At least 55 records · Page 3

Bearing material

A composite material is described which will provide low friction surfaces for materials in rolling or sliding contact and is self-lubricating and oxidation resistant up to and in excess of about 930 C. The composite is comprised of a metal component which lends strength and elasticity to the structure, a fluoride salt component which provides lubrication and, lastly, a glass component which not only provides oxidation protection to the metal but may also enhance the lubrication qualities of the composite.

Sliney, H. E.

Fretting of AISI 9310 and selected fretting resistant surface treatments

Fretting wear experiments were conducted with uncoated AISI 9310 mating surfaces, and with combinations incorporating a selected coating to one of the mating surfaces. Wear measurements and SEM observations indicated that surface fatigue, as made evident by spallation and surface crack formation, is an important mechanism in promoting fretting wear to uncoated 9310. Increasing humidity resulted in accelerated fretting, and a very noticeable difference in nature of the fretting debris. Of the coatings evaluated, alumimum bronze with a polyester additive was most effective at reducing wear and minimizing fretting damage to the mating uncoated surface, by means of a self-lubricating film that developed on the fretting surfaces. Chromium plate performed as an effective protective coating, itself resisting fretting and not accelerating damage to the uncoated surface.

Bill, R. C.

Wear-resistant ball bearings for space applications

Ball bearings consisting of steel parts of which the rings are coated with hard, wear resistant, chemical vapor deposited TiC are described. Experiments conducted in ultrahigh vacuum, using cages of various materials with self-lubricating properties, show that such bearings are suitable for space applications. The results of laboratory tests on the ESA Meteosat Radiometer Focalizing mechanism, which contains six coated bearings, are summarized.

Boving, H.

Graphite-fiber-reinforced polyimide liners of various compositions in plain spherical bearings

A plain spherical bearing design with a ball diameter of 28.6 mm, a race length of 12.7 mm, and a 1.7-mm-thick, molded composite liner was evaluated. The liner material is a self-lubricating composite of graphite-fiber-reinforced polyimide resin (GFRPI). The liner is prepared by transfer molding a mixture of one part chopped graphite fiber and one part partially polymerized resin into the space between the bearing ball and the outer race and then completing the polymerization under heat and pressure. Several liner compositions were evaluated: two types of polyimide, condensation and addition; two types of graphite fiber, low and high modulus; and four powder additives - cadmium oxide, cadmium iodide, graphite fluoride, and molybdenum disulfide. The bearings were oscillated + or - 15 deg at 1 Hz for 20 kilocycles under a radial unit load of 29 MN sq m (4200 psi) in dry air at 25, 200, or 315 C. Both types of fiber and polyimide gave low friction and wear. A simple equation was developed to fit the wear-time data and adequately predicted wear to 100 kilocycles.

Sliney, H. E.

Friction and wear of sintered fibermetal abradable seal materials

Three abradable gas-path seal-material systems based on a sintered NiCrAlY fiber metal structure were evaluated under a range of wear conditions representative of those likely to be encountered in various knife-edge seal (labyrinth or shrouded turbine) applications. Conditions leading to undesirable wear of the rotating knife were identified, and a model proposed based on thermal effects arising under different rub conditions. It was found, and predicted by the model, that low incursion (plunge) rates tended to promote smearing of the low-density sintered material with consequent wear to the knife edge. Tradeoff benefits between baseline 19 percent dense material, a similar material of increased density, and a self-lubricating coating applied to the 19 percent dense material were identified on the basis of relative rub tolerance and erosion resistance.

Bill, R. C.

Method of making bearing materials

A method is described for making a composite material which provides low friction surfaces for materials in rolling or sliding contact. The composite material which is self-lubricating and oxidation resistant up to and in excess of about 930 C is comprised of a metal component which lends strength and elasticity to the structure and a fluorine salt component which provides oxidation protection to the metal but may also enhance the lubrication qualities of the composite.

Sliney, H. E.

Wear-resistant ball bearings for space applications

Ball bearings for hostile environments were developed. They consist of normal ball bearing steel parts of which the rings are coated with hard, wear-resistant, chemical vapor deposited (C.V.D) TiC. Experiments in ultrahigh vacuum, using cages of various materials with self-lubricating properties, have shown that such bearings are suitable for space applications.

Boving, H.

Graphite-fiber-reinforced polyimide liners of various compositions in plain spherical bearings

Composites made of graphite-fiber-reinforced polyimide (GFRPI) with a fiber-resin ratio (by weight) of about 1 were evaluated as molded outer-race liners in plain spherical bearings. Several compositions were examined: two types of polyimide (addition and condensation polymers), two types of graphite fiber (high and low modulus) and four powder additives (CdO, CdI2, (CF1.1)n, and MoS2). Friction and wear were measured during oscillation at 25, 200, and 315 C. It is shown that all compositions provided good lubrication in dry air, that neither type of polyimide or graphite fiber nor the additives gave a clear advantage, and that wear rates were always higher during run-in, before conditions stabilized. It is concluded that GFRPI composites are self-lubricating under all but the most extreme moisture-free conditions at 25 C. The additives are helpful only with very high loads or extremely dry environments.

Sliney, H. E.

Friction and wear of plasma-sprayed coatings containing cobalt alloys from 25 deg to 650 deg in air

Four different compositions of self-lubricating, plasma-sprayed, composite coatings with calcium fluoride dispersed throughout cobalt alloy-silver matrices were evaluated on a friction and wear apparatus. In addition, coatings of the cobalt alloys alone and one coating with a nickel alloy-silver matrix were evaluated for comparison. The wear specimens consisted of two, diametrically opposed, flat rub shoes sliding on the coated, cylindrical surface of a rotating disk. Two of the cobalt composite coatings gave a friction coefficient of about 0.25 and low wear at room temperature, 400 and 650 C. Wear rates were lower than those of the cobalt alloys alone or the nickel alloy composite coating. However, oxidation limited the maximum useful temperature of the cobalt composite coating to about 650 C compared to about 900 C for the nickel composite coating.

Sliney, H. E.

Preparation of cast aluminum alloy-mica particle composites

A method for making aluminum-mica particle composites is presented in which mica particles are stirred in molten aluminum alloys followed by casting in permanent molds. Magnesium is added either as an alloying element or in the form of pieces to the surface of the alloy melts to disperse up to 3 wt% mica powders in the melts and to obtain high recoveries of mica in the castings. The mechanical properties of the aluminum alloy-mica composite decrease with increasing mica content; however, even at 2.2% it has a tensile strength of 14.22 kg/sq mm with 1.1% elongation, a compression strength of 42.61 kg/sq mm, and an impact strength of 0.30 kgm/sq cm. Cryogenic and self-lubricating bearing are mentioned applications.

Deonath, MR.

Friction and wear of plasma-sprayed coatings containing cobalt alloys from 25 deg to 650 deg in air

Four different compositions of self-lubricating, plasma-sprayed, composite coatings with calcium fluoride dispersed throughout cobalt alloy-silver matrices were evaluated on a friction and wear apparatus. In addition, coatings of the cobalt alloys alone and of one coating with a nickel alloy-silver matrix were evaluated for comparison. The wear specimens consisted of two, diametrically opposed, flat rub shoes sliding on the coated, cylindrical surface of a rotating disk. Two of the cobalt composite coatings gave a friction coefficient of about 0.25 and low wear at room temperature, 400 and 650 C. Wear rates were lower than those of the cobalt alloys alone or the nickel alloy composite coating. However, oxidation limited the maximum useful temperature of the cobalt composite coating to about 650 C compared to about 900 C for the nickel composite coating.

Sliney, H. E.

Structural and compositional characterization of RF sputter-deposited Ni-Cr + Cr2O3 films

An RF-sputtered chrome oxide coating with metallic binders was developed. The chrome oxide coating has high-temperature capabilities and is wear resistant, and has some self-lubricating properties. A nichrome metallic binder was added in the coating to improve its ductility without significant loss in the hardness. The sputtering parameters were optimized to obtain a smooth coating with the maximum adherence. The coatings were applied using bias-sputter and sputter-deposit modes on the heat treated and annealed foil substrates. The coating applied on annealed foils using the sputter-deposit mode was smooth and had the best adherence. Metallurgical examinations showed that the coating was Ni-Cr + Cr2O3. The coating as applied was amorphous and it crystallized during substrate heat treatment.

Bhushan, B.

Process Sprays Uniforms Plasma Coatings

Composite-powder processing procedure developed along with plasma-spray parameters to achieve homogeneous, well-bonded, low-porosity, self-lubricating coatings. Multicomponent plasma coatings are applied without segretation of components.

Sliney, H. E.

Effect of aluminum phosphate additions on composition of three-component plasma-sprayed solid lubricant

Image analysis (IA) and electron microprobe X-ray analysis (EMXA) were used to characterize a plasma-sprayed, self-lubricating coating, NASA LUBE PS106, specified by weight percent as 35NiCr-35Ag-30CaF2. To minimize segregation of the powder mixture during the plasma-spraying procedure, monoaluminum phosphate was added to form agglomerate particles. Three concentrations of AlPO4 were added to the mixtures: 1.25, 2.5, and 6.25 percent by weight. Analysis showed that 1.25 wt% AlPO4 yielded a CaF2 deficiency, 2.5 wt% kept the coating closest to specification, and 6.25 wt% yielded excess CaF2 as well as more impurities and voids and a deficiency in silver. Photomicrographs and X-ray maps are presented. The methods of IA and EMXA complement each other, and the reasonable agreement in the results increases the confidence in determining the coating composition.

Jacobson, T. P.

A commentary on solid lubricants and wear resistant solids for use in extreme environments

The need for high temperature tribological coatings and self-lubricating materials in advanced technology is discussed. A qualitative model for the mechanism of solid lubrication is proposed. The model is based upon microscopic observations of the dynamics of third-body solids in lubricated contacts. In this model, the rheology of plastic flow is suggested as a more general criterion for predicting the lubricating potential of a solid material than, for example, a specific crystal structure. Some examples of layer-lattice and nonlayer-lattice solids that lubricate by virtue of their extreme plasticity, film coherence, and adhesion to the lubricated metal are described. Circumstantial evidence for the model is presented for low shear-strength solids at room temperature and for solids such as calcium fluoride that become lubricative only when their brittle-to-ductile transition temperature is exceeded. Some materials considerations in the selection of hard-coat materials for wear control are also presented.

Sliney, H. E.

Improved uniformity of multiphase ceramic-metal plasma-sprayed coats

Processing-technology development of a multiphase, self-lubricating, plasma-spray powder resulted in greater uniformity and reproducibility of plasma-sprayed coats. The effect of particle-size variation, binder concentration, and reproducible processing parameters are reported. Greater adhesive strengths of coats to substrates were achieved by particle-size variation, use of an intermediate bond coat such as Ni-Cr, or heat treatment. Quantitative analyses of polished, coated specimens are also given.

Nakamura, H. H.

Effects of silver and group 2 fluorides addition to plasma sprayed chromium carbide high temperature solid lubricant for foil gas bearing to 650 deg C

A new self-lubricating coating composition of nickel aluminide-bonded chromium carbide formulated with silver and Group II fluorides was developed in a research program on high temperature solid lubricants. One of the proposed applications for this new coating composition is as a wide temperature spectrum solid lubricant for complaint foil gas bearings. Friction and wear properties were obtained using a foil gas bearing start/stop apparatus at temperatures from 25 to 650 C. The journals were Inconel 718. Some were coated with the plasma sprayed experimental coating, others with unmodified nickel aluminide/chromium carbide as a baseline for comparison. The addtitional components were provided to assist in achieving low friction over the temperature range of interest. Uncoated, preoxidized Inconel X-750 foil bearings were operated against these surfaces. The foils were subjected to repeated start/stop cycles under a 14-kPa (2-psi) bearing unit loading. Sliding contact occurred during lift-off and coastdown at surface velocities less than 6 m/s (3000 rpm). Testing continued until 9000 start/stop cycles were accumulated or until a rise in starting torque indicated the journal/bearing had failed. Comparison in coating performance as well as discussions of their properties and methods of application are given.

Wagner, R. C.