Engineering PapersSearch

SEARCH · Engineering Papers

Results for “oxide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

A statistical analysis of elevated temperature gravimetric cyclic oxidation data of 36 Ni- and Co-base superalloys based on an oxidation attack parameter

A large body of high temperature cyclic oxidation data generated from tests at NASA Lewis Research Center involving gravimetric/time values for 36 Ni- and Co-base superalloys was reduced to a single attack parameter, K(sub a), for each run. This K(sub a) value was used to rank the cyclic oxidation resistance of each alloy at 1000, 1100, and 1150 C. These K(sub a) values were also used to derive an estimating equation using multiple linear regression involving log(sub 10)K(sub a) as a function of alloy chemistry and test temperature. This estimating equation has a high degree of fit and could be used to predict cyclic oxidation behavior for similar alloys and to design an optimum high strength Ni-base superalloy with maximum high temperature cyclic oxidation resistance. The critical alloy elements found to be beneficial were Al, Cr, and Ta.

Barrett, Charles A.

Some Properties of Beryllium Oxide and Beryllium Oxide - Columbium Ceramals

High-temperature tensile and thermal-shock investigations were conducted on beryllium oxide and beryllium oxide plus columbium metal additions. X-ray diffraction and metallographic results are given. The tensile strength of 6150 pounds per square inch for beryllium oxide at 1800 degrees F compared favorably with the zirconia bodies previously tested. Additions of 2, 5, 8, 10, 12, and 15 percent by weight of columbium metal failed to improve the shock resistance over that of pure beryllium oxide.

Robards, C F

Oxide_Oxide Ceramic Matrix Composite (CMC) Exhaust Mixer Development in the NASA Environmentally Responsible Aviation (ERA) Project

Rolls-Royce North American Technologies, Inc. (LibertyWorksLW) began considering the development of CMC exhaust forced mixers in 2008, as a means of obtaining reduced weight and hotter operating temperature capability, while minimizing shape distortion during operation, which would improve mixing efficiency and reduce fuel burn. Increased component durability, enhanced ability to fabricate complex-shaped components, and engine noise reduction are other potential advantages of CMC mixers (compared to metallic mixers). In 2010, NASA was pursuing the reduction of NOx emissions, fuel burn, and noise from turbine engines in Phase I of the Environmentally Responsible Aviation (ERA) Project. ERA subtasks, including those focused on CMC components, were formulated with the goal of maturing technology from proof of concept validation (TRL 3) to a systemsubsystem or prototype demonstration in a relevant environment (TRL 6). In April 2010, the NASA Glenn Research Center (GRC) and LibertyWorks jointly initiated a CMC Exhaust System Validation Program within the ERA Project, teaming on CMC exhaust mixer development for subsonic jet engines capable of operating with increased performance. Our initial focus was on designing, fabricating, and characterizing the thrust and acoustic performance of a roughly quarter-scale 16-lobe oxide oxide CMC mixer and tail cone along with a conventional low bypass exhaust nozzle. Support Services, LLC (Allendale, MI) and ATK COI Ceramics, Inc. (COIC, in San Diego, CA) supported the design of a subscale nozzle assembly that consisted of an oxide oxide CMC mixer and center body, with each component mounted on a metallic attachment ring. That design was based upon the operating conditions a mixer would experience in a turbofan engine. Validation of the aerodynamic and acoustic performance of the subscale mixer via testing and the achievement of TRL 4 encouraged the NASALWCOIC team to move to the next phase where a full scale CMC mixer sized for a RR AE3007 engine and a compatible attachment flange were designed, followed by CMC component fabrication by COIC, and vibration testing at GRC under conditions simulating the structural and dynamic environment encountered during engine operation. AFRL (WPAFB) supported this testing by performing 3D laser vibrometry to identify the mixer mode shapes and modal frequencies. The successful fabrication and testing of such a component has been achieved. The CMC mixer demonstrated good durability during vibration testing at room and elevated temperature (TRL5). This has cleared the article for a ground-based test on a Rolls-Royce AE3007 engine, where the performance and benefits of the component can be further assessed.

exhaust nozzles

The effects of dispersed oxides on the oxidation characteristics of superalloys

The high-temperature oxidation behavior of thoriated nickel and chromium superalloys is discussed on the basis of scanning electron micrographs and other experimental data. The beneficial effects of dispersed oxide particles are identified as a lower chromium content needed for the formation of external scale, an increased adhesion of scale, and lower growth rates of chromia as compared with those in alloys without dispersed oxide particles.

Jaffee, R. I.

Bonding of sapphire to sapphire by eutectic mixture of aluminum oxide and zirconium oxide

Bonding of an element comprising sapphire, ruby or blue sapphire to another element of such material with a eutectic mixture of aluminum oxide and zirconium oxide is discussed. The bonding mixture may be applied in the form of a distilled water slurry or by electron beam vapor deposition. In one embodiment the eutectic is formed in situ by applying a layer of zirconium oxide and then heating the assembly to a temperature above the eutectic temperature and below the melting point of the material from which the elements are formed. The formation of a sapphire rubidium maser cell utilizing eutectic bonding is shown.

Deluca, J. J.

High gas velocity oxidation and hot corrosion testing of oxide dispersion-strengthened nickel-base alloys

Several oxide dispersion strengthened (ODS) nickel-base alloys were tested in high velocity gases for cyclic oxidation resistance at temperatures to 1200 C and times to 500 hours and for hot corrosion resistance at 900 C for 200 hours. Nickel-chromium-aluminum ODS alloys were found to have superior resistance to oxidation and hot corrosion when compared to bare and coated nickel-chromium ODS alloys. The best of the alloys tested had compositions of nickel - 15.5 to 16 weight percent chromium with aluminum weight percents between 4.5 and 5.0. All of the nickel-chromium-aluminum ODS materials experienced small weight losses (less than 16 mg/sq cm).

Deadmore, D. L.

Thermochemical analyses of the oxidative vaporization of metals and oxides by oxygen molecules and atoms

Equilibrium thermochemical analyses are employed to describe the vaporization processes of metals and metal oxides upon exposure to molecular and atomic oxygen. Specific analytic results for the chromium-, platinum-, aluminum-, and silicon-oxygen systems are presented. Maximum rates of oxidative vaporization predicted from the thermochemical considerations are compared with experimental results for chromium and platinum. The oxidative vaporization rates of chromium and platinum are considerably enhanced by oxygen atoms.

Kohl, F. J.

Bonding of sapphire to sapphire by eutectic mixture of aluminum oxide and zirconium oxide

An element comprising sapphire, ruby or blue sapphire can be bonded to another element of such material with a eutectic mixture of aluminum oxide and zirconium oxide. The bonding mixture may be applied in the form of a distilled water slurry or by electron beam vapor deposition. In one embodiment the eutectic is formed in situ by applying a layer of zirconium oxide and then heating the assembly to a temperature above the eutectic temperature and below the melting point of the material from which the elements are formed. The formation of a sapphire rubidium maser cell utilizing eutectic bonding is shown.

Deluca, J. J.

Silicon carbide as an oxidation-resistant high-temperature material. 1: Oxidation and heat corrosion behavior

The oxidation and corrosion behavior of SiC (in the form of a SiC powder) and hot-pressed and reaction-bound material were studied. The excellent stability of SiC in an oxidizing atmosphere is due to the development of protective SiO2 coatings. Any changes in these protective layers (e.g., due to impurities, reaction with corrosive media, high porosity of SiC, etc.) lead in most cases to increased rates of oxidation and thus restrict the field of SiC application.

Schlichting, J.

Strength distributions of SiC ceramics after oxidation and oxidation under load

The room-temperature strength distributions of a sintered and a hot-pressed SiC were examined as-machined, after oxidation at 1370 C, and after oxidation under load at 1370 C. The strengths were observed to be dependent on both the duration of oxidation and the magnitude of the applied load. Processes resulting in both strengthening and weakening behavior were observed to occur, at times simultaneously within the same strength distribution. This dynamic situation indicates that the strength-controlling flaw populations are highly transient in nature.

Easler, T. E.

Effects of oxidation and oxidation under load on strength distributions of Si3N4

The room-temperature strength distributions of a sintered and a hot-pressed Si3N4 were examined in the as-machined condition, after oxidation at 1370 C and after oxidation under load at 1370 C. The strength-controlling flaw populations were highly transient in nature. Both the duration of oxidation and the magnitude of the applied load were observed to effect changes in strength. This dynamic situation is related to both strengthening and weakening processes, which at times may occur simultaneously in the same strength distribution.

Easler, T. E.

Rare isotope studies involving catalytic oxidation of CO over platinum-tin oxide

Results of studies utilizing normal and rare oxygen isotopes in the catalytic oxidation of carbon monoxide over a platinum-tin oxide catalyst substrate are presented. Chemisorption of labeled carbon monoxide on the catalyst followed by thermal desorption yielded a carbon dioxide product with an oxygen-18 composition consistent with the formation of a carbonate-like intermediate in the chemisorption process. The efficacy of a method developed for the oxygen-18 labeling of the platinum-tin oxide catalyst surface for use in closed cycle pulsed care isotope carbon dioxide lasers is demonstrated for the equivalent of 10 to the 6th power pulses at 10 pulses per second.

Upchurch, Billy T.

The oxidation of carbon monoxide using tin oxide based catalysts

The preparation conditions for precious metal/tin oxide catalysts were optimized for maximum carbon monoxide/oxygen recombination efficiency. This was achieved by controlling the tin digestion, the peptization to form the sol, the calcination process and the method of adding the precious metals. Extensive studies of the tin oxide structure were carried out over the temperature range 20 to 500 C in air or hydrogen environments using Raman scattering and X ray diffraction. Adsorbed species on tin oxide, generated in an environment containing carbon monoxide, gave rise to a Raman band at about 1600 cm(exp -1) which was assigned to carbonaceous groups, possible carbonate.

Sampson, Christopher F.

The high temperature creep behavior of oxides and oxide fibers

A thorough review of the literature was conducted on the high-temperature creep behavior of single and polycrystalline oxides which potentially could serve as fiber reinforcements in ceramics or metal matrix applications. Sapphire when oriented with the basal plane perpendicular to the fiber axis (c-axis oriented) is highly creep resistant at temperatures in excess of 1600 C and applied loads of 100 MPa and higher. Pyramidal slip is preferentially activated in sapphire under these conditions and steady-state creep rates in the range of 10(exp -7) to 10 (exp -8)/s were reported. Data on the creep resistance of polycrystalline beryllia suggest that C-axiz oriented single crystal beryllia may be a viable candidate as a fiber reinforcement material; however, the issure of fabricability and moisture sensitivity must be addressed for this material. Yttrium aluminum garnet (YAG) also appears to be a fiber candidate material having a high resistance to creep which is due to it's complex crystal structure and high Peierl resistance. The high creep resistance of garnet suggests that there may be other complex ternary oxides such as single crystal mullite which may also be candidate materials for fiber reinforcements. Finally, CVD and single crystal SiC, although not oxides, do possess a high resistance to creep in the temperature range between 1550 and 1850 C and under stresses of 110 to 220 MPa. From a review of the literature, it appears that for high creep resistant applications sapphire, silicon carbide, yttrium aluminum garnet, mullite, and beryllia are desirable candidate materials which require further investigation.

Jones, Linda E.

Diffusional transport and predicting oxidative failure during cyclic oxidation of beta-NiAl alloys

Nickel aluminides (NiAl) containing 40-50 at. percent Al and up to 0.1 at. percent Zr have been studied following cyclic oxidation at 1200, 1300, 1350 and 1400 C. The selective oxidation of aluminum resulted in the formation of protective Al2O3 scales on each alloy composition at each temperature. However, repeated cycling eventually resulted in the gradual formation of less protective NiAl2O4. The appearance of the NiAl2O4, signaling the end of the protective scale-forming capability of the alloy, was related to the presence of gamma-prime-(Ni3Al) which formed as a result of the loss of aluminum from the sample. A simple methodology is presented to predict the protective life of beta-NiAl alloys. This method predicts the oxidative lifetime due to aluminum depletion when the aluminum concentration decreases to a critical concentration. The time interval preceding NiAl2O4 formation (i.e., the lifetime based on protective Al2O3 formation) and predicted lifetimes are compared and discussed. Use of the method to predict the maximum use temperature for NiAl-Zr alloys is also discussed.

Nesbitt, J. A.

Thermal-oxidative Pretreatment and Evaluation of Poly (hexafluoropropene Oxide) Fluids

Two commercial poly(hexafluoropropene oxide) fluids were thermally pretreated at 343 C in pure oxygen. IR and NMR spectra indicate that this pretreatment was effective in removing hydrogen end-capped impurities. Decrease in the quantity of volatile material produced during thermal oxidative decomposition and increase in the thermal decomposition temperature indicated improvement in the stability of the fluids. However, this pretreatment failed to render the fluids completely stable in oxidizing atmospheres at 316 C in the presence of metal alloys.

Paciorek, K. J. L.