Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SWELLING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Temperature-dependent cavity swelling in dual-ion irradiated Fe and Fe-Cr ferritic alloys

Fe-Cr ferritic-martensitic (FM) steels are promising structural material candidates for fusion and advanced fission reactors due to their attractive mechanical properties and volumetric swelling resistance. However, significant discrepancies exist regarding the effect of solutes and irradiation temperature on cavity swelling under ion versus neutron irradiation conditions. In this study, simultaneous dual ion irradiations (8 MeV Ni 3+ ions and energy-degraded 3.5 MeV He 2+ ions) were used to quantify the cavity swelling behavior in ultra-high purity Fe and Fe-Cr alloys (3-14 wt.% Cr), Fe-10 wt.% Cr-780 wt.ppm C, and Eurofer97 FM steel. The irradiations were conducted over a wide temperature range (400-550°C) with a mid-range dose of ~30 displacements per atom (dpa) and 0.1 appm/dpa He implantation rate. Here, using state-of-the-art transmission electron microscopy (TEM), we reveal that pure Fe has a ~50°C lower peak swelling temperature difference than Fe-Cr alloys, which is attributed to higher vacancy mobility in pure Fe. Chromium solute appears to strongly suppress cavity swelling in Fe-Cr alloys for temperatures below ~470°C, but seems to have little effect or slightly enhances swelling above ~470°C. Cavities were observed in all the irradiated samples between 400-550°C. This indicates that the narrow temperature range of observable cavities reported in prior ion irradiated Fe-Cr ferritic alloy studies is likely an artifact associated with the use of low ion energies (<5 MeV), which leads to pronounced near-surface and implanted ion effects that suppress cavity swelling even at midrange depths (particularly at high temperatures).

36 MATERIALS SCIENCE↗

HT9 swelling in high burnup fast reactor fuel pin components

The irradiation-induced void swelling of HT9 stainless steel has been observed many times, but there are little data available to quantify the amount of swelling expected as a function of neutron exposure and temperature. This is further complicated by potential heat-to-heat chemical variations or heat treatment conditions during fabrication. Herein, this paper summarizes the results of most of the relevant previously completed studies, then focuses on the swelling behavior of HT9 mixed-oxide fuel cladding and wrapper wire irradiated to high neutron exposures. Note that the hexagonal duct used for the ACO-3 experiment (in the Fast Flux Test Facility, or FFTF) was also made from HT9 and has been studied previously by other researchers. The cladding enables a wider range of operating temperatures. Immersion density and transmission electron microscopy were used to identify a peak in the amount of swelling located axially, just below core centerline, for both the cladding and the wire. The peak roughly coincided with a peak seen in the cladding diameter profile. The wrapper wire showed enhanced swelling compared to the cladding, likely due to over-tempering during wire fabrication heat treatment. The grains showed decreased martensitic structure were larger in size. These data do not provide for the means to fully characterize the swelling of HT9, but do provide further insight into the factors controlling it. The onset of breakaway swelling was not indicated in this data.

36 MATERIALS SCIENCE↗

Influence of injected interstitials on the void swelling in two structural variants of 304L stainless steel induced by self-ion irradiation at 500 °C

The two variants of AISI 304L stainless steel (SS) with different grain size distributions were ion irradiated at 500 °C to a peak dose of ~60 dpa. In the coarse-grained annealed variant, a peak swelling of ~12% was observed closer to the specimen surface rather than at the depth of peak displacement damage. The forward shift in depth between peak swelling and peak dose is proposed to be a consequence of suppression of void nucleation by injected interstitials. The swelling behavior in the front portion of the ion range mirrors that of neutron-induced swelling in this steel, exhibiting significant curvature with increasing dose as the swelling rate approaches the terminal swelling rate of 1%/dpa. Furthermore, an ultrafine grain variant of this steel produced by severely plastic deformation exhibits a similar suppression of void nucleation in the injected interstitial region, but also shows a significantly extended transient regime, not reaching the terminal swelling rate by 60 dpa.

304 stainless steel↗

Dimensional stability and anisotropy of SiC and SiC-based composites in transition swelling regime

Swelling, or volumetric expansion, is an inevitable consequence of the atomic displacement damage in crystalline silicon carbide (SiC) caused by energetic neutron irradiation. Because of its steep temperature and dose dependence, understanding swelling is essential for designing SiC-based components for nuclear applications. Here in this study, swelling behaviors of monolithic CVD SiC and nuclear grade SiC fiber – SiC matrix (SiC/SiC) composites were accurately determined, supported by the irradiation temperature determination for individual samples, following neutron irradiation within the lower transition swelling temperature regime. Slightly anisotropic swelling behaviors were found for the SiC/SiC samples and attributed primarily to the combined effects of the pre-existing microcracking, fiber architecture, and specimen dimension. A semi-empirical model of SiC swelling was calibrated and presented. Finally, implications of the refined model to selected swelling-related issues for SiC-based nuclar reactor components are discussed.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Super-swelled lyotropic single crystals

Lipids self-assemble into diverse supramolecular structures that exhibit thermotropic and/or lyotropic behavior. Lyotropic mesophases, where membranes conform to periodic minimal surfaces dividing two nonpenetrating aqueous subspaces, are arguably one of the most intriguing phases of lipid materials. Traditional 3D bicontinuous cubic lipid materials appear as a polycrystal of varying degrees of order. When exposed to water, the properties of the molecular building blocks of the membrane determine specific swelling limits setting the lattice dimensions at about 15 nm. This limited swelling severely impairs their application as delivery vehicles of large drugs or as matrices for guiding protein crystallization. We report the discovery of self-assembly strategies leading to the emergence of lipid bicontinuous single crystals with unprecedented swelling capacity. Here, the conventional strategy to increase unit cell size is tweaking membrane composition to include charged building blocks, a process to achieve electrostatic-driven swelling. In this paper, we demonstrate that controlling self-assembly external conditions when coupled to membrane composition yields 3D bicontinuous cubic phases that swell up to lattice dimensions of 68 nm. Importantly, and contrary to what is perceived for soft lyotropic materials in general, the self-assembly methodology enables the development of large super-swelled monocrystals. Utilizing small-angle X-ray scattering and cryoelectron microscopy, we underpin three crucial factors dictating the stabilization of super-swelled lipid bicontinuous cubic single crystals: (i) organic solvent drying speed, (ii) membrane charge density, and (iii) polyethylene glycol-conjugated lipids amount.

36 MATERIALS SCIENCE↗

Sea floor swells and mantle plumes

Most of the intraplate oceanic hot spots are located on the crest of broad topographic swells in the sea floor. These swells have Gaussian shaped profiles, with up to 1.6 km of relief and half widths of 200 to 300 km. Swells are accompanied by positive geoid height anomalies with amplitudes of 6 to 8 m. In the Atlantic and Pacific basins swells cover an area equal to 10% of the Earth's surface. Next to boundary layer contraction, swells are the most important cause of uplift and subsidence in oceanic lithosphere. Calculation of buoyancy supported topography and geoid height were combined with uplift data from laboratory experiments to assess whether sea floor swell can be produced by mantle plumes. The critical constraints are: (1) swell topographic profiles; (2) geoid height/topographic height ratios; and (3) uplift rates, estimated to be 0.2 km/ma.

Olson, P.↗

A Study of the Swelling and Bursting of the High Pressure Coupling (HPC) of a Two-Stage Light Gas Gun

• Need for data at muzzle velocities of 7.0 km/s and above to simulate impacts of space debris and naturally occurring meteoroids • The two-stage light gas gun is a well known way of achieving these velocities • There is a danger of significant swelling and even bursting of the HPC (high pressure coupling). • A consistent picture of the swelling and bursting of the HPCs of two Ames two-stage light gas guns is developed, based on the following: 1. Experimental measurements of the swelling and bursting of the HPCs of two two-stage light gas guns. 2. Stress-strain calculations of the swelling and bursting of thick walled steel tubes. 3. Experimental measurements swelling and bursting of thick walled steel tubes. 4. CFD calculations of the maximum pressures in the HPC of a two-stage light gas gun using the code LGGUN. • It is shown that model developed predicts swelling and bursting that agrees reasonably well with measured data. • Hence, it is suggested that the model could be used in the design of a two-stage light gas guns to assess the risk of swelling and bursting and to give maximum suggested operating conditions for an existing gun.

Ballistic Range↗

Shrinkage and Swelling of Coal Induced by Desorption and Sorption of Fluids: Theoretical Model and Interpretation of a Field Project

Geologic sequestration in deep unmineable coal seams and enhanced coalbed methane production is a promising choice, economically and environmentally, to reduce anthropogenic gases such as carbon dioxide in the atmosphere. Unmineable coal seams are typically known to adsorb large amounts of carbon dioxide in comparison to the sizeable amounts of sorbed methane, which raises the potential for large scale sequestration projects. During the process of sequestration, carbon dioxide is injected into the coalbed and desorbed methane is produced. The coal matrix is believed to shrink when a gas is desorbed and swell when a gas is sorbed, sometimes causing profound changes in the cleat porosity and permeability of the coal seam. These changes may have significant impact on the reservoir performance. Therefore, it is necessary to understand the combined influence of swelling and shrinkage, and geomechanical properties including elastic modulus, cleat porosity, and permeability of the reservoir. The present paper deals with the influence of swelling and shrinkage on the reservoir performance, and the geomechanical response of the reservoir system during the process of geologic sequestration of carbon dioxide and enhanced coalbed methane production in an actual field project located in northern New Mexico. A three-dimensional swelling and shrinkage model was developed and implemented into an existing reservoir model to understand the influence of geomechanical parameters, as well as swelling and shrinkage properties, on the reservoir performance. Numerical results obtained from the modified simulator were compared to available measured values from that site and previous studies. Results show that swelling and shrinkage, and the combination of geomechanical and operational parameters, have a significant influence on the performance of the reservoir system.

01 COAL, LIGNITE, AND PEAT↗

Detecting self-ion irradiation-induced void swelling in pure copper using transient grating spectroscopy

Irradiation-induced void swelling remains a major challenge to nuclear reactor operation. Swelling may take years to initiate and often results in rapid material property degradation once started. Alloy development for advanced nuclear systems will require rapid characterization of the swelling breakaway dose in new alloys, yet this capability does not yet exist. In this paper, we demonstrate that transient grating spectroscopy (TGS) can detect void swelling in single crystal copper via changes in surface acoustic wave (SAW) velocity. Scanning transmission electron microscopy (STEM) links the TGS-observed changes with void swelling-induced microstructural evolution. Finally, these results are considered in the context of previous work to suggest that in situ TGS will be able to rapidly determine when new bulk materials begin void swelling, shortening alloy development and testing times.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Model for radiation damage-induced grain subdivision and its influence in U 3 Si 2 fuel swelling

Here, the swelling mechanisms of U 3 Si 2 from neutron irradiation under reactor conditions are not unequivocally known. The limited experimental evidence that is available suggests that the main driver of the swelling in this material would be fission gases accumulation at crystalline grain boundaries. The steps that lead to the accumulation of fission gases at these locations are multiple and complex. However, gradually, the gaseous fission products migrate by diffusion. Upon reaching a grain boundary, which acts as a trap, the gaseous fission products start to accumulate, thus leading to formation of bubbles and hence to induced swelling. Therefore, a quantitative model of swelling requires the incorporation of phenomena that increase the presence of grain boundaries and decrease grain sizes, thus creating sites for bubble formation and growth while concurrently deceasing the distance from gas species formation to gas accumulation sites. It is assumed that grain boundary formation results from the conversion of stored energy from accumulated dislocations into energy for the formation of new grain boundaries. This work attempts to develop a quantitative model for grain subdivision in U 3 Si 2 based on the above mentioned phenomena to quantitatively corroborate the presence of such a mechanism. Then the model is used in conjunction with swelling codes to evaluate the total swelling of a fuel pellet during its lifetime in the I 2 S-LWR reactor.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Irradiation-induced swelling of pure chromium with 5 MeV Fe ions in the temperature range 450–650 °C

A surface coating using pure chromium has been proposed to increase the accident tolerance of Zircaloy cladding in pressurized water reactors. However, there is not much irradiation experience with Cr alloys and especially pure Cr. In the present study, pure chromium was irradiated with 5 MeV Fe ions to 50 peak dpa (displacements per atom) at temperatures of 450, 500, 550, 600 and 650 °C. Then irradiation at the peak swelling temperature of 550 °C was conducted to 50, 100, 150 peak dpa. Swelling at 50 dpa was observed over the entire temperature range studied, 450–650 °C, but appeared to be decreasing strongly at the temperature boundaries of the experiment. After an initial transient of rapid swelling, chromium was observed to swell at a rate of ~0.03–0.04%/dpa (up to 120 local dpa), which is much lower than pure Fe at 0.2%/dpa. This low swelling rate was found to be relatively insensitive to dpa rate, which varied by a factor of ~2 over the depth of data collection. Here, swelling was observed to begin quickly with an incubation period less than 10 dpa. Self-organization in the form of void ordering was observed to be developing at 50 dpa, becoming better defined with increasing dose. The void alignment direction is determined to be the $\langle$111$\rangle$ axial direction.

36 MATERIALS SCIENCE↗

From suppressed void growth to significant void swelling in NiCoFeCr complex concentrated solid-solution alloy

Void swelling can result in dimensional instability and undermine the safe operation of nuclear reactors. Current strategies to inhibit void swelling mainly focus on enhancing defect absorption and recombination by introducing high-density defect sinks. Complex concentrated solid-solution alloys (CSAs), including high-entropy alloys, can withstand severe radiation damage due to their inherent chemical complexity without interfaces. However, the underlying mechanisms for void suppression in CSAs are far from clear. In this research, we studied the void evolution with respect to irradiation depths, doses, and temperatures in equiatomic NiCoFeCr under 3 MeV Ni ion irradiations. At relatively low doses (16 and 54 displacements per atom, dpa), voids form mainly outside of the ion-damaged region, and void formation in the peak damage region is suppressed, leading to negligible swelling. However, with further increase of dose (86 up to 250 dpa), significant void growth occurs in the peak damage region and extended dislocation lines dominate instead of short dislocation lines and loops formed at lower doses. From 500 to 700 °C, the dislocation density decreases while dislocations grow. Although the overall void swelling increases dramatically from 500 to 580 °C at 54 dpa, void growth in the peak damage region is still suppressed. The transition from suppressed void growth to significant void swelling is attributed to dislocation evolution and local chemical inhomogeneity (enrichment of Fe/Cr in the matrix) at higher doses. Our study shows that controlling element diffusion and defect evolution through tuning chemical complexity can further enhance the swelling resistance of CSAs.

36 MATERIALS SCIENCE↗

A Rate Theory Model of Radiation-Induced Swelling in an Austenitic Stainless Steel

Many rate theory models of cavity (void) swelling have been published over the past 50 years, all having the same, or similar, structures. A rigorous validation of the models has not been possible because of the dearth of information concerning the microstructures that correspond with the swelling data. Whereas the lack of microstructure information is still an issue for historical swelling data, in the past 10–20 years data have been published on the evolution of the microstructure (point defect yields from collision cascades, cavity number densities, and dislocation densities/yield strengths) allowing certain gaps in information to be filled when considering historic swelling data. With reasonable estimates of key microstructure parameters, a standard rate theory model can be applied, and the model parameter space explored, in connection with historical swelling data. By using published data on: (i) yield strength as a function of dose and temperature (to establish an empirical expression for dislocation density evolution); (ii) cavity number densities as a function of temperature; and (iii) freely migrating defect (FMD) production as a function of primary knock-on atom (PKA) spectrum, the necessary parameter and microstructure inputs that were previously unknown can be used in model development. This paper describes a rate-theory model for void swelling of 316 stainless steel irradiated in the EBR-2 reactor as a function of irradiation temperature and neutron dose.

36 MATERIALS SCIENCE↗

Tamoxifen does not inhibit the swell activated chloride channel in human neutrophils during the respiratory burst

Effective functioning of neutrophils relies upon electron translocation through the NADPH oxidase (NOX). The electron current generated (I{sub e}) by the neutrophil NADPH oxidase is electrogenic and rapidly depolarises the membrane potential in activated human neutrophils. Swelling activated chloride channels have been demonstrated in part to counteract the depolarisation generated by the NADPH oxidase I{sub e}. In the present study, the effects of inhibitors of swell activated chloride channels on ROS production and on the swelling activated chloride conductance was investigated in activated human neutrophils. Tamoxifen (10 {mu}M), a specific inhibitor for swell activated chloride channels in neutrophils, completely inhibited both the PMA and FMLP stimulated respiratory burst. This inhibition of the neutrophil respiratory burst was not due to the blocking effect of tamoxifen on the swelling activated chloride conductance in these cells. These results demonstrate that a tamoxifen insensitive swell activated chloride channel has important significance during the neutrophil respiratory burst.

60 APPLIED LIFE SCIENCES↗

Effects of internal swelling on residual elasticity of a quasi-brittle material through a composite sphere model

This work describes the development of a micromechanical-based constitutive model accounting for the effect of internal expansion on the residual elasticity of a Hashin composite material. This material is made of spherical inclusions that are subjected to gradual swelling within a quasi-brittle matrix. The main focus of this work is to describe and analyze the material mechanical response, with an additional focus on the internal swelling’s effect on the stress–strain response and residual elasticity. Microstructural features and parameters of major importance for the mechanical responses were identified. The innovative characteristics of the proposed approach are summarized as follows: (1) a full determination of the physics of a complete-damage problem throughout the whole process of inclusion swelling with upscaling techniques, which transfers the microcrack-related properties from the lower scale to upper scale; and (2) an evolution of the mechanical fields and the corresponding residual elasticity for various inclusion swelling levels. Concerning the matrix–inclusion composite, it was hypothesized that only the matrix was susceptible to cracking, with varied degrees of damage, whereas the inclusions behave elastically and the elastic modulus of the expanding inclusions remains constant. It is to emphasize that the gradual swelling of inclusions is modeled by an increasing strain in the current micromechanical-based constitutive model, and the microcracks are represented by a set of randomly oriented penny-shaped microcracks with identical radii (namely, closed cracks). The main contribution of the current research is to establish the exact mathematical solutions for the mechanical fields (stress, strain) caused by the swelling of the inclusions (mechanical loading) and derive the effective residual elasticity of a composite (structural response) subject to internal expansion and quasi-brittle damage. Based on the assumption of closed cracks that could be extended to open cracks in the upcoming work, the results proposed by the present paper help to understand the non-linear mechanical behavior of quasi-brittle materials subject to microcracking and provide a theoretical framework to be used as academical benchmark for numerical simulations.

36 MATERIALS SCIENCE↗

Influence of solidification structures on radiation-induced swelling in an additively-manufactured austenitic stainless steel

Metal additive manufacturing offers potential advantages for producing structural materials, such as austenitic stainless steels, in nuclear power systems. However, the microstructure developed during metal additive processing is notably different from the one developed in conventional processing, and the influence of the microstructural differences on performance in radiation environments has not been fully quantified. Using heavy ion irradiation and transmission electron microscopy, the radiation-induced swelling response of a laser powder-bed fusion-manufactured austenitic stainless steel was investigated at high doses. The influence of solidification-induced dislocation and precipitate structures was studied by comparing the radiation-induced swelling response of a 316L stainless steel in three microstructural states: as-fabricated, solution annealed, and fully recrystallized. Void swelling was approximately twice as pronounced in the as-fabricated state compared to post-processed states. In the framework of the rate theory for radiation effects, the higher swelling in the as-fabricated state can be explained by the strong sink bias for interstitial point defects exerted by the intermediate density of pre-existing dislocations. Void swelling was inhibited in the vicinity of pre-existing precipitates, but the density of precipitates in the as-fabricated material was not enough to compensate for the increase in swelling caused by dislocations.

36 MATERIALS SCIENCE↗

Machine learning models for volumetric swelling in uranium nitride

Machine learning methods are applied to predict the volumetric swelling rate of the nuclear fuel uranium nitride (UN) over various temperatures, irradiation conditions, and power densities. Both kernel-based methods and symbolic regression models for UN swelling are developed and compared with multiple experimental datasets. We find that the UN pellet geometry and dimensions must be taken into account to accurately model swelling behavior. Strong agreement is observed between the developed machine learning models and the data. The predictive error generated by the machine learning models improves on empirical models taken from the literature. Sensitivity analysis is performed to determine which properties such as temperature, burnup, and power density, are most important in the swelling process. We find that machine learning can be used to quickly develop accurate swelling models for nuclear materials. In conclusion, the presented results illustrate the potential of machine learning to determine volumetric swelling in UN.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Rate dependence of swelling in lithium-ion cells

Swelling of a commercial 5 Ah lithium-ion cell with a nickel/manganese/cobalt-oxide cathode is investigated as a function of the charge state and the charge/discharge rate. In combination with sensitive displacement measurements, knowledge of the electrode configuration within this prismatic cell's interior allows macroscopic deformations of the casing to be correlated to electrochemical and mechanical transformations in individual anode/separator/cathode layers. Thermal expansion and interior charge state are both found to cause significant swelling. At low rates, where thermal expansion is negligible, the electrode sandwich dilates by as much as 1.5% as the charge state swings from 0% to 100% because of lithium-ion intercalation. At high rates a comparably large residual swelling was observed at the end of discharge. Thermal expansion caused by joule heating at high discharge rate results in battery swelling. The changes in displacement with respect to capacity at low rate correlate well with the potential changes known to accompany phase transitions in the electrode materials. Although the potential response changes minimally with the C-rate, the extent of swelling varies significantly, suggesting that measurements of swelling may provide a sensitive gauge for characterizing dynamic operating states. (C) 2014 Elsevier B.V. All rights reserved.

Oh, KY↗