Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “adhesives”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Thermal Characterization of Adhesive

The current Space Shuttle Reusable Solid Rocket Motor (RSRM) nozzle adhesive bond system is being replaced due to obsolescence. Down-selection and performance testing of the structural adhesives resulted in the selection of two candidate replacement adhesives, Resin Technology Group's Tiga 321 and 3M's EC2615XLW. This paper describes rocket motor testing of these two adhesives. Four forty-pound charge motors were fabricated in configurations that would allow side by side comparison testing of the candidate replacement adhesives and the current RSRM adhesives. The motors provided an environment where the thermal performance of adhesives in flame surface bondlines was compared. Results of the FPC testing show that: 1) The phenolic char depths on radial bond lines is approximately the same and vary depending on the position in the blast tube regardless of which adhesive was used; 2) The adhesive char depth of the candidate replacement adhesives is less than the char depth of the current adhesives; 3) The heat-affected depth of the candidate replacement adhesives is less than the heat-affected depth of the current adhesives; and 4) The ablation rates for both replacement adhesives are slower than that of the current adhesives.

Spomer, Ken A.↗

Thermal Characterization of Epoxy Adhesive by Hotfire Testing

This paper describes subscale solid-rocket motor hot-fire testing of epoxy adhesives in flame surface bondlines to evaluate heat-affected depth, char depth and ablation rate. Hot-fire testing is part of an adhesive down-selection program on the Space Shuttle Solid Rocket Motor Nozzle to provide additional confidence in the down-selected adhesives. The current nozzle structural adhesive bond system is being replaced due to obsolescence. Prior to hot-fire testing, adhesives were tested for chemical, physical and mechanical properties, which resulted in the selection of two potential replacement adhesives, Resin Technology Group's TIGA 321 and 3M's EC2615XLW. Hot-fire testing consisted of four forty-pound charge (FPC) motors fabricated in configurations that would allow side-by-side comparison testing of the candidate replacement adhesives with the current RSRM adhesives. Results of the FPC motor testing show that: 1) the phenolic char depths on radial bondlines is approximately the same and vary depending on the position in the blast tube regardless of which adhesive was used, 2) the replacement candidate adhesive char depths are equivalent to the char depths of the current adhesives, 3) the heat-affected depths of the candidate and current adhesives are equivalent, and 4) the ablation rates for both replacement adhesives were equivalent to the current adhesives.

Spomer, Ken A.↗

Chemically Recyclable and Tunable Polyolefin-Like Multiblock Copolymer Adhesives

Adhesives are important in creating multilayer products, such as in packaging and construction. Most current hot-melt adhesives such as poly(ethylene-co-vinyl acetate) (EVA) and polyurethanes lack chemical recyclability and do not easily de-bond, complicating recycling. Here, we achieved tunable adhesive properties of chemically recyclable polyolefin-like multiblock copolymers through regulating the incorporation of crystalline hard blocks, amorphous soft blocks, and ester content highlighted by adhesive strengths up to 6.80 MPa. We further demonstrated applications of these adhesives in multi-layer films and showed that the adhesives can be readily de-bonded, recovered, and chemically recycled. Overall, this study into structure-property relationships, including effects of crystallinity, soft-block incorporation, and ester content of the multiblock copolymers on adhesive properties, has resulted in a modular hot-melt adhesive platform that exhibits chemical recyclability for virgin-quality adhesive re-generation, reprocessability for repeated reuse of the recovered adhesive, and tunability for designing adhesives with a wide range of low to high (up to ~80% stronger than EVA) adhesion strengths.

36 MATERIALS SCIENCE↗

Cohesive and adhesive degradation in PET-based photovoltaic backsheets subjected to ultraviolet accelerated weathering

Delamination between layers in photovoltaic (PV) backsheets is often reported in the literature, causing voids that can collect moisture, diminish module backside heat dissipation, and reduce the backsheet’s effectiveness as a physical barrier. While backsheets with weathering-resistant fluoropolymer outer layers have traditionally been used in modules, more recent backsheets using non-fluoropolymer outer layers, such as polyethylene terephthalate (PET), have been developed. These backsheets have shown signs of premature degradation, and their adhesion degradation, in particular, has not been widely studied. In the present work, the single cantilever beam (SCB) adhesion test was used to quantify the adhesion energy in two commercially available PET-based backsheets. To study the effect of minor changes in formulation, the backsheets were obtained from same manufacturer and product line but during different years. To study the effect of environmental variables on adhesion degradation, the backsheets were subjected to artificial weathering at controlled temperature, humidity, and ultraviolet (UV) radiation in an indoor weathering chamber, and the adhesion energy was quantified at several intervals of exposure time. Layering structure, composition, and adhesion failure mode were compared between the backsheets, using Raman and infrared spectroscopy and thermogravimetric analysis. The results show a large difference in initial (unexposed) adhesion energy between the backsheets, despite very similar structures and compositions. Following exposure, adhesion energy dropped significantly, primarily due to thermo-hydrolytic degradation of the polyurethane (PU)-based adhesive layers. Significant UV-induced adhesion degradation of the PET outer layer surface was also observed. The study represents an important step in understanding adhesion degradation in PET-based backsheets, suggesting ways in which adhesion integrity – and, correspondingly, module service life – can be improved.

14 SOLAR ENERGY↗

An Ultrasonic Technique to Determine the Residual Strength of Adhesive Bonds

In this work, ultrasonic techniques to nondestructively evaluate adhesive bond degradation have been studied. The key to the present approach is the introduction of an external factor which pulls the adhesive bond in the nonlinear range, simultaneously with the application of an ultrasonic technique. With the aid of an external static tensile loading, a superimposed longitudinal wave has.been used to obtain the slopes of the stress-strain curve of an adhesive bond at a series of load levels. The critical load, at which a reduction of the slope is detected by the superimposed longitudinal wave, is an indication of the onset of nonlinear behavior of the adhesive bond, and therefore of bond degradation. This approach has been applied to the detection of adhesive bond degradation induced by cyclic fatigue loading. Analogously to the longitudinal wave case, a superimposed shear wave has been used to obtain the effective shear modulus of adhesive layers at different shear load levels. The onset of the nonlinear behavior of an adhesive bond under shear loading has been detected by the use of a superimposed shear wave. Experiments show that a longitudinal wave can also detect the nonlinear behavior when an adhesive bond is subjected to shear loading. An optimal combination of ultrasonic testing and mechanical loading methods for the detection of degradation related nonlinear behavior of adhesive bonds has been discussed. For the purpose of a practical application, an ultrasonic technique that uses a temperature increase as an alternative to static loading has also been investigated. A general strain-temperature correspondence principle that relates a mechanical strain to a temperature has been presented. Explicit strain-temperature correspondence relations for both the tension and shear cases have been derived. An important parameter which quantifies the relation between the wave velocity and temperature has been defined. This parameter, which is indicative of adhesive bond nonlinearity and which can be conveniently obtained by an ultrasonic measurement, has been used as an indication of adhesive bond degradation. Experimental results have shown that the temperature increase method is a convenient and productive alternative to static loading. A technique which uses the reflected waveform data to obtain the fundamental ultrasonic parameters (transit time, reflection coefficient and attenuation coefficient) of an adhesive bond has also been presented.

Achenbach, J. D.↗

Adhesion Capabilities of Permanent Foaming Fixatives

DOE-EM have identified an operational requirement for a fixative that can immobilize and/or encapsulate residual contamination in 3D void volumes (pipes, gloveboxes, waste containers, etc.) during D and D activities. Failure to safely and effectively immobilize residual contamination can: Put workers at risk; Contaminate the public and environment; Drive up costs. Commercial-off-the-shelf (COTS) polyurethane (PU) foams is one possible solution and is currently being investigated by Savannah River National Lab (SRNL). Adhesion testing will dictate how well PU foams will adhere and immobilize residual contamination onto a substrate. Results can provide a performance criteria for Section 5 of ASTM E3191: Standard Specification for Permanent Foaming Fixatives Used to Mitigate Spread of Radioactive Contamination. Initial mechanical testing showed intumescent rigid PU foams were best in class (tensile, compression, TGA/DSC) Application of intumescent rigid PU foam in pipe scenario with 'contamination' showed excellent adhesion capabilities as long as foam had contact with pipe. The foam, however, was not able to penetrate 'contamination' but created pockets where the contamination interacted with the substrate. Pretreatment options of pipe were considered to produce better immobilization capabilities. Pretreatment options included COTS products like baking spray, rubber cement, and soap. Foam was still able to immobilize on a global sense, but not a local sense. Essentially acted as a mechanical plug. A tensile tester (MTS Criterion Series 43) was utilized to evaluate the tensile adhesion strength of 6 COTS PU foams. ASTM D1623: Tensile and Tensile Adhesion Properties of Rigid Cellular Plastics. Procedures: PU foams were cured between two smooth 2'' x 2'' 304 stainless steel coupons with hinges glued on plates for gripping support. Parameters Used: Pull rate of 0.1 in/min. Calculations: Tensile adhesion strength, elongation, and ImageJ analysis of how PU foam is left on substrate. Outcome: The PU foam with the best adhesion capabilities would be downselected for further evaluation to be used as a permanent foaming fixative. The rigid PU foams had the best adhesion capabilities with the R1 foam having a max load of 236 N. One of the I-R2 samples reached almost 450 N and another sample reached 2500 N before slipping. The other intumescent foam, I-F4, had the most coverage on the stainless steel coupon's surface from the ImageJ results (61.43% surface coverage). The intumescent foam, I-R2, will be the foam of choice for future testing due its fire retardant and adhesion capabilities. Future directions: Conduct the following experiment in a pipe scenario with the down-selected PU foam. Procedures: PU foam will be cured between in a 304 stainless steel pipe (ID: 4'', OD: 4.5'', Height: 4''). Parameters Used: Compression testing results will be referenced to determine if foam's adhesion strength would be greater its compression strength as its being compressed. Calculations: Compression strength, shear stress, total time elapsed. Conduct further adhesion testing with the down-selected PU foam (I-R2) to be treated as a permanent foaming fixative (PFF). Determine the minimum contact the PFF should have with the substrate for adequate results. Evaluate if PFF's adhesion capabilities is time dependent (3.1.5 of ASTM E3911). Subject PFF to seismic stressors addressed in Safety Basis of Interim Operation documents (SBIO) to further evaluate adhesion capabilities.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of a composite flame retardant system on the flame retardancy and mechanical performance of epoxy resin adhesive

Abstract A flame‐retarded epoxy resin (ER) adhesive with strong flame retardancy and adhesion performance was prepared. The coated ammonium polyphosphate (MFAPP), melamine (MEL), and organic montmorillonite (OMMT) were mixed to prepare a composite flame retardant. It was subsequently blended with a toughened ER thoroughly and then the mixture was cured with polyamide. The resultant ER adhesive thermosets achieved UL‐94 V‐0 rating during vertical burning test, and the limiting oxygen index value was as high as 31.6%. The shear strength of the ER adhesive was 27.9 MPa when 25 wt% MFAPP/MEL/OMMT was introduced. Compared with the pure adhesive, the flame retardant epoxy adhesive maintained outstanding adhesion performance because of the good compatibility between the composite flame retardant additives and the toughened ER adhesive. Cone calorimetry tests indicated that the release of heat and smoke were obviously declined with the incorporation of the composite flame retardant system in comparison to pure ER adhesive thermoset. The investigation of flame retardant mechanism revealed that the composite MFAPP/MEL/OMMT flame retardant system stimulated the generation of highly expanded, integral, and strong char layer and the formed char layer exerted superior insulation effect during combusiton. The present work provided an alternative approach to prepare flame retardant ER adhesive with the similar excellent adhesive performance.

Li, Sheng↗

Nonlinear adhesive behavior effects in a cracked orthotropic sheet stiffened by a semi-infinite orthotropic sheet

The stress-intensity factors are determined for a cracked orthotropic sheet adhesively bonded to an orthotropic stringer where the adhesive layer is modeled with a nonlinear stress-strain curve. By the use of Green's functions and the complex variable theory of orthotropic elasticity, a set of integral equations is obtained. The integral equations are replaced by an equivalent set of algebraic equations, which are solved to obtain the shear stress distribution in the adhesive layer, with which the crack-tip stress-intensity factors are found. When the adhesive was modeled with a nonlinear stress-strain curve, the peak shear stresses in the adhesive were considerably reduced in comparison to the solution for the linear elastic adhesive. This resulted in increases in the stress-intensity factors for the nonlinear adhesive solution compared to the linear adhesive solution. The nonlinear adhesive has no significant effect on the stress-intensity factor unless the near crack tip is beneath the stringer. It is assumed that the adhesive bond remains intact and it is predicted that onset of adhesive failure occurs at decreasing levels of applied stress as the crack propagates beneath the stringer.

Bigelow, C. A.↗

Nonlinear adhesive behavior effects in a cracked orthotropic sheet stiffened by a semi-infinite orthotropic sheet

The stress-intensity factors are determined for a cracked orthotropic sheet adhesively bonded to an orthotropic stringer where the adhesive layer is modeled with a nonlinear stress-strain curve. By the use of Green's functions and the complex variable theory of orthotropic elasticity, a set of integral equations is obtained. The integral equations are replaced by an equivalent set of algebraic equations, which are solved to obtain the shear stress distribution in the adhesive layer, with which the crack-tip stress-intensity factors are found. When the adhesive was modeled with a nonlinear stress-strain curve, the peak shear stresses in the adhesive were considerably reduced in comparison to the solution for the linear elastic adhesive. This resulted in increases in the stress-intensity factors for the nonlinear adhesive solution compared to the linear adhesive solution. The nonlinear adhesive has no significant effect on the stress-intensity factor unless the near crack tip is beneath the stringer. It is assumed that the adhesive bond remains intact and it is predicted that onset of adhesive failure occurs at decreasing levels of applied stress as the crack propagates beneath the stringer.

Bigelow, C. A.↗

Structure, Function, and Application of Self–Healing Adhesives from Mistletoe Viscin

Berries from the European Mistletoe (Viscum album) possess a sticky tissue called viscin that facilitates adhesion and germination onto host trees. Recent studies of viscin have demonstrated its adhesive capacity on a range of natural and synthetic surfaces including wood, skin, metals, and plastic. Yet, the underlying mechanisms remain poorly understood. Here, an investigation of the adhesive performance of mistletoe viscin is performed, demonstrating its hygroscopic nature and ability to self-heal following adhesive failure. It is identified that adhesion originates from a water-soluble adhesive component that can be extracted, isolated, and characterized independently. Lap shear mechanical testing indicates that the mistletoe adhesive extract (MAE) outperforms native viscin tissue, as well as gum arabic and arabinogalactan—common plant-based adhesives. Furthermore, humidity uptake experiments reveal that MAE can reversibly absorb nearly 100% of its mass in water from the atmosphere. In-depth spectroscopic and mass spectrometry investigations reveal a composition consisting primarily of an atypical arabinogalactan, with additional sugar alcohols. Finally, several proof-of-concept applications are demonstrated using MAE for hygro-responsive reversible adhesion between various surfaces including skin, plastic, PDMS, and paper, revealing that MAE holds potential as a biorenewable and reusable adhesive for applications in cosmetics, packaging, and potentially, tissue engineering.

36 MATERIALS SCIENCE↗

Small-scale roughness entraps water and controls underwater adhesion

While controlling underwater adhesion is critical for designing biological adhesives and in improving the traction of tires, haptics, or adhesives for health monitoring devices, it is hindered by a lack of fundamental understanding of how the presence of trapped water impedes interfacial bonding. Here, by using well-characterized polycrystal diamond surfaces and soft, nonhysteretic, low–surface energy elastomers, we show a reduction in adhesion during approach and four times higher adhesion during retraction as compared to the thermodynamic work of adhesion. Our findings reveal how the loading phase of contact is governed by the entrapment of water by ultrasmall (10-nanometer-scale) surface features. In contrast, the same nanofeatures that reduce adhesion during approach serve to increase adhesion during separation. The explanation for this counterintuitive result lies in the incompressibility-inextensibility of trapped water and the work needed to deform the polymer around water pockets. Unlike the well-known viscoelastic contribution to adhesion, this science unlocks strategies for tailoring surface topography to enhance underwater adhesion.

59 BASIC BIOLOGICAL SCIENCES↗

Shuttle active thermal control system development testing. Volume 7: Improved radiator coating adhesive tests

Silver/Teflon thermal control coatings have been tested on a modular radiator system projected for use on the space shuttle. Seven candidate adhesives have been evaluated in a thermal vacuum test on radiator panels similar to the anticipated flight hardware configuration. Several classes of adhesives based on polyester, silicone, and urethane resin systems were tested. These included contact adhesives, heat cured adhesives, heat and pressure cured adhesives, pressure sensitive adhesives, and two part paint on or spray on adhesives. The coatings attached with four of the adhesives, two silicones and two urethanes, had no changes develop during the thermal vacuum test. The two silicone adhesives, both of which were applied to the silver/Teflon as transfer laminates to form a tape, offered the most promise based on application process and thermal performance. Each of the successful silicone adhesives required a heat and pressure cure to adhere during the cryogenic temperature excursion of the thermal-vacuum test.

Reed, M. W.↗

Design guidelines for hybrid microcircuits; organic adhesives for hybrid microcircuits

The properties of organic adhesives were studied to acquire an adequate information base to generate a guideline document for the selection of adhesives for use in high reliability hybrid microcircuits. Specific areas covered include: (1) alternate methods for determining the outgassing of cured adhesives; (2) effects of long term aging at 150C on the electrical properties of conductive adhesives; (3) effects of shelf life age on adhesive characteristics; (4) bond strengths of electrically conductive adhesives on thick film gold metallization, (5) a copper filled adhesive; (6) effects of products outgassed from cured adhesives on device electrical parameters; (7) metal migration from electrically conductive adhesives; and (8) ionic content of electrically insulative adhesives. The tests performed during these investigations are described, and the results obtained are discussed in detail.

Perkins, K. L.↗

Investigation of organic adhesives for hybrid microcircuits

The properties of organic adhesives were investigated to acquire information for a guideline document regarding the selection of adhesives for use in high reliability hybrid microcircuits. Specifically, investigations were made of (1) alternate methods for determining the outgassing of cured adhesives, (2) effects of long term aging at 150 C on the electrical properties of conductive adhesives, (3) effects of shelf life age on adhesive characteristics, (4) bond strengths of electrically conductive adhesives on thick film gold metallization, (5) a copper filled adhesive, (6) effects of products outgassed from cured adhesives on device electrical parameters, (7) metal migration from electrically conductive adhesives, and (8) ionic content of electrically insulative adhesives. The tests performed during these investigations are described, and the results obtained are discussed.

Perkins, K. L.↗

Effect of adhesive debond on stress-intensity factors in bonded composite panels

Stress-intensity factors are calculated for a cracked infinite sheet adhesively bonded to a stringer, and debonding of the adhesive layer is predicted. The stringer is modeled as a semiinfinite sheet. Adhesive nonlinearity is also included. Both the sheet and stringer are treated as homogeneous, orthotropic materials, a set of integral equations is formulated and solved to obtain the adhesive shear stresses and crack-tip stress-intensity factors. Adhesive debonding is predicted using a rupture criterion based on the combined adhesive stresses. A through-the-thickness crack is located in the infinite sheet perpendicular to the edge of the stringer. When the crack is not under the stringer, the debond extends along the edge of the stringer. When the crack tip is beneath the stringer, the debond extends to the crack tip, then along the edge of the stringer. Stress levels required for debond initiation decrease as the crack tip is moved beneath the stringer. With a nonlinear adhesive, the debond initiates at higher applied stress levels than in linear adhesive cases. Compared with the linear adhesive solution, modeling a nonlinear adhesive causes the stress-intensity factor to decrease when debonding is included.

Bigelow, C. A.↗

Structural Evaluation of the RSRM Nozzle Replacement Adhesive

This paper describes the structural performance evaluation of a replacement adhesive for the Reusable Solid Rocket Motor (RSRM) nozzle utilizing finite element analysis. Due to material obsolescence and industrial safety issues, the two current structural adhesives, EA 913 and EA 946 are to be replaced with a new adhesive. TIGA 321. The structural evaluation in support of the adhesive replacement effort includes residual stress, transportation, and flight analyses. Factors of safety are calculated using the stress response from each analysis. The factors of safety are used as the limiting criteria to compare the replacement adhesive against the current adhesives. Included in this paper are the analytical approach, assumptions and modeling techniques as well as the results of the evaluation. An important factor to the evaluation is the similarity in constitutive material properties (elastic modulus and Poisson's ratio) between TIGA 321 and EA 913. This similarity leads to equivalent material response from the two adhesives. However, TIGA 321 surpasses EA 913's performance due to higher material capabilities. Conversely, the change in stress response from EA 946 to TIGA 321 is more apparent: this is primarily attributed to the difference in the modulii of the two adhesives, which differ by two orders of magnitude. The results of the bondline evaluation indicate that the replacement adhesive provides superior performance than the current adhesives with only minor exceptions. Furthermore, TIGA 321 causes only a minor chance in the response of the phenolic and metal components.

Batista-Rodriguez, A.↗

Sources of Uncertainty in Ultrasonic Phase-Based Assessment of Interfacial Stiffness in Adhesive Joints

Quantitative nondestructive evaluation (NDE) of adhesive joint strength is critical for certifying fastener-free bonded aerospace structures. Unfortunately, available adhesive NDE approaches are only suitable for detecting gross defects and delamination and cannot reliably detect variations in strength in intact bonds. Intact (i.e., nominally defect free) bonds are challenging to inspect because they, by definition, contain no macroscopic defects that would produce a strong NDE signature. Even in the absence of obvious defects, however, bond strength can vary substantially due to factors such as contamination, variations in the adhesive cure processes, and environmental exposure. For ultrasonic bond inspections, the effect of interactions from an imperfect adhesive interface are subtle and may include changes in the frequency content or phase of the ultrasonic signal. The bond condition can be deduced from these subtle changes in the acoustic response using an accompanying physics-based model of adhesive joint interaction. For example, researchers have used the spring network adhesion model of Baik and Thompson [1] to determine the interfacial stiffness of the joint from its ultrasonic response (e.g., [2]). This interfacial stiffness metric describes the bonds resistance to separation between the adhesive and adherent and has shown a strong correlation with joint strength. In this study, interfacial stiffness is assessed using the ultrasonic phase change associated with bond interaction in varying bond conditions. The phase change is measured precisely using a phase-locked-loop instrument over a swept range of frequencies. The phase transition at resonance, where the bond thickness is half the acoustic wavelength, produces a unique signature with which to fit a physics-based model. Interfacial stiffness is determined by minimizing the difference between the theoretical and experimental phase response. Experimental results are presented for glass specimens bonded with aerospace adhesives and a sensitivity analysis is performed to examine the effects of parameters that may be uncertain in the industrial inspection environment – namely bond thickness, adhesive and adherent properties, and porosity. The results are a first step toward an uncertainty quantified version of the measurement technique, show correlation between interfacial stiffness and bond strength, and are another key step toward maturing this approach for use in complex materials and joint geometries. [1] Baik, J.M. and Thompson, R.B., 1984. “Ultrasonic scattering from imperfect interfaces: a quasi-static model”. Journal of Nondestructive Evaluation, 4. [2] Haldren, H.A., Perey, D.F., Yost, W.T., Cramer, K.E., and Gupta, M.C., 2019. “Swept-frequency ultrasonic phase evaluation of adhesive bonding in tri-layer structures”. Journal of the Acoustical Society of America, 145.

Matt Webster↗

Autonomous Self-Healing Elastomers with Unprecedented Adhesion Force

Self-healable elastomers are extremely attractive due to their ability to prolong product lifetime. An additional function that could further expand their applications is strong adhesion force to clean and dusty surfaces. This study reports a series of autonomous self-healable and highly adhesive elastomers (ASHA-Elastomer) that are fabricated via a simple, efficient, and scalable process. The obtained elastomers exhibit outstanding mechanical properties with elongation at break up to 2102% and toughness (modulus of toughness) of 1.73 MJ m -3 . The damaged ASHA-Elastomer can autonomously self-heal with full recovery of functionalities, and the healing process is not affected by the presence of water. The elastomers are found to possess an ultrahigh adhesion force up to 3488 N m -1 , greatly outperforming previously reported self-healing adhesive elastomers. Furthermore, the adhesion force of the ASHA-Elastomer is negligibly affected by dust on the surface, in stark contrast with regular adhesive polymers that have adhesion strengths extremely sensitive to dust. The successful development of high-toughness, autonomous self-healable, and ultra-adhesive elastomers will enable a wide range of applications with enhanced longevity and versatility, including their use in sealants, adhesives, and stretchable devices.

36 MATERIALS SCIENCE↗