Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SOLDERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Age-aware solder performance models : level 2 milestone completion.

Legislated requirements and industry standards are replacing eutectic lead-tin (Pb-Sn) solders with lead-free (Pb-free) solders in future component designs and in replacements and retrofits. Since Pb-free solders have not yet seen service for long periods, their long-term behavior is poorly characterized. Because understanding the reliability of Pb-free solders is critical to supporting the next generation of circuit board designs, it is imperative that we develop, validate and exercise a solder lifetime model that can capture the thermomechanical response of Pb-free solder joints in stockpile components. To this end, an ASC Level 2 milestone was identified for fiscal year 2010: Milestone 3605: Utilize experimentally validated constitutive model for lead-free solder to simulate aging and reliability of solder joints in stockpile components. This report documents the completion of this milestone, including evidence that the milestone completion criteria were met and a summary of the milestone Program Review.

36 MATERIALS SCIENCE↗

Study on the Reliability of Carbon Nanotube-Reinforced Sn-58Bi Lead-Free Solder Joints

The wettability, microstructure and mechanical properties of multi-walled carbon nanotube (CNT)-reinforced Sn-58Bi composite solder joints were investigated. The results indicate that the wettability of the Sn-58Bi solder is improved and the growth of interfacial intermetallic (IMC) compounds for solder joints is restrained by CNTs. The thickness of the IMC layers is decreased with increasing CNTs concentration. The microstructure of the Sn-58Bi composite solders is refined, the maximum tensile strength and shear strength are obtained by adding the optimum CNTs content about 0.01 wt.%. However, excessive content of CNTs addition can deteriorate the properties. The creep rupture life of Sn-58Bi solder joint and Sn-58Bi-0.01CNTs solder joint is decreased with increasing load, temperature and current density. The average creep rupture life of Sn-58Bi-0.01CNTs composite solder joint is 60% higher than that of the plain solder joint.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microstructural development and mechanical properties of a near-eutectic directionally solidified Sn–Bi solder alloy

Sn–Bi solders may be applied for electronic applications where low-temperature soldering is required, i.e., sensitive components, step soldering and soldering LEDs. In spite of their potential to cover such applications, the mechanical response of soldered joints of Sn–Bi alloys in some cases does not meet the strength requirements due to inappropriate resulting microstructures. Hence, careful examination and control of as-soldered microstructures become necessary with a view to pre-programming reliable final properties. The present study aims to investigate the effects of solidification thermal parameters (growth rate — V{sub L} and cooling rate — T-dot{sub L}) on the microstructure of the Sn–52 wt.%Bi solder solidified under unsteady-state conditions. Samples were obtained by upward directional solidification (DS), followed by characterization through metallography and scanning electron microscopy (SEM). The microstructures are shown to be formed by Sn-rich dendrites decorated with Bi precipitates surrounded by a complex regular eutectic mixture, with alternated Bi-rich and Sn-rich phases. Experimental correlations of primary (λ{sub 1}), secondary (λ{sub 2}), tertiary (λ{sub 3}) dendritic and eutectic spacings (λ{sub coarse} and λ{sub fine}) with cooling rate and growth rate are established. Two ranges of lamellar eutectic sizes were determined, described by two experimental equations λ = 1.1 V{sub L}{sup −1/2} and λ = 0.67 V{sub L}{sup −1/2}. The onset of tertiary branches within the dendritic array along the Sn–52 wt.%Bi alloy DS casting is shown to occur for cooling rates lower than 1.5 °C/s. - Highlights: • The Sn–52 wt.%Bi solder was shown to have two eutectic sizes. • The fishbone eutectic is preferably located adjacent to the Bi-rich lamellar phases. • The onset of tertiary dendritic branches in Sn–Bi is associated with T-dot{sub L} < 1.5 °C/s. • Higher eutectic fraction and λ{sub 3} provoked a reverse increase in σ{sub u} and σ{sub y}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A novel interface strengthening layer: Nanoscale AuCu super-structure formed during Au80Sn20/Cu rapid solidification soldering process

Highlights: • The nanoscale AuCu super-structure formed in Au80Sn20/Cu soldering joint. • The phase-transformation diffusion mechanism of Au80Sn20/Cu soldering process was studied. • The orientation relationship of Au80Sn20/Cu intermetallic compounds was investigated. • The interfacial strengthening mechanism of nanoscale AuCu layer was discussed. - Abstract: Phase composition and orientation of intermetallic compounds layers determine the functional and mechanical properties of solder joints. In this paper, interfacial reaction and strengthening mechanism of Au80Sn20/Cu joint by rapid solidification reflow soldering were studied. The Au80Sn20/Cu solder joint by rapid solidification reflow soldering exhibit a superior shear property, and the shear strength reaches up to 90 MPa. It is found that a new nanoscale AuCu super-structure formed in the interfacial intermetallic compounds layer, which is coherent with the [001] Cu substrate. The orientation relationship of Cu matrix/interfacial intermetallic compounds is determined to be [001]{sub Cu}∥[001]{sub AuCu}∥[ 2-bar 4 2-bar 3]{sub (AuCu){sub 5Sn}} and (200){sub Cu}∥(200){sub AuCu}∥(10 1-bar 0){sub (AuCu){sub 5Sn}}. Nanoscale AuCu super-structure influences the interface slip direction and provides interface misfit dislocation, hinder the dislocation movement, lead to the interface strengthening effect. Our finding on nanoscale AuCu super-structure formed during Au80Sn20/Cu soldering process not only sheds light on future research direction but also provides practical guidance to the engineers in solder industry.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Activation Energy for Solder Bond Degradation: Thermal Cycling of Field-aged Modules at Multiple Upper Temperatures

The reliability of solder joints in the solar cell metallization-interconnect system influences the lifetime of photovoltaic modules. Two field-aged modules-one with Sn 62 Pb 36 Ag 2 solder at the solder joints (Solarex MSX 60), and the other with the standard Sn 60 Pb 40 solder (Siemens M55)-were subjected to a modified thermal cycling (TC) test of IEC 61215. Three sections in each module were maintained at 85 degrees C, 95 degrees C, and 105 degrees C during the 15-minute high temperature dwell time. Current equivalent to the module short-circuit current was injected through the module when the chamber temperature was above 25 degrees C to simulate regular field operation. This novel approach aims to induce thermomechanical fatigue (TMF) at the solder joints and intermetallic compound (IMC) formation at the metal/solder interfaces. The activation energy (E a ) for solder bond degradation was calculated based on the series resistance (R s ) increase in TC testing rather than power drop to avoid the effect of confounding variables. Module-level R s increase in MSX 60 module after TC800 cycles and in M55 module after TC400 cycles was 1.22% and 183.7%, respectively. The E a determined for the module with 2wt% Ag is 0.24 eV and for that with the standard solder is 0.27 eV. The solder bond degradation seems to have been driven by TMF rather than IMC formation for both modules.

14 SOLAR ENERGY↗

Stability of molybdenum nanoparticles in Sn-3.8Ag-0.7Cu solder during multiple reflow and their influence on interfacial intermetallic compounds

This work investigates the effects of molybdenum nanoparticles on the growth of interfacial intermetallic compound between Sn-3.8Ag-0.7Cu solder and copper substrate during multiple reflow. Molybdenum nanoparticles were mixed with Sn-3.8Ag-0.7Cu solder paste by manual mixing. Solder samples were reflowed on a copper substrate in a 250 Degree-Sign C reflow oven up to six times. The molybdenum content of the bulk solder was determined by inductive coupled plasma-optical emission spectrometry. It is found that upon the addition of molybdenum nanoparticles to Sn-3.8Ag-0.7Cu solder, the interfacial intermetallic compound thickness and scallop diameter decreases under all reflow conditions. Molybdenum nanoparticles do not appear to dissolve or react with the solder. They tend to adsorb preferentially at the interface between solder and the intermetallic compound scallops. It is suggested that molybdenum nanoparticles impart their influence on the interfacial intermetallic compound as discrete particles. The intact, discrete nanoparticles, by absorbing preferentially at the interface, hinder the diffusion flux of the substrate and thereby suppress the intermetallic compound growth. - Highlights: Black-Right-Pointing-Pointer Mo nanoparticles do not dissolve or react with the SAC solder during reflow. Black-Right-Pointing-Pointer Addition of Mo nanoparticles results smaller IMC thickness and scallop diameter. Black-Right-Pointing-Pointer Mo nanoparticles influence the interfacial IMC through discrete particle effect.

36 MATERIALS SCIENCE↗

Understanding the Reliability of Solder Joints Used in Advanced Structural and Electronics Applications: Part 2 - Reliability Performance.

Whether structural or electronic, all solder joints must provide the necessary level of reliability for the application. The Part 1 report examined the effects of filler metal properties and the soldering process on joint reliability. Filler metal solderability and mechanical properties, as well as the extents of base material dissolution and interface reaction that occur during the soldering process, were shown to affect reliability performance. The continuation of this discussion is presented in this Part 2 report, which highlights those factors that directly affect solder joint reliability. There is the growth of an intermetallic compound (IMC) reaction layer at the solder/base material interface by means of solid-state diffusion processes. In terms of mechanical response by the solder joint, fatigue remains as the foremost concern for long-term performance. Thermal mechanical fatigue (TMF), a form of low-cycle fatigue (LCF), occurs when temperature cycling is combined with mismatched values of the coefficient of thermal expansion (CTE) between materials comprising the solder joint “system.” Vibration environments give rise to high-cycle fatigue (HCF) degradation. Although accelerated aging studies provide valuable empirical data, too many variants of filler metals, base materials, joint geometries, and service environments are forcing design engineers to embrace computational modeling to predict the long-term reliability of solder joints.

42 ENGINEERING↗

Rapidly solidifying Pb-free Sn-Ag-Cu-Al or Sn-Cu-Al solder

A solder alloy includes Sn, optional Ag, Cu, and Al wherein the solder alloy composition together with the solder alloy superheat temperature and rapid cooling rate from the superheat temperature are controlled to provide a dispersion of fine hard Cu—Al intermetallic particles in an as-solidified solder alloy microstructure wherein the particles are retained even after multiple solder reflow cycles often used in modern electronic assembly procedures to provide a particle strengthening to the solder joint microstructure as well as exert a grain refining effect on the solder joint microstructure, providing a strong, impact- and thermal aging-resistant solder joint that has beneficial microstructural features and is substantially devoid of Ag3Sn blades.

36 MATERIALS SCIENCE↗

Effect of Ag3Sn nanoparticles and temperature on Cu6Sn5 IMC growth in Sn-xAg/Cu solder joints

Highlights: • The number density of Ag{sub 3}Sn grains precipitated upon Cu{sub 6}Sn{sub 5}, increases with Ag content and reflow temperature (T). • Raising of wt. % of Ag in solder and lowering of T can cause an increase in grain diameter of Ag{sub 3}Sn nanoparticles. • The blockading effect of Ag{sub 3}Sn particles on Cu{sub 6}Sn{sub 5} IMC growth is more pronounced in Sn-3Ag and Sn-3.5Ag alloys. • IMC suppressing nanoparticles can be utilized for solder materials design. - Abstract: The growing importance of Pb-free Sn-xAg solders and high cost of Ag has attracted the attention of researchers to perform experiment with solders with varied content of Ag element. In this study, Sn-xAg(0,1,2,3.5) solder balls on Cu substrate have been reflowed at 250/275/300 °C for 60 s and air cooled. Finite element method has been utilized to simulate the concentration and temperature during cooling. The experimental results suggest that the Cu flux through grain boundary diffusion is the dominant mechanism for Cu{sub 6}Sn{sub 5} intermetallic compound growth in Pure Sn and Sn-1Ag solders. When the Ag content is increased, as in case of Sn-3Ag and Sn-3.5Ag alloys; the shielding effect of Ag{sub 3}Sn nanoparticles is the determinant factor for affecting the thickness of Cu{sub 6}Sn{sub 5} IMC. Both Cu influx rate and shielding effect of Ag{sub 3}Sn nanoparticles are enhanced with the raise in pre-cooled isothermal reflow temperature. Sn-1Ag solder is observed to have the thickest Cu{sub 6}Sn{sub 5} IMC.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Comparison of Extensive Thermal Cycling Effects on Microstructure Development in Micro-alloyed Sn-Ag-Cu Solder Joints

Pb-free solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic have promise for widespread adoption across assembly conditions and operating environments, but enhanced microstructural control is needed. Micro-alloying with elements such as Zn was demonstrated for promoting a preferred solidification path and joint microstructure earlier in simple (Cu/Cu) solder joints studies for different cooling rates. This beneficial behavior now has been verified in reworked ball grid array (BGA) joints, using dissimilar SAC305 (Sn-3.0Ag-0.5Cu, wt.%) solder paste. After industrial assembly, BGA components joined with Sn-3.5Ag-0.74Cu-0.21Zn solder were tested in thermal cycling (-55 C/+125 C) along with baseline SAC305 BGA joints beyond 3000 cycles with continuous failure monitoring. Weibull analysis of the results demonstrated that BGA components joined with SAC + Zn/SAC305 have less joint integrity than SAC305 joints, but their lifetime is sufficient for severe applications in consumer, defense, and avionics electronic product field environments. Failure analysis of the BGA joints revealed that cracking did not deviate from the typical top area (BGA component side) of each joint, in spite of different Ag3Sn blade content. Thus, SAC + Zn solder has not shown any advantage over SAC305 solder in these thermal cycling trials, but other characteristics of SAC + Zn solder may make it more attractive for use across the full range of harsh conditions of avionics or defense applications.

36 MATERIALS SCIENCE↗

Development of Sn-Ag-Cu-X Solders for Electronic Assembly by Micro-Alloying with Al

Of Pb-free solder choices, an array of solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic (T eut = 217°C) composition have emerged with potential for broad use, including ball grid array (BGA) joints that cool slowly. This work investigated minor substitutional additions of Al (<0.25 wt.%) to Sn-3.5Ag-0.95Cu (SAC3595) solders to promote more consistent solder joint microstructures and to avoid deleterious product phases, e.g., Ag3Sn “blades,” for BGA cooling rates, since such Al additions to SAC had already demonstrated excellent thermal aging stability. Consistent with past work, blade formation was suppressed for increased Al content (>0.05Al), but the suppression effect faded for >0.20Al. Undercooling suppression did not correlate specifically with blade suppression since it became significant at 0.10Al and increased continuously with greater Al to 0.25Al. Surprisingly, an intermediate range of Al content (0.10 wt.% to 0.20 wt.% Al) promoted formation of significant populations of 2-μm to 5-μm faceted Cu-Al particles, identified as Cu33Al17, that clustered at the top of the solder joint matrix and exhibited extraordinary hardness. Clustering of Cu33Al17 was attributed to its buoyancy, from a lower density than Sn liquid, and its early position in the nucleation sequence within the solder matrix, permitting unrestricted migration to the top interface. Joint microstructures and implications for the full nucleation sequence for these SAC + Al solder joints are discussed, along with possible benefits from the clustered particles for improved thermal cycling resistance.

36 MATERIALS SCIENCE↗

Interconnection of thermal parameters, microstructure and mechanical properties in directionally solidified Sn–Sb lead-free solder alloys

Considerable effort is being made to develop lead-free solders for assembling in environmental-conscious electronics, due to the inherent toxicity of Pb. The search for substitute alloys of Pb–Sn solders has increased in order to comply with different soldering purposes. The solder must not only meet the expected levels of electrical performance but may also have appropriate mechanical strength, with the absence of cracks in the solder joints. The Sn–Sb alloy system has a range of compositions that can be potentially included in the class of high temperature solders. This study aims to establish interrelations of solidification thermal parameters, microstructure and mechanical properties of Sn–Sb alloys (2 wt.%Sb and 5.5 wt.%Sb) samples, which were directionally solidified under cooling rates similar to those of reflow procedures in industrial practice. A complete high-cooling rate cellular growth is shown to be associated with the Sn–2.0 wt.%Sb alloy and a reverse dendrite-to-cell transition is observed for the Sn–5.5 wt.%Sb alloy. Strength and ductility of the Sn–2.0 wt.%Sb alloy are shown not to be affected by the cellular spacing. On the other hand, a considerable variation in these properties is associated with the cellular region of the Sn–5.5 wt.%Sb alloy casting. - Graphical abstract: Display Omitted - Highlights: • The microstructure of the Sn–2 wt.%Sb alloy is characterized by high-cooling rates cells. • Reverse dendrite > cell transition occurs for Sn–5.5 wt.%Sb alloy: cells prevail for cooling rates > 1.2 K/s. • Sn–5.5 wt.%Sb alloy: the dendritic region occurs for cooling rates < 0.9 K/s. • Sn–5.5 wt.%Sb alloy: tensile properties are improved with decreasing cellular spacing.

36 MATERIALS SCIENCE↗

Effect of gamma radiation on micromechanical hardness of lead-free solder joint

Lead-free solders are important material in nano and microelectronic surface mounting technology for various applications in bio medicine, environmental monitoring, spacecraft and satellite instrumentation. Nevertheless solder joint in radiation environment needs higher reliability and resistance to any damage caused by ionizing radiations. In this study a lead-free 99.0Sn0.3Ag0.7Cu wt.% (SAC) solder joint was developed and subjected to various doses of gamma radiation to investigate the effects of the ionizing radiation to micromechanical hardness of the solder. Averaged hardness of the SAC joint was obtained from nanoindentation test. The results show a relationship between hardness values of indentations and the increment of radiation dose. Highest mean hardness, 0.2290 ± 0.0270 GPa was calculated on solder joint which was exposed to 5 Gray dose of gamma radiation. This value indicates possible radiation hardening effect on irradiated solder. The hardness gradually decreased to 0.1933 ± 0.0210 GPa and 0.1631 ± 0.0173 GPa when exposed to doses 50 and 500 gray respectively. These values are also lower than the hardness of non irradiated sample which was calculated as 0.2084 ± 0.0.3633 GPa indicating possible radiation damage and needs further related atomic dislocation study.

36 MATERIALS SCIENCE↗

Dark Lock-in Thermography Identifies Solder Bond Failure as the Root Cause of Series Resistance Increase in Fielded Solar Modules

Correlating the electrical performance of photovoltaic modules to the spatially resolved photoluminescence, electroluminescence, and dark lock-in thermography (DLIT) images is an important long-term goal for developing solar cell technology. These images offer highly sophisticated and detailed information about the spatial distribution and (if imaged at successive time intervals) temporal degradation of local series and shunt resistances. There have been extensive studies to correlate these imaging techniques to local characteristics at the cell level. However, it has been difficult to extract and quantify module-level information from the techniques. In this study, we interpret module current-voltage (I-V) measurements along with corresponding DLIT images within a module-scale simulation framework, demonstrating that series resistance degradation of the module I-V characteristics, in this case, can be attributed to solder bond failures. Our simulations highlight how current crowding associated with a failed solder joint (or a section of the solder pad) translates to the characteristic point-like (asymmetric doublet) heating pattern in neighboring solder joints (or the neighboring regions of the solder pad). Overall, the correlation between series resistance and solder joint degradation could inform expedited diagnosis of field degradation of solar modules.

42 ENGINEERING↗

An analysis of the pull strength behaviors of fine-pitch, flip chip solder interconnections using a Au-Pt-Pd thick film conductor on Low-Temperature, Co-fired Ceramic (LTCC) substrates.

The assembly of the BDYE detector requires the attachment of sixteen silicon (Si) processor dice (eight on the top side; eight on the bottom side) onto a low-temperature, co-fired ceramic (LTCC) substrate using 63Sn-37Pb (wt.%, Sn-Pb) in a double-reflow soldering process (nitrogen). There are 132 solder joints per die. The bond pads were gold-platinum-palladium (71Au-26Pt-3Pd, wt.%) thick film layers fired onto the LTCC in a post-process sequence. The pull strength and failure modes provided the quality metrics for the Sn-Pb solder joints. Pull strengths were measured in both the as-fabricated condition and after exposure to thermal cycling (-55/125 C; 15 min hold times; 20 cycles). Extremely low pull strengths--referred to as the low pull strength phenomenon--were observed intermittently throughout the product build, resulting in added program costs, schedule delays, and a long-term reliability concern for the detector. There was no statistically significant correlation between the low pull strength phenomenon and (1) the LTCC 'sub-floor' lot; (2) grit blasting the LTCC surfaces prior to the post-process steps; (3) the post-process parameters; (4) the conductor pad height (thickness); (5) the dice soldering assembly sequence; or (5) the dice pull test sequence. Formation of an intermetallic compound (IMC)/LTCC interface caused by thick film consumption during either the soldering process or by solid-state IMC formation was not directly responsible for the low-strength phenomenon. Metallographic cross sections of solder joints from dice that exhibited the low pull strength behavior, revealed the presence of a reaction layer resulting from an interaction between Sn from the molten Sn-Pb and the glassy phase at the TKN/LTCC interface. The thick film porosity did not contribute, explicitly, to the occurrence of reaction layer. Rather, the process of printing the very thin conductor pads was too sensitive to minor thixotropic changes to ink, which resulted in inconsistent proportions of metal and glassy phase particles present during the subsequent firing process. The consequences were subtle, intermittent changes to the thick film microstructure that gave rise to the reaction layer and, thus, the low pull strength phenomenon. A mitigation strategy would be the use of physical vapor deposition (PVD) techniques to create thin film bond pads; this is multi-chip module, deposited (MCM-D) technology.

36 MATERIALS SCIENCE↗

An Accelerated Method for Testing Soldering Tendency of Core Pins

An accelerated method for testing die soldering has been developed. High intensity ultrasonic vibrations has been used to simulate the die casting conditions such as high pressure and high impingement speed of molten metal on the pin. Soldering tendency of steels and coated pins has been examined. The results indicate that in the low carbon steel/Al system, the onset of soldering is 60 times faster with ultrasonic vibration than that without ultrasonic vibration. In the H13/A380 system, the onset of soldering reaction is accelerated to 30-60 times. Coating significantly reduces the soldering tendency of the core pins.

36 MATERIALS SCIENCE↗

Advances in Pb-free solder microstructure control and interconnect design

New electronics applications demanding enhanced performance and higher operating temperatures have led to continued research in the field of Pb-free solder designs and interconnect solutions. In this paper, recent advances in the microstructural design of Pb-free solders and interconnect systems were discussed by highlighting two topics: increasing β-Sn nucleation in Sn-based solders, and isothermally solidified interconnects using transient liquid phases. Issues in β-Sn nucleation in Sn-based solders were summarized in the context of Swenson’s 2007 review of the topic. Recent advancements in the areas of alloy composition manipulation, nucleating heterogeneities, and rapid solidification were discussed, and a proposal based on a multi-faceted solidification approach involving the promotion of constitutional undercooling and nucleating heterogeneities was outlined for future research. The second half of the paper analyzed two different approaches to liquid phase diffusion bonding as a replacement for high-Pb solders, one based on the application of the pseudo-binary Cu-Ni-Sn ternary system, and the other on a proposed thermodynamic framework for identifying potential ternary alloys for liquid phase diffusion bonding. Furthermore, all of the concepts reviewed relied upon the fundamentals of thermodynamics, kinetics, and solidification, to which Jack Smith substantially contributed during his scientific career.

36 MATERIALS SCIENCE↗

Depressing effect of 0.1 wt.% Cr addition into Sn-9Zn solder alloy on the intermetallic growth with Cu substrate during isothermal aging

In this paper, the effect of 0.1 wt.% Cr addition into Sn-9Zn lead-free solder alloys on the growth of intermetallic compound (IMC) with Cu substrate during soldering and subsequent isothermal aging was investigated. During soldering, it was found that 0.1 wt.% Cr addition did not contribute to forming the IMC, which was verified as the same phase structure as the IMC for Sn-9Zn/Cu. However, during solid-state isothermal aging, the IMC growth was remarkably depressed by 0.1 wt.% Cr addition in the Sn-9Zn solder, and this effect tended to be more prominent at higher aging temperature. The activation energy for IMC growth was determined as 21.2 kJ mol{sup -1} and 42.9 kJ mol{sup -1} for Sn-9Zn/Cu and Sn-9Zn-Cr/Cu, respectively. The reduced diffusion coefficient was confirmed for the 0.1Cr-containing solder/Cu. Energy-dispersive X-ray mapping and point analysis also showed ZnCr phase existing in solder matrix, which can reduce diffusion rate of Zn atoms.

36 MATERIALS SCIENCE↗