Analysis of governing factors controlling gas transport through fresh and aged triptycene-based polyimide films

In this report the fundamental gas transport properties and physical aging behavior of a series of triptycene-based polyimides with various substitution groups were investigated. Wide-angle x-ray diffraction revealed that the 6FDA-1,4-triptycene polyimides exhibit two chain packing domains with d-spacing values of ~6.7 Å and ~5.3 Å, corresponding to triptycene-induced chain packing disruption and chain segments lacking the triptycene moiety, respectively. Positron annihilation lifetime spectroscopy (PALS) showed a bimodal distribution of microcavity size made up of triptycene cleft cavities that are ~3 Å diameter and larger interchain cavities with an average diameter of ~7 Å. Additionally, PALS confirmed 6FDA-1,4-trip_CH 3 has the lowest fractional free volume, primarily due to smaller contributions from the interchain cavities, and 6FDA-1,4-trip_CF 3 has the largest fractional free volume. It was also found that the addition of substituent groups had a unique and positive effect on the aging properties over nine months, in which the addition of CH 3 and CF 3 groups led to permeability increases of ~20% and ~40%, respectively. This is caused by the combination of the lowered driving force for physical aging, the substituent groups sterically hindering tighter packing with time, and the interconnectivity and/or unblocking of free volume over time through small-scale, local chain motion.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Free volume manipulation of a 6FDA-HAB polyimide using a solid-state protection/deprotection strategy

We report tert-butoxycarbonyl (t-BOC) is a thermally labile moiety that can be used to protect hydroxyl groups on polymers. In this study, t-BOC was appended onto a polyimide consisting of 2,2'-bis-(3,4-dicarboxyphenyl) hexafluoropropane dianhydride (6FDA) and 3,3'-dihydroxy-4,4'-diamino-biphenyl (HAB), after which the polymer was formed into self-standing films. Solid-state thermal treatments were performed to systematically remove t-BOC moieties to alter the physical packing structure and concomitant gas transport properties of the polymer. Despite performing deprotection reactions well below the glass transition temperature of 6FDA-HAB (~300 °C), this free volume manipulation (FVM) approach produced only subtle differences in polymer density, fractional free volume, average free volume element size, and gas transport properties relative to the unprotected polymer. While these findings suggest that thermally removing covalently bound functional groups from polymer films can be used to manipulate free volume and gas transport performance for glassy polymers, more robust polymer systems than linear polyimides are required to preserve the nascent free volume architecture generated from this approach.

36 MATERIALS SCIENCE↗

Tuning gas separation performance of polyimide membranes with macrocyclic crown ether units

Membrane-based gas separation is an energy-efficient alternative to conventional thermally-driven separation processes. However, polymer membranes face the permeability-selectivity trade-off challenge, which stems from the broad size distribution of free volume voids. Here, this study reports a molecular design strategy to address this challenge through incorporating macrocyclic crown ether (CE) moieties into the backbone of Matrimid® polyimide, a commercial gas separation membrane. A series of CE-containing Matrimid®-like copolyimides were synthesized with systematically varied CE molar contents ranging from 3 to 20%. These copolyimides formed ductile, defect-free thin films suitable for membrane fabrication. Gas permeation tests revealed a non-monotonic relationship between permeability/selectivity and CE content. Notably, the copolyimide with only 5% CE demonstrated a 61% increase in CO 2 /CH 4 selectivity and a 13% increase in CO 2 permeability relative to pristine Matrimid®. Higher CE contents did not yield further performance improvements, which is likely due to the competing effects of chain packing disruption and π–π interactions among CE moieties at high content. This hypothesis was supported by wide-angle X-ray scattering (WAXS) analysis, density measurements, and fractional free volume calculations. These findings highlight the potential of macrocyclic crown ether incorporation strategies in fine tuning the microstructure of commercial polyimide gas separation membranes to surpass the traditional permeability-selectivity trade-off.

CO2 separation↗

A novel polyimide based micro heater with high temperature uniformity

MEMS based micro heaters are a key component in micro bio-calorimetry, nondispersive infrared gas sensors, semiconductor gas sensors and microfluidic actuators. A micro heater with a uniform temperature distribution in the heating area and short response time is desirable in ultrasensitive temperature-dependent measurements. In this study, we propose a novel micro heater design to reach a uniform temperature in a large heating area by optimizing the heating power density distribution in the heating area. A polyimide membrane is utilized as the substrate to reduce the thermal mass and heat loss which allows for fast thermal response as well as a simplified fabrication process. A gold and titanium heating element is fabricated on the flexible polyimide substrate using the standard MEMS technique. The temperature distribution in the heating area for a certain power input is measured by an IR camera, and is consistent with FEA simulation results. Finally, this design can achieve fast response and uniform temperature distribution, which is quite suitable for the programmable heating such as impulse and step driving.

42 ENGINEERING↗

Molecular design of nanometric zinc borate-containing polyimide as a route to flame retardant materials

Zinc borate (Zn{sub 2}B{sub 6}O{sub 11}.3H{sub 2}O) nanoparticles were successfully prepared by using an emulsion liquid membrane (W/O/W emulsion) to control the size of particles with Na{sub 2}B{sub 4}O{sub 7}.10H{sub 2}O, boric acid and ZnSO{sub 4}.7H{sub 2}O as raw materials. All materials were dispersed with the polyimide (PI) precursor, poly (amic acid). Using a combination of dissolving the poly (amic acid) and mixing fatty acid surfactant-coated zinc borate nanoparticles; we have demonstrated the formation of nanocomposites with uniform nanoparticles dispersion. We report the first deposition of nanocomposite polyimides from solution using spin-coating. The microstructures and morphology of the as-obtained samples were studied by X-ray diffraction (XRD), infrared spectra (IR), scanning electron microscopy (SEM) equipped with an energy-dispersive X-ray spectrometer (EDX), transmission electron microscopy (TEM) and thermogravimetric analysis (TGA)

36 MATERIALS SCIENCE↗

6FDA-DETDA: DABE polyimide-derived carbon molecular sieve hollow fiber membranes: Circumventing unusual aging phenomena

Transport properties are discussed for asymmetric carbon molecular sieve (CMS) hollow fiber membranes based on polyimide precursors derived from a butanol esterified diamino benzoic acid (DABA) based polyimide, 6FDA-DETDA:DABE. Precursor fiber pretreatment with 10% Ethenyl(trimethoxy)silane [vinyltrimethoxysilane (VTMS)] solution in hexane followed by pyrolysis at 550 °C in ultra-high purity argon created asymmetric CMS fibers with CO 2 permeance above 1000 GPU and CO 2 /CH 4 selectivities > 25. Storage of the as-made modules for 72 days in 7 bar CO 2 suppressed undesirable aging typically seen under vacuum or atmospheric pressure air and provided CO 2 permeance and CO 2 /CH 4 selectivity of 780 GPU and 48 respectively. These results are in contrast to significant losses in CO 2 permeance and CO 2 /CH 4 selectivity for CMS created under equivalent pyrolysis conditions from non-esterified 6FDA-DETDA: DABA variant, even under CO 2 storage. The 6FDA-DETDA: DABA-derived CMS results were surprising, since dense film CMS samples from the same precursors did not show the undesirable permeance and selectivity changes. Moreover, other non-DABA containing precursors in dense film and asymmetric fiber forms can be effectively stabilized under CO 2 storage. Such findings suggest that high residual stress in the freshly formed thin selective layers of asymmetric structures in DABA-derived CMS causes undesirable micro-scale rearrangements. In dense films and even asymmetric skins of non-DABA derived CMS membranes, evidence of such undesirable rearrangements are not apparent. DABA-derived cross-links are presumably the cause of these effects. Mono-esterification of 6FDA-DETDA: DABA to form 6FDA-DETDA: DABE controls such crosslinking-derived stresses and resultant instabilities in the CMS fibers, thereby providing stable high performance gas separation properties under CO 2 storage or use in mixed gas feeds.

03 NATURAL GAS↗

Polyimide aerogels for ballistic impact protection

The ballistic performance of edge-clamped monolithic polyimide aerogel blocks (12 mm thickness) has been studied through a series of impact tests using a helium-filled gas gun connected to a vacuum chamber and a spherical steel projectile (approximately 3 mm diameter) with an impact velocity range of 150–1300 m s -1 . The aerogels had an average bulk density of 0.17 g cm -3 with high porosity of approximately 88%. The ballistic limit velocity of the aerogels was estimated to be in the range of 175–179 m s -1 . Moreover, the aerogels showed a robust ballistic energy absorption performance (e.g., at the impact velocity of 1283 m s -1 at least 18% of the impact energy was absorbed). At low impact velocities, the aerogels failed by ductile hole enlargement followed by a tensile failure. By contrast, at high impact velocities, the aerogels failed through an adiabatic shearing process. Given the substantially robust ballistic performance, the polyimide aerogels have a potential to combat multiple constraints such as cost, weight, and volume restrictions in aeronautical and aerospace applications with high blast resistance and ballistic performance requirements such as in stuffed Whipple shields for orbital debris containment application.

42 ENGINEERING↗

Mechanical and electrical changes in electrochemically active polyimide binders for Li-ion batteries

Polyimide binders are often used in electrodes made with silicon for lithium-ion batteries for their mechanical strength and adhesion, which help mitigate mechanical issues associated with large volumetric expansion. These binders can be electrochemically active, but it is difficult to characterize what physical and chemical changes occur due to a composite electrode with multiple components and processes at play. Here, in this work, we study electrodes consisting only of polyimide binder and conductive carbon, using scanning probe-based techniques—contact resonance, force volume, and scanning spreading resistance microscopy—along with cryo-scanning transmission electron microscopy, electron energy loss spectroscopy, and energy dispersive X-ray spectroscopy. We show that lithium becomes trapped in the binder during cycling and results in large initial capacity losses, the formation of dendrite-like features, column-like domains of significantly increased mechanical modulus, and a slight increase in electronic resistivity.

25 ENERGY STORAGE↗

Efficient production of a collimated MeV proton beam from a polyimide target driven by an intense femtosecond laser pulse

High-flux energetic protons whose maximum energies are up to 4 MeV are generated by an intense femtosecond titanium:sapphire laser pulse interacting with 7.5, 12.5, and 25 {mu}m thick polyimide tape targets. Laser pulse with an energy of 1.7 J and with a duration of 34 fs is focused with an f/3.4 parabolic mirror giving an intensity of 3x10{sup 19} W cm{sup -2}. The main pulse to amplified spontaneous emission (ASE) intensity contrast ratio is 2.5x10{sup 7}. The conversion efficiency from the laser energy into the proton kinetic energies is achieved to be {approx}3%, which is comparable to or even higher than those achieved in the previous works; using nanometer-thick targets, in combination with the short-pulse lasers that have almost the same pulse width and the intensity but different main pulse to ASE intensity contrast of {approx}10{sup 10} [Neely et al., Appl. Phys. Lett. 89, 021502 (2006)], in which the authors claim that the main mechanism is target normal sheath acceleration; or using the 7.5 {mu}m thick polyimide target, in combination with the short-pulse laser, which has almost the same pulse width and the intensity, but the main pulse to ASE intensity contrast ratio was controlled to be 2.5x10{sup 5} [Yogo et al., Phys. Rev. E 77, 016401 (2008)], in which the authors claim the efficient acceleration by the mechanism of the underdense plasma model. The contrast ratio of the present experiment is in between these two experiments. The possible mechanism of this regime is discussed.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Mechanical Failure of Thin Ta and Cu/Ta Layers on Polyimide Substrates: A Synchrotron-Based Technique for In Situ Characterization

In situ synchrotron radiation diffraction and confocal light microscopy is used to study fragmentation and buckling of thin brittle Ta layers with thicknesses of 50 nm, 100 nm and 200 nm on polyimide substrates. Synchrotron-based stress measurements confirm that cracking leads to relaxation of tensile stress. Simultaneously, compressive stress arises in transverse direction, which finally leads to buckling. This behavior can be explained quantitatively by a two-dimensional shear lag model. It is well established that the properties of the coating-substrate interface determine the processes of coating fragmentation and delamination. A possible approach for influencing and controlling these processes is given by the incorporation of a ductile interlayer. It can be observed that the presence of Cu interlayers with thicknesses of 5 nm, 20 nm and 50 nm reduces the fracture strength of brittle Ta coatings on polyimide substrates, whereas the resistance to buckling is increased significantly.

36 MATERIALS SCIENCE↗

Outgassing and degradation of polyimide induced by swift heavy ion irradiation at cryogenic temperature

Polyimide foils were irradiated with energetic Kr (740 MeV) and Pb (890 MeV) ions at cryogenic temperature (12 K). Beam-induced degradation processes were monitored by residual gas analysis and online infrared spectroscopy. The outgassing components observed at low irradiation temperatures differ in quantity but are similar in mass distribution to those identified at room temperature exposure. Besides CO as major volatile fragment, a significant contribution of short hydrocarbons like C{sub 2}H{sub x} is released. In situ infrared spectroscopy indicates accumulation of CO and CO{sub 2} molecules at 12 K in the foils. During heat-up cycles, most of these frozen gases become mobile and outgas at a temperature between 35 and 55 K. The study is motivated by the application of polyimide foils as insulating material in high radiation environment of the future accelerator facility for antiproton and ion research (FAIR).

36 MATERIALS SCIENCE↗

Pyrolytic carbon free-radical evolution and irradiation damage of polyimide under low-energy proton irradiation

Ionization and displacement effects are basic phenomena in damage processes of materials under space-particle irradiation. In this paper, the damage behaviors were investigated on the polyimide under proton irradiation using electron paramagnetic resonance (EPR) spectra analysis and optical absorbance valuation. The results indicate that the proton irradiation induces the formation of pyrolytic carbon free-radical with a g value of 2.0025, and the population of free radicals increases with the irradiation fluence. The most important finding is that the irradiation-induced free-radical population increases linearly with the displacement damage dose, as does the optical degradation, whereas the ionization effect alone, during the irradiation, cannot induce the formation of pyrolytic carbon free radical. Furthermore, during the post storage, after irradiation, the free-radical population decreases following a sum of an exponential and a linear mode with the storage time. It is interesting that, during the post storage, the recovery of the degraded optical absorbance of the polyimide follows a similar mode to that of free radicals, and the characteristic time constant changes with the wavelength of the optical spectra.

36 MATERIALS SCIENCE↗

Temperature dependence and the dispersion of nonlinear optical properties of chromophore-containing polyimide thin films

Detailed investigations of the quadratic nonlinear response of a series of new polyimides with covalently attached chromophore DR13 are performed by the Maker fringes method in the range of fundamental wavelength from 850 to 1450 nm. Polymer films with thickness of 100–400 nm were spin-coated on glass substrates and corona poled. For these materials, the maximum values of the second harmonic generation coefficients d{sub 33} are 80–120 pm/V. A red shift of the nonlinear response dispersion with respect to the linear absorption spectrum was observed for the DR13 chromophore. The temperature dependences of linear absorption and nonlinear coefficients d{sub 33} for studied structures are observed. It was found that the temperature changes of the absorption spectra lead to appreciable contribution to the value of the nonlinear coefficient d{sub 33}. The demonstrated high temperature stability (up to 120 °C) of chromophore-containing polyimide thin films makes it possible to eliminate the degradation of their nonlinear optical properties in the future applications of such structures.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

High-temperature polyimide coating for optical fibres

We present our first results on the fabrication of new, high-performance polyimide coatings. The key components of the coatings are polyimides containing various cardo and/or fluoroalkylene groups, which allows the coatings to retain their high-temperature stability and facilitates the storage of the starting polymer and the optical fibre coating process owing to the good solubility of such copolymers in many organic solvents. Annealing for 30 s, 1 h and 24 h at temperatures of 430, 350 and 300 °C, respectively, reduces the strength of optical fibres having such coating by no more than 10%. (optical fibres)

36 MATERIALS SCIENCE↗

The Effect of γ Irradiation on Phase Transitions in the Polyimide–YBa{sub 2}Cu{sub 3}O{sub 6+} {sub x} System

The effect of γ irradiation on optical properties of films of the polyimide–YBa{sub 2}Cu{sub 3}O{sub 6.7} system with different concentrations of the filler in the form of the finely crystalline compound YBa{sub 2}Cu{sub 3}O{sub 6.7} (0.05 wt %, 0.10 wt %, and 0.50 wt %) has been investigated. The properties were studied on an IKS-29 infrared spectrophotometer in a spectral range of 400–4200 cm{sup –1} at room temperature. The samples were irradiated in air under room conditions on an RKhM-γ-20 by doses of 150, 250, and 600 kGy. The power of the exposure dose of the {sup 60}Co source was 0.16 rad/s. It has been established that irradiation with a dose of up to 600 kGy of the abovementioned system slightly affects the structure of the polyimide matrix but decreases the number of free radical groups in the film structure with the formation of hydrogen bonds. In the range of 400–4200 cm{sup –1} at D = 150 kGy, the most intense changes in spectra of polymeric composite samples have been revealed. In the range of 2850–3350 cm{sup –1}, the wide absorption spectrum band is preserved, which is caused by the presence of Cu, Y, and Ba crystallohydrates. The band is related to deformation vibrations of the Cu–O bond in YBa{sub 2}- Cu{sub 3}O{sub 6.7} (YBCO) chains due to properties of barium carbonate, formation of oxygen vacancies in the filler, and vibrations of the Cu(I)–O(I) bonds near one or several O(4) vacancies. Irradiation by doses of 250 and 600 kGy for different concentrations of the filler leads to a decrease in the signal intensity in the range of 1800–3600 cm{sup –1} by 20–35% on average. Peaks related to interband transitions (transitions of the Cu(I)–Cu(IY)–Cu(II) system) and bending vibrations O(I)–Cu(I) are not changed by strains of O(IY)–Cu(I) bonds. This testifies to the radiation-stimulated diffusion of oxygen atoms to O(IY) sites determining the orthorhombic phase of YBa{sub 2}Cu{sub 3}O{sub 6.7} from the occupied positions in the Cu–O sublattice.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Key Features of Polyimide-Derived Carbon Molecular Sieves

Carbon molecular sieve (CMS) membranes have impressive separation properties; however, both chemical and morphology structures need to be understood better. Here we characterize CMS with the simplest polyimide (PI) PMDA/pPDA (PMDA=pyromellitic dianhydride, pPDA=p-phenylenediamine), using FTIR, solid-state 15 N-NMR and 13 C-NMR, XPS, XRD, and Raman spectra to study chemical structure. Here we also compare gas separation properties for this CMS to a CMS derived from a more conventional PI precursor. The detailed characterization shows the presence of aromatic pyridinic, pyrrolic rings as well as graphitic, pyridonic components and a few other groups in both CMS types derived from the very different precursors. The CMS morphologies, while related to precursor and pyrolysis temperature details, show similarities consistent with a physical picture comprising distributed molecular sieving plate-like structures. These results assist in understanding diverse CMS membrane separation performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High solvent-resistant and integrally crosslinked polyimide-based composite membranes for organic solvent nanofiltration

This study reports a new class of integral polyimide (PI)-based thin film composite (TFC) membranes (with improved solvent resistance in both the skin layer and the substrate) for organic solvent nanofiltration (OSN). The OSN membrane was prepared via interfacial polymerization (IP) onto a PI ultrafiltration (UF) substrate, followed by an imidization, a chemical crosslinking, and a solvent activation process. During the IP process, m-phenylenediamine (MPD), dopamine (DA), and 1,2,4,5-benzene tetracarboxylic acyl chloride (BTAC) were respectively used as an aqueous monomer, an aqueous additive, and an organic monomer. We proved that amide bonding formed between MPD and the PI substrate during the immersion of the substrate in the aqueous MPD solution, thus providing a strong binding between the substrate and the subsequently formed skin layer of polyamide acid (PAA), which was formed due to reaction between MPD and BTAC during the IP process. DA contains amine group and could also help build a strong binding between the substrate and the skin layer during the same IP process. The subsequent imidization step converted the PAA molecules of the skin layer into PI polymers, which was quite similar to that of the substrate. The final crosslinking step crosslinked not only the inner molecules of the skin layer, and the inner molecules of the substrate, but also the interface molecules between the skin and substrate so as to form an integral composite membrane with improving solvent resistance. Finally, the fabricated OSN membranes under optimal preparation conditions exhibited an ethanol permeance of 2.03 L m -2 h -1 bar -1 with a rejection of 98% for Rhodamine B (479 Da) and exhibited an outstanding organic solvent resistance without compromising separation performance during the persistent immersion in DMF at 80 °C for two weeks, indicating a promising prospective in OSN applications.

36 MATERIALS SCIENCE↗

Polyimide as a durable cathode for all-solid-state Li(Na)–organic batteries with boosted cell-level energy density

The integration of organic electrode materials (OEMs) with solid-state electrolytes (SSEs) is expected to build an all-solid-state battery (ASSB) with long-term sustainability, high safety, and high energy density. Despite this great promise, the cell-level energy density is still far from practically applicable, which stems from the ultrathick SSE layer and thin cathode layer used in a pellet-type ASSB design. Here, a cost-effective polyimide (PI) material was first exploited as an organic cathode for sulfide-based ASSBs. A capacity of ~190 mAh g -1 was delivered with almost no capacity decay over 300 cycles. Moreover, for the first time, a dry-film approach was introduced to manufacture a sheet-type Li–organic ASSB with an ultrathin SSE layer and a high-areal-loading PI cathode. Notably, PI is a perfect candidate for dry-film technology due to its high thermal stability and extraordinary chemical inertness toward sulfide SSEs. Remarkably, the free-standing SSE membrane was merely 46 μm thick, and an ultralow areal resistance of 3.3 Ω cm 2 was achieved, more than tenfold lower than that of reported SSE pellets. One order of magnitude boost in the cell-level energy density was achieved. This work presents a significant leap in transferring organic ASSB technology from laboratory research to factory manufacturing.

25 ENERGY STORAGE↗