Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SODIUM OXIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Insights into the Effects of Zinc Doping on Structural Phase Transition of P2-Type Sodium Nickel Manganese Oxide Cathodes for High-Energy Sodium Ion Batteries

P2-type sodium nickel manganese oxide-based cathode materials with higher energy densities are prime candidates for applications in rechargeable sodium ion batteries. A systematic study combining in situ high energy X-ray diffraction (HEXRD), ex situ Xray absorption fine spectroscopy (XAFS), transmission electron microscopy (TEM), and solid-state nuclear magnetic resonance (SSNMR) techniques was carried out to gain a deep insight into the structural evolution of P2-Na 0.66 Ni 0.33-x Zn x Mn 0.67 O 2 (x = 0, 0.07) during cycling. In situ HEXRD and ex situ TEM measurements indicate that an irreversible phase transition occurs upon sodium insertion-extraction of Na 0.66 Ni 0.33 Mn 0.67 O 2 . Zinc doping of this system results in a high structural reversibility. XAFS measurements indicate that both materials are almost completely dependent on the Ni 4+ /Ni 3+ / Ni 2+ redox couple to provide charge/discharge capacity. SS-NMR measurements indicate that both reversible and irreversible migration of transition metal ions into the sodium layer occurs in the material at the fully charged state. The irreversible migration of transition metal ions triggers a structural distortion, leading to the observed capacity and voltage fading. Our results allow a new understanding of the importance of improving the stability of transition metal layers.

36 MATERIALS SCIENCE↗

Coupling Anionic Oxygen Redox with Selenium for Stable High‐Voltage Sodium Layered Oxide Cathodes

Utilizing anion redox reaction is crucial for developing the next generation of high-energy density, low-cost sodium-ion batteries. However, the irreversible oxygen redox reaction in Na-ion layered cathodes, which leads to voltage fading and reduced overall lifespan, has hindered their practical application. In this study, selenium is incorporated as a synergistic redox active center of oxygen to improve the stability of Na-ion cathodes. The redesigned cathode maintains stable voltage by demonstrating reversible oxygen redox while significantly suppressing the redox activity of manganese. The anionic redox contribution capacity of the selenium-doped Na 0.6 Li 0.2 Mn 0.8 O 2 cathode remains as high as 84% after 50 cycles, while the pristine Na 0.6 Li 0.2 Mn 0.8 O 2 cathode experiences a reduction to 39% of its initial capacity. The X-ray photoelectron spectroscopy data and computational analysis further revealed that selenium doping participates in redox as Se +4/5 which stabilizes the charged state and increases the energy step for O─O dimerization, thus improving the stability and lifespan of Na 0.6 Li 0.2 Mn 0.8 O 2 cathodes. In conclusion, the findings highlight the potential of redox coupling design to address the issue of voltage fade caused by irreversible anionic redox.

25 ENERGY STORAGE↗

Fast oxygen redox enabled by flexible Al–O bonds in P2-type layered oxides for sodium batteries

Sodium-ion batteries (SIBs) exhibit significant potential for large-scale energy storage systems due to the abundance and low cost of sodium resources. Triggering lattice oxygen redox (LOR) in P2-type transition metal oxides is considered a promising approach to enhance energy density in SIB cathodes, providing high operating potential and substantial capacity. However, irreversible phase transitions associated with LOR, particularly from prisms (P-type stacking) to octahedrons (O-type stacking), lead to severe structural distortions and sluggish Na + diffusion kinetics. In this work, an Al-substitution strategy is proposed to suppress the formation of O-type stacking and instead promote the formation of a beneficial Z phase. Furthermore, the flexible Al-O bonds accommodate asymmetric variations in their occupied states during the sodiation process, mitigating local structural distortions through Al-O bond contraction. Stabilization of the local structure ensures the maintenance of a robust Na + diffusion pathway. As a result, the Al-substituted cathode achieves a low Na + diffusion barrier of 0.47 eV and delivers a capacity of 86 mAh/g even at a high current density of 1 A/g within 1.5–4.5 V, maintaining 62.5% capacity retention over 100 cycles.

36 MATERIALS SCIENCE↗

A Dual Stage Sodium Thermo-Electro-Chemical Converter

The need for reliable and distributable energy sources is evident given the current forecasting of the world’s energy demand [1]. One prominent obstacle is the lack of an efficient direct heat-to-electricity conversion technology. The sodium thermo-electro-chemical converter (Na-TECC) is a highly efficient thermally regenerative electrochemical system (TRES) that can fill this void. The advantage of the Na-TECC over other direct conversion technologies is that it is a closed device (unlike fuel cells) requiring nothing more than a heat input (similar to thermoelectrics). It also has a high power density (> 1 W/cm2) and specific power up to 0.5 kW/kg , with the potential to achieve > 45% heat to electricity conversion efficiencies [2]. Furthermore, the converter rejects heat at a temperature hot enough to make it amenable for cogeneration, potentially under air-cooled operation. This electrochemical technology uses a special ion-selective solid-electrolyte called beta-alumina (Na2O•11Al2O3), that is highly conductive to sodium cations. A more conducting variation of this compound is beta”-alumina (Na2O•MgO•5Al2O3), where the magnesium acts as a stabilizer [3]. In the device, liquid sodium enters an evaporator where it is heated isobarically and vaporizes. The vapor is then oxidized at the interface between the anode and the solid-electrolyte. The Na-TECC generates electric power by allowing the high pressure oxidized sodium vapor ions to expand isothermally through the solid-electrolyte from the anode to the cathode. The liberated electrons are simultaneously conducted through an external load and recombine with the cations at the cathode. The low pressure sodium vapor is subsequently condensed and a wick pumps the liquid into the high pressure plenum to complete the cycle. Previous Na-TECCs have achieved efficiencies of 18% due to practical losses, whereas the potential efficiencies are above 45% [4]. Thermodynamic limitations and design constraints have limited previous devices from attaining these record efficiencies. Specifically, the maximum potential voltage in these previous devices was substantially reduced by the kinetic limitations of the charge transfer in the cathode (referred to as the overpotential) and by Joule heating losses due to the solid-electrolyte resistance, electrode resistance, and current collector resistance. Moreover, previous devices experienced a steady loss in performance throughout their lifetime. The drop in performance has been attributed to the electrolyte undergoing thermal and chemical breakdown due to crack propagation, loss of sodium oxide, and the formation of molten dendrites that create electrical shorts [5]. Finally, previous designs have also had a substantial problem with proper thermal management, with some showing thermal losses as great as 50% of the heat input. To improve the efficiency, a dual stage conversion process is being explored. Rather than using one isothermal expansion step, the dual cycle will employ two separate electrolytes to allow two separate expansion steps: one at the high temperature, and another at an intermediate temperature. This new cycle is thermodynamically favorable as it allows for regeneration from the isobaric cooling of the first expansion step, and reheat to complete the expansion in the second step. This allows the engine to reach a lower condenser temperature than its single stage counterpart, thus increasing the overall efficiency. The temperature drop across each electrolyte in the dual stage device (e.g., ~ 400 K) is smaller than the temperature drop across a comparable single stage device (e.g., ~ 800 K). This is amenable for better thermal management and allows for less heat loss. This will also mitigate the thermal shock across the very thin (< 1 mm) solid electrolytes, reduce crack propagation and limit the percolation of the molten dendrites, and ultimately increase the lifetime of the device. As an additional benefit the dual stage can be designed using planer geometries, rather than tubular geometries used in previous single stage models, which can be manufactured less expensively. This modified geometry can be tailored to improve the thermal management by reducing the radiation losses, which has been the biggest source of thermal losses [2]. A dual stage concept for the Na-TECC has never been demonstrated in literature. In this presentation, the operation of a single stage device will be revisited and, by adopting concepts used for similar converters, the thermodynamic operation of the dual stage will be developed [6]. Using the dual stage approach, the efficiency and power equations have been redefined to include regeneration and reheat. Questions such as what current densities optimize the power output or which intermediate temperature maximizes the efficiency will also be answered. Initial calculations of the dual stage show that the thermal management is the most sensitive parameter. Although the ideal voltage produced by the dual stage can be higher, there are potential drawbacks. For example, by using a lower condenser temperature the dual stage device will have a higher open circuit voltage, but it will also have a larger overpotential due to the limited cathodic kinetics that occur at a lower temperature. In short, there are several trade-offs in this device that need to be balanced. It will be demonstrated that the dual stage device must have lower thermal losses than a single stage device if it is to have a higher efficiency.

14 SOLAR ENERGY↗

Understanding the Beneficial Role of Transition-Metal Layer Na + Substitution on the Structure and Electrochemical Properties of the P2-Layered Cathode Na 2+ x Ni 2– x /2 TeO 6

Layered Na x MO 2 sodium oxide positive electrode materials have experienced renewed interest owing to the current commercial attention on sodium-ion batteries. Although there are many attractive qualities of these materials, they suffer from serious shortcomings owing to Na + ordering and transition-metal layer gliding that cause a plethora of voltage plateaus during cycling. The P2-layered Na 2+x Ni 2–x/2 TeO 6 (0 ≤ x ≤ 0.5) system provides a framework for investigating the effect of dual Na + substitution into the sodium layer and the transition-metal layer of the structure and its effects on the electrochemical properties of the materials. A careful investigation into the synthesis and properties of these materials reveals that the sodium content used during material preparation has a drastic effect on the composition and electrochemical profile of these materials. The sodium substitution disrupts ordering within the transition-metal layer, thereby disrupting Na + ordering in the adjacent sodium layers. Beyond a critical sodium concentration, the layer stacking shifts, and all voltage plateaus of the P2-Na 2 Ni 2 TeO 6 material are no longer observed at 4.4 V versus Na + /Na. These results also question the common belief that additional sodium precursor is required when preparing layered sodium oxide cathodes, providing new guidelines for material synthesis and characterization.

36 MATERIALS SCIENCE↗

Impact of sodium vanadium oxide (NaV 3 O 8 , NVO) material synthesis conditions on charge storage mechanism in Zn-ion aqueous batteries

The electrochemical charge storage of sodium vanadate (NaV 3 O 8 or NVO) cathodes in aqueous Zn-ion batteries has been hypothesized to be influenced by the inclusion of structural water for facilitating ion transfer in the material. Materials properties considered important (morphology, crystallite and particle size, surface area) are systematically studied herein through investigation of two NVO materials, NaV 3 O 8 ·0.34H 2 O [NVO(300)] and NaV 3 O 8 ·0.05H 2 O [NVO(500)], with different water content, acicular morphologies with different size and surface area achieved via post-synthesis heat treatment. The electrochemistry of the two materials was evaluated in aqueous Zn-ion cells with 2 M ZnSO 4 electrolyte using cyclic voltammetry, galvanostatic cycling, and rate capability testing. Furthermore, the thinner NVO(300) nanobelts (0.13 μm) demonstrate greater specific capacities and higher effective diffusion coefficients relative to the thicker NVO(500) nanorods. Notably however, while cells containing NVO(500) deliver lower specific capacity, they demonstrate enhanced capacity retention with cycling. The structural changes accompanying oxidation and reduction are elucidated via ex situ X-ray diffraction, transmission electron microscopy, and operando V K-edge X-ray absorption spectroscopy (XAS), where NVO material properties are shown to influence the ion insertion. Operando XAS verified that electron transfer corresponds directly to change in vanadium oxidation state, affirming vanadium redox as the governing electrochemical process.

25 ENERGY STORAGE↗

NITRATE DESTRUCTION LITERATURE SURVEY AND EVALUATION CRITERIA

This report satisfies the initial phase of Task WP-2.3.4 Alternative Sodium Recovery Technology, Subtask 1; Develop Near-Tank Nitrate/Nitrite Destruction Technology. Some of the more common anions in carbon steel waste tanks at SRS and Hanford Site are nitrate which is corrosive, and nitrite and hydroxide which are corrosion inhibitors. At present it is necessary to periodically add large quantities of 50 wt% caustic to waste tanks. There are three primary reasons for this addition. First, when the contents of salt tanks are dissolved, sodium hydroxide preferentially dissolves and is removed. During the dissolution process the concentration of free hydroxide in the tank liquid can decrease from 9 M to less than 0.2 M. As a result, roughly half way through the dissolution process large quantities of sodium hydroxide must be added to the tank to comply with requirements for corrosion control. Second, hydroxide is continuously consumed by reaction with carbon dioxide which occurs naturally in purge air used to prevent buildup of hydrogen gas inside the tanks. The hydrogen is generated by radiolysis of water. Third, increasing the concentration of hydroxide increases solubility of some aluminum compounds, which is desirable in processing waste. A process that converts nitrate and nitrite to hydroxide would reduce certain costs. (1) Less caustic would be purchased. (2) Some of the aluminum solid compounds in the waste tanks would become more soluble so less mass of solids would be sent to High Level Vitrification and therefore it would be not be necessary to make as much expensive high level vitrified product. (3) Less mass of sodium would be fed to Saltstone at SRS or Low Level Vitrification at Hanford Site so it would not be necessary to make as much low level product. (4) At SRS less nitrite and nitrate would be sent to Defense Waste Processing Facility (DWPF) so less formic acid would be consumed there and less hydrogen gas would be generated. This task involves literature survey of technologies to perform the nitrate to hydroxide conversion, selection of the most promising technologies, preparation of a flowsheet and design of a system. The most promising technologies are electrochemical reduction of nitrates and chemical reduction with hydrogen or ammonia. The primary reviewed technologies are listed and they aredescribed in more detail later in the report: (1) Electrochemical destruction; (2) Chemical reduction with agents such as ammonia, hydrazine or hydrogen; (3) Hydrothermal reduction process; and (4) Calcination. Only three of the technologies on the list have been demonstrated to generate usable amounts of caustic; electrochemical reduction and chemical reduction with ammonia, hydrazine or hydrogen and hydrothermal reduction. Chemical reduction with an organic reactant such as formic acid generates carbon dioxide which reacts with caustic and is thus counterproductive. Treatment of nitrate with aluminum or other active metals generates a solid product. High temperature calcination has the potential to generate sodium oxide which may be hydrated to sodium hydroxide, but this is unproven. The following criteria were developed to evaluate the most suitable option. The numbers in brackets after the criteria are relative weighting factors to account for importance: (1) Personnel exposure to radiation for installation, routine operation and maintenance; (2) Non-radioactive safety issues; (3) Whether the technology generates caustic and how many moles of caustic are generated per mole of nitrate plus nitrite decomposed; (4) Whether the technology can handle nitrate and nitrite at the concentrations encountered in waste; (5) Maturity of technology; (6) Estimated annual cost of operation (labor, depreciation, materials, utilities); (7) Capital cost; (8) Selectivity to nitrogen as decomposition product (other products are flammable and/or toxic); (9) Impact of introduced species; (10) Selectivity for destruction of nitrate vs. nitrite; and (11) Cost of deactivation and demolition. Each technology was given a score from one to five, five being most desirable, in each criterion. The results for the evaluation, in order from most to least promising was, Electrochemical, Chemical Reduction, Hydrothermal and Calcining. Another report [Steimke and Steeper, 2011] contains a flowsheet and design of an in-tank Electrochemical unit.

08 HYDROGEN↗

Unlocking anionic redox activity in O3-type sodium 3 d layered oxides via Li substitution

Sodium ion batteries, because of their sustainability attributes, could be an attractive alternative to Li-ion technology for specific applications. However, it remains challenging to design high energy density and moisture stable Na-based positive electrodes. Here, we report an O3-type NaLi 1/3 Mn 2/3 O 2 phase showing anionic redox activity, obtained through a ceramic process by carefully adjusting synthesis conditions and stoichiometry. This phase shows a sustained reversible capacity of 190 mAh g -1 that is rooted in cumulative oxygen and manganese redox processes as deduced by combined spectroscopy techniques. Unlike many other anionic redox layered oxides so far reported, O3-NaLi 1/3 Mn 2/3 O 2 electrodes do not show discernible voltage fade on cycling. This finding, rationalized by density functional theory, sheds light on the role of inter- versus intralayer 3d cationic migration in ruling voltage fade in anionic redox electrodes. Another practical asset of this material stems from its moisture stability, hence facilitating its handling and electrode processing. Altogether, this work offers future directions towards designing highly performing sodium electrodes for advanced Na-ion batteries.

25 ENERGY STORAGE↗

The optical constants of several atmospheric aerosol species - Ammonium sulfate, aluminum oxide, and sodium chloride

An investigation is conducted of problems which are related to a use of measured optical constants in the simulation of the optical constants of real atmospheric aerosols. The techniques of measuring optical constants are discussed, taking into account transmission measurements through homogeneous and inhomogeneous materials, the immersion of a material in a liquid of a known refractive index, the consideration of the minimum deviation angle of prism measurement, the interference of multiply reflected light, reflectivity measurements, and aspects of mathematical analysis. Graphs show the real and the imaginary part of the refractive index as a function of wavelength for aluminum oxide, NaCl, and ammonium sulfate. Tables are provided for the dispersion parameters and the optical constants.

Toon, O. B.↗

Anomalous phase separation behavior of gel-derived soda-silica glasses

The effects of retained bound hydroxyl groups on amorphous immiscibility behavior and on the kinetics of phase separation were studied in glasses containing from 10 to 19 percent sodium oxide preparaed by the gel process. Differences in behavior as functions of preliminary thermal treatment of the gel precursor and of melting conditions were studied, employing IR spectroscopy, SAXS and WAXD to monitor the variation in glass microstructure. Both the initial gel treatment and the OH concentration in the prepared glasses were found to affect the immiscibility temperatures, and the magnitude of the maximum temperature increase was also a function of the sodium oxide concentration. It is suggested that the variation in thermodynamic behavior may be caused by the structural arrangement attained by the OH groups during the gel condensation process, which in turn affects the extent of hydrogen bonding to nonbridging oxygen ions.

Neilson, G. F.↗

Stabilizing Reversible Oxygen Redox Chemistry in Layered Oxides for Sodium‐Ion Batteries

Abstract Triggering oxygen‐related activity is demonstrated as a promising strategy to effectively boost energy density of layered cathodes for sodium‐ion batteries. However, irreversible lattice oxygen loss will induce detrimental structure distortion, resulting in voltage decay and cycle degradation. Herein, a layered structure P2‐type Na 0.66 Li 0.22 Ru 0.78 O 2 cathode is designed, delivering reversible oxygen‐related and Ru‐based redox chemistry simultaneously. Benefiting from the combination of strong Ru 4d‐O 2p covalency and stable Li location within the transition metal layer, reversible anionic/cationic redox chemistry is achieved successfully, which is proved by systematic bulk/surface analysis by in/ex situ spectroscopy (operando Raman and hard X‐ray absorption spectroscopy, etc.). Moreover, the robust structure and reversible phase transition evolution revealed by operando X‐ray diffraction further establish a high degree reversible (de)intercalation processes (≈150 mAh g −1 , reversible capacity) and long‐term cycling (average capacity drop of 0.018%, 500 cycles).

Cao, Xin↗

Antiphase boundary migration as a diffusion mechanism in a P3 sodium layered oxide

The electrode materials of Na-ion batteries must exhibit fast ion transport, a property that is often negatively impacted when mobile cations order. Many layered Na (and K) intercalation compounds adopt the P3 crystal structure, which tends to stabilize cation-vacancy orderings over a wide range of Na concentrations. The ordered phases have been predicted to consist of domains that are periodically separated by antiphase boundaries (APBs) to accommodate variations in Na concentration. The mechanisms and rates with which Na diffuses within such ordered phases of P3 are not understood. We have conducted a first-principles study of Na diffusion in the P3 structure, using Na x CoO 2 as a model system. We find that most simple nearest-neighbor hops in Na-vacancy ordered phases in P3 result in unstable configurations and are therefore forbidden. We identify an alternative mechanism of Na transport that is mediated by APB migration via the formation and expansion of kinks along domain boundaries. The limiting kinetic barriers for this mechanism are quite low (0.03 to 0.30 eV). Vacancy defects are not required, and furthermore have formation energies that are higher than those of the APB kink defects. Furthermore, our results suggest that APB migration is a fundamental diffusion mechanism in the P3 structure.

36 MATERIALS SCIENCE↗