Is It Homogeneous or Heterogeneous Catalysis Derived from [RhCp*Cl2]2? In Operando-XAFS, Kinetic and Crucial Kinetic Poisoning Evidence for Subnanometer Rh4 Cluster-Based Benzene Hydrogenation Catalysis

Determining the true, kinetically dominant catalytically active species, in the classic benzene hydrogenation system pioneered by Maitlis and co-workers 34 years ago starting with [RhCp*Cl2]2 (Cp* = [{eta}5-C5(CH3)5]), has proven to be one of the most challenging case studies in the quest to distinguish single-metal-based 'homogeneous' from polymetallic, 'heterogeneous' catalysis. The reason, this study will show, is the previous failure to use the proper combination of (i) operando spectroscopy to determine the dominant form(s) of the precatalyst's mass under catalysis (i.e., operating) conditions, plus then and crucially also (ii) the previous lack of the necessary kinetic studies, catalysis being a 'wholly kinetic phenomenon' as J. Halpern long ago noted. An important contribution from this study will be to reveal the power of quantitiative kinetic poisoning experiments for distinguishing single-metal, or in this case subnanometer Rh4 cluster-based catalysis from larger, polymetallic Rh(0)n nanoparticle catalysis, at least under favorable conditions. The combined operando-XAFS (X-ray absorption fine structure) spectroscopy and kinetic evidences provide a compelling case for Rh4-based, with average stoichiometry 'Rh4Cp*2.4Cl4Hc', benzene hydrogenation catalysis in 2-propanol with added Et3N and at 100 C and 50 atm initial H2 pressure. The results also reveal, however, that if even ca. 1.4% of the total soluble Rh(0)n had formed nanoparticles, then those Rh(0)n nanoparticles would have been able to account for all the observed benzene hydrogenation catalytic rate (using commercial, ca. 2 nm, polyethyleneglycol-dodecylether hydrosol stabilized Rh(0)n nanoparticles as a model system). The results 'especially the poisoning methodology developed and employed' are of significant, broader interest since determining the nature of the true catalyst continues to be a central, often vexing issue in any and all catalytic reactions. The results are also of fundamental interest in that they add to a growing body of evidence indicating that certain, appropriately ligated, coordinatively unsaturated, subnanometer M4 transition-metal clusters can be relatively robust catalysts. Also demonstrated herein is that Rh4 clusters are poisoned by Hg(0), demonstrating for the first time that the classic Hg(0) poisoning test of 'homogeneous' vs 'heterogeneous'catalysts cannot distinguish Rh4-based subnanometer catalysts from Rh(0)n nanoparticle catalysts, at least for the present examples of these two specific, Rh-based catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Insights into palladium poisoning of Cu/SSZ-13 selective catalytic reduction catalysts

Here, the impacts of Pd poisoning to the activity, selectivity, and hydrothermal stability of Cu/SSZ-13 selective catalytic reduction (SCR) catalysts are reported. Pd lowers DeNOx efficiency of Cu/SSZ-13 via two mechanisms: (1) displacing SCR active sites in the form of isolated Pd-ions, and (2) catalyzing non-selective NH 3 oxidation in the form of PdO. The first mechanism works by the diffusion of isolated Pd-ions into chabazite cages to displace ZCu II OH SCR active species, and it occurs on Cu/SSZ-13 catalysts with and without external surface CuO clusters in similar fashion. In contrast, the second mechanism works differently with and without external surface CuO clusters. For Cu/SSZ-13 catalyst without external CuO clusters (i.e., primarily isolated Cu-ions), PdO leads to significant decrease of DeNOx efficiency at reaction temperatures above ~400°C due to its non-selective NH 3 oxidation activity at high temperatures. However, this poisoning effect becomes much less impactful on Cu/SSZ-13 catalyst containing CuO clusters. This is due to the formation of CuO-PdO solid solution via interactions between CuO and PdO, which reduces non-selective NH 3 oxidation potential. Furthermore, this solid solution formation even mitigates adverse effects caused by hydrothermal aging. Hence, the poisoning effects of Pd are closely related to Cu speciation and spatial distribution of a Cu/SSZ-13 catalyst. Finally, this study suggests a strategy in eliminating Pd poisoning, that is, the introduction of an oxide phase that effectively traps PdO but does not adversely influence SCR.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The SUMO protease SENP1 is required for cohesion maintenance and mitotic arrest following spindle poison treatment

Highlights: Black-Right-Pointing-Pointer SENP1 knockout chicken DT40 cells are hypersensitive to spindle poisons. Black-Right-Pointing-Pointer Spindle poison treatment of SENP1{sup -/-} cells leads to increased mitotic slippage. Black-Right-Pointing-Pointer Mitotic slippage in SENP1{sup -/-} cells associates with apoptosis and endoreplication. Black-Right-Pointing-Pointer SENP1 counteracts sister chromatid separation during mitotic arrest. Black-Right-Pointing-Pointer Plk1-mediated cohesion down-regulation is involved in colcemid cytotoxicity. -- Abstract: SUMO conjugation is a reversible posttranslational modification that regulates protein function. SENP1 is one of the six SUMO-specific proteases present in vertebrate cells and its altered expression is observed in several carcinomas. To characterize SENP1 role in genome integrity, we generated Senp1 knockout chicken DT40 cells. SENP1{sup -/-} cells show normal proliferation, but are sensitive to spindle poisons. This hypersensitivity correlates with increased sister chromatid separation, mitotic slippage, and apoptosis. To test whether the cohesion defect had a causal relationship with the observed mitotic events, we restored the cohesive status of sister chromatids by introducing the TOP2{alpha}{sup +/-} mutation, which leads to increased catenation, or by inhibiting Plk1 and Aurora B kinases that promote cohesin release from chromosomes during prolonged mitotic arrest. Although TOP2{alpha} is SUMOylated during mitosis, the TOP2{alpha}{sup +/-} mutation had no obvious effect. By contrast, inhibition of Plk1 or Aurora B rescued the hypersensitivity of SENP1{sup -/-} cells to colcemid. In conclusion, we identify SENP1 as a novel factor required for mitotic arrest and cohesion maintenance during prolonged mitotic arrest induced by spindle poisons.

60 APPLIED LIFE SCIENCES↗

Minimal physical requirements for crystal growth self-poisoning

Self-poisoning is a kinetic trap that can impair or prevent crystal growth in a wide variety of physical settings. In this paper, we use dynamic mean-field theory and computer simulation to argue that poisoning is ubiquitous because its emergence requires only the notion that a molecule can bind in two (or more) ways to a crystal; that those ways are not energetically equivalent; and that the associated binding events occur with sufficiently unequal probability. If these conditions are met then the steady-state growth rate is in general a non-monotonic function of the thermodynamic driving force for crystal growth, which is the characteristic of poisoning. Finally, our results also indicate that relatively small changes of system parameters could be used to induce recovery from poisoning.

36 MATERIALS SCIENCE↗

Cadmium poisoning of oxygen reduction on platinum electrode in potassium hydroxide

Experiment with a rotating disk and ring apparatus showed no poisoning by cadmium in 8.5 M KOH, alone or with Cl(-) or CO3(=). Poisoning does not occur either in 0.1 M KOH supernatant at CdO, but a partially reversible poisoning results from .0001 M CdCl2 and traces of fatty acid are present. Evidence indicates that the catastrophic poisoning affects the four-electron O2 reduction more than it does the one-electron H3O(+) discharge.

Miller, R. O.↗

Understanding Sulfur Poisoning and Regeneration of Nickel Biomass Conditioning Catalysts using X-Ray Absorption Spectroscopy

The production of biofuels can proceed via a biomass gasification to produce syngas, which can then undergo catalytic conditioning and reforming reactions prior to being sent to a fuel synthesis reactor. Catalysts used for biomass conditioning are plagued by short lifetimes which are a result of, among other things, poisoning. Syngas produced from biomass gasification may contain between 30-300 ppm H2S, depending on the feedstock and gasification conditions, and H2S is a key catalyst poison. In order to overcome catalyst poisoning, either an H2S-tolerant catalyst or an efficient regeneration protocol should be employed. In this study, sulfur K-edge X-ray absorption near edge spectroscopy (XANES) was used to monitor sulfur species on spent catalyst samples and the transformation of these species from sulfides to sulfates during steam and air regeneration on a Ni/Mg/K/Al2O3 catalyst used to condition biomass-derived syngas. Additionally, nickel K-edge EXAFS and XANES are used to examine the state of nickel species on the catalysts. Post-reaction samples showed the presence of sulfides on the H2S-poisoned nickel catalyst and although some gaseous sulfur species were observed to leave the catalyst bed during regeneration, sulfur remained on the catalyst and a transformation from sulfides to sulfates was observed. The subsequent H2 reduction led to a partial reduction of sulfates back to sulfides. A proposed reaction sequence is presented and recommended regeneration strategies are discussed.

09 BIOMASS FUELS↗

Carbon Monoxide Poisoning Resistance and Structural Stability of Single Atom Alloys

Platinum group metals (PGMs) serve as highly active catalysts in a variety of heterogeneous chemical processes. Unfortunately, their high activity is accompanied by a high affinity for CO and thus, PGMs are susceptible to poisoning. Alloying PGMs with metals exhibiting lower affinity to CO could be an effective strategy toward preventing such poisoning. In this work, we use density functional theory to demonstrate this strategy, focusing on highly dilute alloys of PGMs (Pd, Pt, Rh, Ir and Ni) with poison resistant coinage metal hosts (Cu, Ag, Au), such that individual PGM atoms are dispersed at the atomic limit forming single atom alloys (SAAs). We show that compared to the pure metals, CO exhibits lower binding strength on the majority of SAAs studied, and we use kinetic Monte Carlo simulation to obtain relevant temperature programed desorption spectra, which are found to be in good agreement with experiments. Additionally, we consider the effects of CO adsorption on the structure of SAAs. We calculate segregation energies which are indicative of the stability of dopant atoms in the bulk compared to the surface layer, as well as aggregation energies to determine the stability of isolated surface dopant atoms compared to dimer and trimer configurations. Our calculations reveal that CO adsorption induces dopant atom segregation into the surface layer for all SAAs considered here, whereas aggregation and island formation may be promoted or inhibited depending on alloy constitution and CO coverage. Furthermore, this observation suggests the possibility of controlling ensemble effects in novel catalyst architectures through CO-induced aggregation and kinetic trapping.

36 MATERIALS SCIENCE↗

Sulfur poisoning of CeO[subscript 2]-Al[subscript 2]O[subscript 3]-supported mono- and bi-metallic Ni and Rh catalysts in steam reforming of liquid hydrocarbons at low and high temperatures

In order to develop a better understanding on sulfur poisoning of reforming catalysts in fuel processing for hydrogen production, steam reforming of liquid hydrocarbons was performed over CeO{sub 2}-Al{sub 2}O{sub 3} supported monometallic Ni and Rh and bimetallic Rh-Ni catalysts at 550 and 800 C. XANES was used to identify the sulfur species in the used catalysts and to study their impacts on the metal surface properties probed by XPS. It was found that both monometallic catalysts rapidly deactivated at 550 C, and showed poor sulfur tolerance. Although ineffective for the Ni catalyst, increasing the temperature to 800 C dramatically improved the sulfur tolerance of the Rh catalyst. XANES revealed that metal sulfide and organic sulfide are the dominant sulfur species on the used Ni catalyst, while sulfonate and sulfate predominate on the used Rh catalyst. The presence of sulfur induced severe carbon deposition on the Ni catalyst at 800 C. The superior sulfur tolerance of the Rh catalyst at 800 C may be associated with its capability in sulfur oxidation. It is likely that the formation of the oxygen-shielded sulfur structure of sulfonate and sulfate can suppress the poisoning impact of sulfur on Rh by inhibiting direct rhodium-sulfur interaction. Moreover, XPS indicated that the metal surface properties of the Rh catalysts after the reaction without and with sulfur at 800 C are similar, suggesting that sulfur poisoning on Rh was mitigated under the high-temperature condition. Although the Rh-Ni catalyst exhibited better sulfur tolerance than the monometallic catalysts at 550 C, its catalytic performance was inferior compared with the Rh catalyst in the sulfur-containing reaction at 800 C probably due to the severe carbon deposition on the bimetallic catalyst.

08 HYDROGEN↗

The polonium-210 poisoning of Mr Alexander Litvinenko

Mr Litvinenko died on 23rd November 2006 after having been poisoned with polonium-210 on 1st November. Measurements of the polonium-210 content of post-mortem tissue samples and samples of urine and blood showed the presence of large amounts of 210 Po. Furthermore, autoradiography of hair samples showed two regions of 210Po activity, providing evidence of an earlier poisoning attempt during October 2006, resulting in absorption to blood of about one-hundredth of that estimated for 1st November. Intake by ingestion on 1st November was estimated to be around 4 GBq, assuming 10% absorption to blood, and the resulting organ doses reached estimated values that were generally in a range from about 20 Gy to over 100 Gy. In comparison with estimates of protracted alpha particle the doses required to cause irreversible organ damage support the conclusion that death was the inevitable consequence of multiple organ failure, with destruction of the haemopoietic bone marrow, as well as damage to kidneys and liver, being important contributors. If the earlier poisoning during October 2006 had not been followed by a second major intake on 1st November, it is possible that the earlier intake of around 40 MBq, with absorption of 4 MBq to blood, might have proved fatal over a prolonged period of months or years, primarily as a result of kidney damage following a dose of approaching 3 Gy.

61 RADIATION PROTECTION AND DOSIMETRY↗

Sulfur poisoning mechanism of LSCF cathode material in the presence of SO 2 : a computational and experimental study

Aiming at the comprehensive understanding of the single sulfur poisoning effect and, eventually, the multiple impurities poisoning phenomena on the SOFC (Solid Oxide Fuel Cell) cathode materials, the sulfur poisoning effect on the (La 0.6 Sr 0.4 ) 0.95 Co 0.2 Fe 0.8 O 3 (LSCF-6428) has been investigated in the presence of 10 ppm SO 2 at 800, 900, and 1000°C, respectively, with a combined computational and experimental approach. The good agreement between the CALPHAD (Computer Coupling of Phase Diagrams and Thermochemistry) simulations and the XRD (X-Ray Diffraction), SEM (Scanning Electron Microscopy), and TEM (Transmission Electron Microscopy) characterization results support the reliability of the CALPHAD approach in the SOFC field. Furthermore, comprehensive simulations were made to understand the impact of temperature, P(SO 2 ), P(O 2 ), and Sr concentration on the threshold of SrSO 4 stability. Results showed that the formation of SrSO4 is thermodynamically favored at lower temperatures, higher P(SO 2 ), higher P(O 2 ), and higher Sr concentration. Finally, comparisons were also made between LSCF-6428 and LSM20 (La 0.8 Sr 0.2 MnO 3 ) using simulations, which confirmed that LSCF-6428 is a poor sulfur-tolerant cathode, in agreement with the literature.

36 MATERIALS SCIENCE↗

Self-Cleaning Cathodes for Endurance to Chromium Poisoning

Chromium (Cr) poisoning remains a significant issue in long-term solid oxide fuel cell (SOFC) operation. While the addition of Cr in the interconnect and balance-of-plant (BOP) materials is effective in improving their resistance to oxidation, it also causes the deposition of resistive phases in the air electrode and thus cell performance loss. Previous work has investigated the mitigation of chromium deposition using getters, Cr diffusion resistant coatings, and more chromium-tolerant air electrode materials. However, these mitigation strategies merely postpone the degradation of performance due to Cr poisoning. Additionally, some strategies require the replacement of components, e.g., use of getters. Here we investigated a new, in-situ Cr poisoning mitigation strategy.

30 DIRECT ENERGY CONVERSION↗

Multi-Constituent Airborne Contaminants Capture with Low Cost Oxide Getters and Mitigation of Cathode Poisoning in Solid Oxide Fuel Cell

The technical effort and scientific findings, discussed in this report, documents operational barriers and associated long term performance stability challenges posed by the presence of trace airborne multi-constituent contaminants present in high-temperature electrochemical systems, including Solid Oxide Fuel Cells (SOFCs), Solid Oxide Electrolysis Cells (SOECs), Ion Transport Membranes, and Gas Separation systems. Above systems, offering promises for cleanliness and energy efficiency, face challenges with electrode poisoning stemming from the presence of trace contaminants including gaseous Cr/B/Si vapors in the presence of intrinsic contaminants SO 2 /CO 2 /H 2 O gases. The study indicates that the long-term electrical performance degradation in SOFC systems can be traced to electrochemical, structural, and mechanical changes across cell, stack, and balance of plant components resulting from interactions with trace contaminants leading to increase in both ohmic and non-ohmic polarizations. The degradation primarily results from solid-state and gas-phase materials migration, electrode poisoning, and interactions at the cell and stack levels. Cathode degradation emerges as a significant factor impacting overall SOFC performance, especially related to the presence of intrinsic and extrinsic airborne impurities such as SOx, CrOx(OH)y, SOx, Si(OH)x, and HBOx. Although at trace levels, prolong systems operation at higher airflow (3-10X stoichiometric) allow the accumulation of contaminants within the cell components leading to electrical performance degradation through poisoning and electrode deactivation.

20 FOSSIL-FUELED POWER PLANTS↗

THE CALCULATION OF BURNABLE POISON CORRECTION FACTORS FOR PWR FRESH FUEL ACTIVE COLLAR MEASUREMENTS

Verification of commercial low enriched uranium light water reactor fuel takes place at the fuel fabrication facility as part of the overall international nuclear safeguards solution to the civilian use of nuclear technology. The fissile mass per unit length is determined nondestructively by active neutron coincidence counting using a neutron collar. A collar comprises four slabs of high density polyethylene that surround the assembly. Three of the slabs contain {sup 3}He filled proportional counters to detect time correlated fission neutrons induced by an AmLi source placed in the fourth slab. Historically, the response of a particular collar design to a particular fuel assembly type has been established by careful cross-calibration to experimental absolute calibrations. Traceability exists to sources and materials held at Los Alamos National Laboratory for over 35 years. This simple yet powerful approach has ensured consistency of application. Since the 1980's there has been a steady improvement in fuel performance. The trend has been to higher burn up. This requires the use of both higher initial enrichment and greater concentrations of burnable poisons. The original analytical relationships to correct for varying fuel composition are consequently being challenged because the experimental basis for them made use of fuels of lower enrichment and lower poison content than is in use today and is envisioned for use in the near term. Thus a reassessment of the correction factors is needed. Experimental reassessment is expensive and time consuming given the great variation between fuel assemblies in circulation. Fortunately current modeling methods enable relative response functions to be calculated with high accuracy. Hence modeling provides a more convenient and cost effective means to derive correction factors which are fit for purpose with confidence. In this work we use the Monte Carlo code MCNPX with neutron coincidence tallies to calculate the influence of Gd{sub 2}O{sub 3} burnable poison on the measurement of fresh pressurized water reactor fuel. To empirically determine the response function over the range of historical and future use we have considered enrichments up to 5 wt% {sup 235}U/{sup tot}U and Gd weight fractions of up to 10 % Gd/UO{sub 2}. Parameterized correction factors are presented.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A comparison of opioid‐involved fatalities captured in the National Poison Data System to data derived from US death certificate literal text

Abstract Purpose The purpose of the study is to describe and compare the number and characteristics of opioid‐involved fatal cases captured in the National Poison Data System (NPDS) and in US death certificates. Methods NPDS, which collects data on all calls to US poison control centers, and Drug‐Involved Mortality (DIM), which combines information from literal text of US death certificates and National Vital Statistics Systems, were queried for opioid‐involved fatal cases from 2010 to 2015. Characteristics of the two case series were compared. Results DIM contained 154 016 opioid‐involved overdose deaths, and NPDS contained 2524 fatal opioid exposures, a ratio of 61:1. The number of opioid deaths remained stable in NPDS but increased in DIM over the 6‐year period. On average, deaths involving opioids with higher mean dosage strength (in morphine milligram equivalents) per unit among dispensed prescriptions were more likely to be captured in DIM relative to NPDS, as compared with those with a lower mean dosage strength per unit. The increase in fentanyl‐related deaths seen in DIM since 2013 was not observed in NPDS. Conclusions NPDS is a valuable drug safety surveillance resource due to its timeliness and drug specificity. However, it captures only a small fraction of opioid‐involved fatal poisonings, and comparisons with data derived from death certificate literal text indicate that caution is warranted in making inferences about opioid‐involved fatality trends over time or comparisons across opioids.

Mallama, Celeste A.↗

Poisoning and competitive adsorption effects during phenol hydrogenation on platinum in water-alcohol mixtures

Here the effect of other bio-oil components on the aqueous phase hydrogenation of phenol on a Pt/C catalyst was investigated at a temperature of 353 K and a total pressure of 250 psi. Cyclohexanone and cyclohexanol were primary products; cyclohexanone was further converted to cylcohexanol. Methanol or ethanol as additives in water could completely stop ring hydrogenation in phenol (and in other test compounds: benzene, toluene) and decelerated the hydrogenation of cyclohexanone. Formic acid also suppressed hydrogenation reactions. The poisoning effect resulted from CO, formed by decomposition of alcohols or formic acid on platinum. Ab initio density-functional theory calculations afforded adsorption geometries, binding energies and diffusion barriers of relevant species. Phenol hydrogenation on platinum is more susceptible to CO poisoning than cyclohexanone hydrogenation because it needs a large ensemble site. The poisoning effect of alcohols can be avoided by mixing the components in a specific order.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Alkaloids are associated with increased microbial diversity and metabolic function in poison frogs

Shifts in host-associated microbiomes can impact both host and microbes. It is of interest to understand how perturbations, like the introduction of exogenous chemicals, impact microbiomes. In poison frogs (family Dendrobatidae), the skin microbiome is exposed to alkaloids that the frogs sequester for defense. These alkaloids are antimicrobial; however, their effect on the frogs’ skin microbiome is unknown. To test this, we characterized microbial communities from field-collected dendrobatid frogs. Then, we conducted a laboratory experiment to monitor the effect of the alkaloid decahydroquinoline (DHQ) on the microbiome of two frog species with contrasting alkaloid loads in nature. In both datasets, we found that alkaloid-exposed microbiomes were more phylogenetically diverse, with an increase in diversity among rare taxa. Further, to better understand the isolate-specific response to alkaloids, we cultured microbial isolates from poison frog skin and found that many isolates exhibited enhanced growth or were not impacted by the addition of DHQ. To further explore the microbial response to alkaloids, we sequenced the metagenomes from high- and low-alkaloid frogs and observed a greater diversity of genes associated with nitrogen and carbon metabolism in high-alkaloid frogs. From these data, we hypothesized that some strains may metabolize the alkaloids. We used stable isotope tracing coupled to nanoSIMS (nanoscale secondary ion mass spectrometry), which supported the idea that some of these isolates are able to metabolize DHQ. Together, these data suggest that poison frog alkaloids open new niches for skin-associated microbes with specific adaptations, such as alkaloid metabolism, that enable survival in this environment.

59 BASIC BIOLOGICAL SCIENCES↗

Electrical, thermal, and H 2 O and CO 2 poisoning behaviors of PrNi 0.5 Co 0.5 O 3-δ electrode for intermediate temperature protonic ceramic electrochemical cells

PrNi 0.5 Co 0.5 O 3-δ (PNC) exhibits adequate total electrical conductivity (~300 S/cm at 400–600 °C) and moisture has no significant effect on it. The thermal expansion coefficient of PNC is 17.6 × 10 –6 /K by dilatometry and 18.43 × 10 –6 /K by in situ XRD. PNC also demonstrates chemical stability against H 2 O and CO 2 . However, PNC symmetrical cell over proton-conducting BaZr 0.4 Ce 0.4 Y 0.1 Yb 0.1 O 3-δ (BZCYYb4411) electrolyte shows significant H 2 O and CO 2 poisoning when those are introduced into O 2 –N 2 mixture. In comparison, symmetrical cells with PNC electrode over the oxygen ion conducting Ce 0.9 Gd 0.1 O 2-δ (GDC) electrolyte show no H 2 O and CO 2 poisoning under similar conditions. Here, it is hypothesized that poisoning from H 2 O and CO 2 of the PNC proton conducting symmetrical cell is caused by their adsorption on the BZCYYb4411 electrolyte instead of PNC electrode. Such a hypothesis is supported by the H 2 O and CO 2 adsorption behaviors on PNC and BZCYYb4411 powder surfaces, as measured by temperature programmed desorption (TPD).

08 HYDROGEN↗

Interface engineering for a rational design of poison-free bimetallic CO oxidation catalysts

We use density functional theory calculations of Pt@Cu core@shell nanoparticles (NPs) to design bifunctional poison-free CO oxidation catalysts. By calculating the adsorption chemistry under CO oxidation conditions, we find that the Pt@Cu NPs will be active for CO oxidation with resistance to CO-poisoning. The CO oxidation pathway at the Pt–Cu interface is determined on the Pt NP covered with a full- and partial-shell of Cu. The exposed portion of the Pt core preferentially binds CO and the Cu shell binds O2, supplying oxygen for the reaction. The Pt–Cu interface provides CO-oxidation sites that are not poisoned by either CO or O2. Additional computational screening shows that this separation of reactant binding sites is possible for several other core@shell NPs. Our results indicate that the metal–metal interface within a single NP can be optimized for design of bifunctional catalytic systems with improved performance.

Shin, Kihyun↗