon anodes. Reversible capacities as high as 499 mAh g -1 at a 5 mA g -1 rate were observed for silicon clathrate with composition Ba 8 Al 8.54 S i37.46 , corresponding to Li:Si of 1.18:1. The results show that silicon clathrates could be promising durable anodes for lithium-ion batteries.

36 MATERIALS SCIENCE↗

Inactive Overhang in Silicon Anodes

Li-ion batteries contain excess anode area to improve manufacturability and prevent Li plating. These overhang areas in graphite electrodes are active but experience decreased Li + flux during cycling. Over time, the overhang and the anode portions directly opposite to the cathode can exchange Li + , driven by differences in local electrical potential across the electrode, which artificially inflates or decreases the measured cell capacity. Here, we show that lithiation of the overhang is less likely to happen in silicon anodes paired with layered oxide cathodes. The large voltage hysteresis of silicon creates a lower driving force for Li + exchange as lithium ions transit into the overhang, rendering this exchange highly inefficient. For crystalline Si particles, Li + storage at the overhang is prohibitive, because the low potential required for the initial lithiation can act as thermodynamic barrier for this exchange. We use micro-Raman spectroscopy to demonstrate that crystalline Si particles at the overhang are never lithiated even after cell storage at 45 °C for four months. Because the anode overhang can affect the forecasting of cell life, cells using silicon anodes may require different methodologies for life estimation compared to those used for traditional graphite-based Li-ion batteries.

25 ENERGY STORAGE↗

Surface SiO 2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid–electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiO x coatings of varying thicknesses that form the true surface of the electrode. Here, the lithiation of SiO 2 -coated Si is studied in a controlled manner using SiO 2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO 2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li + . Si lithiation is reversible, and SiO 2 lithiation is largely irreversible. Above 2 nm SiO 2 , voltammetric currents decrease exponentially with SiO 2 thickness. For 2–3 nm SiO 2 , SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO 2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO 2 coating is thicker than 3–4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO 2 /Si interface radially outward from an existing pinhole, followed by the lithiation of SiO 2 from the interface outward.

25 ENERGY STORAGE↗

Restorable Neutralization of Poly(acrylic acid) Binders toward Balanced Processing Properties and Cycling Performance for Silicon Anodes in Lithium-Ion Batteries

Neutralization of poly(acrylic acid) (PAA)-based binders using lithium hydroxide is a common strategy for fabricating silicon anode laminates, which improves rheological properties of slurries toward high-quality electrode laminates. However, the significantly increased basicity causes degradation of Si particles while the irreversible conversion of carboxylic acid groups to lithium carboxylates undermines the binding strength, collectively leading to adverse cycling performance of the fabricated Si anodes. Herein, a novel neutralization process for PAA binders is developed. A weak base, ammonia (NH 3 ), was discovered as a neutralizing agent that still promotes rheological response of binder solutions but results in a reduced pH increase. Interestingly, the resulting ammonium carboxylate groups may cleave during the drying process to restore the neutralized PAA (PAA-NH 3 ) binders to their pristine states. The best-performing composition of 50% neutralization (PAA-50%NH 3 ) provides comparable rheological response as a PAA-Li binder as well as much improved cycling performance. Additionally, the half-cells using the PAA-50%NH 3 binder can deliver 60% capacity retention over 100 cycles at C/3 rate, affording a 23.8% increase compared to PAA-Li half-cells. This restorable neutralization process of PAA binders represents an innovative strategy of mitigating issues from slurry processing of Si particles to achieve concurrent improvements in high-quality lamination and cycling performance.

25 ENERGY STORAGE↗

Physicochemical Heterogeneity in Silicon Anodes from Cycled Lithium-Ion Cells

The severe capacity fade of lithium-ion cells with silicon-dominant anodes has hindered their widescale commercialization. In this work, we link cell capacity fade to the heterogeneous physicochemical evolution of silicon anodes during battery cycling. Through a multi-length scale characterization approach, we demonstrate that silicon particles near the anode surface react differently than those near the copper current collector. In particular, near the anode surface we find an amorphized wispy silicon encased in a highly fluorinated matrix of electrolyte-reduction products. In contrast, closer to the current collector, the silicon retains more of its initial morphology and structure, suggesting the presence of isolated particles. Here, the results show that accessibility of active silicon to lithium-ions varies across the anode matrix. Material and cell designs, which minimize electrode expansion resulting from the in-filling of pores with the solid electrolyte interphase (SEI), are needed to enhance anode homogeneity during the electrochemical cycling.

25 ENERGY STORAGE↗

Characterization of Annealing-Induced Phase Segregation in Composite Silicon Anodes for Li-ion Batteries

Silicon (Si) anodes present a promising alternative to graphite anodes for lithium-ion batteries (LIBs), as Si has a greater specific capacity. However, one major constraint is the volumetric change of Si during lithiation that results in an unstable solid-electrolyte interphase (SEI), so Si-containing electrodes require the use of various strategies to mitigate these effects and improve performance. One such solution is the use of Si nanoparticles (NPs) that maximize the surface area to volume ratio. Here, we discuss electrodes made with Si NPs treated with polyethylene oxide (PEO) (for improving dispersion during processing), conductive carbon NPs, and P84 polyimide binder which shows significant impacts of annealing treatment on improvements of active material utilization, first cycle efficiency, and capacity retention with extensive cycling . We used air-free argon ion polishing to create electrode cross sections and imaged through the electrode thickness using atomic force microscopy (AFM)-based nano-electrical characterization of scanning spreading resistance microscopy (SSRM), nano-mechanical characterizations of contact resonance and force volume (CR-FV), and scanning electron microscopy-based energy dispersive x-ray spectroscopy (SEM-EDS). Results show that the Si and conductive carbon segregate into phases with a distinctive carbon-rich banded morphology that surrounds the Si-rich phase during annealing. In pristine electrodes, the carbon- and SEI-rich bands exhibit a higher electronic conductivity and a lower elastic modulus than the Si active material phase. These structures, as well as distinct electronic and mechanical properties, remain during cycling, suggesting an improvement of electrical conduction pathways and a mechanical strain buffer for active Si material expansion during cycling. This phase separation may be a major factor in the improvement seen in electrochemical performance due to annealing. Additionally, our nm-scale and multi-mode characterizations provide a novel route for understanding and improving energy storage devices, which is advantageous due to the highly inhomogeneous of composite electrodes in nm-mm scales.

ENERGY STORAGE↗

A Commercially Scalable Process for Silicon Anode Prelithiation

During the project, Amprius successfully evaluated new methods and processes for silicon anode prelithiation. Amprius reached several important conclusions: Amprius found that while “in cell” methods are less disruptive to anode production process flows, they are difficult to control with enough reproducibility for high-volume manufacturing. Among the methods evaluated, Amprius determined that the electrochemical prelithiation method is the most flexible, controllable and reproducible. However, the method requires a controlled environment, which would add less than 5% to cell production costs – and potentially much less than 5% if anodes and cells are produced in factories that already have a controlled moisture environment for cell assembly. (In recent years, these factories have become more common as a result of similar moisture sensitivity requirements for high voltage LCO and Nickel-rich NCM cathodes). In developing electrochemical prelithiation electrolyte formulations, Amprius introduced new classes of electrochemical additives for SEI formation and surface protection. These additives are used exclusively in prelithiation and form a more stable SEI structure that increases cycle life by as much as 50%. Since the chemistry and electrochemistry of electrolyte additives is inexhaustible and the SEI affects most performance parameters of lithium-ion cells, the work Amprius performed in this project is only the beginning of a comprehensive study in this direction.

25 ENERGY STORAGE↗

Understanding why poly(acrylic acid) works: decarbonylation and cross-linking provide an ionically conductive passivation layer in silicon anodes

Poly(acrylic acid) (PAA) is commonly used as a binder for fabricating silicon (Si) anode active materials in lithium-ion batteries due to its useful properties including high polar solvent solubility, good rheology, and strong adhesive properties. However, the role and evolution of PAA during electrode fabrication, cycling, and calendar aging are not well understood. In this work, we reveal the evolution of PAA during electrode curing and relate its chemical change to the final electrode properties and performance. These studies are made possible using two types of in situ attenuated total reflectance-infrared Fourier transform (ATR-FTIR) spectroscopy: thermal ATR-FTIR to probe the cross-linking reaction, and ATR-FTIR spectroelectrochemistry of three-dimensional composite electrodes, a unique technique developed herein that probes the solvation dynamics of lithium ions at the silicon anode interface under electrochemical polarization. Specifically, we show that PAA undergoes a thermally-mediated, cross-linking decarbonylation reaction to form an ether-based network polymer. To show the importance of the polyether moieties, we synthesize partially esterified PAA analogues that do not undergo this cross-linking decarbonylation reaction and correlate the degree of cross-linking to half-cell performance metrics. Finally, we unveil the mechanism of the polyether binder performance through in situ ATR-FTIR spectroelectrochemistry and show that PAA acts as an interfacial material that conducts lithium-ions, limits solvent molecule access to the Si surface, and stabilizes the electrode against parasitic lithium inventory loss at high state of charge for an extended period of time.

25 ENERGY STORAGE↗

Enabling Silicon Anodes with Novel Isosorbide-Based Electrolytes

Silicon is seen as one of the most promising anode candidates for next-generation lithium-ion batteries, due to its high theoretical capacity and energy density. However, many technical barriers remain to its implementation, due to its high chemical/electrochemical reactivities with standard electrolytes and incomplete passivation from large volume changes. Herein, we report an isosorbide dimethyl ether (IDE) based electrolyte, which exhibits greatly improved stability, as evidenced by long cycle life and calendar life. An analysis of the cycled silicon surface shows minimal decomposition of organic species from IDE solvent, confirming that the electrolyte maintains a limited chemical reactivity with nucleophilic lithiated silicon (Li x Si). Here, this research opens up new avenues for designing new electrolytes which could ultimately enable the practical application of silicon anodes.

25 ENERGY STORAGE↗

Nanoparticle Surface Passivation Strategies to Improve the Cycle and Calendar Lifetime of Silicon Anodes in Standard Carbonate Electrolytes

Silicon Lithium alloys (SiLix) as the anode active material in a Li-Ion battery configuration offer possible energy densities paralleled only by pure lithium metal. However, the extreme mechanical deformation of alloying and dealloying SiLix through charge/discharge cycles paired with the highly reactive interface of SiLix which generates an interfacial layer known as the solid-electrolyte-interphase are large barriers to industrial adoption of high-silicon-content negative electrodes. Moreover, these challenges are magnified when the thickness of the electrode is brought to relevant levels (>3 mg/cm2). Here, I describe our efforts to address these challenges by utilizing single-nanometer-scale silicon nanoparticles to reduce capacity fade related to mechanical failure. I also detail our efforts to modify the silicon surface through interfacial chemical engineering strategies to passivate the silicon surface. This development three different majority silicon electrodes (50-74 wt%) to achieve cycle capacity retention of greater than 73% through 1000 charge/discharge cycles against capacity-matched NMC-based cathodes and calendar lifetimes greater than one year. This research is a part of the multi-national lab Silicon Consortium Project.

anodes↗

Surface and Bulk Stabilization of Silicon Anodes with Mixed-Multivalent Additives: Ca(TFSI) 2 and Mg(TFSI) 2

Here, silicon is drawing attention as the upcoming anode material for the next generation of lithium-ion batteries due to its higher capacity compared to commercial graphite. However, silicon anions formed during lithiation are highly reactive with binder and electrolyte components creating an unstable SEI layer and limiting the calendar life of silicon anodes. The reactivity of lithium silicide and the formation of an unstable SEI layer is mitigated by utilizing the use of a mixture of Ca and Mg multivalent cations as an electrolyte additive for Si anodes to improve their calendar life. The effect of mixed salts on the bulk and surface of silicon anodes was studied by multiple structural characterization techniques. Ca and Mg ions in the electrolyte formed relatively thermodynamically stable quaternary Li-Ca-Mg-Si Zintl phases in an in-situ fashion and more stable and denser SEI layer on the Si particles. These in turn protect silicon particles against side reactions with electrolytes in a coin cell. The full cell with the mixed cation electrolyte demonstrates enhanced calendar life performance with lower measured current and current leakage than that of the baseline electrolyte due to reduced side reactions. Electron Microscopy, HRXRD, and solid-state NMR results showed that electrodes with mixed cations tended to have less cracking on the electrode surface compared to Si electrodes with Gen2 + FEC and the presence of mixed cations enhances cation migration and formation of quaternary Zintl phases stabilizing bulk and forming a more stable SEI.

25 ENERGY STORAGE↗

Direct determination of solid-electrolyte interphase thickness and composition as a function of state of charge on a silicon anode

Using neutron reflectometry we have determined the thickness and chemistry of the solid-electrolyte interphase (SEI) layer grown on a silicon anode as a function of state of charge and during cycling. We show the chemistry of this SEI layer becomes more LiF like with increasing lithiation and more Li-C-O-F like with delithiation. More importantly the SEI layer thickness appears to increase (about 250 ) as the electrode becomes less lithiated and thins to 180 with increasing Li content (Li 3.7 Si). We attribute this breathing to the continual consumption of electrolyte with cycling.

25 ENERGY STORAGE↗

Multi-phase characterization of pitch-carbon coated nano-silicon anodes for lithium-ion batteries

Silicon (Si) is a leading next-generation Li-ion battery anode candidate that meets rigorous performance demands for portable power including enhanced power and energy density with robust cycling performance. However, a series of complex and interrelated reactions lead to reduced calendar life in Si-containing systems and therefore challenge practical adoption. In the present work, we probe the mechanisms underlying observed performance improvements by adding a pitch-carbon coating onto nano-Si material. We pair solid-phase (X-ray photoemission spectroscopy, Fourier-transform infrared), semi-volatile phase (solid-phase microextraction-gas chromatography-mass spectrometry), and gas-phase (gas chromatography-flame-ionization detector) characterization signals to comprehensively evaluate the impact of pitch-carbon coating on the evolution of the Si solid-electrolyte interphase (SEI) and the associated impacts on electrode/electrolyte reactivity. The pitch-carbon is found to serve as a physicochemical barrier, reducing the electro-active surface area for Si/electrolyte reactivity and preventing Si oxidation. Further, the pitch-carbon coating promotes the evolution of a more-favorable SEI by subsuming substantial functionality typically associated with the fluoroethylene carbonate (FEC) electrolyte additive - such as alkoxide scavenging and suppression of transesterification pathways - and by shifting the competitive electrolyte degradation pathways' favorability. The multi-phase characterization approach enables holistic end-products evaluation from complex (electro)chemical interfacial reactions, which informs a robust interpretation of the carbon coating's role in electrochemical performance improvements. The present mechanistic evaluation aids the rational design for improved nano-Si materials.

25 ENERGY STORAGE↗

Chemical contributions to silicon anode calendar aging are dominant over mechanical contributions

Silicon (Si) anodes are a promising candidate for increasing the energy density of lithium (Li)-ion batteries for electric vehicles. However, they have recently been identified as having poor calendar life that is insufficient for commercial needs, in addition to the well-known issue of their poor cycle life resulting from large volume expansion. Here, a specially designed protocol with variable rest periods between intermittent cycling is used to evaluate the impact of the mechanical disruption of Si and solid electrolyte interphase (SEI) from cycling on calendar aging measurements. Si was found to undergo more mechanical degradation during calendar aging with intermittent cycling than graphite. However, Si anode capacity fade was still dominated by time, especially for rest periods greater than or equal to 1 month between cycling. Postmortem dQ/dV half-cell analysis indicated this was mainly due to Li inventory loss and an increase in electrode resistance. Isothermal microcalorimetry further demonstrated that Si passivation is more disrupted than graphite passivation with intermittent cycling and suggested that there may be a chemical buildup of a detrimental species in the electrolyte, leading to a large spike in heat after the Si and SEI are disrupted by cycling.

25 ENERGY STORAGE↗

Spatial Molecular Layer Deposition of Ultrathin Polyamide To Stabilize Silicon Anodes in Lithium-Ion Batteries

Cycling stability is central to implementing silicon (Si) anodes in next-generation high-energy lithium-ion batteries. However, challenges remain due to the lack of effective strategies to enhance the structural integrity of the anode during electrochemical cycling. Here, we develop a nanoscale polyamide coating, using spatial molecular layer deposition (MLD) of m-phenylenediamine and trimesoyl chloride precursors, to preserve the structural integrity of Si anodes. Poly(acrylic acid) (PAA) has been widely used in Si-based anodes as a binding agent due to its effective binding interactions with Si particles. However, the structural integrity of the anode is compromised by thermochemical decomposition of the poly(acrylic acid) binder, which can occur during electrode drying or during electrochemical cycling. Decomposition causes a 62% decrease in the elastic modulus of the Si anode, as measured by nanoindentation in electrolyte-soaked conditions. This study shows that an ultrathin polyamide coating counteracts this structural degradation, increases the elastic modulus of the degraded anode by 345%, and improves cohesion. Electrochemical analysis of polyamide-coated anodes reveals a film thickness dependence in cycling behavior. High overpotentials and fast capacity fading are observed for Si anodes with a 15 nm coating, whereas Si anodes with a 0.5 nm coating demonstrate stable cycling over 150 cycles with a capacity >1400 mAh g-1. Our findings identify polyamide as an effective electrode coating material to enhance structural integrity, leading to excellent cyclability with higher capacity retention. Furthermore, the use of the spatial MLD approach to deposit the coating enables short deposition time and a facile route to scale-up.

25 ENERGY STORAGE↗