Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Sintering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Sintering, properties and fabrication of Si3N4 + Y2O3 based ceramics

Pure silicon nitride shows a remarkable resistance to sintering without the use of densification additives. The present investigation is concerned with results which show the effect of chemical content on sinterability, taking into account the composition, raw material impurities, and processing contaminants. Aspects of sintering are discussed along with strength characteristics, and oxidation relations. Attention is given to phase field I and II materials, phase field III and IV materials, tungsten carbide and oxidation at 600 C, and studies involving shape fabrication by injection molding. It was found that in sintering Si3N4 + Y2O3 an increase in the amount of Y2O3 and, in particular, the addition of Al2O3 enhances the fluidity of the liquid phase.

Quackenbush, C. L.↗

Sintered Lining for Heat-Pipe Evaporator

Hotspots eliminated by lining inner wall. Distribution of heat transfer liquid in heat-pipe evaporator improved by lining inner wall with layer of sintered metal. Sintered layer takes place of layer of screen wick formerly sintered or bonded to wall. Since sintered layer always full of liquid, no hotspot of type that previously arose where former screen wick did not fit properly against wall.

Ernst, D. M.↗

Fabrication of highly dense SiN4 ceramics without additives by high pressure sintering

Silicon nitride (Si3N4) is one of candidate materials for the engineering ceramics which is used at high temperatures. The mechanical strengths of hot pressed or sintered Si2N4 ceramics containing some amount of additives, however, are deteriorated at elevated temperatures. To improve the high temperature strength of Si3N4 ceramics, an attempt to consolidate Si3N4 without additives was made by high pressure sintering technique. Scanning electron micrographs of fracture surfaces of the sintered bodies showed the bodies had finely grained and fully self-bonded sintered bodies were 310N sq m at room temperature and 174N/sq m at 1200 C.

Takatori, K.↗

Manufacture of dense sintered bodies containing silicon nitride

Sintered bodies containing 1-32.5 Si oxide and 1.5 wt.% SiC (Si oxide/SiC wt. ratio 3/2) are prepared and kept in a 10-3000 kg/2 sq. cm. N (g) atmosphere at 1500-2300 degrees, while simultaneously maintaining the CO (g) partial pressure around the body lower than the nitrogenation equil. pressure to give a dense sintered body. The prepared dense sintered body has high strength at high temperatures. Thus, SiC 40, oxide 30 and Si3N4 30 wt% were fired to a body which was kept in 1500 kg/sq. cm. N (g) for 20 h at 2000 degrees to give a dense sintered body having high bending strength at high temperatures.

Hirota, K.↗

On the sintering of silicon carbide

This document deals with the sintering of silicon carbide using pressureless sintering. This technique makes it possible to sinter a primarily covalent material to usable densities up to over 98% thD without having to use a high amount of sinter additives as is the case with other non-oxide ceramic materials. The process takes place rapidly, and it is also possible to produce relatively thick-walled structural parts without major problems. This sheds more light on the true characteristics of silicon carbide in one structural part, since there is no second or nearly no second phase. Heat pressing has improved stability.

Gugel, E.↗

Strength of hot isostatically pressed and sintered reaction bonded silicon nitrides containing Y2O3

The hot isostatic pressing of reaction bonded Si3N4 containing Y2O3 produced specimens with greater room temperature strengths than those by high pressure nitrogen sintering of the same material. Average room temperature bend strengths for hot isostatically pressed reaction bonded silicon nitride and high pressure nitrogen sintered reaction bonded silicon nitride were 767 and 670 MPa, respectively. Values of 472 and 495 MPa were observed at 1370 C. For specimens of similar but lower Y2O3 content produced from Si3N4 powder using the same high pressure nitrogen sintering conditions, the room temperature strength was 664 MPa and the 1370 C strength was 402 MPa. The greater strengths of the reaction bonded silicon nitride materials in comparison to the sintered silicon nitride powder material are attributed to the combined effect of processing method and higher Y2O3 content.

William A Sanders↗

Ultrasonic imaging of porosity variations produced during sintering

A silicon carbide disk was sintered from 2090 to 2190 C in 25-C steps. After each sintering step, the disk was examined using a precision acoustic scanning system to determine acoustic attenuation and velocity. The bulk density was found to vary nonmonotonically with sintering temperature. The density varied as much as 10 percent from its value at 2090 C during the sintering process. Local density fluctuations occurred in an organized and history-dependent way. These local density fluctuations varied up to + or - 7 percent of the bulk density and were made visible by acoustic attenuation and velocity mapping.

Generazio, Edward R.↗

Laboratory studies on cometary crust formation: The importance of sintering

It is demonstrated by experiments and theoretical considerations that sintering processes, so far used to describe the densification of metal and ceramic powders, are relevant for icy materials and therefore probably also for comets. A theoretical model is presented which describes the evolution of so called sinter necks, the contact zone between ice particles. With this model the strength increase of a porous, loosley packed icy body is calculated in which the sinter necks grow by evaporation and condensation of water vapor at a constant temperature. Experiments with ice powders validate the model qualitatively. An increase in strength up to a factor of four is observed during isothermal sintering. In order to check the relevance of the experimental results and the basic theoretical ideas with respect to real comets, more exact theories and improved experiments taking into account additional mass transport mechanisms are needed.

Ratke, L.↗

Permeability and Strength Measurements on Sintered, Porous, Hollow Turbine Blades Made by the American Electro Metal Corporation under Office of Naval Research Contract N-ONR-295 (01)

An experimental investigation was made to determine the permeability and strength characteristics of a number of sintered, porous, hollow turbine rotor blades and to determine the effectiveness of the blade fabrication method on permeability control. The test blades were fabricated by the American Electro Metal Corporation under a contract with the Office of Naval Research, Department of the Navy, and were submitted to the NACA for testing. Of the 22 test blades submitted, ten were sintered but not coined, five were sintered and coined, and seven were sintered and not coined but contained perforated reinforcements integral with the blade shells. Representative samples of each group of blades were tested. Large variations in permeability in both chordwise and spanwise directions were found. Local deviations as large as 155 to -85 percent from prescribed values were found in chordwise permeability. Only one blade, an uncoined one, had a chordwise permeability variations which reasonably approached that specified. Even for this blade, local deviations exceeded 10 percent. Spanwise permeability, specified to be held constant, varied as much as 50 percent from root to tip for both an uncoined and a coined blade. Previous NACA analyses have shown that in order to maintain proper control of blade wall temperatures, permeability variations must not exceed plus or minus 10 percent. Satisfactory control of permeability in either the chordwise or the spanwise direction was not achieved in the blades tested. Spin tests made at room temperature for six blades revealed the highest material rupture strength to be 8926 pounds per square inch. This value is about one third the strength required for rotor blades in present-day turbojet engines. The lowest value of blade strength was 1436 pounds per square inch.

Richards, Hadley T.↗

Implementation Challenges for Sintered Silicon Carbide Fiber Bonded Ceramic Materials for High Temperature Applications

During the last decades, a number of fiber reinforced ceramic composites have been developed and tested for various aerospace and ground based applications. However, a number of challenges still remain slowing the wide scale implementation of these materials. In addition to continuous fiber reinforced composites, other innovative materials have been developed including the fibrous monoliths and sintered fiber bonded ceramics. The sintered silicon carbide fiber bonded ceramics have been fabricated by the hot pressing and sintering of silicon carbide fibers. However, in this system reliable property database as well as various issues related to thermomechanical performance, integration, and fabrication of large and complex shape components has yet to be addressed. In this presentation, thermomechanical properties of sintered silicon carbide fiber bonded ceramics (as fabricated and joined) will be presented. In addition, critical need for manufacturing and integration technologies in successful implementation of these materials will be discussed.

Singh, M.↗

Sintering Characteristics of Multilayered Thermal Barrier Coatings Under Thermal Gradient and Isothermal High Temperature Annealing Conditions

Pyrochlore oxides have most of the relevant attributes for use as next generation thermal barrier coatings such as phase stability, low sintering kinetics and low thermal conductivity. One of the issues with the pyrochlore oxides is their lower toughness and therefore higher erosion rate compared to the current state-of-the-art TBC material, yttria (6 to 8 wt%) stabilized zirconia (YSZ). In this work, sintering characteristics were investigated for novel multilayered coating consisted of alternating layers of pyrochlore oxide viz Gd2Zr2O7 and t' low k (rare earth oxide doped YSZ). Thermal gradient and isothermal high temperature (1316 C) annealing conditions were used to investigate sintering and cracking in these coatings. The results are then compared with that of relevant monolayered coatings and a baseline YSZ coating.

Thermal Barrier Coatings↗

Vacuum Sintering of Highland Simulant CSM-LHT-1G

Sintering of lunar regolith is a process of interest to consolidate the ubiquitous granular material in durable structures on the lunar surface such as platforms, landing/launch pads, roads, and foundations for long-term robotic and human activities. Many publications do not report quantitative assessment of the effects of processing conditions on the strength properties of the sintered products. The work presented is an investigation into such effects on a carefully selected simulant, CSM-LHT-1G prepared for high temperature processing to eliminate undesired components that would not be present from lunar materials. Careful experiments under vacuum were conducted to identify the relevant factors that dominate the properties and the quality of the sintered product. CSM-LHT-1G simulant is a variant of the CSM-LHT-1 lunar highland simulant produced by Colorado School of Mines. The original mineralogical composition of CSM-LHT-1 (70 wt.% Greenspar, 30 wt.% Merriam Crater basalt) was modified to obtain a 30 wt.% glass content with the addition of NU-LHT-5M glass balanced with pyroxene (augite) to yield CSM-LHT-1G.

Vacuum Sintering↗

Activated sintering of ThO2 and ThO2-Y2O3 with NiO.

Scanning electron microscopy and isothermal shrinkage measurements were used to study the effects of additives on the sintering of Thoria-Yttria compacts and loose powders. Small amounts of the oxides of Ni, Zn, Co, and Cu were found to reduce the sintering temperature (which is normally above 2000 C). In particular, NiO, at a concentration of 0.8 wt %, was found to yield high-density bodies at temperatures below 1500 C. Densification occurs very rapidly, and is followed by a much slower sintering process typical of volume diffusion.

Halbfinger, G. P.↗

Sintering and hot pressing of Fra Mauro composition glass and the lithification of lunar breccias.

It is proposed that Apollo 14 type breccias lithify by sintering of particles of matrix glass under stress-free conditions. Meteorite impacts generate the heat necessary for sintering. Compacted angular particles of glass with the composition of an Apollo 14 rock were sintered experimentally. Loose clods of sub 37 micron grains form in several days at 700 C. Synthetic rocks, which texturally resemble the breccias, were produced at 795 C and above in 7.5 hours. Glass devitrified with increasing temperature. At 850 C, devitrification prevents much further densification of the synthetic breccias after 2 hours. Experiments compressing glass at 500 bars at 600 C produced dense vitreous masses which did not resemble lunar breccias. Confining pressure does not play a major role in lithifying the breccias. It is concluded that Apollo 14 type lunar breccias form at shallow depths at 800 C+ in a period of minutes to days.

Simonds, C. H.↗

Dislocation generation during early stage sintering.

Discussion of the effects of capillarity-induced stresses on dislocations during early stage sintering. A special version of Hirth's (1963) theoretical calculation procedures modified to describe dislocation nucleation on planes meeting the sintering body's neck surface obliquely is shown to predict plastic flow at stress levels know to exist between micron size metal particles in the early stages of sintering.

Sheehan, J. E.↗

Liquid phase sintered compacts in space

A model that will explain the effect of gravity on liquid phase sintering was developed. Wetting characteristics and density segregation which are the two important phenomena in liquid phase sintering are considered in the model development. Experiments were conducted on some selected material combinations to study the gravity effects on liquid phase sintering, and to verify the validity of the model. It is concluded that: (1) The surface tension forces acting on solid particles in a one-g environment are not appreciably different from those anticipated in a 0.00001g/g sub 0 (or lower) environment. (2) The capillary forces are dependent on the contact angle, the quantity of the liquid phase, and the distance between solid particles. (3) The pores (i.e., bubbles) do not appear to be driven to the surface by gravity-produced buoyancy forces. (4) The length of time to produce the same degree of settling in a low-gravity environment will be increased significantly. (5) A low gravity environment would appear to offer a unique means of satisfactorily infiltrating a larger and/or complex shaped compact.

Mookherji, T. K.↗

Silicon nitride-aluminum oxide solid solution (SiAION) formation and densification by pressure sintering

Stirred-ball-mill-blended Si3N4 and Al2O3 powders were pressure sintered in order to investigate the mechanism of solid solution formation and densification in the Si3N4-Al2O3 system. Powder blends with Si3N4:Al2O3 mole ratios of 4:1, 3:2, and 2:3 were pressure sintered at 27.6-MN/sq m pressure at temperatures to 17000 C (3090 F). The compaction behavior of the powder blends during pressure sintering was determined by observing the density of the powder compact as a function of temperature and time starting from room temperature. This information, combined with the results of X-ray diffraction and metallographic analyses regarding solutioning and phase transformation phenomena in the Si3N4-Al2O3 system, was used to describe the densification behavior.

Yeh, H. C.↗