Fatigue Crack Growth in Peened Friction Stir Welds

Friction stir welding induces residual stresses that accelerates fatigue crack growth in the weld nugget. Shot peening over the weld had little effect on growth rate. Laser peening over the weld retarded the growth rate: Final crack growth rate was comparable to the base, un-welded material. Crack tunneling evident from residual compressive stresses. 2195-T8 fracture surfaces were highly textured. Texturing makes comparisons difficult as the material system is affecting the data as much as the processing. Material usage becoming more common in space applications requiring additional work to develop useful datasets for damage tolerance analyses.

Forth, Scott C.↗

Spray Application of Rapidly Solidified Metals

Fast and economical process now available. New process applies rapidly solidified (RS) metal coatings to substrates. RS metals made directly from molten material. Have amorphous or microcrystalline structures and yield coatings having superior wear and corrosion resistance. Mixture of RS metal powder and peening particles sprayed from nozzle against surface coated. Powder and peening particles strike surface simultaneously, and impact bonds powder to surface as uniform coating. New process, which employs shot peening, is safe, fast, and inexpensive.

Chu, H. P.↗

Validation of Hole-Drilling Residual Stress Measurements in Workpieces of Various Thickness

A recent revision to the ASTM E837 standard for near-surface residual stress measurement by the hole-drilling method describes a new thickness-dependent stress calculation procedure applicable to “thin” and “intermediate” workpieces for which strain versus depth response depends on workpiece thickness. This new calculation procedure differs from that of the prior standard, which applies only to thick workpieces with strain versus depth response independent of thickness. Herein we assess the new calculation procedures by performing hole-drilling residual stress measurements in samples with a range of thickness. Near-surface residual stress is measured in a thick aluminum plate containing near-surface residual stress from a uniform shot peening treatment, and in samples of different thickness removed from the plate at the peened surface. A finite element (FE) model is used to assess consistency between measured residual stress across the range of sample thickness. Measured residual stress varies with sample thickness, with thinner samples exhibiting smaller near-surface compressive stress and a larger gradient of subsurface stress. These trends are consistent with both observed bending (curvature) of the removed samples and the trend in FE-calculated expected residual stress. The measured and expected residual stresses are in good agreement for samples of intermediate thickness, but the agreement decreases with sample thickness. Measured residual stress is invariant with gage circle diameter. The new thickness-dependent stress calculation procedure for hole-drilling provides meaningful improvement compared to thick-workpiece calculations.

42 ENGINEERING↗

Residual Stress in Cold Spray SS304L Measured Via Neutron Diffraction and Comparison of Analytical Models to Predict the Residual Stress

Here, this study employs neutron diffraction to investigate the relationship between residual stress and coating thickness in cold sprayed 304L austenitic stainless steel. Results show that shot peening predominantly impacts the residual stress profile, leading to substantial in-plane compressive force. The impact of laser heating, a widely used method to alter cold spray's microstructural properties, on the coating's residual stress is also analyzed. The findings indicate that the maximum compressive residual stress in the in-plane component is mainly independent of coating thickness, which suggests that the material properties determine the maximum residual stress. The cold sprayed deposits possessed compressive, nearly biaxial strain and stresses. After laser heating, these stresses were replaced by tensile residual stresses. Two analytical models, the Tsui and Clyne and the Boruah models, for predicting residual stresses are also evaluated, and both models provide reasonable fits to the experimental data. At this point, the deviations between the experimental results and the models are principally caused by the inability of the current models to address plastic deformation and relaxation, and the residual stresses generated by thermal gradients.

36 MATERIALS SCIENCE↗

Resonant ultrasound spectroscopy for crystalline samples containing initial strain

Resonant ultrasound spectroscopy (RUS) is a mature and robust technique for the nondestructive characterization of the elastic properties of solids capable of providing the elastic constants of anisotropic crystalline solids. The traditional method is based on assuming that the solid is linear elastic and, therefore, obeys a linearized Hookean constitutive relationship (Hooke’s law). In this work, an alternative constitutive law is provided that allows for an initial strain or prestrain to be present stemming from residual stress. Then, the constitutive relationship is integrated into the RUS framework. The model is demonstrated using a realistic prestrain field obtained by simulating shot-peening processing of a polycrystalline Cu sample. The sensitivity of the resonances to the developed prestrain is established and discussed. This work allows researchers to consider the influence of initial strain or residual stress in their samples and the potential influence on accurate elastic constant estimates. The model also supports the potential of RUS for the nondestructive characterization of prestrain in materials.

42 ENGINEERING↗

Increased resistance to stress corrosion of aluminum alloys

Stress corrosion resistance is increased by distorting surface grain-boundary structure and by interrupting the corrosion and stress corrosion. The first is accomplished by machining or shot peening and the second by removal from and later reexposure to the corrosive environment.

Brummer, S. B.↗

Rolling element fatigue testing of gear materials

Rolling element fatigue lives of nine alloys were evaluated in Rolling Contact (RC) rigs. Test conditions included a Hertzian stress at 4,826 MPa (700 ksi), a rolling speed of 6.23 m/sec (245 in/sec.). Tests were run with a Type I oil (MIL-L-7808G) at room temperature. B-10 lives (10% failure rate) of alloys were compared versus reference alloys, VIM-VAR AISI M-50 and VAR AISI 9310. Six case carburizing alloys (AISI 9310, CBS600, CBS1000M, EX00014, Vasco X-2 and EX00053) and three through-hardening alloys (AISI M-50, VascoMax 350 and Vasco Matrix 2 evaluated, showed RCF performance inferior or equivalent to that of AISI 9310 and AISI M-50. It was also found that the effects of vacuum melting processes, different tempering temperatures, freezing cycle during heat treating, shot peening, gold plating and chrome plating employed in the present investigation did not significantly affect RCF life.

Nahm, A. H.↗

Locating Cracks Amid Pitting and Corrosion

Use of two fluorescent penetrants reveals cracks. New inspection technique for locating cracks in metal parts. Dual-dye technique used to inspect metal parts having surface-roughness-height ratings from 125 to 450 microinch (3.2 to 11.4 micrometer). Parts have included shot-peened machined aluminum extrusions; partially machined aluminum castings; aluminum, steel, and titanium tabular weldments; aircraft landing-gear components; chemically milled aluminum sheet and extrusions; and rough-machined aluminum and steel forgings. Also used on nonporous ceraminc parts.

Fahey, P. P.↗

New methodology for shaft design based on life expectancy

The design of power transmission shafting for reliability has not historically received a great deal of attention. However, weight sensitive aerospace and vehicle applications and those where the penalties of shaft failure are great, require greater confidence in shaft design than earlier methods provided. This report summarizes a fatigue strength-based, design method for sizing shafts under variable amplitude loading histories for limited or nonlimited service life. Moreover, applications factors such as press-fitted collars, shaft size, residual stresses from shot peening or plating, corrosive environments can be readily accommodated into the framework of the analysis. Examples are given which illustrate the use of the method, pointing out the large life penalties due to occasional cyclic overloads.

Loewenthal, S. H.↗

Space Shuttle Main Engine High Pressure Fuel Turbopump Turbine Blade Cracking

The analytical results from two-dimensional (2D) and three-dimensional (3D) finite element model investigations into the cracking of Space Shuttle Main Engine (SSME) High Pressure Fuel Turbopump (HPFTP) first- and second-stage turbine blades are presented. Specifically, the initiation causes for transverse cracks on the pressure side of the firststage blade fir tree lobes and face/corner cracks on the downstream fir tree face of the second-state blade are evaluated. Because the blade material, MAR-M-246 Hf (DS), is highly susceptible to hydrogen embrittlement in the -100 F to 400 F thermal environment, a steady-state condition (full power level = 109 percent) rather than a start-up or shut-down transient was considered to be the most likely candidate for generating a high-strain state in the fir tree areas. Results of the analyses yielded strain levels on both first- and second-stage blade fir tree regions that are of a magnitude to cause hydrogen assisted low cycle fatigue cracking. Also evident from the analysis is that a positive margin against fir tree cracking exists for the planned design modifications, which include shot peening for both first- and second-stage blade fir tree areas.

Lee, Henry↗

Eddy current characterization of magnetic treatment of materials

Eddy current impedance measuring methods have been applied to study the effect that magnetically treated materials have on service life extension. Eddy current impedance measurements have been performed on Nickel 200 specimens that have been subjected to many mechanical and magnetic engineering processes: annealing, applied strain, magnetic field, shot peening, and magnetic field after peening. Experimental results have demonstrated a functional relationship between coil impedance, resistance and reactance, and specimens subjected to various engineering processes. It has shown that magnetic treatment does induce changes in a material's electromagnetic properties and does exhibit evidence of stress relief. However, further fundamental studies are necessary for a thorough understanding of the exact mechanism of the magnetic-field processing effect on machine tool service life.

Chern, E. James↗

Eddy current characterization of magnetic treatment of nickel 200

Eddy current methods have been applied to characterize the effect of magnetic treatments on component service-life extension. Coil impedance measurements were acquired and analyzed on nickel 200 specimens that have been subjected to many mechanical and magnetic engineering processes: annealing, applied strain, magnetic field, shot peening, and magnetic field after peening. Experimental results have demonstrated a functional relationship between coil impedance, resistance and reactance, and specimens subjected to various engineering processes. It has shown that magnetic treatment does induce changes in electromagnetic properties of nickel 200 that then exhibit evidence of stress relief. However, further fundamental studies are necessary for a thorough understanding of the exact mechanism of the magnetic field processing effect on machine-tool service life.

Chern, E. J.↗

ETP-0474: Evaluation of Electroless Nickel Coatings to Achieve Interference Fit in the RSRM Without Fretting

Part of the redesign of the SRMs for the Space Shuttle involved the substitution of three new capture cylinders for three of the previously used cylinders. These new cylinders mate with the old standard case segments in each of the three field joints. The new capture cylinders contain an integral capture latch on the tang end which mates with a case clevis during stackup at KSC. The capture cylinders also contain a groove in the capture latch to provide for a third 0-ring in the joint and are designed to achieve a metal-to- metal interference fit between the capture latch and the mating clevis. An unexpected fretting problem has occurred on the tang capture feature and the inner clevis leg interference fit surfaces on flight hardware since STS-26. Varying degrees of fretting damage have been found on the case segments from different flight motors. Fretting is a wear phenomena that occurs when two tightly fitting metal surfaces are subject to cyclic relative motion of extremely small amplitudes (generally less than 0.010-inch) in the absence of adequate lubrication. It is adhesive ("cold" - welding) in nature and vibration is its essential causative factor. This problem has manifested itself on the flight motors as a series of pits and axial gouges on the inside diameter (ID) surfaces of the inner clevis legs and the outside diameter (OD) surfaces of the tang capture features. The problem occurs in varying degrees of severity in all of the field joints. It is not believed that fretting is a flight safety issue. However, it could become a reusability issue if left unattended. Fretting has been encountered in other industries for many years and measures that will prevent or reduce it have been devised. These include: elimination or reduction of vibration (amplitudes and/or frequencies), elimination of slip, improved lubrication between parts, increased surface separation, increased interference, inducing residual compressive stresses in the surfaces of the mating parts, and employing non-fretting interference shims. Looking at each of these separately; vibration and slip occur in varying degrees and magnitudes in the field joints (as part of the roll-out, launch, flight, splashdown, flotation, and/or tow back) and are difficult to define or eliminate. Improved lubrication is something that was evaluated since it would be the simplest change to incorporate, but little or no improvement was found. Increasing surface separation would defeat the purpose of the interference fit. The effect of increasing the interference fit is unknown. Additional shot peening and/or surface rolling to impart residual compressive stresses in the joints undoubtedly would alter the characteristics and finish of the sealing surfaces of the motor cases. Also, experimental data' indicate that the tangs and clevises already have residual compressive stress fields on their surfaces yet fretting occurs. These stresses probably result from the case machining and the glass beading used to clean these surfaces.

Schaffnit, William O.↗

How Surface Treatments Enhance Ground Handling

Several runway surface treatments developed in recent years are described in terms of how aircraft tire landing and takeoff friction requirements are met, particularly during adverse weather conditions. Changing the surface texture with grooving, grinding and shot peening, use of chemicals to remove or prevent accumulation of natural or man-made contaminants, and the use of new techniques and materials are discussed as means of improving surface friction performance. Test data are presented to illustrate the effects of runway conditions on aircraft ground performance. The severity of the problem of operating on runway surfaces which cannot provide sufficient aircraft tire friction capability is also illustrated from documented aircraft accident/incident reports. The paper concludes with recommendations for future pavement research activities.

Yager, Thomas J.↗

RDS-21 Face-Gear Surface Durability Tests

Experimental fatigue tests were performed to determine the surface durability life of a face gear in mesh with a tapered spur involute pinion. Twenty-four sets of gears were tested at three load levels: 7200, 8185, and 9075 lb-in face gear torque, and 2190 to 3280 rpm face gear speed. The gears were carburized and ground, shot-peened and vibro-honed, and made from VIM-VAR Pyrowear 53 steel per AMS 6308. The tests produced 17 gear tooth spalling failures and 7 suspensions. For all the failed sets, spalling occurred on at least one tooth of all the pinions. In some cases, the spalling initiated a crack in the pinion teeth which progressed to tooth fracture. Also, spalling occurred on some face gear teeth. The AGMA endurance allowable stress for a tapered spur involute pinion in mesh with a face gear was determined to be 275 ksi for the material tested. For the application of a tapered spur involute pinion in mesh with a face gear, proper face gear shim controlled the desired gear tooth contact pattern while proper pinion shim was an effective way of adjusting backlash without severely affecting the contact pattern.

Lewicki, David G.↗

Computational Modeling Develops Ultra-Hard Steel

Glenn Research Center's Mechanical Components Branch developed a spiral bevel or face gear test rig for testing thermal behavior, surface fatigue, strain, vibration, and noise; a full-scale, 500-horsepower helicopter main-rotor transmission testing stand; a gear rig that allows fundamental studies of the dynamic behavior of gear systems and gear noise; and a high-speed helical gear test for analyzing thermal behavior for rotorcraft. The test rig provides accelerated fatigue life testing for standard spur gears at speeds of up to 10,000 rotations per minute. The test rig enables engineers to investigate the effects of materials, heat treat, shot peen, lubricants, and other factors on the gear's performance. QuesTek Innovations LLC, based in Evanston, Illinois, recently developed a carburized, martensitic gear steel with an ultra-hard case using its computational design methodology, but needed to verify surface fatigue, lifecycle performance, and overall reliability. The Battelle Memorial Institute introduced the company to researchers at Glenn's Mechanical Components Branch and facilitated a partnership allowing researchers at the NASA Center to conduct spur gear fatigue testing for the company. Testing revealed that QuesTek's gear steel outperforms the current state-of-the-art alloys used for aviation gears in contact fatigue by almost 300 percent. With the confidence and credibility provided by the NASA testing, QuesTek is commercializing two new steel alloys. Uses for this new class of steel are limitless in areas that demand exceptional strength for high throughput applications.

Source record↗

Applications for Gradient Metal Alloys Fabricated Using Additive Manufacturing

Recently, additive manufacturing (AM) techniques have been developed that may shift the paradigm of traditional metal production by allowing complex net-shaped hardware to be built up layer-by-layer, rather than being machined from a billet. The AM process is ubiquitous with polymers due to their low melting temperatures, fast curing, and controllable viscosity, and 3D printers are widely available as commercial or consumer products. 3D printing with metals is inherently more complicated than with polymers due to their higher melting temperatures and reactivity with air, particularly when heated or molten. The process generally requires a high-power laser or other focused heat source, like an electron beam, for precise melting and deposition. Several promising metal AM techniques have been developed, including laser deposition (also called laser engineered net shaping or LENS® and laser deposition technology (LDT)), direct metal laser sintering (DMLS), and electron beam free-form (EBF). These machines typically use powders or wire feedstock that are melted and deposited using a laser or electron beam. Complex net-shape parts have been widely demonstrated using these (and other) AM techniques and the process appears to be a promising alternative to machining in some cases. Rather than simply competing with traditional machining for cost and time savings, the true advantage of AM involves the fabrication of hardware that cannot be produced using other techniques. This could include parts with "blind" features (like foams or trusses), parts that are difficult to machine conventionally, or parts made from materials that do not exist in bulk forms. In this work, the inventors identify that several AM techniques can be used to develop metal parts that change composition from one location in the part to another, allowing for complete control over the mechanical or physical properties. This changes the paradigm for conventional metal fabrication, which relies on an assortment of "post-processing" methods to locally alter properties (such as coating, heat treating, work hardening, shot peening, etching, anodizing, among others). Building the final part in an additive process allows for the development of an entirely new class of metals, so-called "functionally graded metals" or "gradient alloys." By carefully blending feedstock materials with different properties in an AM process, hardware can be developed with properties that cannot be obtained using other techniques but with the added benefit of the net-shaped fabrication that AM allows.

Hofmann, Douglas C.↗