Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Strain microscopy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Validation of a Crystal Plasticity Model Using High Energy Diffraction Microscopy

High energy diffraction microscopy is used to measure the crystallographic orientation and evolution of lattice strain in an Al Li alloy. The relative spatial arrangement of the several pancake-shaped grains in a tensile sample is determined through in situ and ex situ techniques. A model for crystal plasticity with continuity of lattice spin is posed, where grains are represented by layers in a finite element mesh following the arrangement indicated by experiment. Comparison is drawn between experiment and simulation.

Beaudoin, A. J.↗

The Evolution of the Deformation Substructure in a Ni-Co-Cr Equiatomic Solid Solution Alloy

The equiatomic NiCoCr alloy exhibits an excellent combination of strength and ductility, even greater than the FeNiCrCoMn high entropy alloy, and also displays a simultaneous increase in strength and ductility with decreasing the testing temperature. To systemically investigate the origin of the exceptional properties of NiCoCr alloy, which are related to the evolution of the deformation substructure with strain, interrupted tensile testing was conducted on the equiatomic NiCoCr single-phase solid solution alloy at both cryogenic and room temperatures at five different plastic strain levels of 1.5%, 6.5%, 29%, 50% and 70%. The evolution of deformation substructure was examined using electron backscatter diffraction (EBSD), transmission Kikuchi diffraction (TKD), conventional transmission electron microscopy (CTEM), diffraction contrast imaging using STEM (DCI-STEM) and atomic resolution scanning transmission electron microscopy. While the deformation substructure mainly consisted of planar dislocation slip and the dissociation of dislocations into stacking faults at small strain levels (≤6.5%), at larger strain levels, additional substructures including nanotwins and a new phase with hexagonal close packed (HCP) lamellae also appeared. The volume fraction of the HCP lamellae increases with increasing deformation, especially at cryogenic temperature. First principles calculations at 0 K indicate that the HCP phase is indeed energetically favorable relative to FCC for this composition. The effects of the nanotwin and HCP lamellar structures on hardening rate and ductility at both cryogenic and room temperature are qualitatively discussed.

Twinning↗

Microstructural Evaluation of Forging Parameters for Superalloy Disks

Forgings of nickel base superalloy were formed under several different strain rates and forging temperatures. Samples were taken from each forging condition to find the ASTM grain size, and the as large as grain (ALA). The specimens were mounted in bakelite, polished, etched and then optical microscopy was used to determine grain size. The specimens ASTM grain sizes from each forging condition were plotted against strain rate, forging temperature, and presoak time. Grain sizes increased with increasing forging temperature. Grain sizes also increased with decreasing strain rates and increasing forging presoak time. The ALA had been determined from each forging condition using the ASTM standard method. Each ALA was compared with the ASTM grain size of each forging condition to determine if the grain sizes were uniform or not. The forging condition of a strain rate of .03/sec and supersolvus heat treatment produced non uniform grains indicated by critical grain growth. Other anomalies are noted as well.

Falsey, John R.↗

InAs/Ga(1-x)In(x)Sb superlattices for infrared detector applications

The successful growth of InAs/Ga(1-x)In(x)Sb superlattices and their optical and structural characterization is discussed. Samples were grown by molecular beam epitaxy at fairly low substrate temperatures (less than 400 C). Structural quality was assessed by reflection high energy electron difrraction, transmission electron microscopy, and x ray diffraction. Excellent structures were achieved for growth on thick, strain relaxed GaSb buffer layers on GaAs substrates, despite a residual threading dislocation density of 10(exp 9)cm(exp -2) originating at the GaSb/GaAs interface. Despite a lattice mismatch of 1.7 percent, InAs/Ga(0.75)In(0.25)Sb superlattices are observed to be free of misfit dislocations at the thicknesses examined here, owing to the close lattice match between the superlattice and GaSb, which evenly distributes compressive and tensile stresses between the InAs and Ga(0.75)In(0.25)Sb layers. Photoluminescence and photoconductivity measurements indicate that the energy gaps of the strain-layer superlattices are smaller than those of InAs/GaSb superlattices with the same layer thicknesses, and are in agreement with the theoretical predictions of Smith and Mailhiot. Energy gaps of 80 to 250 meV (15 to 5 microns) have been measured for InAs/Ga(0.75)In(0.25)Sb superlattices with 45 to 25 A/25 A layer thickness. Results demonstrate that far-infrared cutoff wavelengths are compatible with the thin superlattice layers required for strong optical absorption in type-II superlattices.

Miles, Richard H.↗

Scanning electron acoustic microscopy of residual stresses in ceramics - Theory and experiment

The paper presents a three-dimensional mathematical model of signal generation and contrast in brittle materials and uses the model to simulate the effect of residual stress fields on the scanning electron acoustic microscopy (SEAM)-generated electron acoustic signal. According to the model, a positive (tensile) strain produces an increase in the output signal, whereas a negative (compressive) strain produces a decrease in the ouput signal. Dark field contrast conditions occur at a chopping frequency at which V2 - V1 is greater than 0 (where V2 = V is the SEAM output in a region of residual stresses, and V1 is the output in a stress-free region of the sample). Under ideal conditions (maximum contrast) V1 approaches zero. It was found that tensile strains of the order 0.2-0.3 percent, possible in brittle materials, would produce a variation of the acoustic output signal of the order 10 nV (about 1 percent), well within the image contrast and signal processing capability of the SEAM electronics.

Cantrell, John H.↗

Cytology of long-term desiccation in the desert cyanobacterium Chroococcidiopsis (Chroococcales)

Young and old cultures (up to 66 months) of two Chroococcidiopsis sp. strains isolated from the Negev desert, Israel, were examined by epifluorescence and electron microscopy. In old cultures, cell viability and autofluorescence were lower than in young cultures. An increase was seen with age in the polysaccharide content of the sheaths of nanocytes and nanocyte mother cells, and a decrease of phycobiliproteins was also seen. In the oldest cultures most of the cells were dead and in various stages of degeneration. Single living cells were scattered among the dead ones. No resting cells were formed in the oldest cultures, but many cell groups showed highly electron-dense sheaths and, in the cytoplasm, ribosomes and glycogen. These changes in cell structure may have a role in preventing water loss from the cell.

NASA Discipline Exobiology↗

Impact Ice Adhesion at NASA Glenn: Current Experimental Methods and Supporting Measurements

When examining the literature on the adhesion strength of impact ice, there have been a wide range of methodologies tried to measure the required stresses to induce interfacial delamination. Utilizing the Icing Research Tunnel at the NASA Glenn Research Center to generate the impact ice required for this work, several different mechanical tests have been and are being developed to determine the stresses along the interface between ice and coupon. This set of tests includes the technical mature modified lap joint test which has been used to conduct ice adhesion studies through a wide sweep of icing conditions. To conduct in situ ice adhesion measurements inside of the Icing Research Tunnel, several new experiments are currently being developed to make ice adhesion measurements during and immediately after ice accretion. In addition to these experimental methods, several supporting measurement techniques have been developed to allow for a better understanding on the influence of icing cloud conditions on the mechanical behavior of impact ice. Digital image correlation has been successfully implemented to augment the data generated by the modified lap joint test with full field surface displacement and strain measurements which allow for insight into the deformation processes present during a test. Both optical microscopy of impact ice samples along with ice replication techniques have been used to study the grain structure of the impact ice. This has led to a deeper understanding of the results from the modified lap joint method and how the structure of impact ice changes as it is accreted during an icing spray. The freezing process of impact ice generated by supercooled liquid water is not a volume conserving process, which leads to the presence of residual strains along the interface between ice and substrate. These strains have been observed using both a simplified flat geometry and a representative airfoil. The data gathered by these experimental adhesion methods and supporting measurements allows for a comprehensive understanding on the behavior of impact ice which will be critical to the development of future ice shedding models.

Ice Adhesion↗

Impact Ice Adhesion at NASA Glenn: Current Experimental Methods and Supporting Measurements

When examining the literature on the adhesion strength of impact ice, there have been a wide range of methodologies tried to measure the required stresses to induce interfacial delamination. Utilizing the Icing Research Tunnel at the NASA Glenn Research Center to generate the impact ice required for this work, several different mechanical tests have been and are being developed to determine the stresses along the interface between ice and coupon. This set of tests includes the technical mature modified lap joint test which has been used to conduct ice adhesion studies through a wide sweep of icing conditions. To conduct in situ ice adhesion measurements inside of the Icing Research Tunnel, several new experiments are currently being developed to make ice adhesion measurements during and immediately after ice accretion. In addition to these experimental methods, several supporting measurement techniques have been developed to allow for a better understanding on the influence of icing cloud conditions on the mechanical behavior of impact ice. Digital image correlation has been successfully implemented to augment the data generated by the modified lap joint test with full field surface displacement and strain measurements which allow for insight into the deformation processes present during a test. Both optical microscopy of impact ice samples along with ice replication techniques have been used to study the grain structure of the impact ice. This has led to a deeper understanding of the results from the modified lap join method and how the structure of impact ice changes as it is accreted during an icing spray. The freezing process of impact ice generated by supercooled liquid water is not a volume conserving process, which leads to the presence of residual strains along the interface between ice and substrate. These strains have been observed using both a simplified flat geometry and a representative airfoil. The data gathered by these experimental adhesion methods and supporting measurements allows for a compressive understanding on the behavior of impact ice which will be critical to the development of future ice shedding models.

Ice Adhesion↗

Dynamic recrystallization and grain boundary migration in B2 FeAl

Transmission electron microscopy and optical microscopy were used to examine polycrystalline specimens of the B2-structured alloy FeAl strained under tension to fracture at elevated temperature. Strain-induced grain boundary migration was observed above 900 K and dynamic recrystallization was found at 1000 K and 1100 K. Little evidence of dynamic recovery was evident but some networks were formed at 1100 K.

Baker, I.↗

Left ventricular hypertrophy in ascending aortic stenosis mice: anoikis and the progression to early failure

BACKGROUND: To determine potential mechanisms of the transition from hypertrophy to very early failure, we examined apoptosis in a model of ascending aortic stenosis (AS) in male FVB/n mice. METHODS AND RESULTS: Compared with age-matched controls, 4-week and 7-week AS animals (n=12 to 16 per group) had increased ratios of left ventricular weight to body weight (4.7+/-0.7 versus 3.1+/-0.2 and 5. 7+/-0.4 versus 2.7+/-0.1 mg/g, respectively, P<0.05) with similar body weights. Myocyte width was also increased in 4-week and 7-week AS mice compared with controls (19.0+/-0.8 and 25.2+/-1.8 versus 14. 1+/-0.5 microm, respectively, P<0.01). By 7 weeks, AS myocytes displayed branching with distinct differences in intercalated disk size and staining for beta(1)-integrin on both cell surface and adjacent extracellular matrix. In vivo left ventricular systolic developed pressure per gram as well as endocardial fractional shortening were similar in 4-week AS and controls but depressed in 7-week AS mice. Myocyte apoptosis estimated by in situ nick end-labeling (TUNEL) was extremely rare in 4-week AS and control mice; however, a low prevalence of TUNEL-positive myocytes and DNA laddering were detected in 7-week AS mice. The specificity of TUNEL labeling was confirmed by in situ ligation of hairpin oligonucleotides. CONCLUSIONS: Our findings indicate that myocyte apoptosis develops during the transition from hypertrophy to early failure in mice with chronic biomechanical stress and support the hypothesis that the disruption of normal myocyte anchorage to adjacent extracellular matrix and cells, a process called anoikis, may signal apoptosis.

NASA Discipline Cardiopulmonary↗

Study of Dislocation-Ordered In(x)Ga(1-x)As/GaAs Quantum Dots

A report describes an experimental study of dislocation-induced spatial ordering of quantum dots (QDs) comprising nanometer-sized In(x)Ga(1-x)As islands surrounded by GaAs. Metastable heteroepitaxial structures were grown by molecular-beam epitaxy of In(x)Ga(1-x)As onto n+ GaAs and semi-insulating GaAs substrates. Then the structures were relaxed during a post-growth annealing/self-organizing process leading to the formation of surface undulations that acted as preferential sites for the nucleation of QDs. Structural effects of annealing times and temperatures on the strain-relaxed In(x)Ga(1-x)As/GaAs and the subsequent spatial ordering of the QDs were analyzed by atomic-force microscopy and transmission electron microscopy. Continuous-wave spectral and time-resolved photoluminescence (PL) measurements were performed to study the effects, upon optical properties, of increased QD positional ordering, increased QD uniformity, and proximity of QDs to arrays of dislocations. PL spectral peaks of ordered QD structures formed on strain-relaxed In(x)Ga(1-x)As/GaAs layers were found to be narrower than those of structures not so formed and ordered. Rise and decay times of time-resolved PL were found to be lower at lower temperatures -- apparently as a consequence of decreased carrier-transport times within the barriers surrounding the QDs.

Leon, Rose↗

Crack Opening Displacement Behavior in Ceramic Matrix Composites

Ceramic Matrix Composites (CMC) modeling and life prediction strongly depend on oxidation, and therefore require a thorough understanding of when matrix cracks occur, the extent of cracking for given conditions (time-temperature-environment-stress), and the interactions of matrix cracks with fibers and interfaces. In this work, the evolution of matrix cracks in a melt-infiltrated Silicon Carbide/Silicon Carbide (SiC/SiC) CMC under uniaxial tension was examined using scanning electron microscopy (SEM) combined with digital image correlation (DIC) and manual crack opening displacement (COD) measurements. Strain relaxation due to matrix cracking, the relationship between COD's and applied stress, and damage evolution at stresses below the proportional limit were assessed. Direct experimental observation of strain relaxation adjacent to regions of matrix cracking is presented and discussed. Additionally, crack openings were found to increase linearly with increasing applied stress, and no crack was found to pass fully through the gage cross-section. This observation is discussed in the context of the assumption of through-cracks for all loading conditions and fiber architectures in oxidation modeling. Finally, the combination of SEM with DIC is demonstrated throughout to be a powerful means for damage identification and quantification in CMC's at stresses well below the proportional limit.

acoustic emission↗

Toughening mechanisms in elastomer-modified epoxies. I - Mechanical studies. II - Microscopy studies

Tensile dilatometry at constant displacement rates is presently used to ascertain whether voiding, crazing or shear banding are the deformation mechanisms at work in the toughening of brittle epoxies through the addition of an elastomeric phase. The results obtained for epoxies toughened by various levels of several types of carbonyl-terminated butadiene nitrile liquid rubber indicate that, at low strain rates, the rubber particles simply enhance shear deformation; at sufficiently high strain rates, the particles cavitate and promote further shear deformation. Examinations of these materials are conducted by means of SEM, TEM, and optical microscopy in the second part of this study. Toughening is hypothesized to involve cavitation's relieving of triaxial tension at the crack tip, as well as shear band formation, which creates a plastic zone.

Yee, A. F.↗

Off-axis tensile properties and fracture in a unidirectional graphite/polyimide composite (Celion 6000/PMR 15)

Tensile properties of unidirectional Celion 6000 graphite/PMR 15 polyimide composites prepared by hot molding and cold molding processes were measured at room temperature and 316 C, the upper use temperature of the polyimide resin, at both 45 and 90 deg to the fiber axis. The resulting fractures were characterized by scanning electron microscopy and materialographic techniques. Variation in tensile properties with processing history occurred in the elastic modulus and strain to failure for specimens loaded at 90 deg at 316 C, and in the fracture stress, and hence the in-plane shear stress, for those loaded at 45 deg at room temperature. Significant plastic deformation was observed in the 45 deg orientation at 316 C for material produced by both processing methods. In general, fracture occurred by both failure within the matrix and at the fiber-matrix interface; the degree of interfacial failure increased with temperature. Secondary cracking below the primary fracture surface was also observed.

Harper, J.↗

The Relationship Between Constraint and Ductile Fracture Initiation as Defined by Micromechanical Analyses

The use of small laboratory specimens to predict the integrity of large, complex structures relies on the validity of single parameter fracture mechanics. Unfortunately, the constraint loss associated with large scale yielding, whether in a laboratory specimen because of its small size or in a structure because it contains shallow flaws loaded in tension, can cause the breakdown of classical fracture mechanics and the loss of transferability of critical, global fracture parameters. Although the issue of constraint loss can be eliminated by testing actual structural configurations, such an approach can be prohibitively costly. Hence, a methodology that can correct global fracture parameters for constraint effects is desirable. This research uses micromechanical analyses to define the relationship between global, ductile fracture initiation parameters and constraint in two specimen geometries (SECT and SECB with varying a/w ratios) and one structural geometry (circumferentially cracked pipe). Two local fracture criteria corresponding to ductile fracture micromechanisms are evaluated: a constraint-modified, critical strain criterion for void coalescence proposed by Hancock and Cowling and a critical void ratio criterion for void growth based on the Rice and Tracey model. Crack initiation is assumed to occur when the critical value in each case is reached over some critical length. The primary material of interest is A516-70, a high-hardening pressure vessel steel sensitive to constraint; however, a low-hardening structural steel that is less sensitive to constraint is also being studied. Critical values of local fracture parameters are obtained by numerical analysis and experimental testing of circumferentially notched tensile specimens of varying constraint (e.g., notch radius). These parameters are then used in conjunction with large strain, large deformation, two- and three-dimensional finite element analyses of the geometries listed above to predict crack initiation loads and to calculate the associated (critical) global fracture parameters. The loads are verified experimentally, and microscopy is used to measure pre-crack length, crack tip opening displacement (CTOD), and the amount of stable crack growth. Results for A516-70 steel indicate that the constraint-modified, critical strain criterion with a critical length approximately equal to the grain size (0.0025 inch) provides accurate predictions of crack initiation. The critical void growth criterion is shown to considerably underpredict crack initiation loads with the same critical length. The relationship between the critical value of the J-integral for ductile crack initiation and crack depth for SECT and SECB specimens has been determined using the constraint-modified, critical strain criterion, demonstrating that this micromechanical model can be used to correct in-plane constraint effects due to crack depth and bending vs. tension loading. Finally, the relationship developed for the SECT specimens is used to predict the behavior of circumferentially cracked pipe specimens.

Panontin, Tina L.↗

The Effect of Cross-Link Density on the Toughening Mechanism of Elastomer-Modified Epoxies

A DGEBA epoxide resin (EPON 828) was elastomer modified by using three different carboxyl terminated butadiene acrylonitrile copolymers. The fracture toughness of these elastomer modified epoxies was measured in terms of the critical strain energy release rate, G sub IC. The toughening mechanism was elucidated using a tensile dilatometry technique. A plot of volume strain versus longitudinal strain often reveals the types of micromechanical deformations occurring in the uniaxial tensile specimen up to yield. Several microscopy techniques were employed to corroborate the tensile dilatometry results. The role of matrix ductility on the toughening mechanism of elastomer modified epoxies was investigated. By reducing the cross link density with various equivalent weight epoxide resins. Fracture toughness was again measured in terms of G sub IC. The characterization of the toughening mechanism was performed using a uniaxial tensile dilatometry technique and corroborated using various microscopy techniques.

Pearson, R. A.↗