51 records · Page 3

Cost Competitive Process of Battery Grade Oxides Preparation from Aged LIBS

The increasing demand for lithium-ion batteries (LIBs) is driving development of advanced recycling and refining methods. In this project, new cathode active materials are prepared from recycled lithium battery materials and subsequently electrochemically evaluated in coin cells. In detail, scrap LIBs were mechanically processed into a metal rich black mass, then reductive acid leached into an aqueous metal solution, and finally high-purity metal hydroxide precursor materials were prepared by selective electrochemical flow precipitation. Closed-loop LIB recycling into active electrode materials will enable US manufacturers to break their reliance on foreign sources of critical materials. For example, electroextraction process used here has potential to significantly reduce chemical & water use as compared to traditional metallurgic techniques. To this end, electroextracted materials refined from used batteries were collected and processed to be tested as precursor cathode active material (pCam). During this project , samples of high-purity recycled NMC hydroxide (~2 kg each) were received from Nth Cycle. In the first received batch some impurities like cadmium, calcium, and sodium are present in quantities that would negatively impact battery performance. Nth Cycle indicated that the impurities such as cadmium are present due to poor battery separation and co-shredding of NiCd batteries with with LIB. Cadmium was not present in the two subsequent batches as Nth Cycle processed cadmium free black mass. Thus, effective recycled battery sorting is critical to closed-loop LIB recycling into active electrode materials.

25 ENERGY STORAGE

Cost Competitive Process of Battery Grade Oxides Preparation from Aged LIBs

The increasing demand for lithium-ion batteries (LIBs) is driving development of advanced recycling and refining methods. In this project, new cathode active materials are prepared from recycled lithium battery materials and subsequently electrochemically evaluated in coin cells. In detail, scrap LIBs were mechanically processed into a metal rich black mass, then reductive acid leached into an aqueous metal solution, and finally high-purity metal hydroxide precursor materials were prepared by selective electrochemical flow precipitation. Closed-loop LIB recycling into active electrode materials will enable US manufacturers to break their reliance on foreign sources of critical materials. For example, electroextraction process used here has potential to significantly reduce chemical & water use as well as waste production as compared to traditional metallurgic techniques. To this end, electroextracted materials refined from used batteries were collected and processed to be tested as precursor cathode active material (pCAM). For this project, two samples of high purity recycled NMC hydroxide (~1 kg each) were received from N th Cycle’s Ohio demonstration facility. The NMC compositions of the two materials are similar, and the levels of impurities have been confirmed. Indeed, impurities like copper, boron and sodium are present in quantities that could negatively impact battery performance. However, some studies have demonstrated that the control of the quantity of elements like copper or boron may improve the electrochemistry properties of Lithium-NMC batteries. The principal objective is to determine the electrochemical performance of these 2 NMC hydroxide batches and clearly determine the effect of the impurities on the performance.

25 ENERGY STORAGE

Constructing synthetic organosulfur additive for high voltage lithium-ion batteries

Despite its high anodic stability, common organosulfur solvents such as ethyl methyl sulfone and sulfolane typically exhibit poor solid-electrolyte interphase (SEI) formation capability. Here, to address this, the fluorinated organic sulfate 4-(trifluoromethyl)-1,3,2-dioxathiolane 2,2-dioxide (TFDTD) was developed as an effective additive for tailoring organosulfur-based electrolytes in lithium-ion batteries. This development was guided by the functionality selection principle and careful evaluation of feasibility in organic synthesis. TFDTD can be readily synthesized through the reaction between trifluoropropylene glycol and sulfuryl chloride. The ring structure of the organic sulfate enables the formation of a stable SEI on the anode, while the fluorination of the sulfate not only enhances its chemical stability and oxidation potential, but also its effectiveness to protect the anode by increasing its reduction potential, rendering it preferentially reduced on the anode surface before the decomposition of other electrolyte components. Introducing TFDTD facilitates the generation of a robust solidelectrolyte interphase on the graphite anode, significantly enhancing cell performance. Moreover, coupling the use of TFDTD with vinylene carbonate provides further protection on the cathode surface, enabling exceptionally stable, high-voltage, long-term cycling of Gr||NMC full cells.

Functionality selection principle

Modeling Structured Electrodes and Graded Porosity for Improving Discharge Rate Capability in Ultra-Thick Graphite|LiNi 0.6 Mn 0.2 Co 0.2 O 2 Batteries

Long-range electric vehicles (EVs) require high-energy-density batteries that also meet the power demands of high current charge and discharge. Ultra-thick (>100 μm) Lithium-ion battery electrodes are critical to enable this need, but slow ion transport in conventional uniform electrodes (UEs) reduces battery capacity at increasing charge/discharge rates. We present a 3D computational analysis on the impact of structured electrode (SE) and graded electrode (GE) geometries on the discharge rate capability of ultra-thick graphite|LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC-622) battery cells based on the footprint of a commercial EV pouch cell. SE cathodes with either a “grid” or “line” geometry and GEs with two layers of porosity were modeled. Based on the results of 230 models, we found that the electrolyte volume fraction is a key parameter that impacts capacity improvements in UEs, GEs, and SEs at 2 C–6 C discharge rates. SEs have the greatest discharge rate capability, outperforming GEs and UEs due to reduced Lithium-ion concentration gradients across the electrode thickness, which mitigates electrolyte depletion at high rates. The best SE model has a “grid” geometry with gravimetric and volumetric energy density improvements of 0.9%–4% at C/2–2 C and 18%–24% at 4 C–6 C relative to UEs.

25 ENERGY STORAGE

Interfacial Chemistry Involved in Selective Separation of NMC/LMO and LCO/LMO Binary Cathode Materials by Froth Flotation Using Oleic Acid

The variability in cathode compositions within recycled lithium-ion battery (LIB) feedstocks poses a significant challenge to efficient downstream refining processes. This study demonstrates the feasibility of using froth flotation with oleic acid as a collector to selectively separate lithium nickel-manganese-cobalt oxide (NMC) and lithium cobalt oxide (LCO) from lithium manganese oxide (LMO) materials. Laboratory-scale flotation tests achieved an 80% separation efficiency in a single stage, producing a froth product with >90% purity of NMC/LCO at approximately 90% yield. Concurrently, the LMO materials were enriched in the sink product with ∼90% purity and ∼90% yield. This approach was further validated using recycled cathode materials, confirming its applicability to realistic feedstocks. The underlying mechanism governing the selective separation of NMC/LCO from LMO was investigated using ζ-potential measurements, contact angle measurements, bubble-particle attachment experiments, and X-ray photoelectron spectroscopy (XPS) analysis. Both contact angle and bubble-particle attachment results confirmed that oleic acid adsorption rendered NMC and LCO surfaces hydrophobic, thereby enhancing flotation recovery. At pH 5, oleic acid adsorbed preferentially onto NMC and LCO surfaces via electrostatic interactions, while exhibiting minimal adsorption on LMO surfaces. However, separation efficiency deteriorated at higher pH, which was attributed to the co-flotation of LMO materials caused by oleate chemisorption on MnOH + species. This work establishes froth flotation as a viable cathode/cathode separation strategy, providing a low-cost, scalable pathway to preconcentrate and enrich nickel-rich and cobalt-rich cathode active materials from incompatible cathode chemistries for direct recycling or hydrometallurgical processing. Furthermore, this study reveals, for the first time, the mechanism of oleate adsorption on the surface of different cathode materials.

PH

Toward Sustainable Lithium Recovery: A Universal Hydrothermal Approach for Lithium Extraction

The rapid growth of lithium-ion battery (LIB) deployment presents critical challenges in sustainable end-of-life management and raw material recovery. Conventional pyrometallurgical and hydrometallurgical methods suffer from high energy demand, lithium loss, and complex wastewater treatment. This study established a universal, highly efficient, and sustainable hydrothermal route for lithium extraction and material recovery from various spent lithium-ion battery cathodes using 1,2,4,5-benzenetetracarboxylic acid (BTCA). The optimized process achieved over 99% lithium leaching efficiency for lithium iron phosphate (LFP) and LiNi x Mn y Co 1–x–y O 2 (NMC), with transition metal coleaching below 1%. It was also broadly applicable to lithium manganese oxide, lithium cobalt oxide, and black mass, achieving 98.5%, 98.95%, and 94.06% leaching efficiencies, respectively. The extracted lithium was directly converted into battery-grade lithium sources, while transition metals were recovered as oxides. Unreacted BTCA was efficiently regenerated and reused without degradation. Electrochemical evaluation confirmed that cathode materials synthesized with recovered lithium exhibit comparable performance to commercial products. Compared to conventional hydrometallurgy, the BTCA-based process increased revenue by over 40% and reduced greenhouse gas emissions by up to 39%. This closed-loop, chemistry-agnostic strategy offered a scalable and economically viable solution for industrial LIB recycling, enabling resource circularity and reducing dependency on primary critical materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

Ionic liquid-enhanced recycling of lithium-ion battery black mass via heavy liquid centrifugal separation

Direct recycling of lithium-ion batteries (LIBs) is of great significance to supply chain security and environmental protection by restoring spent battery materials to their original purpose without destroying their chemical structure. One of the key processes for direct recycling is to separate valuable anode and cathode active materials from black mass. This study evaluates ionic liquid-enhanced Heavy Liquid Centrifugal Separation (HLCS) as an efficient method for separating LIB black mass into its constituent anode and cathode materials. The optimized HLCS process achieved a separation efficiency of over 95%, yielding a graphite-rich upper layer and an NMC-rich lower layer. Characterization by thermogravimetric analysis (TGA), X-ray diffraction (XRD), and inductively coupled plasma-optical emission spectroscopy (ICP-OES) confirmed the purity and structural integrity of the recovered fractions. The addition of N-methyl-2-pyrrolidone and ionic liquid 1-ethyl-3-methylimidazolium bromide decoupled entangled particles, while subsequent treatment of the anode layer with 1-(2,3-dihydroxypropyl)-3-methylimidazolium chloride further enhanced separation purity. The recycled graphite exhibited comparable battery performance to pristine graphite. These results demonstrate HLCS as a promising LIB recycling strategy, advancing sustainable battery manufacturing.

Adigun, Babafemi [Univ. of Tennessee, Knoxville, T

Recent Developments in Lithium-Manganese-Nickel Oxide Electrochemistry: The Alchemy of LiMn 0.5 Ni 0.5 O 2

Efforts have been underway for some time at Argonne National Laboratory to design structurally integrated and stabilized lithium-manganese-nickel-oxide cathode materials. The goal has been to find a cobalt-free, high-capacity cathode for a Li-ion battery that is competitive, both cost- and energy-wise, with lithium-nickel-manganese-cobalt-oxide (NMC) and lithium-iron-phosphate (LFP) products. This brief synopsis highlights the remarkable alchemy of LiMn 0.5 Ni 0.5 O 2 resulting from its well-known, slightly disordered layered structure and the recently discovered lithiated spinel phase and totally disordered rock-salt configurations. All three arrangements share a structurally compatible cubic-close-packed oxygen array. The lithiated spinel and layered components provide an intersecting network of two- and three-dimensional channels that facilitate Li + -ion transport, while a minor amount of an extensively disordered rock-salt component likely serves to enhance the structural and electrochemical stability of the electrode. The synopsis also encompasses the historical development of lithiated spinel electrode materials and structurally integrated systems.

Thackeray, Michael M. [Argonne National Laboratory

In-Situ FTIR Detection of Transition Metal (TM)-Ion Dissolution From Cathodes in Li-Ion Batteries

Transition metal (TM) ions, commonly Ni and Mn, play a crucial role in Li-ion battery cathodes as the reaction centers for rapid redox reactions. A major challenge with TM-based cathodes is capacity degradation, particularly at higher operating voltages. This degradation is closely linked to the dissolution of TMs from the cathode materials and their subsequent deposition on the anode. This process not only modifies the surface structure of the cathode but, more significantly, alters the SEI composition on the anode [1-2]. The dissolution of TMs cations into a liquid electrolyte from cathode materials, such as Mn-ion dissolution from Mn-rich cathode (LMR), is detrimental to the cycling performance of Li-ion batteries [3-4]. Much attention has been paid to this issue but there remains a lack of characterization techniques which can detect the TM-ion dissolution from the cathode during electrochemical measurements. In our study, we use in-situ ATR-FTIR as an effective technique to probe the TM-ion dissolution from the cathode. We have first demonstrated the detrimental effects of TM ions on the electrochemical performance of Li-ion batteries by adding a small amount of TM salt (50 mM Mn(PF6)) to the electrolyte of a Li-ion coin cell with LFP and graphite electrode. We observed a rapid capacity fade after the first delithiation cycle. To investigate TM ion dissolution, we established a baseline IR spectrum for various TM solvation states (such as Mn and Ni) by measuring concentration-dependent IR spectra. This baseline spectrum helps us detect TM ion dissolution during battery cycling. In this work, we discuss in detail the effect of TM ions on the electrochemical performance of Li-ion batteries and the detection of TM ions during battery cycling using in-situ FTIR spectroscopy. We will compare TM dissolution between coated and uncoated cathodes to examine the effect of cathode coatings to mitigate degradation due to TM dissolution and cross-over from cathode to anode. References: (1) Zhan, C.; Wu, T.; Lu, J.; Amine, K. Dissolution, migration, anddeposition of transition metal ions in Li-ion batteries exemplified byMn-based cathodes - a critical review. Energy Environ. Sci. 2018, 11,243-257. (2) Jung, R.; Linsenmann, F.; Thomas, R.; Wandt, J.; Solchenbach,S.; Maglia, F.; Stinner, C.; Tromp, M.; Gasteiger, H. A. Nickel,Manganese, and Cobalt Dissolution from Ni-Rich NMC and TheirEffects on NMC622-Graphite Cells. J. Electrochem. Soc. 2019, 166,A378-A389. (3) Zhao, L.; Chenard, E.; Capraz, O. O.; Sottos, N. R.; White, S.R. Direct Detection of Manganese Ions in Organic Electrolyte by UV-Vis Spectroscopy. J. Electrochem. Soc. 2018, 165, A345-A348 (4) Zhang, Y.; Hu, A.; Xia, D.; Hwang, S.; Sainio, S.; Nordlund, D.;Michel, F. M.; Moore, R. B.; Li, L.; Lin, F. Operando characterization and regulation of metal dissolution and redeposition dynamics nearbattery electrode surface. Nat. Nanotechnol. 2023, 18, 790.

25 ENERGY STORAGE

A technoeconomic analysis of poly- and single-crystalline NMCxyz from material synthesis to battery pack design

A process model was developed for estimating the cost of manufacturing lithium nickel manganese cobalt oxide (LiNi x Mn y Co z O 2 , NMCxyz), the main cathode active material in lithium-ion batteries used for electric vehicles in the United States. The model was used to estimate the prices of NMC622, NMC811, and NMC955 with poly- and single-crystalline morphologies. The Battery Performance and Cost Model (BatPaC) was used to translate the NMC prices into battery pack prices. A decrease in cobalt content from NMC622 (20% Co) to NMC955 (5% Ni) decreases the material price by $\$$0.85/kg (−3%) due to a decrease in the cost of battery materials, which account for >60% of the total price. NMC622 only produce cheaper packs if the nickel sulfate cost is > 4 × its baseline, indicating higher nickel materials will lower pack cost under normal market conditions. Single-crystalline materials are $\$$2/kg (+8%) more expensive than their polycrystalline counterparts due to higher manufacturing costs from longer, hotter calcinations in less densely packed saggars. This increases the pack price by ∼$\$$3/kWh, assuming identical electrochemical properties. In conclusion, the single-crystalline materials could yield cheaper packs if cycled to higher upper cutoff voltages (i.e., 4.35 to 4.43 V for the single-crystalline material vs. 4.25 V for their polycrystalline counterparts).

Cost modeling

Addressing Inherent Challenges to Chemical Relithiation of Cycled End‐of‐Life Cathode Materials

Recycling end‐of‐life (EOL) lithium‐ion batteries (LIBs) is important to retain valuable resources from critical materials present in EOL battery waste. Direct recycling methods offer an opportunity to recover intact valuable cathode materials with minimal re‐processing. An important step of the direct recycling process is relithiation which is used to restore lithium content to EOL cathode materials. However, little has been done to study how preprocessing steps such as washing or binder removal may affect relithiation methods in the direct recycling process. Here, the evolution of fluorine byproducts left over from preprocessing steps during a low‐temperature chemical redox mediator relithiation process is tracked. A facile washing step is presented as a solution for mediating adverse effects of surface contamination on the chemical relithiation performance. The structure, lithium content, and electrochemical performance of relithiated EOL NMC 622 material that underwent a pre‐relithiation washing step to remove fluorine byproducts is shown to match that of pristine NMC 622. In this work, it is showed that redox mediator relithiation as a part of a direct recycling process is a promising low energy method that can be applied to EOL material with inherent surface impurities if the proper pre‐relithiation processing steps are implemented.

25 ENERGY STORAGE

Strategies for Enhancing Battery Life Under Fast Charging: Insights from NMC-Based Cell Cycling

Fast charging improves the usability of consumer electronics and electric vehicles (EVs) by reducing range anxiety and downtime but accelerates battery degradation and raises safety concerns. Optimizing operational conditions during fast-charging is critical to mitigating aging and ensuring safety. This study evaluated multilayer Gr/NMC811 cells under various conditions, including depths of discharge (DODs of 68%, 84%, and 100%), upper charge cutoff voltages (4.1–4.2 V), and post-charge rest periods (2–30 min), using a 20 min fast charging protocol for up to 500 cycles (up to 150,000 miles of EV use assuming 3.3 mi/kWh vehicle level energy efficiency). Surprisingly, higher DODs under fast charging improved battery life and performance compared to lower DODs. Reducing the upper charge cut-off voltage helped mitigate degradation. A brief 2 min rest period after charging further reduced aging effects. The primary aging modes were loss of lithium inventory and cathode active material. Although minor lithium plating was observed within 500 cycles, it did not affect performance significantly. These findings suggest that, with optimized conditions, cells can sustain hundreds of fast charge cycles—equivalent to over 100,000 miles of EV use—without significant adverse effects on performance or longevity.

25 - ENERGY STORAGE

Electric-vehicle battery second-life and recycling pathways: How economics depend on chemistry, processing, and application

We assess the economics of repurposing and recycling electric vehicle (EV) batteries by estimating the maximum acquisition price repurposers and recyclers could pay for used EV packs across cathode chemistries, first-life conditions, second-life applications, and recycling processes. We develop a novel open-source process-based cost model of a UL-1974-certified repurposing facility and leverage battery degradation models to estimate the maximum acquisition price repurposers could pay for used EV batteries while producing second-life battery energy storage systems with life-adjusted costs equivalent to new systems. We compare these maximum price estimates to maximum prices for recyclers based on cost and revenue estimates from the EverBatt model. We find that repurposing is more economical than recycling for lithium iron phosphate (LFP) batteries, due to their relatively long life and low value materials; recycling is generally more economical than repurposing for lithium nickel cobalt aluminum oxide (NCA) batteries, due to their shorter life and higher value materials; and the economics for lithium nickel manganese cobalt oxide (NMC) batteries depend more heavily on first life retirement conditions and second life application intensity. These results suggest an overall strategy: reuse LFP, recycle NCA, and sort NMC into recycling or repurposing pathways based on state of health and second-life application.

25 ENERGY STORAGE

Maximizing Calendering Effects Through the Mechanical Pulverization of Co-Free Nickel-Rich Cathodes in Lithium-Ion Cells

Calendering is a technique used to maximize the volumetric energy density of battery electrodes. However, higher amounts of calendering result in increased tortuosity and particle cracking. We propose a novel packing structure of electrode particles to maximize calendering benefits while minimizing particle fracture. Cobalt-free layered oxide cathode LiNi0.92Mn0.04Al0.04O2 (NMA) particles are pulverized through ball-milling and coated with lithium phosphate. Pulverized and pristine NMA are fabricated into “bimodal” electrodes, whereas “unimodal” electrodes consist of only pristine NMA. Each electrode type was made into 30% porosity, 40% porosity, and uncalendered coin cell samples. X-ray diffraction suggests that the unimodal samples suffer from more particle fracture than the bimodal samples when calendered to the same porosity of 30%. Electrochemical impedance spectroscopy suggests that the bimodal electrodes exhibit lower surface film resistance. This is supported by enhanced capacity retention for the bimodal samples after 100 cycles.