Engineering PapersSearch

SEARCH · Engineering Papers

Results for “THERMOCOUPLE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

High temperature, oxidation resistant noble metal-Al alloy thermocouple

A thermocouple is disclosed. The thermocouple is comprised of an electropositive leg formed of a noble metal-Al alloy and an electronegative leg electrically joined to form a thermocouple junction. The thermocouple provides for accurate and reproducible measurement of high temperatures (600 - 1300 C) in inert, oxidizing or reducing environments, gases, or vacuum. Furthermore, the thermocouple circumvents the need for expensive, strategic precious metals such as rhodium as a constituent component. Selective oxidation of rhodium is also thereby precluded.

Smialek, James L.

Cobra Probes Containing Replaceable Thermocouples

A modification of the basic design of cobra probes provides for relatively easy replacement of broken thermocouples. Cobra probes are standard tube-type pressure probes that may also contain thermocouples and that are routinely used in wind tunnels and aeronautical hardware. They are so named because in side views, they resemble a cobra poised to attack. Heretofore, there has been no easy way to replace a broken thermocouple in a cobra probe: instead, it has been necessary to break the probe apart and then rebuild it, typically at a cost between $2,000 and $4,000 (2004 prices). The modified design makes it possible to replace the thermocouple, in minimal time and at relatively low cost, by inserting new thermocouple wire in a tube.

Jones, John

Smoothed thermocouple tables of extended significance, volume 1

Although thermocouple calibration tables of emf (mv abs) vs temperature usually have enough significant digits for many purposes, the rounding errors often limit the use of these tables (and hence thermocouples) for precise measurements of temperature related effects such as thermal conductivity or specific heat. Fourteen calibration tables for common thermocouples from NBS Circular 561 and for cryogenic thermocouples from NBS Report 9712 were smoothed, and these are given in vol. 2 of this report. In this volume (vol.1), a general discussion of data smoothing techniques and a description of the procedures by which the smoothed tables were prepared are given.

Thermocouples

Design and Operation of a Fast, Thin-Film Thermocouple Probe on a Turbine Engine

As a demonstration of technology maturation, a thin-film temperature sensor probe was fabricated and installed on a F117 turbofan engine via a borescope access port to monitor the temperature experienced in the bleed air passage of the compressor area during an engine checkout test run. To withstand the harsh conditions experienced in this environment, the sensor probe was built from high temperature materials. The thin-film thermocouple sensing elements were deposited by physical vapor deposition using pure metal elements, thus avoiding the inconsistencies of sputter-depositing particular percentages of materials to form standardized alloys commonly found in thermocouples. The sensor probe and assembly were subjected to a strict protocol of multi-axis vibrational testing as well as elevated temperature pressure testing to be qualified for this application. The thin-film thermocouple probe demonstrated a faster response than a traditional embedded thermocouple during the engine checkout run.

thermocouples

High temperature thermocouple development program, part A and part B

The problem of extending the useful life of thermocouples intended for in-core and out-of-core thermionic applications in a vacuum environment at temperatures up to 2273 K for periods of time up to 10,000 hours was investigated. Many factors that may influence this useful life were examined, and a basic probe design was developed. With a few modifications, twenty-three thermocouple assemblies were fabricated. Generally the finished thermocouple consisted of solid doped W-3% Re and W-25% Re wires and high purity and high density BeO insulators, and was sheathed in a high purity tantalum tube. In a few probes, stranded thermocouple wires were substituted; commercial grade BeO was used; and in two cases, CVD W-22% Re tubing was used. Each of the components was made of the highest purity materials available; was subjected to special cleaning steps, and was assembled in a class 10,000 clean room. Pertinent physical and chemical properties were determined on each of the components. Special processing techniques were used in the fabrication of the high purity (99.95%), high density (over 95% of theoretical) BeO.

Toenshoff, D. A.

Studies of noble-metal thermocouple stability at high temperatures

Two investigatory studies on performance characteristics of noble-metal thermocouples are described. (1) thermoelectric stability as affected by preferential oxidation of iridium in the system iridium-40% rhodium versus iridium, and (2) the effects of temperature gradients on the emf stability of the systems platinum-13% rhodium versus platinum and iridium-40% rhodium versus iridium, operating in air. The stability investigation was carried out at three temperatures - 1700, 1850, and 2000 C - by comparing the output of the test thermocouple in air with the output of an identically constructed reference thermocouple in nitrogen. The results show that no calibration shift was observed producing a change in output greater than that corresponding to a 2.0% change in the indicated temperature for all samples tested. The investigation of gradient effects was carried out by subjecting test thermocouples to both severe and mild gradients for periods up to 200 hours. For the platinum system, the operating temperature was 1500 C with gradients of 1475 and 700 C/cm; for the iridium system, 2000 C with gradients of 700, 1500, and 1975 C/cm. Exposure to temperature gradients was found to introduce significant changes in calibration for both systems. In both investigations, the thermoelements were examined by means of electron-probe analysis and by metallographic methods to detect chemical and structural changes. Data and micrographs are presented.

Freeze, P.

Thermocouple time constant measurement by cross power spectra

A method of measuring thermocouple time constants is outlined which requires Fourier signal processing. In this method, two thermocouples of differing time constants are placed in a gas flow as closely as possible to one another, and the time constant of the first thermocouple is determined directly from the extremum of the imaginary part of the ratio of the ensemble averaged cross-power spectrum to the ensemble averaged auto-power spectrum of that thermocouple. A coherence function is given for assuring the quality of the data, and results are presented for an experimental test of the method. Some problems with the method are briefly noted.

Strahle, W. C.

Thermocouples measure very-hot gas temperatures

Thermocouple probe incorporates small jet of inert gas to cool thermocouple. To measure gas temperatures, cooling jet is turned off momentarily, allowing thermocouple to heat up to near its melting point, then cooling is reapplied. Heating curve is recorded by high speed digital system. Computing system extrapolates final temperature thermocouple would have attained.

Glawe, G. E.

Evaluation of miniature single-wire sheathed thermocouples for turbine blade temperature measurement

Chromel Alumel thermocouples were used, with sheath diameters of 0.15 and 0.25 mm. Tests were conducted at temperatures ranging from 750 to 1250 K. Both steady state and thermal cycling tests were performed for times up to 200 hours. Initial testing was performed in a low velocity gas stream for long time periods using a Meker-type burner. Additional testing was done in a high velocity gas stream for short time periods using a hot gas tunnel and also in a J75 jet engine. A total of eleven 0.15 mm diameter thermocouples and six 0.25 mm diameter thermocouples were tested. Drift rates up to 2.5% in 10 hours were observed. Photomicrographs show that this design is near the limit of miniaturization based on present manufacturing capabilities. Results indicate that the effects of miniaturization on reliability and accuracy must be considered when choosing thermocouples for a particular application.

Hollanda, R.

Adhesive-Bonded Tab Attaches Thermocouples to Titanium

Mechanical strength of titanium-alloy structures that support thermocouples is preserved by first spotwelding thermocouples to titanium tabs and then attaching tabs to titanium with a thermosetting adhesive. In contrast to spot welding, a technique previously used for thermocouples, fatigue strength of the titanium is unaffected by adhesive bonding. Technique is also gentler than soldering or attaching thermocouples with a tap screw.

Cook, C. F.

Frequency response in short thermocouple wires

Theoretical expressions are derived for the steady state frequency response of a thermocouple wire. In particular, the effects of axial heat conduction are demonstrated for a nonuniform wire with unequal material properties and wire diameters across the junction. The amplitude ratio at low frequency omega approaches 0 agrees with the results of Scadron and Warshawsky (1952) for a steady state temperature distribution. Moreover, the frequency response for a nonuniform wire in the limit of infinite length l approaches infinity is shown to reduce to a simple expression that is analogous to the classic first order solution for a thermocouple wire with uniform properties. Theoretical expressions are also derived for the steady state frequency response of a supported thermocouple wire. In particular, the effects of axial heat conduction are demonstrated for both a supported one material wire and a two material wire with unequal material properties across the junction. For the case of a one material supported wire, an exact solution is derived which compares favorably with an approximate expression that only matches temperatures at the support junction. Moreover, for the case of a two material supported wire, an analytical expression is derived that closely correlates numerical results. Experimental measurements are made for the steady state frequency response of a supported thermocouple wire. In particular, the effects of axial heat conduction are demonstrated for both a supported one material wire (type K) and a two material wire (type T) with unequal material properties across the junction. The data for the amplitude ratio and phase angle are correlated to within 10 pct. with the theoretical predictions of Forney and Fralick (1991). This is accomplished by choosing a natural frequency omega sub n for the wire data to correlate the first order response at large gas temperature frequencies. It is found that a large bead size, however, will increase the amplitude ratio at low frequencies but decrease the natural frequency of the wire. The phase angle data are also distorted for imperfect junctions.

Forney, L. J.

A computer-controlled apparatus for Seebeck inhomogeneity testing of sheathed thermocouples

Mineral-insulated metal-sheathed (MIMS) thermocouple assemblies are used throughout industry and research facilities as a method of temperature measurement where requirements for either harsh environmental conditions exist, or where rigidity of the measurement probe is required. Seebeck inhomogeneity is the abnormal variation of the Seebeck coefficient from point to point in a material. It is not disclosed in conventional calibration. A standardized method of measuring thermoelectric inhomogeneity along the thermocouple probe length is not available. Therefore, calibration for sheathed probes normally does not include testing of probe inhomogeneity. The measurement accuracy would be severely impacted if significant inhomogeneity and a temperature gradient were present in the same region of the probe. A computer-controlled system for determining inhomogeneities was designed, fabricated, and tested. This system provides an accurate method for the identification of the location of inhomogeneity along the length of a sheathed thermocouple and for the quantification of the inhomogeneity. This paper will discuss the apparatus and procedure used to perform these tests and will present data showing tests performed on sheathed thermocouple probes.

Burkett, Cecil G., Jr.

High-Temperature, Oxidation-Resistant Thermocouples

Aluminum substituted for rhodium, which is scarce and expensive. Electromotive force increases with aluminum content in Pt/Al leg of Pt(Pt/Al) thermocouple. Wires baked longer in aluminizing bed produce larger voltages. Thermocouples containing platinum/aluminum legs used instead of thermocouples of type R in furnaces, heat engines, and chemical reactors. Expecially suited to high-velocity oxidizing environments. Constructed as thin-film sensors on turbine blades and vanes, where pre-oxidation provides insulating film needed between thermocouple legs. Because aluminum content slowly depleted by oxidation, long-term use recommended only where maximum temperature is 1,200 degrees C or less.

Smialek, James L.

Three-Wire Thermocouple: Frequency Response in Constant Flow

Theory and experimental measurements are compared with a novel three-wire thermocouple. Signals from three wires of unequal diameters are recorded from the thermocouple suspended in constant flow with a periodic temperature fluctuation. It is demonstrated that the reconstructed signal from the three-wire thermocouple requires no compensation for omega less than or equal to 5(omega(sub 1)), where omega(sub 1) is the natural frequency of the smaller wire. The latter result represents a significant improvement compared to previous work with two-wire thermocouples. A correction factor has also been derived to account for wires of arbitrary diameter.

Forney, L. J.

Three-wire Thermocouple: Frequency Response in Constant Flow

Theory and experimental measurements are compared with a novel three-wire thermocouple. Signals from three wires of unequal diameters arc recorded from the thermocouple suspended in constant flow with a periodic temperature fluctuation. It is demonstrated that the reconstructed signal from the three-wire thermocouple requires no compensation for omega less than or equal to 5(sub omega1), where omega, is the natural frequency of the smaller wire. The latter result represents a significant improvement compared to previous work with two-wire thermocouples. A correction factor has also been derived to account for wires of arbitrary diameter.

Forney, L. J.

Advanced Microscopic Integrated Thermocouple Arrays

The purpose of this research is to develop and refine a technique for making microscopic thermocouple arrays for use in measuring the temperature gradient across a solid-liquid interface during the solidification process. Current thermocouple technology does not allow for real-time measurements across the interface due to the prohibitive size of available thermocouples. Microscopic thermocouple arrays will offer a much greater accuracy and resolution of temperature measurements across the solid-liquid interface which will lead to a better characterization of the solidification process and interface reaction which affect the properties of the resulting material.

Pettigrew, Penny J.

Thin film ceramic thermocouples

A thin film ceramic thermocouple (10) having two ceramic thermocouple (12, 14) that are in contact with each other in at least on point to form a junction, and wherein each element was prepared in a different oxygen/nitrogen/argon plasma. Since each element is prepared under different plasma conditions, they have different electrical conductivity and different charge carrier concentration. The thin film thermocouple (10) can be transparent. A versatile ceramic sensor system having an RTD heat flux sensor can be combined with a thermocouple and a strain sensor to yield a multifunctional ceramic sensor array. The transparent ceramic temperature sensor that could ultimately be used for calibration of optical sensors.

Gregory, Otto

Design and Implementation of Surface Eroding Thermocouples for Stage-One Modular Divertor Integration at the DIII-D Tokamak

The DIII-D has upgraded its upper divertor to a modular system using copper alloy pedestals to alter the divertor geometry without changing the vessel structure. Six new graphite tiles were designed for the shape and volume rise (SVR) divertor. Here, these new SVR tiles facilitated the formation of a poloidal array of 27 surface eroding thermocouples (SETCs) in the upper divertor region. At one location, a specialized recessed SETC, paired with a standard flush SETC, was installed in one of the ceiling tiles to provide comprehensive heat flux measurements, distinguishing between charged and noncharged particle contributions. Upgrades were made to the SETC system in the small-angle slot (SAS) divertor to improve overall performance. These upgrades included optimizing the feedthrough system to double the thermocouple cable capacity and reallocating cables from the SAS area to the SVR divertor. A compact isolation amplifier system with a fixed gain of 41 was employed to improve the signal level and minimize interference. Additionally, two analog-to-analog fiber systems were implemented for transmitting thermocouple signals over a single fiber, significantly reducing both noise levels and costs. The newly installed SETCs in the SVR divertor successfully completed initial commissioning testing. The SETCs captured the in-out asymmetry in the power distribution between the inner and outer strike points and demonstrated the dependency of the heat flux profile on the outer strike point location. During divertor detachment, heat flux mitigation was noted at the outer strike point location, while significant heat flux contributions from neutral particles were measured in the SVR divertor.

Divertor