Citrate-based sol-gel synthesis of blue- and green-emitting BaLa{sub 2}WO{sub 7}:Tm{sup 3+} or Er{sup 3+} phosphors and their luminescence properties

Highlights: • The BLWO:Tm{sup 3+} or Er{sup 3+} phosphors were prepared by a citrate-based sol-gel method. • The BLWO:Tm{sup 3+} or Er{sup 3+} phosphors exhibited blue and green emissions under UV or NUV excitations. • The blue- and green-emitting BLWO:Tm{sup 3+} or Er{sup 3+} phosphors exhibited good thermal properties. - Abstract: BaLa{sub 2}WO{sub 7}:Tm{sup 3+} or Er{sup 3+} (BLWO:Tm{sup 3+} or Er{sup 3+}) single doped phosphors were prepared by a citrate-based sol-gel method. The crystalline properties of the prepared blue- and green-emitting phosphor materials were analyzed by X-ray diffraction (XRD) after annealing at 1350 °C. The XRD patterns of the both phosphors revealed monoclinic structure with a space group of P21/b. The morphological properties and elemental mappings of the BLWO:0.02Tm{sup 3+} and BLWO:0.01Er{sup 3+} phosphors were measured by field-emission scanning electron microscope images and energy dispersive X-ray spectrum, respectively. The photoluminescence (PL) spectra of BLWO:Tm{sup 3+} phosphors showed characteristic emission peaks of Tm{sup 3+} ions from the visible blue to near-infrared regions with the dominant emission at 799 nm ({sup 3}H{sub 4} → {sup 3}H{sub 6}) under ultraviolet (UV) and near-UV excitation wavelengths. Similarly, Er{sup 3+} ions activated BLWO phosphors exhibited intense green emissions at 548 nm ({sup 4}S{sub 3/2} → {sup 4}I{sub 15/2}) under the characteristic excitation wavelength of 381 nm. Furthermore, the temperature-dependent PL emission spectra and the luminescence decay curves were measured for the optimized BLWO:0.02Tm{sup 3+} and BLWO:0.01Er{sup 3+} phosphors. The chromaticity coordinates for the optimized blue- and green-emitting phosphors were calculated.

36 MATERIALS SCIENCE↗

Reduction and Analysis of Phosphor Thermography Data With the IHEAT Software Package

Detailed aeroheating information is critical to the successful design of a thermal protection system (TPS) for an aerospace vehicle. This report describes NASA Langley Research Center's (LaRC) two-color relative-intensity phosphor thermography method and the IHEAT software package which is used for the efficient data reduction and analysis of the phosphor image data. Development of theory is provided for a new weighted two-color relative-intensity fluorescence theory for quantitatively determining surface temperatures on hypersonic wind tunnel models; an improved application of the one-dimensional conduction theory for use in determining global heating mappings; and extrapolation of wind tunnel data to flight surface temperatures. The phosphor methodology at LaRC is presented including descriptions of phosphor model fabrication, test facilities and phosphor video acquisition systems. A discussion of the calibration procedures, data reduction and data analysis is given. Estimates of the total uncertainties (with a 95% confidence level) associated with the phosphor technique are shown to be approximately 8 to 10 percent in the Langley's 31-Inch Mach 10 Tunnel and 7 to 10 percent in the 20-Inch Mach 6 Tunnel. A comparison with thin-film measurements using two-inch radius hemispheres shows the phosphor data to be within 7 percent of thin-film measurements and to agree even better with predictions via a LATCH computational fluid dynamics solution (CFD). Good agreement between phosphor data and LAURA CFD computations on the forebody of a vertical takeoff/vertical lander configuration at four angles of attack is also shown. In addition, a comparison is given between Mach 6 phosphor data and laminar and turbulent solutions generated using the LAURA, GASP and LATCH CFD codes. Finally, the extrapolation method developed in this report is applied to the X-34 configuration with good agreement between the phosphor extrapolation and LAURA flight surface temperature predictions. The phosphor process outlined in the paper is believed to provide the aerothermodynamic community with a valuable capability for rapidly obtaining (4 to 5 weeks) detailed heating information needed in TPS design.

Merski, N. Ronald↗

LED lamp incorporating remote phosphor with heat dissipation features

An LED lamp or bulb is disclosed that comprises a light source, a heat sink structure and a remote planar phosphor carrier having at least one conversion material. The phosphor carrier can be remote to the light sources and mounted to the heat sink so that heat from the phosphor carrier spreads into the heat sink. The phosphor carrier can comprise a thermally conductive transparent material and a phosphor layer, with an LED based light source mounted to the heat sink such that light from the light source passes through the phosphor carrier. At least some of the LED light is converted by the phosphor carrier, with some lamp embodiments emitting a white light combination of LED and phosphor light. The phosphor arranged according to the present invention can operate at lower temperature to thereby operate at greater phosphor conversion efficiency and with reduced heat related damage to the phosphor.

36 MATERIALS SCIENCE↗

Synthesis and photoluminescence properties of the high-brightness Eu{sup 3+}-doped M{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) red phosphors

A series of red-emitting phosphors Eu{sup 3+}-doped M{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) have been successfully synthesized at 850 Degree-Sign C by solid state reaction. The excitation spectra of the two phosphors reveal two strong excitation bands at 396 nm and 466 nm, respectively, which match well with the two popular emissions from near-UV and blue light-emitting diode chips. The intensity of the emission from {sup 5}D{sub 0} to {sup 7}F{sub 2} of M{sub 2}(Gd{sub 1-x}Eu{sub x}){sub 4}(MoO{sub 4}){sub 7} phosphors with the optimal compositions of x=0.85 for Li or x=0.70 for Na is about five times higher than that of Y{sub 2}O{sub 3}:Eu{sup 3+}. The quantum efficiencies of the entitled phosphors excited under 396 nm and 466 nm are also investigated and compared with commercial phosphors Sr{sub 2}Si{sub 5}N{sub 8}:Eu{sup 2+} and Y{sub 3}A{sub 5}O{sub 12}:Ce{sup 3+}. The experimental results indicate that the Eu{sup 3+}-doped M{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) phosphors are promising red-emitting phosphors pumped by near-UV and blue light. - Graphical Abstract: The intensity of the red emission of M{sub 2}(Gd{sub 1-x}Eu{sub x}){sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) phosphors with the optimal compositions is about five times higher than that of Y{sub 2}O{sub 3}:Eu{sup 3+}. Highlights: Black-Right-Pointing-Pointer Two novel Eu{sup 3+}-doped red phosphors (Na{sub 2}Gd{sub 4}(MoO{sub 4}){sub 2}, Li{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7}) were synthesized. Black-Right-Pointing-Pointer Their emission intensities are about five times higher than that of Y{sub 2}O{sub 3}:Eu{sup 3+}. Black-Right-Pointing-Pointer Their quantum efficiencies are higher than that of commercial red phosphor Sr{sub 2}Si{sub 5}N{sub 8}:Eu{sup 2+}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Luminescence properties of Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+}, R{sup +} (R{sup +}=Li{sup +}, Na{sup +}, and K{sup +}) red emission phosphor

A series of Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+}, Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, R{sup +}, and Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+}, R{sup +} (R{sup +}=Li{sup +}, Na{sup +}, and K{sup +}) phosphors are synthesized by solid-state reaction method in air. All phosphors show bright red emissions centered at ∼617 nm upon excitation with UV light of 397 nm. Bi{sup 3+} is a sensitizer for the luminescence of Eu{sup 3+}, and can improve significantly the PL intensity of Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+} phosphor due to energy transfer between Bi{sup 3+} and Eu{sup 3+} ions. The sensitization mechanism is investigated and discussed by energy level diagrams of Bi{sup 3+} and Eu{sup 3+} ions. R{sup +} ion is used as the charge compensator to improve the luminescence intensity of Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+} and Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+} phosphors, and their PL intensities are enhanced in the sequence K{sup +}→Na{sup +}→Li{sup +}. These phosphors can be promising red emitting candidate for white LED with a ∼397 nm near UV chip excitation owing to the high brightness. - Graphical abstract: Energy transfer and charge compensation can enhance PL intensity of phosphors obviously. - Highlights: • Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+} phosphor is synthesized. • Energy transfer between Eu{sup 3+} and Bi{sup 3+} ions benefit PL intensity of Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+} phosphor. • Alkaline metal ions can further improve the PL intensity of Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+} phosphor. • Ca{sub 3}Ti{sub 2}O{sub 7}:Eu{sup 3+}, Bi{sup 3+}, R{sup +} phosphor may be promising red emitting candidate for white LED.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

An orange emitting phosphor Lu{sub 2−x}CaMg{sub 2}Si{sub 2.9}Ti{sub 0.1}O{sub 12}:xCe with pure garnet phase for warm white LEDs

A new silicate garnet phosphor, Lu{sub 2−x}CaMg{sub 2}Si{sub 2.9}Ti{sub 0.1}O{sub 12}:xCe was synthesized by a high temperature solid-state reaction under reductive atmosphere. X-ray diffraction (XRD) showed that the powder was pure garnet phase. The emission and excitation spectrum indicated that the Lu{sub 2−x}CaMg{sub 2}Si{sub 2.9}Ti{sub 0.1}O{sub 12}:xCe phosphors could absorb blue light in the spectral range of 400–550 nm efficiently and exhibit bright yellow–orange emission in the range of 520–750 nm. With the increase of Ce{sup 3+} concentration, the emission band of Ce{sup 3+} showed a red shift. Interestingly, the concentration quenching occurred when the Ce{sup 3+} concentration exceeded 4 mol%. The temperature-dependent luminescent properties of the phosphors were discussed and the Lu{sub 1.96}CaMg{sub 2}Si{sub 2.9}Ti{sub 0.1}O{sub 12}:0.04Ce phosphors showed good performances in color temperature (2430 K) and potential applications for warm white LEDs. - Graphical Abstract: This image shows that the phosphor of Lu{sub 1.96}CaMg{sub 2}Si{sub 2.9}Ti{sub 0.1}O{sub 12}:0.04Ce can generate a uniform yellow tint under natural light illumination and emit orange–red light when excited by blue light. With a fixed 467 nm emission light, warm white light can be produced by this phosphor, which indicates that the phosphor is potentially applicable in warm white light emitting diodes based on GaN chips. - Highlights: • A new silicate garnet phosphor was synthesized by solid-state method. • Secondary phases can be avoided when a small amount of Si{sup 4+} were replaced by Ti{sup 4+}. • A broad emission band of Ce{sup 3+} in the phosphors was described. • The phosphors are potentially applicable in warm white light emitting diodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Photoluminescence studies of high-efficient red-emitting K{sub 2}Y(WO{sub 4})(PO{sub 4}):Eu{sup 3+} phosphor for NUV LED

Highlights: • Novel K{sub 2}Y(WO{sub 4})(PO{sub 4}):Eu{sup 3+} red phosphors were prepared by solid-state method. • Phosphors exhibit strong red light under NUV excitation with quantum efficiency of 70.5 %. • Judd–Ofelt analysis ascertains the presence of Eu{sup 3+} in a highly asymmetric environment. • The red LED prototype was fabricated with KYWP:Eu{sup 3+} phosphor and InGaN chip. - Abstract: A series of high-efficient red-emitting phosphors K{sub 2}Y(WO{sub 4})(PO{sub 4}):Eu{sup 3+} have been successfully synthesized by conventional solid-state reaction, and its photoluminescence (PL) properties have been investigated. The phosphors can be excited efficiently by NUV light, then exhibit strong red emission with quantum efficiency of 70.5%. The concentration quenching takes place at relatively high concentration of Eu{sup 3+} (x = 0.70), which is further confirmed by the variation of decay curves of the entitled phosphors. Judd–Ofelt analysis ascertains the presence of Eu{sup 3+} in a highly asymmetric environment. The phosphor exhibits good thermal stability (92.5% at 100 °C and 84.1% at 180 °C). The red LED prototype fabricated by opyimized-composition K{sub 2}Y(WO{sub 4})(PO{sub 4}):0.70Eu{sup 3+} phosphor and 395 nm-emitting InGaN chips exhibit bright red emission. The results indicate that the K{sub 2}Y(WO{sub 4})(PO{sub 4}):Eu{sup 3+} phosphors are promising red phosphors for NUV LED.

36 MATERIALS SCIENCE↗

Synthesis, energy transfer and luminescence properties of Ca{sub 2}MgWO{sub 6}:Sm{sup 3+}, Bi{sup 3+} phosphor

Graphical abstract: PL spectra of Ca{sub 2}MgWO{sub 6}:Sm{sup 3+} and Ca{sub 2}MgWO{sub 6}:Sm{sup 3+}, Bi{sup 3+} phosphors with excitation at 407 nm, and the corresponding CIE chromaticity diagram and chromaticity coordinates. - Highlights: • Novel Ca{sub 2}MgWO{sub 6}:Sm{sup 3+}, Bi{sup 3+} phosphor is synthesized by solid-state reaction method in air. • Emission intensity of Ca{sub 2}MgWO{sub 6}:Sm{sup 3+} phosphor is enhanced ∼2 times after co-doped Bi{sup 3+} ion. • Charge compensation and energy transfer may be explained via luminescence properties. • Luminous mechanism is analyzed by energy level diagrams of WO{sub 6}{sup 6−} group, Sm{sup 3+} and Bi{sup 3+} ions. - Abstract: Novel Ca{sub 2}MgWO{sub 6}:Sm{sup 3+}, Bi{sup 3+} phosphor is synthesized by solid-state reaction method in air. Host Ca{sub 2}MgWO{sub 6} with excitation 300 nm emits blue light. Ca{sub 2}MgWO{sub 6}:Bi{sup 3+} phosphor with excitation 300 and 338 nm emits yellow light. Ca{sub 2}MgWO{sub 6}:Sm{sup 3+} phosphor with excitation 300 nm exhibits tunable emission from blue to red light by increasing Sm{sup 3+} doping concentration from 0 to 8 mol%, however, only emits red light with excitation 407 nm. Ca{sub 2}MgWO{sub 6}:Sm{sup 3+}, Bi{sup 3+} phosphor with excitation 300 and 338 nm emits red light. The optimal Sm{sup 3+} doping concentration is ∼5 mol% in Ca{sub 2}MgWO{sub 6}:Sm{sup 3+} phosphor. After Bi{sup 3+} ion is co-doped, luminescence properties of Ca{sub 2}MgWO{sub 6}:Sm{sup 3+} phosphor can be improved obviously because of Bi{sub 2}O{sub 3} as fluxing agent role and energy transfer from Bi{sup 3+} to Sm{sup 3+} ions. The possible luminous mechanism of Ca{sub 2}MgWO{sub 6}:Sm{sup 3+}, Bi{sup 3+} phosphor is analyzed and explained by simplified energy level diagrams of WO{sub 6}{sup 6−} group, Bi{sup 3+} and Sm{sup 3+} ions.

36 MATERIALS SCIENCE↗

Synthesis and control the morphology of Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+}/Eu{sup 2+},Mn{sup 2+} phosphors by precipitation method

Highlights: • Use facile and mild precipitation method obtained Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+}/Eu{sup 2+},Mn{sup 2+} phosphors. • Through controlling the morphology to tune the photoluminescence properties. • The columnar structure Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+} phosphor shows better emission intensity. • Self-assembled phenomenon appears by changing the Mn{sup 2+} concentration of the Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+},Mn{sup 2+} phosphor. - Abstract: Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+}/Eu{sup 2+},Mn{sup 2+} phosphors have been synthesized by the facile and mild precipitation method and they are characterized by X-ray powder diffraction, scanning electron microscopy, photoluminescence spectra. The SEM results indicate the obtained Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+} phosphors have the columnar structure and the Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+},Mn{sup 2+} phosphors is the sphere like. The effects of the stirring and sintering temperature on the morphology of Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+}/Eu{sup 2+},Mn{sup 2+} phosphors have been investigated. The photoluminescence spectra of Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+} and Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+},Mn{sup 2+} phosphors showed that the Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+} phosphors can be excited by 345 nm and exhibit blue emission around 421 nm and the Sr{sub 2}P{sub 2}O{sub 7}:Eu{sup 2+},Mn{sup 2+} phosphors can be excited by 355 nm and exhibited the emission around 420 nm and 578 nm showing the white light.

36 MATERIALS SCIENCE↗

New red phosphor ceramic K 2 SiF 6 :Mn 4+

We report a new transparent ceramic phosphor for use in LED lighting has been fabricated. The previously reported and optimized narrow-emitting red phosphor, K 2 SiF 6 :Mn 4+ (KSF), has been consolidated into a transparent ceramic phosphor for the first time, accomplished via hot-pressing the feedstock phosphor powder in a die under vacuum. KSF ceramics were fabricated with varying doping concentrations of Mn 4+ and their properties studied. The absorption and emission spectra of the ceramics were identical to the feedstock phosphor powders and are ideal for LED lighting with strong absorption at 450 nm and narrow emission around 630 nm. The absorbance of the ceramics was directly proportional to the doping concentration. The ceramics were excited at various blue light fluxes and their emission intensities measured to study the effect of Mn 4+ concentration on intensity-driven “droop” in the emission output. The ceramics with a lower Mn 4+ doping were more efficient under higher light fluxes due to a decrease in Auger upconversion losses. KSF ceramics can allow a much longer path length of the diode light through the phosphor, as compared to phosphor-in-silicone, enabling the use of low optical absorption and the associated reduced activator concentration. The ceramics are measured to have a thermal conductivity of ~1.0 W/m-K, higher than that of phosphor-in-silicone or phosphor-in-glass. Several of these properties make KSF ceramics potentially desirable for use in white light LEDs. Greater thermal conductivity helps with heat dissipation, the lower surface area of the ceramic compared to the powder minimizes the environmental vulnerability of KSF, and the ability to lower the Mn 4+ concentration reduces Auger recombination losses and mitigates the temperature rise, particularly at higher light flux.

36 MATERIALS SCIENCE↗

High Extraction Phosphors for Solid State Lighting

We have developed high-index, high efficiency bulk luminescent materials and novel nano-sized phosphors for improved solid-state white LED lamps. These advances can potentially contribute to reducing the loss in luminous efficiencies due to scattering, re-absorption, and thermal quenching. The bulk and nanostructured luminescent materials investigated are index matched to GaN and have broad and size-tunable absorption bands, size and impurity tuned emission bands, size-driven elimination of scattering effects, and a separation between absorption and emission bands. These innovations were accomplished through the use of novel synthesis techniques suitable for high volume production for LED lamp applications. The program produced a full-color set of high quantum yield phosphors with high chemical stability. In the bulk phosphor study, the ZnSeS:Cu,Ag phosphor was optimized to achieve >91% efficiency using erbium (Er) and other activators as sensitizers. Detailed analysis of temperature quenching effects on a large number of ZnSeS:Cu,Ag,X and strontium- and calcium-thiogallate phosphors lead to a breakthrough in the understanding of the anti-quenching behavior and a physical bandgap model was developed of this phenomena. In a follow up to this study, optimized phosphor blends for high efficiency and color performance were developed and demonstrated a 2-component phosphor system with good white chromaticity, color temperature, and high color rendering. By extending the protocols of quantum dot synthesis, large nanocrystals, greater than 20 nm in diameter were synthesized and exhibited bulk-like behavior and blue light absorption. The optimization of ZnSe:Mn nanophosphors achieved ~85% QE The limitations of core-shell nanocrystal systems were addressed by investigating alternative deltadoped structures. To address the manufacturability of these systems, a one-pot manufacturing protocol was developed for ZnSe:Mn nanophosphors. To enhance the stability of these material systems, the encapsulation of ZnSeS particle phosphors and ZnSeS screens with Al 2 O 3 and TiO 2 using ALD was shown to improve the stability by >8X and also increased the luminescence efficiency due to improved surface passivation and optical coupling. A large-volume fluidized bed ALD system was designed that can be adapted to a commercial ALD or vapor deposition system. Throughout the program, optical simulations were developed to evaluate and optimize various phosphor mixtures and device configurations. For example, to define the scattering properties of nanophosphors in an LED device or in a stand-off screen geometry. Also this work significantly promoted and assisted in the implementation of realistic phosphor material models into commercial modeling programs.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Thermostability and photostability of Sr{sub 3}SiO{sub 5}:Eu{sup 2+} phosphors for white LED applications

Sr{sub 3}SiO{sub 5}:Eu{sup 2+} phosphors were synthesized by solid-state reactions, and their photoluminescence (PL) stability under the impact of heat or light was studied. The thermal degradation in air was observed for the Sr{sub 3}SiO{sub 5}:Eu{sup 2+} phosphor, furthermore, this drop in emission intensity could be accelerated by simultaneously illuminating the phosphor with a high-power blue LED during the heating process. This enhanced thermal degradation phenomenon in the blue light can be ascribed to the photo-assisted thermal oxidation of Eu{sup 2+} ions. A reversible decrease in emission intensity at room temperature was observed on illuminating the Sr{sub 3}SiO{sub 5}:Eu{sup 2+} phosphor alone by the blue light, which could be related to trapping centers in the phosphor. The existence of traps is also responsible for the anomalous increase of emission intensity with increasing temperature from 30 to 100 °C. Considering the influences of Ba{sup 2+} doping on temperature-dependent PL properties of the Sr{sub 3}SiO{sub 5}:Eu{sup 2+} phosphor, the thermal quenching origin may be ascribed to the thermally assisted photoionization process. - Graphical abstract: The photo-induced reversible decrease in emission intensity and the anomalous emission enhancement with increasing temperature are related to trapping centers in the phosphor. - Highlights: • The photo-assisted thermal degradation was observed for the Sr{sub 3}SiO{sub 5}:Eu{sup 2+} phosphor. • The phosphor showed a reversible intensity decrease under the blue light irradiation. • An anomalous emission enhancement with increasing temperature was found. • Ba{sup 2+} substitution could suppress the thermal quenching of Sr{sub 3}SiO{sub 5}:Eu{sup 2+}. • Mechanisms for photostability and thermostability were discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Near-UV and blue wavelength excitable Mg{sub 0.6}Ca{sub 2.16}Mo{sub 0.2}W{sub 0.8}O{sub 6}: Eu{sub 0.12}{sup 3+}/Na{sub 0.12}{sup +} high efficiency red phosphors

Red phosphors with narrow emission around 615 nm (with FWHM~5–10 nm) having chemical compositions of A{sub 0.6}Ca{sub 2.16}Mo{sub 0.2}W{sub 0.8}O{sub 6}: Eu{sub 0.12}{sup 3+}/Na{sub 0.12}{sup +} (A=Mg, Sr) have been found to exhibit the highest luminescence amongst the molybdate–tungstate family when excited by sources in the 380–420 nm wavelength range. Thus they are most suitable for enhancing color rendering index and lowering color temperature in phosphor converted white LEDs (pc-WLEDs) with near-UV/blue LED excitation sources. The excitation band edge in the near UV/blue wavelength in the reported phosphor has been attributed to the coordination environment of the transition metal ion (Mo{sup 6+}, W{sup 6+}) and host crystal structure. Furthermore the quantum efficiency of the phosphors has been enhanced by adjusting activator concentration, suitable compositional alloying using substitutional alkaline earth metal cations and charge compensation mechanisms. - Graphical abstract: The charge transfer excitation of orthorhombic Mg{sub 0.6}Ca{sub 2.16}Mo{sub 0.2}W{sub 0.8}O{sub 6}: Eu{sub 0.12}{sup 3+}/Na{sub 0.12}{sup +} is significantly higher than tetragonal CaMoO{sub 4}: Eu{sup 3+} phosphors making Mg{sub 0.6}Ca{sub 2.16}Mo{sub 0.2}W{sub 0.8}O{sub 6}: Eu{sub 0.12}{sup 3+}/Na{sub 0.12}{sup +} prime candidates for fabrication of warm white phosphor-converted LEDs. - Highlights: • LED excitable Mg{sub 0.6}Ca{sub 2.16}Mo{sub 0.2}W{sub 0.8}O{sub 6}: Eu{sub 0.12}{sup 3+}/Na{sub 0.12}{sup +} phosphors were synthesized. • These phosphors are 10 times more intense than CaMoO{sub 4}: Eu{sup 3+} red phosphors. • Their intensity and efficiency were enhanced by materials optimization techniques. • Such techniques include compositional alloying, charge compensation, etc.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase transition and multicolor luminescence of Eu{sup 2+}/Mn{sup 2+}-activated Ca{sub 3}(PO{sub 4}){sub 2} phosphors

Graphical abstract: We have synthesized Eu{sup 2+} doped and Eu{sup 2+}/Mn{sup 2+} co-doped Ca{sub 3}(PO{sub 4}){sub 2} phosphors. The emitting color varies from blue to green with increasing of Eu{sup 2+} content for the Eu{sup 2+}-doped phosphor, and the quantum yield of the 0.05Eu{sup 2+}: Ca{sub 2.95}(PO{sub 4}){sub 2} sample reaches 56.7%. Interestingly, Mn{sup 2+} co-doping into Eu{sup 2+}: Ca{sub 3}(PO{sub 4}){sub 2} leads to its phase transition from orthorhombic to rhombohedral, and subsequently generates tunable multi-color luminescence from green to red via Eu{sup 2+} → Mn{sup 2+} energy transfer. - Highlights: • A series of novel Eu{sup 2+}: Ca{sub 3}(PO{sub 4}){sub 2} phosphors were successfully synthesized. • Phase transition of Ca{sub 3}(PO{sub 4}){sub 2} from orthorhombic to rhombohedral occurred when Mn{sup 2+} ions were doped. • The phosphors exhibited tunable multi-color luminescence. • The quantum yield of 0.05Eu{sup 2+}: Ca{sub 2.95}(PO{sub 4}){sub 2} phosphor can reach 56.7%. • The analyses of phosphors were carried out by many measurements. - Abstract: Intense blue-green-emitting Eu{sup 2+}: Ca{sub 3}(PO{sub 4}){sub 2} and tunable multicolor-emitting Eu{sup 2+}/Mn{sup 2+}: Ca{sub 3}(PO{sub 4}){sub 2} phosphors are prepared via a solid-state reaction route. Eu{sup 2+}-doped orthorhombic Ca{sub 3}(PO{sub 4}){sub 2} phosphor exhibits a broad emission band in the wavelength range of 400–700 nm with a maximum quantum yield of 56.7%, and the emission peak red-shifts gradually from 479 to 520 nm with increase of Eu{sup 2+} doping content. Broad excitation spectrum (250–420 nm) of Eu{sup 2+}: Ca{sub 3}(PO{sub 4}){sub 2} matches well with the near-ultraviolet LED chip, indicating its potential applications as tri-color phosphors in white LEDs. Interestingly, Mn{sup 2+} co-doping into Eu{sup 2+}: Ca{sub 3}(PO{sub 4}){sub 2} leads to its phase transition from orthorhombic to rhombohedral, and subsequently generates tunable multi-color luminescence from green to red via Eu{sup 2+} → Mn{sup 2+} energy transfer, under 365 nm UV lamp excitation.

36 MATERIALS SCIENCE↗

Quadratic general rotary unitized design for doping concentrations and up-conversion luminescence properties of Er{sup 3+}/Yb{sup 3+} co-doped NaLa(MoO{sub 4}){sub 2} phosphors

Highlights: • NaLa(MoO4)2: Er3+/Yb3+ phosphor is synthesized by solid state method. • QGRUD is first applied to the codoping concentration option. • Optimized phosphor presents more stable UC emissions than the commercial phosphor. - Abstract: It is still a great challenge that designing proper codoping concentrations of rare earth ions for achieving intensest expected emission from the studied phosphor. In this work, the quadratic general rotary unitized design (QGRUD) was introduced into the codoping concentration option of NaLa(MoO{sub 4}){sub 2}: Er{sup 3+}/Yb{sup 3+} phosphor for upconversion (UC) applications, and the optimum doping concentrations of Er{sup 3+} and Yb{sup 3+} for achieving maximum UC luminescence intensity, which is close to commercial NaYF{sub 4}:Er{sup 3+}/Yb{sup 3+} phosphor, were obtained. The two-photon process was assigned to the green UC emissions in the optimized NaLa(MoO{sub 4}){sub 2}: Er{sup 3+}/Yb{sup 3+} phosphor. It was also demonstrated that the optimized phosphor presented more stable upconversion emissions than the commercial NaYF{sub 4}:Er{sup 3+}/Yb{sup 3+} phosphor.

36 MATERIALS SCIENCE↗

Dual preparation of hydrophobic and hydrophilic BaWO{sub 4}:Eu phosphors

Highlights: • Red-emitting BaWO{sub 4}:Eu phosphors were prepared in hexane-water bilayer system. • The hydrophobic nanometer-sized BaWO{sub 4}:Eu phosphors were obtained in hexane. • The hydrophilic micrometer-sized BaWO{sub 4}:Eu dendrites were obtained in water. - Abstract: BaWO{sub 4}:Eu phosphors were prepared by performing a solvothermal reaction in a water–hexane bilayer system. A barium oleate (and europium oleate) complex was obtained in hexane via a phase transfer reaction involving Ba{sup 2+} (and Eu{sup 3+}) ions in an aqueous solution of sodium oleate. The outer surfaces of the nanometer-sized BaWO{sub 4}:Eu phosphors were capped by the long alkyl chain of oleate; therefore, the hydrophobic nanometer-sized BaWO{sub 4}:Eu phosphors preferentially dissolved in the hexane layer. The micrometer-sized BaWO{sub 4}:Eu phosphors were obtained in the water layer. The BaWO{sub 4}:Eu phosphors prepared in hexane and water yielded sharp strong absorption and emission peaks at 464 and 615 nm, respectively, due to the {sup 7}F{sub 0} → {sup 5}D{sub 2} and the {sup 5}D{sub 0} →{sup 7} F{sub 2} transitions of the Eu{sup 3+} ions. The BaWO{sub 4}:Eu phosphors are good candidate red-emitting phosphors for use in InGaN blue-emitting diodes, which have an emission wavelength of 465 nm.

36 MATERIALS SCIENCE↗

A single-phase Ba{sub 9}Lu{sub 2}Si{sub 6}O{sub 24}:Eu{sup 2+}, Ce{sup 3+}, Mn{sup 2+} phosphor with tunable full-color emission for NUV-based white LED applications

Highlights: • A single phase Ba{sub 9}Lu{sub 2}Si{sub 6}O{sub 24}:Eu{sup 2+}, Ce{sup 3+}, Mn{sup 2+} phosphor with full-color emission was obtained by solid-state reactions. • Eu{sup 2+}, Ce{sup 3+}, and Mn{sup 2+} acts as blue, green, and red luminescence centers, respectively. • The BLS:Eu{sup 2+}, Ce{sup 3+}, Mn{sup 2+} phosphor shows a high quantum efficient of ∼62% and a good color stability. • Combining this single phosphor with a 395 nm NUV-chip, an ideal white LED with a high CRI of 85 and a CCT of 6300 K was obtained. - Abstract: We obtained a single phase BLS:Eu{sup 2+}, Ce{sup 3+}, Mn{sup 2+} phosphor by solid-state reactions. Eu{sup 2+}, Ce{sup 3+}, and Mn{sup 2+} gives rise to the blue, green, and red emission, respectively. The Mn{sup 2+} red emission can be effectively enhanced via energy transfers from both Eu{sup 2+} and Ce{sup 3+}. Thus a tunable full color emission from 410 to 750 nm was realized in this single phosphor. The Eu{sup 2+} → Mn{sup 2+} energy transfer mechanism was investigated by the fluorescence decay curves. This single phosphor exhibits an efficient excitation band covering from 390 to 410 nm, which matches well with the emission light of the efficient NUV chips. The optimized BLS:Eu{sup 2+}, Ce{sup 3+}, Mn{sup 2+} phosphor shows a high quantum efficient of ∼62% and a good color stability. When this single phosphor was combined with a 395 nm NUV-chip, an ideal white LED with a high color render index (CRI) of 85 and a correlated color temperature (CCT) of 6300 K was obtained. This demonstrates the promising application of the BLS:Eu{sup 2+}, Ce{sup 3+}, Mn{sup 2+} single phosphor for the NUV-based white LEDs.

36 MATERIALS SCIENCE↗

A simple way to prepare a hydrophobic Sr[LiAl3N4]:Eu2+ phosphor with improved moisture resistance

Highlights: • A simple modification method to transform SrLiAl{sub 3}N{sub 4}:Eu{sup 2+} into hydrophobic phosphor. • A thin organosilica layer (about 5–10 nm) was coated on the surface of SLA phosphor. • The modified phosphor features superior stability under extremely environment. - Abstract: The red-emitting Sr[LiAl{sub 3}N{sub 4}]:Eu{sup 2+} (SLA) phosphor was synthesized under flowing N{sub 2} gas. A thin organosilica layer (about 5–10 nm) was coated on the surface of SLA phosphors by a very simple method, which transformed the phosphor surface from hydrophilicity to hydrophobicity. The contact angle of water droplets on the surface of the packed SLA phosphors was more than 140°. Compared with the unmodified sample, the modified SLA phosphors could keep at a high emission intensity for more than twice the time under an extremely high moisture level (at relative humidity of 100%, 85 °C). The hydrophobic modification could also improve the uniform dispersion of phosphors during assembly process of white LED.

36 MATERIALS SCIENCE↗