Characterization of Precipitation-Strengthening Heat-Resistant Austenitic Stainless Steels for Life-Prediction Modeling

In this study, the role of minor alloying additions in 347H stainless steels (UNS34709, ASTM A240/240M) on creep-rupture properties at 650-750°C and microstructure evolution during isothermal exposure at 750°C has been investigated, aiming to provide the experimental dataset as boundary conditions of physics-based modeling for material/component life prediction. Four different 347H heats containing various amounts of boron and nitrogen additions were prepared and evaluated. The combined additions of B and N are found to stabilize the strengthening secondary M23C6 carbides and retarding the transition from M23C6 to sigma phase precipitates during thermal exposure. The observed kinetics of microstructure evolution reasonably explains the improvement of creep-rupture properties of 347H stainless steels with the B and N additions.

Yamamoto, Yukinori↗

Grain refinement of a nickel and manganese free austenitic stainless steel produced by pressurized solution nitriding

Prolonged exposure at high temperatures during solution nitriding induces grain coarsening which deteriorates the mechanical properties of high nitrogen austenitic stainless steels. In this study, grain refinement of nickel and manganese free Fe–22.75Cr–2.42Mo–1.17N high nitrogen austenitic stainless steel plates was investigated via a two-stage heat treatment procedure. Initially, the coarse-grained austenitic stainless steel samples were subjected to an isothermal heating at 700 °C to be decomposed into the ferrite + Cr{sub 2}N eutectoid structure and then re-austenitized at 1200 °C followed by water quenching. Microstructure and hardness of samples were characterized using X-ray diffraction, optical and scanning electron microscopy, and micro-hardness testing. The results showed that the as-solution-nitrided steel decomposes non-uniformly to the colonies of ferrite and Cr{sub 2}N nitrides with strip like morphology after isothermal heat treatment at 700 °C. Additionally, the complete dissolution of the Cr{sub 2}N precipitates located in the sample edges during re-austenitizing requires longer times than 1 h. In order to avoid this problem an intermediate nitrogen homogenizing heat treatment cycle at 1200 °C for 10 h was applied before grain refinement process. As a result, the initial austenite was uniformly decomposed during the first stage, and a fine grained austenitic structure with average grain size of about 20 μm was successfully obtained by re-austenitizing for 10 min. - Highlights: • Successful grain refinement of Fe–22.75Cr–2.42Mo–1.17N steel by heat treatment • Using the γ → α + Cr{sub 2}N reaction for grain refinement of a Ni and Mn free HNASS • Obtaining a single phase austenitic structure with average grain size of ∼ 20 μm • Incomplete dissolution of Cr{sub 2}N during re-austenitizing at 1200 °C for long times • Reducing re-austenitizing time by homogenizing treatment before grain refinement.

36 MATERIALS SCIENCE↗

Study on the crystallographic orientation relationship and formation mechanism of reversed austenite in economical Cr12 super martensitic stainless steel

Effect of carbides and crystallographic orientation relationship on the formation mechanism of reversed austenite of economical Cr12 super martensitic stainless steel (SMSS) has been investigated mainly by transmission electron microscopy (TEM) and electron backscatter diffraction (EBSD). The results indicate that the M{sub 23}C{sub 6} precipitation and the formation of the reversed austenite have the interaction effect during tempering process in SMSS. The reversed austenite forms intensively at the sub-block boundary and the lath boundary within a misorientation range of 0–60°. M{sub 23}C{sub 6} has the same crystallographic orientation relationship with reversed austenite. There are two different kinds of formation modes for reversed austenite. One is a nondiffusional shear reversion; the other is a diffusion transformation. Both are strictly limited by crystallographic orientation relationship. The austenite variants are limited to two kinds within one packet and five kinds within one prior austenite grain. - Highlights: • Reversed austenite forms at martensite boundaries with misorientation of 0–60° • M{sub 23}C{sub 6} precipitation and reversed austenite formation have the interaction effect. • Two austenite variants with different orientations can be formed inside a packet. • Two reversed austenite formation modes: shear reversion; diffusion transformation.

36 MATERIALS SCIENCE↗

Effect of austenite grain size on acicular ferrite transformation in a HSLA steel

Highlights: • The fraction of acicular ferrite increases with reduced austenite grain sizes. • The reduction of austenite grain size refines and homogenises the microstructure. • There is a limit to increase the acicular ferrite fraction by reducing austenite size. • An equation relating effective grain sizes with processing parameters was proposed. - Abstract: Austenite grain size is well known to have a significant influence on various phase transformations in steels. Although the effects of many thermomechanical processing parameters on acicular ferrite (AF) transformation in HSLA steels have been investigated, little attention has been paid to the influence of austenite grain size. Therefore, in this research, different parameters of solid-solution heat treatment and rough deformation were adopted to generate austenite with different grain sizes and the effects of austenite grain size before deformation on the AF transformation and grain refinement were investigated. It was found that the reduction of prior-austenite grain size (PAGS) from 62.8 μm to 37.0 μm before austenite deformation promotes the AF transformation and simultaneously refines and homogenises the transformed microstructures. A reciprocally increased density of deformation induced dislocations with the reduction of PAGS was proposed to account for these results, which not only increase the nucleation sites of AF but also suppress the lengthening of BF laths. Further reducing PAGS from 37.0 μm to 22.3 μm, the fraction of AF is not increased and the transformed microstructure is not refined. Possible differences in the type, distribution, and density of austenite deformation substructures between austenite with PAGSs of 37.0 μm and 22.3 μm were argued to be responsible for the cease of grain refinement. The relationship between effective grain sizes and the S{sub v} parameter was investigated and an equation relating effective grain sizes with processing parameters was also proposed.

36 MATERIALS SCIENCE↗

Limiting Retained Austenite Decomposition in Quenched and Tempered Steels: Influences of Rapid Tempering and Silicon

Tempering reactions are critical to microstructure and property control in martensitic steels. Here, retained austenite decomposition and cementite precipitation are monitored using Mössbauer spectroscopy in 4340 and 300-M steel under conventional and rapid tempering conditions. Tempering times are compared at a constant tempered hardness by increasing tempering temperatures associated with short time conditions to achieve equivalent matrix softening to that of longer tempering times. Time-temperature combinations that provide equivalent tempered hardness generated microstructures with similar dislocation densities and cementite precipitation fractions; these mechanisms are controlled by self-diffusion. However, systematic differences in retained austenite content were observed at a given degree of softening, where shorter tempering times exhibited higher levels of retained austenite compared to more conventional conditions. At low temperatures, the differences in retained austenite preservation between explored time-temperature conditions are attributed to corresponding differences in carbon diffusion distance (in austenite), the controlling diffusional process of retained austenite decomposition. At higher temperatures, retained austenite decomposition exhibits C-curve kinetic behavior in 4340. Thus, reduced thermodynamic driving force for cementite and ferrite formation at higher temperature is believed to play a role in restricting retained austenite decomposition within some short-time, high temperature tempering regimes. The addition of silicon pushes cementite precipitation and retained austenite decomposition to higher temperatures, although retained austenite decomposition is suppressed to a greater extent than cementite precipitation. Potential is illustrated for coupling rapid tempering with silicon alloying to produce appreciably tempered martensite (~490 HV) with relatively less retained austenite decomposition compared to conventional tempering conditions.

36 MATERIALS SCIENCE↗

Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by austenitic filler metal

The evolution of microstructure and texture across an as-welded dissimilar UNS S32750 super duplex/UNS S30403 austenitic stainless steel joint welded by UNS S30986 (AWS A5.9 ER309LMo) austenitic stainless steel filler metal using gas tungsten arc welding process was evaluated by optical micrography and EBSD techniques. Due to their fabrication through rolling process, both parent metals had texture components resulted from deformation and recrystallization. The weld metal showed the highest amount of residual strain and had large austenite grain colonies of similar orientations with little amounts of skeletal ferrite, both oriented preferentially in the < 001 > direction with cub-on-cube orientation relationship. While the super duplex stainless steel's heat affected zone contained higher ferrite than its parent metal, an excessive grain growth was observed at the austenitic stainless steel's counterpart. At both heat affected zones, austenite underwent some recrystallization and formed twin boundaries which led to an increase in the fraction of high angle boundaries as compared with the respective base metals. These regions showed the least amount of residual strain and highest amount of recrystallized austenite grains. Due to the static recrystallization, the fraction of low degree of fit (Σ) coincident site lattice boundaries, especially Σ3 boundaries, was increased in the austenitic stainless steel heat affected zone, while the formation of subgrains in the ferrite phase increased the content of < 5° low angle boundaries at that of the super duplex stainless steel. - Graphical abstract: Display Omitted - Highlights: • Extensive grain growth in the HAZ of austenitic stainless steel was observed. • Intensification of < 100 > orientated grains was observed adjacent to both fusion lines. • Annealing twins with Σ3 CSL boundaries were formed in the austenite of both HAZ. • Cub-on-cube OR was observed between austenite and ferrite in the weld metal. • Weld metal had the lowest texture intensity and ratio of low angle and CSL boundaries.

36 MATERIALS SCIENCE↗

Effect of small addition of Cr on stability of retained austenite in high carbon steel

High carbon steels with dual phase structures of martensite and austenite have considerable potential for industrial application in high abrasion environments due to their hardness, strength and relatively low cost. To design cost effective high carbon steels with superior properties, it is crucial to identify the effect of Chromium (Cr) on the stability of retained austenite (RA) and to fully understand its effect on solid-state phase transition. This study addresses this important knowledge gap. Using standard compression tests on bulk material, quantitative X-ray diffraction analysis, nano-indentation on individual austenitic grains, transmission electron microscopy and electron backscatter diffraction–based orientation microscopy techniques, the authors investigated the effect of Cr on the microstructure, transformation behaviour and mechanical stability of retained austenite in high carbon steel, with varying Cr contents. The results revealed that increasing the Cr %, altered the morphology of the RA and increased its stability, consequently, increasing the critical pressure for martensitic transformation. This study has critically addressed the elastoplastic behaviour of retained austenite – and provides a deep understanding of the effect of small additions of Cr on the metastable austenite of high carbon steel from the macro- to nano-level. Consequently, it paves the way for new applications for high carbon low alloy steels. - Highlights: • Effect of small addition of Cr on metastable austenite of high carbon steel from the macro- to nano-level • A multi-scale study of elastoplastic behaviour of retained austenite in high carbon steel • The mechanical stability of retained austenite during plastic deformation increased with increasing Cr content • Effect of grain boundary misorientation angle on hardness of individual retained austenite grains in high carbon steel.

36 MATERIALS SCIENCE↗

In-situ determination of austenite and martensite formation in 13Cr6Ni2Mo supermartensitic stainless steel

In-situ analysis of the phase transformations in a 13Cr6Ni2Mo supermartensitic stainless steel (X2CrNiMoV13-5-2) was carried out using a thermo-magnetic technique, dilatometry and high temperature X-ray diffractometry (HT-XRD). A combination of the results obtained by the three applied techniques gives a valuable insight in the phase transformations during the austenitization treatment, including subsequent cooling, of the 13Cr6Ni2Mo supermartensitic stainless steel, where the magnetic technique offers a high accuracy in monitoring the austenite fraction. It was found by dilatometry that the austenite formation during heating takes place in two stages, most likely caused by partitioning of Ni into austenite. The in-situ evolution of the austenite fraction is monitored by high-temperature XRD and dilatometry. The progress of martensite formation during cooling was described with a Koistinen-Marburger relation for the results obtained from the magnetic and dilatometer experiments. Enhanced martensite formation at the sample surface was detected by X-ray diffraction, which is assumed to be due to relaxation of transformation stresses at the sample surface. Due to the high alloy content and high thermodynamic stability of austenite at room temperature, 4 vol.% of austenite was found to be stable at room temperature after the austenitization treatment. - Highlights: Black-Right-Pointing-Pointer We in-situ analyzed phase transformations and fractions of a 13Cr6Ni2Mo SMSS. Black-Right-Pointing-Pointer Higher accuracy of the austenite fraction was obtained from magnetic technique. Black-Right-Pointing-Pointer Austenite formation during heating takes place in two stages. Black-Right-Pointing-Pointer Enhanced martensite formation at the sample surface detected by X-ray diffraction.

36 MATERIALS SCIENCE↗

Ensuring combination of strength, ductility and toughness in medium-manganese steel through optimization of nano-scale metastable austenite

Highlights: • Medium-Mn steel was innovatively designed for medium to heavy steel plates. • Three intercritical annealing processes were adopted to ensure TRIP effect. • Austenite-martensite submicro-laminate structure was obtained after annealing. • The reversed austenite with different stability led to improved ductility. • TRIP effect induced by metastable austenite contributed excellent impact properties. - Abstract: Medium-Mn steel was innovatively designed in terms of alloying elements for medium to heavy steel plates to obtain combination of high strength, good ductility, and excellent low temperature toughness. Martensite was the dominant microstructure in the directly quenched steel plate because of high hardenability obtained by the addition of 5.6 wt% Mn. Three intercritical annealing processes were adopted to ensure transformation-induced-plasticity (TRIP) effect through optimization of the volume fraction, morphology, and C and Mn-enriched reversed austenite. On annealing, the dislocation density of martensite plate was decreased because of recovery and recrystallization, and metastable austenite film nucleated at the interface. Both thermal and mechanical stability of austenite decreased with increase in annealing temperature. The high yield strength of 840 MPa, good elongation after fracture of 24.3%, and excellent toughness at − 60 °C of 130.3 J was obtained at intermediate annealing temperature of 650 °C, and the volume fraction of reversed austenite at room temperature and − 80 °C was 22% and 17%, respectively. The reversed austenite exhibited different stability with increased tensile strain, leading to improved ductility and delayed necking. Moreover, the crack initiation energy and crack propagation energy were increased via dynamic stress partitioning and relaxation together with the transformation of metastable austenite. Thus, significant degree of TRIP effect induced by moderate stability of austenite played an important role in governing mechanical properties.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Compositional analysis on the reverted austenite and tempered martensite in a Ti-stabilized supermartensitic stainless steel: Segregation, partitioning and carbide precipitation

We present that controlling the amount of reverted austenite at room temperature allows for tailoring of mechanical properties in supermartensitic stainless steels. The austenite reversion and stabilization occurs during inter-critical tempering through partitioning of austenite-stabilizing elements. The degree of partitioning greatly depends on the reversion temperature, which dictates the local equilibrium conditions. Atom probe tomography and energy dispersive spectroscopy in transmission electron microscopy were used to study the austenite reversion mechanism in terms of the elemental distribution of austenite-stabilizing, ferrite-stabilizing and carbide forming elements. Synchrotron X-ray diffraction confirmed that the austenite equilibrium phase fraction was reached after 2.5 h of isothermal reversion at 625 °C, allowing for direct comparison with thermodynamic and kinetic calculations. However, such soaking time was not enough to produce compositional homogenization in the reverted austenite. The austenite reversion and stabilization mechanism was related mainly to strong partitioning of Ni. Negligible partitioning of Cr, Mo, Si and Ti were observed. Instead, these elements were strongly segregated at the reverted austenite/martensite interfaces. Carbon and Ti played a secondary role in the austenite stabilization through the precipitation of nano-sized Ti (C,N) with partial substitution of Ti by Mo. Finally, virtually carbon-free austenite and martensite were observed away from the interfaces and precipitates.

36 MATERIALS SCIENCE↗