Consolidation of composite cathodes with NCM and sulfide solid-state electrolytes by hot pressing for all-solid-state Li metal batteries

In this study, hot pressing was evaluated as a method of cell fabrication to increase the energy density of next-generation all-solid-state batteries with NCM active material and sulfide solid-state electrolyte. Hot pressing involves consolidating glassy sulfide electrolyte by the application of pressure at a temperature above the electrolyte’s glass transition temperature. Typically, cell stacks are formed at room temperature and retain 15–30% porosity that limits cell energy density. On the other hand, the porosity of hot-pressed cell stacks is reduced to less than 10%. The electrochemical function of hot-pressed cathode composites was assessed as a function of active material and solid-state electrolyte compositions. Specifically, LiNi 0.85 Co 0.10 Mn 0.05 O 2 and LiNi 0.6 Co 0.2 Mn 0.2 O 2 were studied in combination with either glassy Li 7 P 3 S 11 , glassy Li 3 PS 4 , or β-Li 3 PS 4 solid-state electrolytes. Cathode composites composed of LiNi 0.6 Co 0.2 Mn 0.2 O 2 and Li 3 PS 4 maintained the best function after hot pressing at 200 °C and 370 MPa for 10 min. It was found that LiNi 0.6 Co 0.2 Mn 0.2 O 2 ’s resistance to microcracking and the inherent stability of Li 3 PS 4 ’s fully de-networked local structure are critical to maintain good electrochemical function after hot pressing. Furthermore, the results of this study show that hot pressing reduces porosity in the cathode composite and confirms the feasibility of cathode support of consolidated, reinforced glass separators.

25 ENERGY STORAGE↗

Electrolyte strategies for practically viable all-solid-state lithium-sulfur batteries

All-solid-state lithium-sulfur batteries are a promising platform due to their high gravimetric energy density and enhanced safety. However, they face numerous challenges that currently obstruct commercial adoption. The key to overcoming these challenges lies in the rational selection and targeted development of solid-state electrolytes, where different materials classes present distinct trade-offs between performance and practicality. We assert that sulfide electrolytes offer the best compatibility with the cathode and anode requirements for practical sulfur cells, with halides and borohydrides also showing potential for use in the cathode with further development. We provide cell-level target parameters to ensure that the field moves consistently towards commercial relevance. Looking forward, we call for the adoption of the chlorinated argyrodite with a composition range of Li 6-x PS 5-x Cl 1+x (x = 0 - 0.5) as a standardized solid-state electrolyte to enable rigorous benchmarking across the field and accelerate battery development.

25 ENERGY STORAGE↗

Recent Progress on Dominant Sulfide‐Type Solid‐State Na Superionic Conductors for Solid‐State Sodium Batteries

Abstract Over the past decade, solid‐state batteries have garnered significant attentions due to their potentials to deliver high energy density and excellent safety. Considering the abundant sodium (Na) resources in contrast to lithium (Li), the development of sodium‐based batteries has become increasingly appealing. Sulfide‐based superionic conductors are widely considered as promising solid eletcrolytes (SEs) in solid‐state Na batteries due to the features of high ionic conductivity and cold‐press densification. In recent years, tremendous efforts have been made to investigate sulfide‐based Na‐ion conductors on their synthesis, compositions, conductivity, and the feasibility in batteries. However, there are still several challenges to overcome for their practical applications in high performance solid‐state Na batteries. This article provides a comprehensive update on the synthesis, structure, and properties of three dominant sulfide‐based Na‐ion conductors (Na 3 PS 4 , Na 3 SbS 4 , and Na 11 Sn 2 PS 12 ), and their families that have a variety of anion and cation doping. Additionally, the interface stability of these sulfide electrolytes toward the anode is reviewed, as well as the electrochemical performance of solid‐state Na batteries based on different types of cathode materials (metal sulfides, oxides, and organics). Finally, the perspective and outlook for the development and practical utilization of sulfide‐based SE in solid‐state batteries are discussed.

Guo, Xiaolin↗

Toward Higher Voltage Solid-State Batteries by Metastability and Kinetic Stability Design

The energy density of battery systems is limited largely by the electrochemical window of the electrolyte. Here, the combined thermodynamic and kinetic effects of mechanically induced metastability are shown to greatly widen the operational voltage window of solid-state batteries based on ceramic-sulfide electrolytes. Solid electrolyte voltage stability up to 10 V is achieved with minimal degradation, far beyond the capability of organic liquid electrolytes. Furthermore, combined experiment, ab initio computation, and theoretical modeling identify the nature of mechanically constrained Li 10 GeP 2 S 12 decomposition both within the bulk and at interfaces with cathode materials at very high voltages. Previously unclear kinetic processes are identified that, when properly implemented, can potentially allow solid-state full cells with remarkably high operational voltages.

25 ENERGY STORAGE↗

Phase Field Modeling of Pressure Induced Densification in Solid Electrolytes

Adoption of dense and homogeneous solid electrolytes can possibly mitigate the propagation of lithium dendrites and enable lithium metal anodes. Application of external pressure helps to minimize the sintering temperature in oxide ceramics and can potentially densify softer sulfide electrolytes even under room temperature conditions. Here, a previously developed phase field-based computational scheme for predicting the high-temperature sintering-induced densification of oxide ceramic solid electrolytes is extended in the present context to capture the influence of external pressure for densifying solid electrolytes. Two different bulk deformation mechanisms, namely, "reorganization" and "creep deformation," are dominant under external pressure, which is different from the surface and grain-boundary diffusion-induced densification of solid electrolytes that occurs during high temperature sintering. External pressure also increases the points of contact between the particles, which further enhances the propensity of diffusion-induced sintering process. Results obtained from simulations indicate that densification under external pressure is independent of the solid electrolyte particle morphology. Finally, a phase map is generated between applied pressure and temperature for achieving complete densification of oxide ceramics, which can possibly guide the synthesis of thin and dense solid electrolyte separators.

25 ENERGY STORAGE↗

A Sulfide‐Based Solid Electrolyte With High Humid Air Tolerance for Long Lifespan All‐Solid‐State Sodium Batteries

Abstract Sulfide‐based superionic conductors present great promise to achieve high energy density and safety for all‐solid‐state sodium batteries (ASSSBs). However, the poor electrolyte/electrode interface compatibility and humid air stability seriously hinder their deployment in ASSSBs. Herein, a series of high‐performance Na 3‐□ Sb 1‐4x (SnWCaTi) x S 4 sulfide‐based solid electrolytes (SSEs) are reported by coupling the vacancy effect with configurational entropy, which displays an excellent interface stability against sodium metal and an extraordinary tolerance toward the moist atmosphere, even for water. The optimized electrolyte effectively inhibits the detrimental mixed ion‐electron conducting interphase formation, achieving the ultra‐stable operation of Na–Na symmetric cell up to 1000 h. Furthermore, the Na + diffusion kinetics is obviously enhanced by increasing the Na sites local anisotropy and Na vacancies. Eventually, the assembled TiS 2 //Na 5 Sn ASSSBs deliver a remarkable reversible capacity of 211.6 mAh g −1 at 0.5C with a long‐term cycling performance of 450 cycles at room temperature. More importantly, it achieves a steady running up to 100 cycles at 1C even if this electrolyte is placed in the air with a dew temperature of 13.8 °C for 30 min, the highest values in the state‐of‐the‐art sulfide‐based ASSSBs. The well‐designed SSEs open a new avenue for realizing the advanced and powerful ASSSBs.

Guo, Yayu↗

Investigating dry room compatibility of sulfide solid-state electrolytes for scalable manufacturing

All-solid-state batteries (ASSBs) are viewed as promising next-generation energy storage devices, due to their enhanced safety by replacing organic liquid electrolytes with non-flammable solid-state electrolytes (SSEs). The high ionic conductivity and low Young's modulus of sulfide SSEs make them suitable candidates for commercial ASSBs. Nevertheless, sulfide SSEs are generally reported to be unstable in ambient air. Moreover, instead of gloveboxes used for laboratory scale studies, large scale production of batteries is usually conducted in dry rooms. Thus, this study aims to elucidate the chemical evolution of a sulfide electrolyte, Li 6 PS 5 Cl (LPSCl), during air exposure and to evaluate its dry room compatibility. When LPSCl is exposed to ambient air, hydrolysis, hydration, and carbonate formation can occur. Moreover, hydrolysis can lead to irreversible sulfur loss and therefore LPSCl cannot be fully recovered in the subsequent heat treatment. During heat treatment, exposed LPSCl undergoes dehydration, decomposition of carbonate species, and reformation of the LPSCl phase. Lastly, LPSCl was found to exhibit good stability in a dry room environment and was subject to only minor conductivity loss due to carbonate formation. The dry room exposed LPSCl sample was tested in a LiNi 0.8 Co 0.1 Mn 0.1 O 2 |LiIn half-cell, exhibiting no significant loss of electrochemical performance compared with the pristine LPSCl, proving it to be compatible with dry room manufacturing processes.

36 MATERIALS SCIENCE↗

Sulfide-Based Anode-Free Solid-State Batteries: Key Challenges and Emerging Solutions

Sulfide-based anode-free solid-state batteries (AFSSBs) have emerged as a transformative technology for next-generation energy storage, offering compelling advantages in energy density, safety, and manufacturing scalability. However, these batteries face significant challenges, particularly rapid capacity degradation that currently limits their practical implementation. This comprehensive review critically examines three fundamental issues affecting AFSSBs: nonuniform lithium nucleation on bare current collectors, unstable interfaces between plated lithium and sulfide electrolytes, and formation of interfacial voids during cycling. We systematically evaluate recent strategic advances in addressing these challenges, including metal seed coatings, conversion reaction-based compounds, and carbon-based interlayers. The review also analyzes the crucial role of advanced characterization techniques, from cryo-FIB-SEM to operando methods, in understanding failure mechanisms and validating improvement strategies. Finally, we present a forward-looking perspective on research directions necessary for commercialization. This work provides a thorough framework for understanding and advancing sulfide-based AFSSBs toward practical applications in next-generation energy storage systems.

25 ENERGY STORAGE↗

Multifunctional Coatings on Sulfide‐Based Solid Electrolyte Powders with Enhanced Processability, Stability, and Performance for Solid‐State Batteries

Abstract Sulfide‐based solid‐state electrolytes (SSEs) exhibit many tantalizing properties including high ionic conductivity and favorable mechanical properties for next‐generation solid‐state batteries. Widespread adoption of these materials is hindered by their intrinsic instability under ambient conditions, which makes them difficult to process at scale, and instability at the Li||SSE and cathode||SSE interfaces, which limits cell performance and lifetime. Atomic layer deposition is leveraged to grow thin Al 2 O 3 coatings on Li 6 PS 5 Cl powders to address both issues simultaneously. These coatings can be directly grown onto Li 6 PS 5 Cl particles with negligible chemical modification of the underlying material and enable exposure of powders to pure and H 2 O‐saturated oxygen environments for ≥4 h with minimal reactivity, compared with significant degradation of the uncoated powder. Pellets fabricated from coated powders exhibit ionic conductivities up to 2× higher than those made from uncoated material, with a simultaneous decrease in electronic conductivity and significant suppression of chemical reactivity at the Li‐SSE interface. These benefits result in significantly improved room temperature cycle life at high capacity and current density. It is hypothesized that this enhanced performance derives from improved intergranular properties and improved Li metal adhesion. This work points to a completely new framework for designing active, stable, and scalable materials for next‐generation solid‐state batteries.

36 MATERIALS SCIENCE↗

Deciphering Interfacial Chemical and Electrochemical Reactions of Sulfide-Based All-Solid-State Batteries

Large interfacial resistance resulting from interfacial reactions is widely acknowledged as one of the main challenges in sulfide electrolytes (SEs)-based all-solid-state lithium batteries (ASSLBs). However, the root cause of the large interfacial resistance between the SEs and typical layered oxide cathodes is not fully understood yet. Here we deciphered that interfacial oxygen loss from single-crystal LiNi 0.5 Mn 0.3 Co 0.2 O 2 (SC-NMC532) chemically oxidizes Li 10 GeP 2 S 12 , generating oxygen-containing interfacial species. Meanwhile, the interfacial oxygen loss also induces a structural change of oxide cathodes (layered-to-rocksalt). Besides, the high operation voltage can electrochemically oxidize SEs to form non-oxygen species (e.g. polysulfides). These chemically and electrochemically oxidized species, together with the interfacial structural change, are responsible for the large interfacial resistance at the cathode interface. More importantly, the widely adopted interfacial coating strategy is effective in suppressing chemically oxidized oxygen-containing species and mitigating the coincident interfacial structural change but is unable to prevent electrochemically induced non-oxygen species. These findings provide a deeper insight into the large interfacial resistance between the typical SE and layered oxide cathodes, which may be of assistance for the rational interface design of SE-based ASSLBs in future.

25 ENERGY STORAGE↗

Detection of a Cobalt-Containing Interphase at the Li 6 PS 5 Cl-NMC111 Interface by In Situ μ XANES and EIS

Sulfide electrolyte all-solid-state lithium batteries (ASLBs) with uncoated Li-Ni x Mn y Co 1–x–y O 2 (NMC) cathodes suffer from a large capacity loss during initial cycling and an increase in cell impedance. Decomposition reactions are known to occur at the Li 6 PS 5 Cl-NMC111 interface due to incompatibility between the two materials. If a stabilizing coating is applied to the NMC, it delivers full capacity during initial charge. However, the loss in capacity during discharge still occurs. The interface was studied by μ XANES and through EIS analysis. A chemically-formed interphase was detected by μ XANES, evident from reduction of Co at an uncoated NMC particle surface. This interphase was produced by decomposition at rest. To study the effect of the interphase on electrochemically active surface area, piecewise in situ EIS was performed and the data was modeled using a transmission line model (TLM). The charge transfer resistance R CT was used to estimate the volume specific active surface area (a act ). The median value for a act was 296 cm –1 , a factor of 7.5 lower than the theoretical value of 2216 cm –1 . This provided evidence of a lower electrochemically active surface area in the ASLB.

36 MATERIALS SCIENCE↗

Liquid Copper and Iron Production from Chalcopyrite, in the Absence of Oxygen

Clean energy infrastructure depends on chalcopyrite: the mineral that contains 70% of the world’s copper reserves, as well as a range of precious and critical metals. Smelting is the only commercially viable route to process chalcopyrite, where the oxygen-rich environment dictates the distribution of impurities and numerous upstream and downstream unit operations to manage noxious gases and by-products. However, unique opportunities to address urgent challenges faced by the copper industry arise by excluding oxygen and processing chalcopyrite in the native sulfide regime. Through electrochemical experiments and thermodynamic analysis, gaseous sulfur and electrochemical reduction in a molten sulfide electrolyte are shown to be effective levers to selectively extract the elements in chalcopyrite for the first time. We present a new process flow to supply the increasing demand for copper and byproduct metals using electricity and an inert anode, while decoupling metal production from fugitive gas emissions and oxidized by-products.

36 MATERIALS SCIENCE↗

Review on Interface and Interphase Issues in Sulfide Solid-State Electrolytes for All-Solid-State Li-Metal Batteries

All-solid-state batteries have emerged as promising alternatives to conventional Li-ion batteries owing to their higher energy density and safety, which stem from their use of inorganic solid-state electrolytes instead of flammable organic liquid electrolytes. Among various candidates, sulfide solid-state electrolytes are particularly promising for the development of high-energy all-solid-state Li metal batteries because of their high ionic conductivity and deformability. However, a significant challenge remains as their inherent instability in contact with electrodes forms unstable interfaces and interphases, leading to degradation of the battery performance. In this review article, we provide an overview of the key issues for the interfaces and interphases of sulfide solid-state electrolyte systems as well as recent progress in understanding such interface and interphase formation and potential solutions to stabilize them. In addition, we provide perspectives on future research directions in this field.

25 ENERGY STORAGE↗

Non-Conductive Polymers Enable Higher Ionic Conductivities and Suppress Reactivity in Hybrid Sulfide-Polymer Solid State Electrolytes

Hybrid ceramic-polymer solid state electrolytes are promising candidates to enable energy-dense lithium metal batteries by leveraging inorganic high ionic conductivity and flexible polymer mechanical properties. However, studies of hybrid electrolytes using sulfide-type inorganics such as Li3PS4 (LPS) have largely focused on combining the inorganic with commercial poly(ethylene oxide) (PEO). PEO has proven to be insufficient for use in hybrid systems because it reacts with LPS and provides a competing pathway for ion transport, therefore producing a hybrid with low conductivity. Our work shows that using nonconductive, nonpolar polyethylene (PE) in a hybrid electrolyte with LPS eliminates both polymer and inorganic degradation and remarkably exhibit higher conductivities than those containing PEO at different polymer and salt concentrations. Using tracer-exchange NMR, we observe that the nonconductive nature of PE allows for iontransport through the inorganic whereas PEO provides a separate, competing pathway for lithium transport. Furthermore, compared to pure LPS, these hybrids enable longer term lithium cycling at 60°C. Our work shows that the path to enabling conductive and stable sulfide hybrids for solid state lithium metal batteries may be through the use of nonconductive, nonreactive polymers.

batteries↗

Enabling High Stability of Co-Free LiNiO 2 Cathode via a Sulfide-Enriched Cathode Electrolyte Interface

Cobalt-free lithium nickel oxide (LNO) has garnered significant interest as the end member of high-nickel layered oxide cathodes for next-generation batteries. However, its practical performance notably underperforms expectations because of the structural degradation and unstable interfacial chemistry with electrolytes during cycling. Here, in this study, we report that a durable cathode-electrolyte interface (CEI), enriched by in situ formed sulfides and borides, can inhibit LNO structural degradation and suppress Ni ion dissolution. With the CEI protection, the stability of LNO can be remarkably extended, and batteries demonstrate a capacity retention rate of 84% (30 °C) and 79% (50 °C) after 200 cycles at 1C, respectively. These results demonstrate that enriching CEI with sulfur-containing species can effectively stabilize the interfacial chemistry of LNO, particularly at an elevated temperature of 50 °C. This finding provides valuable perspectives on designing electrolytes for cobalt-free LNO and other high-Ni cathodes toward the development of next-generation high-energy-density lithium-ion batteries.

25 ENERGY STORAGE↗

Synthesis and post-heating treatment of inorganic NaF·Na 3 SbS 4 solid electrolytes

Sulfide-type sodium (Na) solid electrolytes (SEs) with halide doping have attracted serious interest due to their high ionic conductivity and great potential in solid-state Na batteries. While other halogens such as Cl, Br, I have been studied to enhance Na-ion transport in sulfide-type SEs, the introduction of fluorine (F) is rarely investigated. Moreover, synthetic parameters such as heating treatment temperatures strongly influence the structure and conductive properties of halide-doped sulfide SEs. Herein, we prepared xNaF·(1-x)Na 3 SbS 4 nanocomposites with varying concentration of F using a low-temperature (150 °C) heating method, and studied the effects of post-heating treatment on structure and conductivity. In-situ neutron diffraction was employed to investigate the structural evolution of X-doped Na 3 SbS 4 (X = F, Cl) during the post-heating treatment and cooling process. In addition, the post-heating treatment at 300 °C leads to increased ionic conductivity of xNaF·(1-x)Na 3 SbS 4 nanocomposites with various F contents. After 300 °C post-heating treatment, 0.2NaF·0.8Na 3 SbS 4 exhibited the highest conductivity of 0.48 mS cm –1 at room temperature. Moreover, improved electrochemical stability was also observed in Na-Sn symmetric cells, specially, with prolonged stable cycling for 300 h and much lower polarization voltage (<0.35 V). Furthermore, this work highlights the importance of post-heating treatment on the structural evolution and its role in exploring new halide-incorporated sulfide-type SEs, promoting the development of inorganic solid-state ionic conductors.

25 ENERGY STORAGE↗

F and N Rich Solid Electrolyte for Stable All-Solid-State Battery

We report the instability of sulfide solid electrolytes to Li anode and high-voltage LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes limits the cyclic performance of all-solid-state lithium battery (ASSLB). Herein, the stability of Li 6 PS 5 Cl against Li anode is enhanced by mixing a small amount (0.32 wt%) of CuF 2 -LiNO 3 (CL) into Li 6 PS 5 Cl electrolyte layer to in-situ form a mixed-conductive-lithiophobic and self-healing LiF-Li 3 N-Cu solid electrolyte interphase (SEI) at Li 6 PS 5 Cl-CL/Li interface. The critical current density (CCD) of Li 6 PS 5 Cl-CuF 2 -LiNO 3 increases to 1.4 mA cm –2 /1.4 mAh cm –2 at room temperature, which is much higher than that of pristine Li 6 PS 5 Cl (0.4 mA cm –2 /0.4 mAh cm –2 ) even though mixing 0.32 wt% CL into Li 6 PS 5 Cl slightly reduces the ionic conductivity from 2.9 × 10 –3 to 1.5 × 10 –3 S cm –1 . The compatibility of Li 6 PS 5 Cl-CL electrolyte to single-crystalline NMC811 (S-NMC811) is further enhanced by adding a small amount (0.02 wt%) of AlF 3 into Li 6 PS 5 Cl-CL forming Li 6 PS 5 Cl-CuF 2- LiNO 3 -AlF 3 (Li 6 >PS 5 Cl-CLA) as a cathode electrolyte and by doing Cl – on S-NMC811 (Cl@S-NMC811) surface. The Cl@S-NMC811-Li 6 PS 5 Cl-CLA|Li 6 PS 5 Cl-CL|Li cells with areal capacity of 2.55 mAh cm -2 achieve a capacity retention of 69.4% after 100 cycles at 1C (1C = 200 mAh g -1 ). Adding a small amount of SEI and cathode/electrolyte interphase (CEI) former into the sulfide electrolytes with minimal reduction (48.3%) of ionic conductivity is an effective method to enhance the performance of ASSLB.

36 MATERIALS SCIENCE↗