Results for “compression molding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Development and applications of Fluorel

The development of a nonflammable elastomer for use in Apollo spacecraft is discussed. The requirements for the material to be foamed, extruded, compression molded, and cast into various configurations are examined. A fluorine-based hydrocarbon is considered a promising candidate. An acceptable material known as Fluorel is examined. Procedures for applying fluorel to a flood light glare shield are presented. The process for preparing 20 percent homogenized Fluorel is analyzed.

Supkis, D. E.↗

Flame-resistant elastomeric polymers

Family of polymer formulations, which has limiting oxygen indices from 50 to 100, can be extruded through dies to produce elastic fibers, compression molded, dissolved in solvents as required for coatings, and calendered to produce film and embossed sheeting. Applications include upholstery, paint products, automobile products, and coated fabrics.

Howarth, J. T.↗

Composite hub/metal blade compressor rotor

A low cost compressor rotor was designed and fabricated for a small jet engine. The rotor hub and blade keepers were compression molded with graphite epoxy. Each pair of metallic blades was held in the hub by a keeper. All keepers were locked in the hub with circumferential windings. Feasibility of fabrication was demonstrated in this program.

Yao, S.↗

Polymeric compositions and their method of manufacture

Filled polymer compositions are made by dissolving the polymer binder in a suitable sublimable solvent, mixing the filler material with the polymer and its solvent, freezing the resultant mixture, and subliming the frozen solvent from the mixture from which it is then removed. The remaining composition is suitable for conventional processing such as compression molding or extruding. A particular feature of the method of manufacture is pouring the mixed solution slowly in a continuous stream into a cryogenic bath wherein frozen particles of the mixture result. The frozen individual particles are then subjected to the sublimation.

Moser, B. G.↗

Development and demonstration of manufacturing processes for fabricating graphite/LARC 160 polyimide structural elements

The development and demonstration of manufacturing technologies for the structural application of Celion graphite/LARC-160 polyimide composite material is discussed. Process development and fabrication of demonstration components are discussed. Process development included establishing quality assurance of the basic composite material and processing, nondestructive inspection of fabricated components, developing processes for specific structural forms, and qualification of processes through mechanical testing. Demonstration components were fabricated. The demonstration components consisted of flat laminates, skin/stringer panels, honeycomb panels, chopped fiber compression moldings, and a technology demonstrator segment (TDS) representative of the space shuttle aft body flap.

Frost, R. K.↗

Effect of physical aging on stress relaxation of poly/methyl methacrylate/

A study was made on the stress relaxation behavior at 25 C of poly(methyl methacrylate) in uniaxial tension as a function of physical aging at both room temperature and 60 C. Test specimens were compression molded at 165 C, then quenched to room temperature and allowed to age for up to 30 days prior to testing. Stress relaxation curves measured after different aging times could be superposed to a single master curve for each aging temperature. Superposition was achieved by applying vertical and horizontal shifts. Hence, the shape of the response curves was not changed by aging. This is in accordance with observations made by Struik for tensile creep curves. Volume changes as a function of physical aging were also determined. Simple exponential relationships were observed between volume and both horizontal and vertical shifts. The horizontal shift implies a shift in the effective time scale caused by a change in free volume. The vertical shifts could be correlated with changes in Young's modulus caused by a change in density. For the range of aging studied, the response time scale varied over nearly two decades of log-time. For the same conditions modulus varied by 30 percent.

Cizmecioglu, M.↗

Poly/phenylquinoxalines/ containing ethynyl groups

The synthesis of high molecular weight linear poly(phenylquinoxalines) containing pendant ethynyl groups is reported, where thermally-induced reactions of the ethynyl groups provided insoluble, cross-linked polymers with high glass transition temperatures. The ethynyl-containing polymer exhibited fair to poor processability by compression molding due to the thermal reaction of the ethynyl groups, which inhibited polymer flow, depending on ethynyl density. This class of polymers is not expected to be useful as laminating resins or adhesives, due to the processing difficulties. Use for them may be found, however, as solvents and corrosion-resistant high-temperature coatings.

Hergenrother, P. M.↗

Improved high temperature resistant matrix resins

The objective was to develop organic matrix resins suitable for service at temperatures up to 644 K (700 F) and at air pressures up to 0.4 MPa (60 psia) for time durations of a minimum of 100 hours. Matrix resins capable of withstanding these extreme oxidative environmental conditions would lead to increased use of polymer matrix composites in aircraft engines and provide significant weight and cost savings. Six linear condensation, aromatic/heterocyclic polymers containing fluorinated and/or diphenyl linkages were synthesized. The thermo-oxidative stability of the resins was determined at 644 K and compressed air pressures up to 0.4 MPa. Two formulations, both containing perfluoroisopropylidene linkages in the polymer backbone structure, exhibited potential for 644 K service to meet the program objectives. Two other formulations could not be fabricated into compression molded zero defect specimens.

Chang, G. E.↗

PMR polyimides from solutions containing mixed endcaps

Previous studies have shown that partial substitution of p-aminostyrene (PAS) for the monomethylester of endo-5-norbornene-2, 3-dicarboxylic acid (NE) lowered the cure temperature of PMR polyimides from 316 to 260 C, but the modified PMR polyimides required higher compression-molding pressures than state-of-the-art PMR-15. In this study PMR polyimides are prepared employing three encaps: NE, PAS, and endo-N-phenyl-5-norbornene-2,3-dicarboximide (PN). The effect of PN addition on the processing characteristics and glass transition temperatures of graphite fiber-reinforced PMR composites is studied. The room temperature and short-time 316 C mechanical properties of the composites are determined. The weight loss and mechanical property retention characteristics of the composites after exposure in air at 316 C are also determined.

Delvigs, P.↗

Optimal cure cycle design of a resin-fiber composite laminate

A unified computed aided design method was studied for the cure cycle design that incorporates an optimal design technique with the analytical model of a composite cure process. The preliminary results of using this proposed method for optimal cure cycle design are reported and discussed. The cure process of interest is the compression molding of a polyester which is described by a diffusion reaction system. The finite element method is employed to convert the initial boundary value problem into a set of first order differential equations which are solved simultaneously by the DE program. The equations for thermal design sensitivities are derived by using the direct differentiation method and are solved by the DE program. A recursive quadratic programming algorithm with an active set strategy called a linearization method is used to optimally design the cure cycle, subjected to the given design performance requirements. The difficulty of casting the cure cycle design process into a proper mathematical form is recognized. Various optimal design problems are formulated to address theses aspects. The optimal solutions of these formulations are compared and discussed.

Hou, Jean W.↗

Polyarylene Ethers With Improved Properties

Series of new polyarylene ethers (PAE's) prepared from reaction of activated dihalo compounds with various bisphenols. Compounds exhibit excellent processability by compression molding, plus good mechanical properties. All PAE's prepared suitable for use as adhesives, coatings, films, membranes, and composite matrices. Potentially useful for spacecraft and aircraft applications.

Hergenrother, Paul M.↗

Blends of an ethynyl terminated imidothioether with ethynyl terminated arylene ether oligomers

An evaluation has been undertaken of blends of a novel ethynyl-terminated imidothioether with Udel P1700 polysulfone and ethynyl-terminated arylene ether oligomers. Good to excellent processability was obtained with these blends using compression molding; the cured blends displayed poor-to-good resistance to chloroform and low-to-moderately high fracture toughness, depending on the blends' crosslink density. The flexural strength and modulus of unidirectional carbon graphite laminates prepared with the blended resins were good.

Connell, J. W.↗

On processing development for fabrication of fiber reinforced composite, part 2

Fiber-reinforced composite laminates are used in many aerospace and automobile applications. The magnitudes and durations of the cure temperature and the cure pressure applied during the curing process have significant consequences for the performance of the finished product. The objective of this study is to exploit the potential of applying the optimization technique to the cure cycle design. Using the compression molding of a filled polyester sheet molding compound (SMC) as an example, a unified Computer Aided Design (CAD) methodology, consisting of three uncoupled modules, (i.e., optimization, analysis and sensitivity calculations), is developed to systematically generate optimal cure cycle designs. Various optimization formulations for the cure cycle design are investigated. The uniformities in the distributions of the temperature and the degree with those resulting from conventional isothermal processing conditions with pre-warmed platens. Recommendations with regards to further research in the computerization of the cure cycle design are also addressed.

Hou, Tan-Hung↗

Process For Autoclaving HMW PMR-II Composites

Parts made of graphite-reinforced, high-molecular-weight (HMW) PMR-II polyimide easy to fabricate by autoclaving. Study showed autoclaved HMW PMR-II parts equal in quality to those made by compression molding. Well suited to use at temperatures up to 700 degrees F (371 degrees C). In aircraft engines, they offer advantages of strength and light weight.

Vannucci, Raymond D.↗

Low cost space power generation

The success of this study has given a method of fabricating durable copolymer films without size limitations. Previously, only compression molded samples were durable enough to generate electrical energy. The strengthened specimens are very long lived materials. The lifetime was enhanced at least a factor of 1,300 in full pyroelectric conversion cycle experiments compared with extruded, non-strengthened film. The new techniques proved so successful that the lifetime of the resultant copolymer samples was not fully characterized. The lifetime of these new materials is so long that accelerated tests were devised to probe their durability. After a total of more than 67 million high voltage electrical cycles at 100 C, the electrical properties of a copolymer sample remained stable. The test was terminated without any detectable degradation to allow for other experiments. One must be cautious in extrapolating to power cycle performance, but 67 million electrical cycles correspond to 2 years of pyroelectric cycling at 1 Hz. In another series of experiments at reduced temperature and electrical stress, a specimen survived over one-third of a billion electrical cycles during nearly three months of continuous testing. The radiation-limited lifetimes of the copolymer were shown to range from several years to millions of years for most earth orbits. Thus, the pyroelectric copolymer has become a strong candidate for serious consideration for future spacecraft power supplies.

Olsen, Randall B.↗