Structural health monitoring of compression connectors for overhead transmission lines

Two-stage aluminum conductor steel-reinforced (ACSR) compression connectors are extensively used in US overhead transmission lines. The connectors are made by crimping a steel sleeve onto a steel core and an aluminum sleeve over aluminum conductive strands. The connectors are designed to operate at temperatures up to 125 C, but their performance is increasingly degrading because of overloading of lines. Currently, electric utilities conduct routine line inspections using thermal and electrical measurements. However, information about the structural integrity of connectors cannot be obtained. In this work, structural health monitoring (SHM) of compression connectors was studied using electromechanical impedance (EMI) analysis. Lead zirconate titanate (PZT)-5A was identified as a smart material for SHM. A flexible high-temperature bonding layer was used to address challenges in PZT integration due to a significant difference in the coefficients of thermal expansion of PZT and the aluminum substrate. The steel joint on the steel core was investigated because it is responsible for the ultimate tensile strength of the connector. Tensile testing was used to create structural damage to the joint, or steel core pullout, and thermal cycling introduced additional structural perturbations. EMI measurements were conducted between the tests. The root mean square deviation (RMSD) of EMI was identified as a damage index. The use of steel joints has been shown to enable SHM under simulated conditions. The EMI signature is sensitive to variations in structural conditions. RMSD can be correlated to the structural health of a connector and has potential for use in the SHM and structural integrity evaluation.

compression connectors↗

The effect of carbon nanotubes microstructures on reinforcing properties of SWNTs/alumina composite

Alumina reinforced with 1 wt% single-wall carbon nanotubes (SWNTs) was fabricated by hot-pressing. The fracture toughness of SWNTs/Al{sub 2}O{sub 3} composite reaches 6.40 {+-} 0.3 MPa m{sup 1/2}, which is twice as high as that of unreinforced alumina. Nanoindentation introduced controlled cracks and the damage were examined by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). SWNTs reinforcing mechanisms including CNT pullout, CNT fracture, CNT bridging and crack deflection were directly observed, and the relationship between carbon nanotubes microstructures in the matrix and mechanical properties was also discussed in detailed.

36 MATERIALS SCIENCE↗

Sic-Sic Composite Interphase Evaluation via Small Scale Mechanical Testing

Silicon carbide (SiC) has emerged as a highly capable engineering material for extreme environment applications. It has proven particularly useful for high temperature applications where it exhibits exceptional strength, relative chemical inertness, and low coefficient of thermal expansion. Recent studies have shown that SiC also has excellent neutronic properties including low thermal neutron absorption, low tritium permeability, and high radiation tolerance. As a result, SiC-SiC composites are being considered for application in accident tolerant fuel cladding and other structural components for fission and fusion reactors. The standard crystalline form of SiC is inherently brittle and therefore subject to low damage tolerance. In order to increase the material toughness, SiC-SiC fiber-matrix composites have been developed. These composites are divided into three constituents; a highly crystalline and near stoichiometric SiC fiber (commonly Hi-Nicalon{sup TM} Type-S or Tyranno{sup TM}-SA), a (layered) interphase of graphitized pyrolytic carbon (PyC) around the fiber, and a chemical vapor infiltrated (CVI) SiC matrix that consolidates the material. Increased toughness is achieved through two primary mechanisms: increasing the crack length by introducing more barriers, and fiber pullout via interphase shear within the matrix. As a result, it has become critically important to understand the fundamental properties of SiC-SiC composites. However, comprehensive material properties are difficult to predict unless we have an in depth knowledge of the individual constituents (fiber, matrix, interphase) and how their properties interact with one another at the micro-scale. Of specific interest to this work are the interfacial properties of the fiber-matrix interface. This includes the internal friction coefficient and interfacial debond shear stress. (authors)

36 MATERIALS SCIENCE↗

Recent experience in the fabrication and brazing of ceramic beam tubes for kicker magnets at FNAL

Ceramic beam tubes are utilized in numerous kicker magnets in different accelerator rings at Fermi National Accelerator Laboratory. Kovar flanges are brazed onto each beam tube end, since kovar and high alumina ceramic have similar expansion curves. The tube, kovar flange, end piece, and braze foil (titanium/incusil) alloy brazing material are stacked in the furnace and then brazed in the furnace at 1000 C. The ceramic specified is 99.8% Alumina, Al{sub 2}O{sub 3}, a strong recrystallized high-alumina fabricated by slip casting. Recent experience at Fermilab with the fabrication and brazing of these tubes has brought to light numerous problems including tube breakage and cracking and also the difficulty of brazing the tube to produce a leak-tight joint. These problems may be due to the ceramic quality, voids in the ceramic, thinness of the wall, and micro-cracks in the ends which make it difficult to braze because it cannot fill tiny surface cracks which are caused by grain pullout during the cutting process. Solutions which are being investigated include lapping the ends of the tubes before brazing to eliminate the micro-cracks and also metallization of the tubes.

43 PARTICLE ACCELERATORS↗